SU17213A1 - The method of producing mercuric chloride - Google Patents

The method of producing mercuric chloride

Info

Publication number
SU17213A1
SU17213A1 SU13962A SU13962A SU17213A1 SU 17213 A1 SU17213 A1 SU 17213A1 SU 13962 A SU13962 A SU 13962A SU 13962 A SU13962 A SU 13962A SU 17213 A1 SU17213 A1 SU 17213A1
Authority
SU
USSR - Soviet Union
Prior art keywords
mercuric chloride
oxide
producing
mercury
producing mercuric
Prior art date
Application number
SU13962A
Other languages
Russian (ru)
Inventor
Я.П. Беркман
Original Assignee
Я.П. Беркман
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Я.П. Беркман filed Critical Я.П. Беркман
Priority to SU13962A priority Critical patent/SU17213A1/en
Application granted granted Critical
Publication of SU17213A1 publication Critical patent/SU17213A1/en

Description

В патенте № 15278 описан способ получени  сулемы, состо щий в том, что сернокислую окись ртути . замешивают , с сол ной кислотой, после чего прибавл ют поваренную содь и смесь по разведении водой нагревают до кипени ; затем из полученного таким образом раствора к рйс -аллизацией выдел ют хлорную ртуть. С целью исполь-зовани  остающегос  после вышеописанной , обработки маточного раствора, последний по предлагаемому способу обрабатывают окисью ртути дл  очистки еГо от примесей железа и дальнейшей переработки на преципитат.Patent No. 15278 describes a method for producing mercuric chloride, which consists in the production of mercuric acid sulfate. kneaded with hydrochloric acid, after which boiled soda is added and the mixture is heated to boiling after dilution with water; then from the solution obtained in this way, chlorine mercury is separated to the solution by alization. In order to use the remaining after the above, treatment of the mother liquor, the latter, according to the proposed method, is treated with mercury oxide to purify the eGo from iron impurities and further processing to a precipitate.

Способ осуществл етс  следующим образом . Остающиес  от варки, сулемы поThe method is carried out as follows. Remaining from boiling, sublimate by

.патенту № 15278 -маточйые растворы нейтрализуют очищенным и отстоенным едким натром до щелочной реакции, при чем осаждение идет лучше и полнее, если лить маточный раствор в избыточную щелочь, а не наоборот. Образовавшийс  желтый осадок окиси ртути прог ываетс To patent No. 15278, uterine solutions are neutralized with purified and settled caustic soda to an alkaline reaction, and precipitation proceeds better and more completely if pouring the mother liquor into excess alkali and not vice versa. The resulting yellow precipitate of mercury oxide is progressed.

декантацией очищенной от кгшьциевых водой почти до полного удалени  сульфата (слаба  муть от ВаСЬ) и отцеживаетс  от жидкости на кодатурах и.м1 тщательно отстаиваетс  до значительной густоты. Затем производитс  растворение окиси ртути в разведенной сол ной кислоте, при чем достигаетс  прдное удаление железа, не только оставшегос  в окиси, ртути при осаждении ее из ма точных растворов, но даже введенного с сол ной киЬлотой или с водопроводной водой. Далее промытую и отцеженную или отсто вшуюс  окись-ртути перенос т в керамиковую ванну, приливают воды (свободной от кальциевых солей) и технической сол ной кислоты до слабо кислой реакции. Содержимое ванны тщательно перемешивают .веслом По установлении кислой реакции, дают небольшой избыток окиси (до нейтрализации на лакмус реакции ), тщательно р мешивают и провер ют раствор на .содёргкание железа роданистым калием или аммонием., Если отсутствует, дают оСадку осесть и сливают раствор в баллон, где он окон-: чательно отстаиваетс  до полной прозрачности . Раствор, полученный в баллонах , промер етс  iapeoMeTpoM, и по удельному весу устанавливаетс  содержание .сулеиы. . ,.decantation with purified from carbon dioxide water almost to the complete removal of sulphate (weak turbidity from VAS) and strain out the liquid on the codatures of im. 1 carefully settle to a considerable thickness. Then, mercury oxide is dissolved in dilute hydrochloric acid, which results in the removal of iron, not only remaining in oxide, when it is precipitated from wet solutions, but even injected with salt water or tap water. Next, the washed and strained or sedimented oxide-mercury is transferred into a ceramic bath, water (free from calcium salts) and technical hydrochloric acid is added to a weakly acidic reaction. The contents of the bath are thoroughly mixed. After the acid reaction has been established, a small excess of oxide is given (until neutralized by the litmus reaction), the mixture is thoroughly mixed and the solution is checked for iron removal by rhodium or potassium or ammonium. If it is absent, it is sedimented and the solution is drained into balloon, where it is definitively defended to full transparency. The solution obtained in the cylinders is measured by iapeoMeTpoM, and the content of the mixture is determined by specific gravity. . ,

В даЛьнеЗшеи раствор перерабатываетс  на преципитат, как обычйо.In this way, the solution is processed to a precipitate as usual.

Предмет патента. ,The subject of the patent. ,

выполнени  охарактеризованного в патенте Ns 15278 (по за в. свид. № 13963) способа получени  сулемы, отличающийс  тем, что маточВые растворы ртутных солей , с целью их очистки от примесей железа, обрабатывают окисьюрТути. carrying out the method for producing mercuric chloride, characterized in patent Ns 15278 (in accordance with certificate No. 13963), characterized in that the mother liquors of mercury salts are treated with iron oxide to remove them from iron impurities.

SU13962A 1927-02-10 1927-02-10 The method of producing mercuric chloride SU17213A1 (en)