TWI334645B - Semiconductor memory device and method of manufacturing the same - Google Patents
Semiconductor memory device and method of manufacturing the same Download PDFInfo
- Publication number
- TWI334645B TWI334645B TW096114526A TW96114526A TWI334645B TW I334645 B TWI334645 B TW I334645B TW 096114526 A TW096114526 A TW 096114526A TW 96114526 A TW96114526 A TW 96114526A TW I334645 B TWI334645 B TW I334645B
- Authority
- TW
- Taiwan
- Prior art keywords
- layer
- gate electrode
- barrier
- electrode pattern
- high dielectric
- Prior art date
Description
1334645 九、發明說明: 本申請案要求優先權保護,其根據在2006年12月4 曰申請之韓國專利申請案第2006-121512號,其所有內容 皆包含於其中以供參照。 【發明所屬之技術領域】 本發明大致上係關於一種半導體記憶體裝置及特別是 ~種矽氧氮氧矽(SON OS)型半導體記憶體裝置及其製造方 法。 【先前技術】 可根據儲存材料的型及儲存電荷之方法與結構來區分 快閃記憶體(亦即,非揮發記憶體裝置)。SONOS型快閃記 憶體裝置指的是具有矽氧氮氧矽結構的裝置。具有浮動閘 極結構的裝置進行操作,使得電荷被儲存在浮動閘極中。 該SONOS型裝置進行操作,使得電荷被儲存在氮化物層 中。但是,當在閘極圖案化處理期間蝕刻介電層時,在半 導體基板及該氮化物層上可能會產生接合(junction)缺陷。 【發明內容】 本發明揭露半導體記憶體裝置及其製造方法。執行離 子佈植處理及圖案化高介電層,以防止在半導體基板上發 生接合缺陷,其中當在閘極圖案化處理期間蝕刻高介電層 時,該半導體基板可能會遭到破壞。 本發明亦揭露在閘極電極及氮化物層之間形成的阻隔 氧化物層圖案。在進行離子佈植處理之後形成該高介電 層,藉以防止接合形成區域的缺陷。 1334645 根據本發明之一型態,一種半導體記憶體裝置,其包 含半導體基板,其內形成有被摻雜之接合。穿隧絕緣層形 成在該半導體基板上方,電荷儲存層形成在該穿隧絕緣層 上方’阻隔層形成在該電荷儲存層上方。該阻隔層包括阻 隔絕緣層圖案及在該阻隔絕緣層圖案周圍形成的高介電層 圖案’閘極電極圖案形成在該阻隔層上方。
根據本發明之另一型態,提供一種製造半導體記憶體 裝置的方法,該方法包含:在半導體基板上方形成穿隧絕 緣層、電荷儲存層、阻隔絕緣層及閘極電極圖案。執行第 一蝕刻處理來除去該阻隔絕緣層之角隅部分,以在該電荷 儲存層及該閘極電極圖案之間界定出凹部。在該閘極電極 圖案及該基板上形成高介電層,該高介電層塡滿由除去該 阻隔絕緣層之角隅部分所界定之凹部。執行第二蝕刻處 理,以除去該高介電層延伸超過該閘極電極圖案之邊緣以 外的部份》 【實施方式】 將參照附加的圖式來說明本專利之具體實施例。 第1A至1F圖係說明根據本發明之實施例製造半導體 記憶體裝置之方法的截面圖。 參照第1A圖,在包括隔離層(未圖示)之半導體基板 100上連續形成穿險(tunnel)絕緣層102、電荷儲存層104、 阻隔絕緣層1〇6、閘極電極108及硬遮罩層110。可使用氧 化物層來形成該穿隧絕緣層1〇2。可使用氮化物層來形成 該電荷儲存層1〇4。可使用低壓四乙基矽酸鹽(LPTEOS)、 1334645 高溫氧化物 (H TO)、ΡΕ-USG (未摻雜矽玻璃)及氮氧化物 其中之一,來形成爲厚度在大約50到大約1000埃 (angstrom)的該阻隔絕緣層106。使用其內摻雜有雜質的P 型多晶矽、TiN及TaN其中之一來形成該閘極電極108。 參照第1B圖,執行蝕刻處理來形成閘極圖案。透過蝕 刻處理來形成硬遮罩層圖案1 10a、閘極電極圖案108a和阻 隔絕緣層圖案106a。因此,暴露出該電荷儲存層104的一 部份。
參照第1 C圖,透過蝕刻處理來除去該阻隔絕緣層圖案 的角隅,以界定出在該閘極電極圖案108 a和該電荷儲存層 104之間的凹部,藉以形成寬度比該閘極電極圖案108a狹 窄的阻隔絕緣層圖案1 〇6b。可採取使用緩衝氧化物蝕刻劑 (BOE)或HF的濕式蝕刻處理來完成該蝕刻處理。在該蝕刻 處理期間,部分的該阻隔絕緣層l〇6b殘留在該閘極電極圖 案108a下方。該阻隔絕緣層圖案106b之寬度爲該閘極電 極圖案108a之寬度的大約1/20至大約1/2» 參照第1D圖,沿著該硬遮罩層圖案ll〇a來蝕刻部份 的電荷儲存層104,藉以形成電荷儲存層圖案l〇4a。該電 荷儲存層圖案l〇4a之寬度可實質上與該閘極電極圖案 l〇8a之寬度相同。形成該電荷儲存層圖案l(Ma的處理可與 第1B圖所示之形成該閘極電極圖案108a的處理同時執 行。可沿著該閘極圖案來蝕刻或不蝕刻該穿隧絕緣層1 〇2 » 較佳爲該穿隧絕緣層102殘留而用作爲在後續之離子佈植 處理中的屏蔽(screen)氧化物層。執行離子佈植處理,藉以 1334645 在與該閘極圖案相鄰之該半導體基板100中形成接合 (j unction) 1 1 2 〇 在執行該離子佈植處理之後,進行蝕刻該電荷儲存層 的處理。在一個實施例中,在沿著該閘極圖案而蝕刻該電 荷儲存層104之後,執行該離子佈植處理。
參照第1E圖,在該閘極圖案及該半導體基板1〇〇上形 成高介電層114。該高介電層114塡滿在該閘極電極圖案 l〇8a及該電荷儲存層圖案l〇4a之間所界定的空間。該高介 電層114之厚度的範圍係從該阻隔絕緣層圖案1〇 6b之大約 一半的厚度到大約相等的厚度。 用作爲該高介電質的材料包括Al2〇3、Hf02、Zr02、 Ti02或Ta2 05、或者該等之組合物。以具有良好階梯覆蓋 性的原子層沉積(ALD)法來形成該高介電層114,且能塡滿 已除去之該阻隔絕緣層1 0 6的空間。 參照第1F圖,除了在該閘極電極圖案108a和該電荷 儲存層圖案l〇4a之間的該高介電層以外,爲了除去其他的 高介電層而執行蝕刻處理。使用濕式蝕刻法來執行該蝕刻 處理,以除去在該電荷儲存層圖案104 a和該穿隧絕緣層 102彼此接觸之角隅部分所殘留的該高介電層。因此,該 剩餘的高介電層圖案114a圍繞著該阻隔絕緣層圖案 l〇6b,因而形成阻隔層116。當維持定電容量時,該高介 電材料具有優良的漏電流特性。 雖然可以只使用高介電材料來形成該阻隔層116,但 就製程的觀點看來,並不容易獲得所需的外形(profile)。 1334645 爲了形成該閘極圖案而執行乾式蝕刻處理,該高介電層具 有極不易被乾式蝕刻所蝕刻的化學特性。另外,如果透過 該乾式蝕刻法來執行該蝕刻處理,就變得不容易獲得垂直 的閘極外形。這是因爲在該電荷儲存層10 4a和該穿隧絕緣 層102的蝕刻選擇性方面有所差異。因此,該接合112很 有可能遭受破壞,造成該裝置的劣化。
因此,根據本實施例,在透過執行離子佈植處理而在 該半導體基板100中形成該接合112之後,在該阻隔層116 中形成該高介電層圖案114a。因此可防止該破壞接合112 的缺陷。此外,執行該濕式蝕刻處理來形成該高介電層圖 案1 1 4a。所以可輕易地除去位於該閘極之側壁的高介電材 料。 如上所述,根據本實施例,在進行離子佈植處理以後, 執行用以形成阻隔層的圖案化處理。因此可形成接合,其 能防止對半導體基板造成損害並且實現穩定的操作。 雖然已參照具體實施例做出了上述說明,但仍可理解 到熟習本項技術領域者只要不悖離本專利及後述之申請專 利範圍的精神及範圍,即可進行本專利之變化及修改。 【圖式簡單說明】 第1 A至1 F圖係說明根據本發明之實施例製造半導體 記憶體裝置之方法的截面圖。 【主要元件符號說明】 半導體基板 1〇2 穿隧絕緣層 1334645
1 04 電荷儲存層 104a 電荷儲存層圖案 1 06 阻隔絕緣層 106a、 106b 阻隔絕緣層圖案 1 08 閘極電極 108a 閘極電極圖案 110 硬遮罩層 110a 硬遮罩層圖案 112 接合 114 高介電層 114a 高介電層圖案 116 阻隔層 -ίο-
Claims (1)
1334645 . *卜月/日修正替換頁 第096 1 1 45 26號「半導體記憶體裝置及其製造方法」專利案 (2010年10月i日修正) 十、申請專利範圍: 1·—種半導體記憶體裝置,其包含: 半導體基板,其內形成有複數被摻雜之接合; 穿隧絕緣層,形成在該半導體基板上方; 電荷儲存層,形成在該穿隧絕緣層上方; 阻隔層,形成在該電荷儲存層上方,該阻隔層包括阻 隔絕緣層圖案及在該阻隔絕緣層圖案周圍形成的高介電 層圖案;以及 閘極電極圖案,形成在該阻隔層上方;其中,該阻隔 絕緣層圖案之寬度係小於該電荷儲存層之寬度。 2. 如申請專利範圍第1項之半導體記憶體裝置,其中,該 阻隔層之寬度不超過該閘極電極圖案之寬度的約1/2。 3. 如申請專利範圍第1項之半導體記憶體裝置,其中,在 二相鄰的被摻雜之接合之間具備該閘極電極圖案。 4. 一種製造半導體記憶體裝置的方法,該方法包含: 在半導體基板上方形成穿隧絕緣層、電荷儲存層、阻 隔絕緣層及閘極電極圖案; 執行第一蝕刻處理來除去該阻隔絕緣層之角隅部分, 以在該電荷儲存層及該閘極電極圖案之間界定出凹部; 在該閘極電極圖案及該半導體基板上方形成高介電 層,該高介電層塡滿由除去該阻隔絕緣層之角隅部分所 界定之凹部;以及 1334645 _ ♦丨口月ί日修正替換頁 執行第二蝕刻處理’以除去該高介電層延伸超過該閘 極電極圖案之邊緣以外的部份》 5. 如申請專利範圍第4項之方法,其中,使用LPTEOS、 HTO、PE-USG及氮氧化物層其中之一來形成該阻隔絕緣 層。 6. 如申請專利範圍第4項之方法,其中,該阻隔絕緣層係 形成爲厚度在大約50到大約1〇〇〇埃(angstrom) * 7. 如申請專利範圍第4項之方法,其中,該方法更包含: 在於該閘極電極圖案上方形成該高介電層之前,在該半 導體基板上執行離子佈植處理。 8. 如申請專利範圍第7項之方法,其中,更包含: 在該閘極電極圖案上方形成硬遮罩圖案;以及 在執行該離子佈植處理之前,使用該硬遮罩圖案來蝕 刻該電荷儲存層。 9. 如申請專利範圍第7項之方法,其中,更包含: 在執行該離子佈植處理之後,沿著該閘極電極圖案來蝕 刻該電荷儲存層。 10. 如申請專利範圍第4項之方法,其中,使用其內摻雜有 雜質的P型多晶矽、TiN及TaN其中之一來形成該閘極 電極圖案。 11. 如申請專利範圍第4項之方法,其中,使用濕式飩刻處 理來執行該第一蝕刻處理,使用B0E或HF溶液來執行 該濕式鈾刻處理。 12. 如申請專利範圍第4項之方法,其中,更包含在該閘極 -2- 1334645 ______ 伽月f日修正替換頁 « · _____ 電極圖案上方形成硬遮罩圖案,其中使用該硬遮罩圖案 來執行該第二蝕刻處理。 ' 13.如申請專利範圍第4項之方法,其中,在執行該第一蝕 刻處理之後所剩餘的該阻隔絕緣層之寬度不超過該閘極 電極圖案之寬度的大約1/2« 14. 如申請專利範圍第4項之方法,其中,該高介電層之厚 度的範圍係從該阻隔絕緣層之大約一半的厚度到大約相 等的厚度。 15. 如申請專利範圍第4項之方法,其中,使用Al2〇3、H fO 2、 Zr02、Ti02或Ta20 5其中之一或該等之組合物來形成該 高介電材料。 16. 如申請專利範圍第4項之方法,其中,藉由原子層沉積 法來形成該高介電層。 17. 如申請專利範圍第4項之方法,其中,使用濕式蝕刻處 理來執行該第二蝕刻處理。 18. —種製造半導體記億體裝置的方法,該方法包含: 在半導體基板上方形成穿隧絕緣層; 在該穿隧絕緣層上方形成電荷儲存層; 在該電荷儲存層上方形成阻隔絕緣層; 在該阻隔絕緣層上方形成閘極電極圖案; 蝕刻該阻隔絕緣層的一部分,使得在該電荷儲存層及 該閘極電極圖案之間界定出凹部: 在該閘極電極圖案及該半導體基板上形成高介電層, 以塡滿在該電荷儲存層及該閘極電極圖案之間的該凹 -3- 1334645 ..· 月I日2正替疫頁 部;以及 蝕刻該高介電層,使得該高介電層的一部分殘留在該 電荷儲存層及該閘極電極圖案之間的該凹部中。 19.如申請專利範圍第18項之方法,其中,該高介電層塡滿 在該電荷儲存層及該閘極電極圖案之間的該凹部,使該 高介電層環繞該阻隔絕緣層。 20 .如申請專利範圍第1 8項之方法,其中,蝕刻該阻隔絕緣 層之步驟更包含蝕刻該阻隔絕緣層之角隅部。 -4-