ATE38298T1 - Verfahren zur stabilisierung primaerer elektrochemischer generatoren mit aktiven anoden aus zink, aluminium oder magnesium und anode fuer auf diese weise stabilisierten generator. - Google Patents
Verfahren zur stabilisierung primaerer elektrochemischer generatoren mit aktiven anoden aus zink, aluminium oder magnesium und anode fuer auf diese weise stabilisierten generator.Info
- Publication number
- ATE38298T1 ATE38298T1 AT85401352T AT85401352T ATE38298T1 AT E38298 T1 ATE38298 T1 AT E38298T1 AT 85401352 T AT85401352 T AT 85401352T AT 85401352 T AT85401352 T AT 85401352T AT E38298 T1 ATE38298 T1 AT E38298T1
- Authority
- AT
- Austria
- Prior art keywords
- anode
- zinc
- primary electrochemical
- generator
- stabilized
- Prior art date
Links
- FYYHWMGAXLPEAU-UHFFFAOYSA-N Magnesium Chemical compound [Mg] FYYHWMGAXLPEAU-UHFFFAOYSA-N 0.000 title abstract 2
- HCHKCACWOHOZIP-UHFFFAOYSA-N Zinc Chemical compound [Zn] HCHKCACWOHOZIP-UHFFFAOYSA-N 0.000 title abstract 2
- 229910052782 aluminium Inorganic materials 0.000 title abstract 2
- XAGFODPZIPBFFR-UHFFFAOYSA-N aluminium Chemical compound [Al] XAGFODPZIPBFFR-UHFFFAOYSA-N 0.000 title abstract 2
- 239000011777 magnesium Substances 0.000 title abstract 2
- 229910052749 magnesium Inorganic materials 0.000 title abstract 2
- 230000000087 stabilizing effect Effects 0.000 title abstract 2
- 229910052725 zinc Inorganic materials 0.000 title abstract 2
- 239000011701 zinc Substances 0.000 title abstract 2
- 229910052751 metal Inorganic materials 0.000 abstract 2
- 239000002184 metal Substances 0.000 abstract 2
- FAPWRFPIFSIZLT-UHFFFAOYSA-M Sodium chloride Chemical compound [Na+].[Cl-] FAPWRFPIFSIZLT-UHFFFAOYSA-M 0.000 abstract 1
- 239000004411 aluminium Substances 0.000 abstract 1
- 239000003792 electrolyte Substances 0.000 abstract 1
- AQYSYJUIMQTRMV-UHFFFAOYSA-N hypofluorous acid Chemical class FO AQYSYJUIMQTRMV-UHFFFAOYSA-N 0.000 abstract 1
- 150000002894 organic compounds Chemical class 0.000 abstract 1
- 239000011780 sodium chloride Substances 0.000 abstract 1
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/62—Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M6/00—Primary cells; Manufacture thereof
- H01M6/04—Cells with aqueous electrolyte
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Battery Electrode And Active Subsutance (AREA)
- Primary Cells (AREA)
- Agricultural Chemicals And Associated Chemicals (AREA)
- Electrolytic Production Of Metals (AREA)
- Water Treatment By Electricity Or Magnetism (AREA)
- Electrolytic Production Of Non-Metals, Compounds, Apparatuses Therefor (AREA)
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| FR8410632A FR2567328B1 (fr) | 1984-07-04 | 1984-07-04 | Procede de stabilisation des generateurs electrochimiques primaires a anodes reactives en zinc, aluminium ou magnesium et anode pour un tel generateur stabilisee par ce procede |
| EP85401352A EP0171311B1 (de) | 1984-07-04 | 1985-07-03 | Verfahren zur Stabilisierung primärer elektrochemischer Generatoren mit aktiven Anoden aus Zink, Aluminium oder Magnesium und Anode für auf diese Weise stabilisierten Generator |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| ATE38298T1 true ATE38298T1 (de) | 1988-11-15 |
Family
ID=9305802
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| AT85401352T ATE38298T1 (de) | 1984-07-04 | 1985-07-03 | Verfahren zur stabilisierung primaerer elektrochemischer generatoren mit aktiven anoden aus zink, aluminium oder magnesium und anode fuer auf diese weise stabilisierten generator. |
Country Status (10)
| Country | Link |
|---|---|
| US (2) | US4606984A (de) |
| EP (1) | EP0171311B1 (de) |
| JP (1) | JPH07114126B2 (de) |
| AT (1) | ATE38298T1 (de) |
| AU (1) | AU580071B2 (de) |
| CA (1) | CA1256158A (de) |
| DE (1) | DE3565913D1 (de) |
| FR (1) | FR2567328B1 (de) |
| MA (1) | MA20470A1 (de) |
| OA (1) | OA08156A (de) |
Families Citing this family (16)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| FR2627632B1 (fr) * | 1988-02-24 | 1990-08-10 | Cipel | Pile sans mercure a electrolyte salin |
| FR2634595B1 (fr) * | 1988-07-25 | 1995-07-28 | Cipel | Generateur electrochimique a electrolyte alcalin et a electrode negative de zinc |
| FR2634597B1 (fr) * | 1988-07-25 | 1995-07-21 | Cipel | Generateur electrochimique a electrolyte alcalin et a electrode negative de zinc |
| FR2634594B1 (fr) * | 1988-07-25 | 1993-06-18 | Cipel Wonder | Generateur electrochimique a electrolyte alcalin et a electrode negative de zinc |
| US5240793A (en) * | 1988-12-07 | 1993-08-31 | Grillo-Werke Ag | Alkaline batteries containing a zinc powder with indium and bismuth |
| JPH0732015B2 (ja) * | 1989-04-07 | 1995-04-10 | 松下電器産業株式会社 | アルカリ電池 |
| US5168018A (en) * | 1990-05-17 | 1992-12-01 | Matsushita Electric Industrial Co., Ltd. | Method of manufacturing zinc-alkaline batteries |
| CA2046148C (en) * | 1990-08-14 | 1997-01-07 | Dale R. Getz | Alkaline cells that are substantially free of mercury |
| JPH0738306B2 (ja) * | 1991-04-22 | 1995-04-26 | 松下電器産業株式会社 | 亜鉛アルカリ電池 |
| US5316632A (en) * | 1991-07-24 | 1994-05-31 | Dieter Remppel | Method for improving efficiency of electro-chemical cells |
| US5401590A (en) * | 1992-12-07 | 1995-03-28 | Duracell Inc. | Additives for electrochemical cells having zinc anodes |
| US5378559A (en) * | 1993-11-22 | 1995-01-03 | Eveready Battery Company, Inc. | Phosphate ester additive to alkaline cells to reduce gassing |
| US5626988A (en) * | 1994-05-06 | 1997-05-06 | Battery Technologies Inc. | Sealed rechargeable cells containing mercury-free zinc anodes, and a method of manufacture |
| US20020042962A1 (en) * | 2000-02-24 | 2002-04-18 | Willman Kenneth William | Cleaning sheets comprising a polymeric additive to improve particulate pick-up and minimize residue left on surfaces and cleaning implements for use with cleaning sheets |
| US6602629B1 (en) | 2000-05-24 | 2003-08-05 | Eveready Battery Company, Inc. | Zero mercury air cell |
| CN101783422B (zh) * | 2009-01-16 | 2012-11-21 | 比亚迪股份有限公司 | 一种添加剂及含该添加剂的电解液及锂离子电池 |
Family Cites Families (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US2880122A (en) * | 1956-06-13 | 1959-03-31 | Rca Corp | Primary cells |
| US3156587A (en) * | 1962-12-10 | 1964-11-10 | Du Pont | Primary cells |
| BE789556A (fr) * | 1971-10-01 | 1973-03-29 | Union Carbide Corp | Element alcain de pile au zinc |
| US3847669A (en) * | 1971-10-01 | 1974-11-12 | Union Carbide Corp | Reduced mercury containing zinc alkaline cells |
| US4040916A (en) * | 1975-11-28 | 1977-08-09 | General Electric Company | Zinc plating bath and method of forming a non-dendritic zinc layer |
| JPS5836833B2 (ja) * | 1976-11-29 | 1983-08-11 | 古河電気工業株式会社 | 亜鉛を負極とする電池 |
| JPS53142630A (en) * | 1977-05-18 | 1978-12-12 | Sanyo Electric Co | Method of manufacturing cadmium electrode for alkaline battery |
| US4195120A (en) * | 1978-11-03 | 1980-03-25 | P. R. Mallory & Co. Inc. | Hydrogen evolution inhibitors for cells having zinc anodes |
-
1984
- 1984-07-04 FR FR8410632A patent/FR2567328B1/fr not_active Expired
-
1985
- 1985-06-21 AU AU43917/85A patent/AU580071B2/en not_active Ceased
- 1985-06-27 US US06/749,929 patent/US4606984A/en not_active Ceased
- 1985-06-27 CA CA000485523A patent/CA1256158A/en not_active Expired
- 1985-06-28 MA MA20697A patent/MA20470A1/fr unknown
- 1985-07-03 AT AT85401352T patent/ATE38298T1/de active
- 1985-07-03 EP EP85401352A patent/EP0171311B1/de not_active Expired
- 1985-07-03 JP JP60147610A patent/JPH07114126B2/ja not_active Expired - Lifetime
- 1985-07-03 DE DE8585401352T patent/DE3565913D1/de not_active Expired
- 1985-07-04 OA OA58628A patent/OA08156A/xx unknown
-
1987
- 1987-12-30 US US07/143,501 patent/USRE33427E/en not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| US4606984A (en) | 1986-08-19 |
| FR2567328A1 (fr) | 1986-01-10 |
| EP0171311B1 (de) | 1988-10-26 |
| DE3565913D1 (en) | 1988-12-01 |
| USRE33427E (en) | 1990-11-06 |
| AU580071B2 (en) | 1988-12-22 |
| FR2567328B1 (fr) | 1986-07-11 |
| MA20470A1 (fr) | 1985-12-31 |
| OA08156A (fr) | 1987-03-31 |
| JPS6127063A (ja) | 1986-02-06 |
| CA1256158A (en) | 1989-06-20 |
| EP0171311A1 (de) | 1986-02-12 |
| JPH07114126B2 (ja) | 1995-12-06 |
| AU4391785A (en) | 1986-01-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ATE38298T1 (de) | Verfahren zur stabilisierung primaerer elektrochemischer generatoren mit aktiven anoden aus zink, aluminium oder magnesium und anode fuer auf diese weise stabilisierten generator. | |
| DE60203717T2 (de) | Verfahren und produkte für die verbesserung von batterien/brennstoffzellen | |
| FR2447615A1 (fr) | Generateur electrochimique a anode faite d'un metal du groupe ia, a cathode faite d'un compose organique a fonction phtalocyanine ou porphine et a electrolyte inerte | |
| JPS56166388A (en) | Electrically cast screen and method | |
| GB1063503A (en) | Improvements in or relating to electroplating on cast iron | |
| KR850005014A (ko) | 액체전력 공급법에 의한 금속의 전기처리법 | |
| ATE45249T1 (de) | Verfahren zur stabilisierung primaerer elektrochemischer generatoren mit reaktiven anoden aus zink, aluminium oder magnesium, durch dieses verfahren erhaltene stabilisierte anode und solche anode enthaltender generator. | |
| BR8701046A (pt) | Processo para a desalogenacao de acidos cloroaceticos e de acidos bromoaceticos | |
| JPS536213A (en) | Carbon electrode coated with antioxidant for al electrolysis | |
| JPS53122633A (en) | Insoluble anode and electrolytic methdo in electroplating and the like | |
| JPS5644795A (en) | Anodic oxidation of aluminum | |
| JPS5757892A (en) | Manufacture of electrically insulating anodic oxide film | |
| JPS5589500A (en) | Electrolytic multi-coloration for aluminum or aluminum alloy anode oxide film | |
| JPS5585700A (en) | Exfoliation method for copper | |
| SE8303788D0 (sv) | Energibesparnde elektrolytisk elektrod | |
| JPS54152610A (en) | Manufacture of metallic magnesium | |
| JPS5524947A (en) | Formation of nontransparent anodic oxide film in aluminium-clad material | |
| JPS5741398A (en) | Surface treatment of stainless steel | |
| JPS5675595A (en) | Anodic oxidized film coloring method of aluminum or aluminum alloy | |
| JPS5441224A (en) | Zinc alloy for galvanic anticorrosive treatment | |
| JPS54114477A (en) | Electolysis of bromine compounds | |
| RU96122490A (ru) | Водоактивированный химический источник тока | |
| Satô | Studies of Lead Alloy Anode for Cathodic Protection (4th Report) Determination of Limited Current Density | |
| JPS5565388A (en) | Electric manganese plating method of steel strip | |
| HUT37658A (en) | Process for bath arrangement for increasing the effectiveness of electroplating |