AR000999A1 - PROCESS FOR THE PRODUCTION OF A PROTECTIVE COATING ON THE SURFACE OF A GLASS OR CERAMIC ARTICLE. - Google Patents
PROCESS FOR THE PRODUCTION OF A PROTECTIVE COATING ON THE SURFACE OF A GLASS OR CERAMIC ARTICLE.Info
- Publication number
- AR000999A1 AR000999A1 ARP960101463A AR10146396A AR000999A1 AR 000999 A1 AR000999 A1 AR 000999A1 AR P960101463 A ARP960101463 A AR P960101463A AR 10146396 A AR10146396 A AR 10146396A AR 000999 A1 AR000999 A1 AR 000999A1
- Authority
- AR
- Argentina
- Prior art keywords
- precursor
- protective coating
- production
- coating
- thermo
- Prior art date
Abstract
La invención está relacionada con un proceso para la producción de un recubrimiento de protección sobre la superficie de un artículo de vidrio ocerámica, dicho recubrimiento tiene una resistencia mejorada a los tratamientos de lavado cáustico.Para llevar a cabo el proceso de la invención una corrientede un gas portador oxigenado que contiene un precursor termodescomponible de óxido de estano (SnO2) y un precursor termodescomponible de óxido de silicio(SiO2) en una relación molar del primer precursor al precursor posterior entre 0,6 y 3,0, dichos precursores estando presentes en forma evaporada, yademás conteniendo vapor de agua en una cantidad de, al menos, 1 mol por 100 moles de gas portador, es suministrada a chorro uniformemente sobre lasuperficie a ser recubierta, dicha superficie teniendo una temperatura por arriba de las temperaturas de descomposición de dichos precursores ycantidades de al menos 550°C, para depositar un recubrimiento de protección deóxido mezclado que comprende óxido de estano y óxido de silicio, y ladeposición es continuada hasta obtener un espesor del recubrimiento de entre 240 y 1.500 L.The invention relates to a process for the production of a protective coating on the surface of an ceramic glass article, said coating having an improved resistance to caustic washing treatments. To carry out the process of the invention a current of one oxygenated carrier gas containing a thermo-decomposable precursor of tin oxide (SnO2) and a thermo-decomposable precursor of silicon oxide (SiO2) in a molar ratio of the first precursor to the subsequent precursor between 0.6 and 3.0, said precursors being present in evaporated form, and also containing water vapor in an amount of at least 1 mol per 100 moles of carrier gas, is uniformly jetted on the surface to be coated, said surface having a temperature above the decomposition temperatures of said precursors and amounts of at least 550 ° C, to deposit a mixed oxide protective coating or comprising tin oxide and silicon oxide, and deposition is continued until a coating thickness of between 240 and 1,500 L. is obtained.
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| EP95200440 | 1995-02-22 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| AR000999A1 true AR000999A1 (en) | 1997-08-27 |
Family
ID=8220042
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| ARP960101463A AR000999A1 (en) | 1995-02-22 | 1996-02-21 | PROCESS FOR THE PRODUCTION OF A PROTECTIVE COATING ON THE SURFACE OF A GLASS OR CERAMIC ARTICLE. |
Country Status (20)
| Country | Link |
|---|---|
| EP (1) | EP0810980A1 (en) |
| JP (1) | JPH11504610A (en) |
| KR (2) | KR19980702384A (en) |
| CN (1) | CN1175935A (en) |
| AR (1) | AR000999A1 (en) |
| AU (1) | AU4849096A (en) |
| BR (1) | BR9607269A (en) |
| CA (1) | CA2211940A1 (en) |
| CO (1) | CO4560356A1 (en) |
| CZ (1) | CZ260497A3 (en) |
| GT (1) | GT199600008A (en) |
| HU (1) | HUP9801366A3 (en) |
| NO (1) | NO973829L (en) |
| NZ (1) | NZ302437A (en) |
| PE (1) | PE61596A1 (en) |
| PL (1) | PL321863A1 (en) |
| TR (1) | TR199700841T1 (en) |
| UY (1) | UY24173A1 (en) |
| WO (1) | WO1996026163A1 (en) |
| ZA (1) | ZA961390B (en) |
Families Citing this family (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB9920772D0 (en) * | 1999-09-03 | 1999-11-03 | Nycomed Amersham Plc | Improved container composition for radiopharmaceutical agents |
| GB9920758D0 (en) * | 1999-09-03 | 1999-11-03 | Nycomed Amersham Plc | Improved container composition for diagnostic agents |
| EP1236705A1 (en) * | 2001-02-22 | 2002-09-04 | Atofina Vlissingen B.V. | Coated glazed articles and method for producing the same |
| KR20040033869A (en) * | 2002-10-16 | 2004-04-28 | 권원선 | Electronic oven type cooker, and process method of cooker |
| US20080152804A1 (en) * | 2006-07-28 | 2008-06-26 | Gulbrandsen Chemicals, Inc. | Method for depositing a metal-containing coating on a substrate |
| BRPI0809173A2 (en) * | 2007-04-03 | 2014-11-18 | Ppg Ind Ohi Inc | "COATED CERAMIC ITEM AND GLASS BOTTLE" |
| KR100858704B1 (en) * | 2007-10-29 | 2008-09-17 | 에스아이디주식회사 | High resistance thin film coating method of case appearance |
| GB201523156D0 (en) * | 2015-12-31 | 2016-02-17 | Pilkington Group Ltd | High strength glass containers |
| WO2017195539A1 (en) * | 2016-05-12 | 2017-11-16 | 東洋佐々木ガラス株式会社 | Glass container, and method and device for manufacturing same |
| CN110183111B (en) * | 2019-06-19 | 2024-02-02 | 广东健诚高科玻璃制品股份有限公司 | Steaming coating device and steaming coating material for daily glass ceramic and preparation method thereof |
Family Cites Families (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4853257A (en) * | 1987-09-30 | 1989-08-01 | Ppg Industries, Inc. | Chemical vapor deposition of tin oxide on float glass in the tin bath |
| JP2672391B2 (en) * | 1989-07-26 | 1997-11-05 | 麒麟麦酒 株式会社 | Glass bottle and its manufacturing method |
| JPH03115139A (en) * | 1989-09-29 | 1991-05-16 | Hitachi Ltd | Antireflection film and its formation |
| JP3485918B2 (en) * | 1991-12-26 | 2004-01-13 | アトフィナ・ケミカルズ・インコーポレイテッド | Glass substrate coating method |
-
1996
- 1996-02-20 CO CO96007867A patent/CO4560356A1/en unknown
- 1996-02-21 PE PE1996000121A patent/PE61596A1/en not_active Application Discontinuation
- 1996-02-21 ZA ZA961390A patent/ZA961390B/en unknown
- 1996-02-21 GT GT199600008A patent/GT199600008A/en unknown
- 1996-02-21 AR ARP960101463A patent/AR000999A1/en unknown
- 1996-02-22 TR TR97/00841T patent/TR199700841T1/en unknown
- 1996-02-22 KR KR1019970705783A patent/KR19980702384A/en not_active Withdrawn
- 1996-02-22 HU HU9801366A patent/HUP9801366A3/en unknown
- 1996-02-22 NZ NZ302437A patent/NZ302437A/en unknown
- 1996-02-22 CZ CZ972604A patent/CZ260497A3/en unknown
- 1996-02-22 CN CN96192020A patent/CN1175935A/en active Pending
- 1996-02-22 EP EP96904367A patent/EP0810980A1/en not_active Withdrawn
- 1996-02-22 CA CA002211940A patent/CA2211940A1/en not_active Abandoned
- 1996-02-22 UY UY24173A patent/UY24173A1/en unknown
- 1996-02-22 WO PCT/NL1996/000087 patent/WO1996026163A1/en not_active Ceased
- 1996-02-22 BR BR9607269A patent/BR9607269A/en not_active Application Discontinuation
- 1996-02-22 PL PL96321863A patent/PL321863A1/en unknown
- 1996-02-22 AU AU48490/96A patent/AU4849096A/en not_active Abandoned
- 1996-02-22 JP JP8525581A patent/JPH11504610A/en active Pending
-
1997
- 1997-08-20 NO NO973829A patent/NO973829L/en unknown
- 1997-08-21 KR KR19977005783A patent/KR19987002384A/ko active Pending
Also Published As
| Publication number | Publication date |
|---|---|
| AU4849096A (en) | 1996-09-11 |
| MX9706302A (en) | 1998-06-28 |
| HUP9801366A2 (en) | 1998-08-28 |
| JPH11504610A (en) | 1999-04-27 |
| TR199700841T1 (en) | 1998-02-21 |
| EP0810980A1 (en) | 1997-12-10 |
| KR19980702384A (en) | 1998-07-15 |
| GT199600008A (en) | 1997-08-14 |
| NO973829D0 (en) | 1997-08-20 |
| HUP9801366A3 (en) | 1998-12-28 |
| PE61596A1 (en) | 1997-02-01 |
| KR19987002384A (en) | 1998-07-15 |
| CO4560356A1 (en) | 1998-02-10 |
| BR9607269A (en) | 1998-12-15 |
| CN1175935A (en) | 1998-03-11 |
| CA2211940A1 (en) | 1996-08-29 |
| NZ302437A (en) | 1998-04-27 |
| UY24173A1 (en) | 1996-08-06 |
| NO973829L (en) | 1997-08-20 |
| ZA961390B (en) | 1996-07-16 |
| PL321863A1 (en) | 1997-12-22 |
| WO1996026163A1 (en) | 1996-08-29 |
| CZ260497A3 (en) | 1998-01-14 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ES2075146T3 (en) | SILIL-CYCLOBUTANE PLASMA-INDUCED DECOMPOSITION PROCEDURE TO FORM CONTINUOUS AMORPHOUS SILICON CARBIDE COATINGS. | |
| Chu et al. | The preparation and properties of amorphous silicon nitride films | |
| ES2288761T3 (en) | PROTECTIVE COATING BY HIGH-SPEED ARC PLASMA DEPOSITION. | |
| AR000999A1 (en) | PROCESS FOR THE PRODUCTION OF A PROTECTIVE COATING ON THE SURFACE OF A GLASS OR CERAMIC ARTICLE. | |
| DE60123813D1 (en) | LOCKING LAYER FOR GLASSING MATERIALS | |
| ES2069785T3 (en) | DIAMOND THAT HAS MULTIPLE COATINGS, METHODS FOR ITS MANUFACTURE AND USE THEREOF. | |
| BR0113962A (en) | Sputtering deposition process of a coating with photocatalytic properties, transparent or semi-transparent substrate, and glazing | |
| BR9808337A (en) | Photocatalytically activated self-cleaning manufactured article, method for producing the same and method for forming a floated glass band | |
| UY23526A1 (en) | COATED ITEM | |
| ES2186915T3 (en) | PROCEDURE TO SERVE TITANIUM OXIDE AND TITANIUM OXIDE ON A GLASS AND GLASS PLATE COVERED BY MEANS OF THIS PROCEDURE. | |
| IL61877A (en) | Columnar grain ceramic thermal barrier coatings on polished superalloy substrates | |
| ES2162048T3 (en) | PROTECTIVE COATING AGAINST EROSION / CORROSION FOR COMPONENTS EXPOSED TO HIGH TEMPERATURES. | |
| AR059303A2 (en) | A PROCESS FOR THE PRODUCTION OF A PHOTOCATALLYTICALLY ACTIVE COVERED SUBSTRATE | |
| ES2111972T3 (en) | DEPOSIT METHOD IN THE STEAM PHASE OF A CERAMIC COATING USING A CARRIER GAS CONTAINING WATER VAPOR AND NON-ALCOXY XYLANIC PRECURSORS. | |
| ES2139720T3 (en) | DEPOSIT PROCEDURE OF A TITANIUM NITRIDE BASED LAYER ON A TRANSPARENT SUBSTRATE. | |
| MX9304930A (en) | METHOD OF PREPARATION OF SURFACE AND DEPOSITION FOR TITANIUM NITRIDE ON CARBONACEOUS MATERIALS. | |
| ES2118798T3 (en) | ASYMMETRICAL FEED NOZZLE FOR THE REALIZATION OF A COATING LAYER ON A GLASS TAPE, BY PYROLYSIS OF A GAS MIXTURE. | |
| AR009058A1 (en) | A PROCESS TO APPLY INDIAN OXIDE COATINGS ON FLAT GLASSES AND COATED GLASSES SO OBTAINED | |
| JPH11131236A5 (en) | ||
| Zhao et al. | Aluminium oxide thin films prepared by plasma-enhanced chemical vapour deposition | |
| Duret et al. | Protective Coatings for High-Temperature Materials: Chemical Vapor Deposition and Pack Cementation Processes | |
| FR2672044B1 (en) | PROCESS FOR ENAMELLING A GLASS SUBSTRATE AND ENAMEL COMPOSITION USED. | |
| 沈光平 et al. | IRON OXIDE AMORPHOUS FILM MANUFACTURED BY LCVD | |
| Archer | Hard and Wear-Resistant Coatings by Chemical Vapour Deposition | |
| Vogel | Hard Material Coats in Cutting and Forming Technologies |