WO2012033202A1 - Aimant arqué et matrice de moulage à champ magnétique - Google Patents

Aimant arqué et matrice de moulage à champ magnétique Download PDF

Info

Publication number
WO2012033202A1
WO2012033202A1 PCT/JP2011/070631 JP2011070631W WO2012033202A1 WO 2012033202 A1 WO2012033202 A1 WO 2012033202A1 JP 2011070631 W JP2011070631 W JP 2011070631W WO 2012033202 A1 WO2012033202 A1 WO 2012033202A1
Authority
WO
WIPO (PCT)
Prior art keywords
magnet
arcuate
magnetic
arcuate magnet
curved surface
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
PCT/JP2011/070631
Other languages
English (en)
Japanese (ja)
Inventor
一彦 宮城島
貞雄 二橋
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TDK Corp
Original Assignee
TDK Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TDK Corp filed Critical TDK Corp
Priority to CN201180043091.1A priority Critical patent/CN103098354B/zh
Publication of WO2012033202A1 publication Critical patent/WO2012033202A1/fr
Anticipated expiration legal-status Critical
Ceased legal-status Critical Current

Abstract

L'invention porte sur un aimant arqué (10) qui est un aimant contenant une pluralité de particules de poudre magnétique et dont la section transversale est en forme d'arc. Dans l'aimant arqué (10), dans une section transversale coupée suivant un plan orthogonal à sa direction longitudinale, les directions d'orientation des axes d'aimantation faciles de la pluralité de particules de poudre magnétique sont orientées de manière à converger en deux points, c'est-à-dire des points en lesquels deux axes différents (Zca, Zcb) coupent la section transversale. De ce fait, des flux magnétiques provenant de l'aimant arqué (10) vont vers les deux axes différents (Zca, Zcb). Par conséquent, l'aimant arqué (10) permet d'obtenir une augmentation de la densité de flux magnétique effectivement utilisable.
PCT/JP2011/070631 2010-09-10 2011-09-09 Aimant arqué et matrice de moulage à champ magnétique Ceased WO2012033202A1 (fr)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201180043091.1A CN103098354B (zh) 2010-09-10 2011-09-09 弓形磁铁和磁场成形用模具

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2010203620 2010-09-10
JP2010-203620 2010-09-10

Publications (1)

Publication Number Publication Date
WO2012033202A1 true WO2012033202A1 (fr) 2012-03-15

Family

ID=45810797

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2011/070631 Ceased WO2012033202A1 (fr) 2010-09-10 2011-09-09 Aimant arqué et matrice de moulage à champ magnétique

Country Status (3)

Country Link
JP (1) JP5870567B2 (fr)
CN (1) CN103098354B (fr)
WO (1) WO2012033202A1 (fr)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2016189238A1 (fr) 2015-05-22 2016-12-01 Saint-Gobain Glass France Vitrage feuillete comprenant un cordon profile de clippage a ruban polymerique supplementaire et cordon profile
JP2020078231A (ja) * 2018-10-04 2020-05-21 日東電工株式会社 複数のモータ製品、モータ、モータ群、駆動装置、および磁石群
EP4489265A1 (fr) * 2023-07-04 2025-01-08 LG Electronics Inc. Aimant, moteur comprenant celui-ci et machine à laver comprenant celui-ci
EP4489043A1 (fr) * 2023-07-04 2025-01-08 LG Electronics Inc. Dispositif d'orientation d'aimant et aimant

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP5722944B2 (ja) * 2013-04-26 2015-05-27 株式会社日本製鋼所 プラスチック磁石の製造方法
US9583244B2 (en) * 2014-09-30 2017-02-28 Nichia Corporation Bonded magnet, bonded magnet component, and bonded magnet production method
JP6706487B2 (ja) * 2015-11-19 2020-06-10 日東電工株式会社 希土類永久磁石をもった回転子を備える回転電機
CN113785473A (zh) * 2019-03-11 2021-12-10 西门子歌美飒可再生能源公司 包括各自具有聚焦磁畴对准模式的磁体装置的磁体组件

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS4995116A (fr) * 1973-01-16 1974-09-10
JPS5710729U (fr) * 1980-06-20 1982-01-20
JP2002110417A (ja) * 2000-09-29 2002-04-12 Toda Kogyo Corp 異方性セグメント形状磁石及びこれを用いたモーター
JP2009142144A (ja) * 2007-11-12 2009-06-25 Panasonic Corp 異方性永久磁石型モータ

Family Cites Families (11)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5772305A (en) * 1980-10-24 1982-05-06 Tdk Corp Permanent magnet composition with patterned magnetization
JPH0620826A (ja) * 1991-11-26 1994-01-28 Kawasaki Steel Corp 集束配向磁石とその製造用金型
JPH07212994A (ja) * 1994-01-24 1995-08-11 Toshiba Corp 永久磁石形モータ
JPH0995116A (ja) * 1995-10-02 1997-04-08 Nittetsu Semiconductor Kk 物品搬送車
JP4057092B2 (ja) * 1997-03-24 2008-03-05 Tdk株式会社 円弧状フェライト磁石の乾式磁場成型装置
JP3697375B2 (ja) * 1999-12-17 2005-09-21 Tdk株式会社 直流モータ用フェライト磁石の磁場成型用金型
CN1162235C (zh) * 2000-03-28 2004-08-18 住友特殊金属株式会社 粉体压制装置及稀土合金磁性粉末成型体的制作方法
JP4826704B2 (ja) * 2003-10-15 2011-11-30 日立金属株式会社 極集中型磁気回路および磁気分離装置
KR100908424B1 (ko) * 2004-12-17 2009-07-21 히타치 긴조쿠 가부시키가이샤 자기 회로용 부품 및 그 제조 방법
JP5267459B2 (ja) * 2007-06-28 2013-08-21 日立金属株式会社 R−tm−b系ラジアル異方性リング磁石、その製造方法、及びそれを製造するための金型、並びにブラシレスモータ用ロータ
JP2009043926A (ja) * 2007-08-08 2009-02-26 Kaneka Corp マグネットローラ

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS4995116A (fr) * 1973-01-16 1974-09-10
JPS5710729U (fr) * 1980-06-20 1982-01-20
JP2002110417A (ja) * 2000-09-29 2002-04-12 Toda Kogyo Corp 異方性セグメント形状磁石及びこれを用いたモーター
JP2009142144A (ja) * 2007-11-12 2009-06-25 Panasonic Corp 異方性永久磁石型モータ

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2016189238A1 (fr) 2015-05-22 2016-12-01 Saint-Gobain Glass France Vitrage feuillete comprenant un cordon profile de clippage a ruban polymerique supplementaire et cordon profile
JP2020078231A (ja) * 2018-10-04 2020-05-21 日東電工株式会社 複数のモータ製品、モータ、モータ群、駆動装置、および磁石群
EP4489265A1 (fr) * 2023-07-04 2025-01-08 LG Electronics Inc. Aimant, moteur comprenant celui-ci et machine à laver comprenant celui-ci
EP4489043A1 (fr) * 2023-07-04 2025-01-08 LG Electronics Inc. Dispositif d'orientation d'aimant et aimant
US20250015652A1 (en) * 2023-07-04 2025-01-09 Lg Electronics Inc. Magnet for motor and washing machine including the same
US20250014797A1 (en) * 2023-07-04 2025-01-09 Lg Electronics Inc. Magnet orientation device and magnet

Also Published As

Publication number Publication date
JP2012080097A (ja) 2012-04-19
CN103098354A (zh) 2013-05-08
CN103098354B (zh) 2016-05-04
JP5870567B2 (ja) 2016-03-01

Similar Documents

Publication Publication Date Title
JP5870567B2 (ja) 弓形磁石及び磁場成形用金型
JP6596191B2 (ja) 等高線に沿った磁場の磁石
JP6308205B2 (ja) 異方性磁石の製造方法、異方性軟磁性体の製造方法および回転電機のロータ製造方法
EP1830451A1 (fr) Rotor pour moteur et son procede de fabrication
WO2012169043A1 (fr) Rotor pour machine électrique rotative, machine électrique rotative, et procédé de production d'un rotor pour machine électrique rotative
JP2005184916A (ja) 圧粉磁心およびステータコア
JP2015133839A (ja) 磁石埋込型ロータ
WO2021200361A1 (fr) Élément de génération d'énergie, capteur magnétique le mettant en œuvre, codeur et moteur
JP2010183684A (ja) 回転機用永久磁石型回転子
JP2003257762A (ja) リング磁石とその製造法及び回転子と回転機並びにその磁界発生装置及びリング磁石製造装置
JP4029679B2 (ja) モータ用ボンド磁石及びモータ
TW200845540A (en) Voice coil motor and magnetic circuit therefor
JP4507208B2 (ja) 磁石回転子及びこれを用いた回転角度検出装置
JP5766134B2 (ja) シャフト型リニアモータ可動子、永久磁石、リニアモータ
US11069464B2 (en) Method and assembly for producing a magnet
JP7081145B2 (ja) 磁石構造体、回転角度検出器および電動パワーステアリング装置
CN107394917A (zh) 定向磁化装置以及磁铁埋入型转子
WO2020129866A1 (fr) Noyau, stator et machine électrique tournante
WO2011061806A1 (fr) Procédé de fabrication d'un rotor de moteur électrique
CN104160599B (zh) 用于制造机器元件的方法和用于电机的机器元件
JP5177661B2 (ja) トルクセンサ
JP2010148309A (ja) 界磁子及び界磁子の製造方法
JP2021100329A (ja) ステータコア、ステータ、回転電機、及びステータコアの製造方法
JPH06260328A (ja) 円筒状異方性磁石およびその製造方法
JP7810974B2 (ja) ブラシレスspmモータおよびその回転子の製造方法

Legal Events

Date Code Title Description
WWE Wipo information: entry into national phase

Ref document number: 201180043091.1

Country of ref document: CN

121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 11823676

Country of ref document: EP

Kind code of ref document: A1

NENP Non-entry into the national phase

Ref country code: DE

122 Ep: pct application non-entry in european phase

Ref document number: 11823676

Country of ref document: EP

Kind code of ref document: A1