WO2012004886A1 - Batterie rechargeable et procédé de fabrication d'un groupe d'électrodes en enroulement plat - Google Patents
Batterie rechargeable et procédé de fabrication d'un groupe d'électrodes en enroulement plat Download PDFInfo
- Publication number
- WO2012004886A1 WO2012004886A1 PCT/JP2010/061690 JP2010061690W WO2012004886A1 WO 2012004886 A1 WO2012004886 A1 WO 2012004886A1 JP 2010061690 W JP2010061690 W JP 2010061690W WO 2012004886 A1 WO2012004886 A1 WO 2012004886A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- secondary battery
- shaft core
- electrode group
- negative electrode
- flat
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Abstract
La présente invention concerne une batterie rechargeable configurée de façon que l'épaisseur (TB0) d'un cœur (30), considérée au centre du noyau dans le sens de la largeur, soit supérieure à l'épaisseur (TA0) du cœur (30), considérée à ses deux extrémités dans le sens de la largeur. Au cours de l'opération d'enroulement, des forces de tension (A, A') font qu'une force de liaison (B) agisse sur une surface large (30W) du cœur (30). La force de liaison (B) agit de l'extérieur vers l'intérieur sur l'anode (1), sur la cathode (2) et sur les séparateurs (3a, 3b) en direction du cœur (30). L'anode (1), la cathode (2), et les séparateurs (3a, 3b) sont dotés d'une force élastique agissant dans le sens de la périphérie extérieure, la force de liaison (B) reliant fermement entre eux l'anode (1), la cathode (2), et les séparateurs (3a, 3b) en s'opposant à la force élastique. Il résulte de cette configuration qu'il ne se forme pas d'intervalle entre l'anode (1) et la cathode (2), si bien que la densité du groupe d'électrodes en enroulement plat (4) est accrue de façon à augmenter la capacité de la batterie rechargeable.
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PCT/JP2010/061690 WO2012004886A1 (fr) | 2010-07-09 | 2010-07-09 | Batterie rechargeable et procédé de fabrication d'un groupe d'électrodes en enroulement plat |
| JP2012523483A JPWO2012004886A1 (ja) | 2010-07-09 | 2010-07-09 | 二次電池および扁平捲回形電極群の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PCT/JP2010/061690 WO2012004886A1 (fr) | 2010-07-09 | 2010-07-09 | Batterie rechargeable et procédé de fabrication d'un groupe d'électrodes en enroulement plat |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| WO2012004886A1 true WO2012004886A1 (fr) | 2012-01-12 |
Family
ID=45440885
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PCT/JP2010/061690 Ceased WO2012004886A1 (fr) | 2010-07-09 | 2010-07-09 | Batterie rechargeable et procédé de fabrication d'un groupe d'électrodes en enroulement plat |
Country Status (2)
| Country | Link |
|---|---|
| JP (1) | JPWO2012004886A1 (fr) |
| WO (1) | WO2012004886A1 (fr) |
Cited By (9)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2013136478A1 (fr) * | 2012-03-15 | 2013-09-19 | 日立ビークルエナジー株式会社 | Module de batteries secondaires rectangulaires |
| JP2013239313A (ja) * | 2012-05-14 | 2013-11-28 | Hitachi Vehicle Energy Ltd | リチウムイオン角形二次電池 |
| WO2014199822A1 (fr) * | 2013-06-11 | 2014-12-18 | 日立オートモティブシステムズ株式会社 | Pile secondaire au lithium-ion et pile assemblée |
| JP2015002086A (ja) * | 2013-06-14 | 2015-01-05 | 株式会社Gsユアサ | 蓄電素子、芯材及び蓄電素子の製造方法 |
| DE102014214619A1 (de) * | 2014-07-25 | 2016-01-28 | Robert Bosch Gmbh | Verfahren zur Herstellung einer prismatischen Batteriezelle |
| JP2016110768A (ja) * | 2014-12-04 | 2016-06-20 | Ckd株式会社 | 捲回装置 |
| JP2016181396A (ja) * | 2015-03-24 | 2016-10-13 | 株式会社Gsユアサ | 巻回装置、蓄電素子の製造方法、及び蓄電素子 |
| WO2019235476A1 (fr) * | 2018-06-07 | 2019-12-12 | 株式会社Gsユアサ | Élément de stockage d'énergie |
| JP2021017327A (ja) * | 2019-07-19 | 2021-02-15 | 株式会社皆藤製作所 | 巻芯、巻回ユニット、及び巻回装置 |
Citations (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2001236996A (ja) * | 2000-02-22 | 2001-08-31 | Sony Corp | 非水電解質電池の製造方法 |
| JP2002280055A (ja) * | 2001-03-21 | 2002-09-27 | Shin Kobe Electric Mach Co Ltd | 扁平捲回群製造方法及び捲回装置 |
| JP2003068350A (ja) * | 2001-08-29 | 2003-03-07 | Denso Corp | 扁平型電極体の製造装置 |
| JP2007026939A (ja) * | 2005-07-19 | 2007-02-01 | Toyota Motor Corp | 捲回型電池とその製造方法 |
| WO2007097172A1 (fr) * | 2006-02-21 | 2007-08-30 | Matsushita Electric Industrial Co., Ltd. | Procede de fabrication de batterie secondaire plate carree |
| JP2010146872A (ja) * | 2008-12-19 | 2010-07-01 | Hitachi Vehicle Energy Ltd | 扁平形二次電池 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2001229970A (ja) * | 2000-02-16 | 2001-08-24 | Shin Kobe Electric Mach Co Ltd | 円筒形リチウムイオン電池 |
| US7642566B2 (en) * | 2006-06-12 | 2010-01-05 | Dsm Solutions, Inc. | Scalable process and structure of JFET for small and decreasing line widths |
-
2010
- 2010-07-09 JP JP2012523483A patent/JPWO2012004886A1/ja active Pending
- 2010-07-09 WO PCT/JP2010/061690 patent/WO2012004886A1/fr not_active Ceased
Patent Citations (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2001236996A (ja) * | 2000-02-22 | 2001-08-31 | Sony Corp | 非水電解質電池の製造方法 |
| JP2002280055A (ja) * | 2001-03-21 | 2002-09-27 | Shin Kobe Electric Mach Co Ltd | 扁平捲回群製造方法及び捲回装置 |
| JP2003068350A (ja) * | 2001-08-29 | 2003-03-07 | Denso Corp | 扁平型電極体の製造装置 |
| JP2007026939A (ja) * | 2005-07-19 | 2007-02-01 | Toyota Motor Corp | 捲回型電池とその製造方法 |
| WO2007097172A1 (fr) * | 2006-02-21 | 2007-08-30 | Matsushita Electric Industrial Co., Ltd. | Procede de fabrication de batterie secondaire plate carree |
| JP2010146872A (ja) * | 2008-12-19 | 2010-07-01 | Hitachi Vehicle Energy Ltd | 扁平形二次電池 |
Cited By (12)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2013136478A1 (fr) * | 2012-03-15 | 2013-09-19 | 日立ビークルエナジー株式会社 | Module de batteries secondaires rectangulaires |
| JPWO2013136478A1 (ja) * | 2012-03-15 | 2015-08-03 | 日立オートモティブシステムズ株式会社 | 角形二次電池モジュール |
| JP2013239313A (ja) * | 2012-05-14 | 2013-11-28 | Hitachi Vehicle Energy Ltd | リチウムイオン角形二次電池 |
| WO2014199822A1 (fr) * | 2013-06-11 | 2014-12-18 | 日立オートモティブシステムズ株式会社 | Pile secondaire au lithium-ion et pile assemblée |
| JP2015002086A (ja) * | 2013-06-14 | 2015-01-05 | 株式会社Gsユアサ | 蓄電素子、芯材及び蓄電素子の製造方法 |
| DE102014214619A1 (de) * | 2014-07-25 | 2016-01-28 | Robert Bosch Gmbh | Verfahren zur Herstellung einer prismatischen Batteriezelle |
| US10263291B2 (en) | 2014-07-25 | 2019-04-16 | Robert Bosch Gmbh | Method of producing a prismatic battery cell |
| JP2016110768A (ja) * | 2014-12-04 | 2016-06-20 | Ckd株式会社 | 捲回装置 |
| JP2016181396A (ja) * | 2015-03-24 | 2016-10-13 | 株式会社Gsユアサ | 巻回装置、蓄電素子の製造方法、及び蓄電素子 |
| WO2019235476A1 (fr) * | 2018-06-07 | 2019-12-12 | 株式会社Gsユアサ | Élément de stockage d'énergie |
| US11837700B2 (en) | 2018-06-07 | 2023-12-05 | Gs Yuasa International Ltd. | Energy storage device |
| JP2021017327A (ja) * | 2019-07-19 | 2021-02-15 | 株式会社皆藤製作所 | 巻芯、巻回ユニット、及び巻回装置 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPWO2012004886A1 (ja) | 2013-09-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP5456542B2 (ja) | 角形二次電池および角形二次電池の製造方法 | |
| JP5417241B2 (ja) | 角形リチウムイオン二次電池および角形リチウムイオン二次電池の製造方法 | |
| JP3368877B2 (ja) | 円筒形リチウムイオン電池 | |
| CN103682232B (zh) | 电池 | |
| JP6198844B2 (ja) | 組電池 | |
| WO2012004886A1 (fr) | Batterie rechargeable et procédé de fabrication d'un groupe d'électrodes en enroulement plat | |
| JP5651614B2 (ja) | 角形二次電池及びモジュール | |
| JP2012074287A (ja) | 角形二次電池 | |
| JP5334894B2 (ja) | リチウムイオン二次電池 | |
| WO2013027296A1 (fr) | Batterie secondaire aux ions de lithium et procédé de fabrication associé | |
| JP6106774B2 (ja) | 角形リチウムイオン電池 | |
| US20130323557A1 (en) | Secondary battery and method for manufacturing same | |
| JP2013073809A (ja) | リチウムイオン二次電池 | |
| JP2001229970A (ja) | 円筒形リチウムイオン電池 | |
| JP6562726B2 (ja) | 角形二次電池及びその製造方法 | |
| JP2001143759A (ja) | 円筒形リチウムイオン電池 | |
| JP6182061B2 (ja) | 二次電池 | |
| JP4934318B2 (ja) | 二次電池 | |
| JP2015088247A (ja) | 二次電池 | |
| JP2005100955A (ja) | 捲回式リチウムイオン電池 | |
| JP2001185220A (ja) | 円筒形リチウムイオン電池 | |
| JP5882697B2 (ja) | 角形リチウムイオン電池 | |
| JP5914635B2 (ja) | 角形二次電池モジュール | |
| JP3511966B2 (ja) | 円筒形リチウムイオン電池 | |
| JP6382336B2 (ja) | 角形二次電池 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| 121 | Ep: the epo has been informed by wipo that ep was designated in this application |
Ref document number: 10854440 Country of ref document: EP Kind code of ref document: A1 |
|
| WWE | Wipo information: entry into national phase |
Ref document number: 2012523483 Country of ref document: JP |
|
| NENP | Non-entry into the national phase |
Ref country code: DE |
|
| 122 | Ep: pct application non-entry in european phase |
Ref document number: 10854440 Country of ref document: EP Kind code of ref document: A1 |