US20130087284A1 - Organic line width roughness with h2 plasma treatment - Google Patents
Organic line width roughness with h2 plasma treatment Download PDFInfo
- Publication number
- US20130087284A1 US20130087284A1 US13/627,901 US201213627901A US2013087284A1 US 20130087284 A1 US20130087284 A1 US 20130087284A1 US 201213627901 A US201213627901 A US 201213627901A US 2013087284 A1 US2013087284 A1 US 2013087284A1
- Authority
- US
- United States
- Prior art keywords
- computer readable
- readable code
- gas
- plasma processing
- processing chamber
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Abstract
An apparatus for reducing very low frequency line width roughness (LWR) is provided. A plasma processing chamber is provided, comprising a chamber wall, a substrate support, a pressure regulator, at least one antenna, a gas inlet, and a gas outlet. A gas source comprises an etchant gas source and a H2 treatment gas source. A controller comprises at least one processor and computer readable media, comprising computer readable code for treating a patterned organic mask, comprising computer readable code for flowing a treatment gas comprising H2, wherein the treatment gas has a flow rate and H2 has a flow rate that is at least 50% of the flow rate of the treatment gas, computer readable code for forming a plasma, and computer readable code for stopping the flow of the treatment gas, and computer readable code for etching the etch layer through the treated patterned organic mask.
Description
- This application is a divisional of and claims benefit to co-pending U.S. patent application Ser. No. 12/175,153 filed on Jul. 17, 2008, entitled “Organic Line Width Roughness with H2 Plasma Treatment,” by Adams et al., which is hereby incorporated by reference for all purposes.
- The present invention relates to the formation of semiconductor devices.
- During semiconductor wafer processing, features of the semiconductor device are defined in the wafer using well-known patterning and etching processes. In these processes, a photoresist (PR) material is deposited on the wafer and then is exposed to light filtered by a reticle. The reticle is generally a glass plate that is patterned with exemplary feature geometries that block light from propagating through the reticle.
- After passing through the reticle, the light contacts the surface of the photoresist material. The light changes the chemical composition of the photoresist material such that a developer can remove a portion of the photoresist material. In the case of positive photoresist materials, the exposed regions are removed, and in the case of negative photoresist materials, the unexposed regions are removed. Thereafter, the wafer is etched to remove the underlying material from the areas that are no longer protected by the photoresist material, and thereby define the desired features in the wafer.
- To achieve the foregoing and in accordance with the purpose of the present invention, a method for reducing very low frequency line width roughness (LWR) in forming etched features in an etch layer disposed below a patterned organic mask is provided. The patterned organic mask is treated to reduce very low frequency line width roughness of the patterned organic mask, comprising flowing a treatment gas comprising H2, wherein the treatment gas has a flow rate and H2 has a flow rate that is at least 50% of the flow rate of the treatment gas, forming a plasma from the treatment gas, and stopping the flow of the treatment gas. The etch layer is etched through the treated patterned organic mask with the reduced very low LWR.
- In another manifestation of the invention a method for reducing very low frequency line width roughness (LWR) in forming etched features in a conductive layer disposed below a hard mask layer disposed below an etch layer disposed below a patterned photoresist mask forming a stack on a wafer is provided. The wafer is placed in a process chamber. The patterned photoresist mask is treated to reduce very low frequency line width roughness of the patterned photoresist mask, comprising flowing a treatment gas comprising H2, wherein the treatment gas has a flow rate and H2 has a flow rate that is at least 50% of the flow rate of the treatment gas into the process chamber, forming a plasma from the treatment gas, and stopping the flow of the treatment gas. The etch layer is etched through the treated patterned photoresist mask. The hard mask layer is etched through the etched layer. The conductive layer is etched through the hard mask layer. The wafer is removed from the process chamber, so that the treating the patterned organic mask, etching the etch layer, etching the hard mask layer, and etching the conductive layer are all done in situ in the same process chamber.
- In another manifestation of the invention an apparatus for reducing very low frequency line width roughness (LWR) in forming etched features in an etch layer, disposed below a patterned organic mask with mask features is provided. A plasma processing chamber is provided, comprising a chamber wall forming a plasma processing chamber enclosure, a substrate support for supporting a wafer within the plasma processing chamber enclosure, a pressure regulator for regulating the pressure in the plasma processing chamber enclosure, at least one antenna for providing inductively coupled power to the plasma processing chamber enclosure for sustaining a plasma, a gas inlet for providing gas into the plasma processing chamber enclosure, and a gas outlet for exhausting gas from the plasma processing chamber enclosure. A gas source is in fluid connection with the gas inlet and comprises an etchant gas source and a H2 treatment gas source. A controller is controllably connected to the gas source and the at least one antenna and comprises at least one processor and computer readable media. The computer readable media comprises computer readable code for treating the patterned organic mask to reduce very low frequency line width roughness of the patterned organic mask, comprising computer readable code for flowing a treatment gas comprising H2, wherein the treatment gas has a flow rate and H2 has a flow rate that is at least 50% of the flow rate of the treatment gas, computer readable code for forming a plasma from the treatment gas, and computer readable code for stopping the flow of the treatment gas, and computer readable code for etching the etch layer through the treated patterned organic mask with the reduced very low LWR.
- These and other features of the present invention will be described in more detail below in the detailed description of the invention and in conjunction with the following figures.
- The present invention is illustrated by way of example, and not by way of limitation, in the figures of the accompanying drawings and in which like reference numerals refer to similar elements and in which:
-
FIG. 1 is a high level flow chart of a process that may be used in an embodiment of the invention. -
FIGS. 2A-C are schematic cross-sectional views of a stack etched according to an embodiment of the invention. -
FIG. 3 is a schematic view of a plasma processing chamber that may be used in practicing the invention. -
FIGS. 4A-B illustrate a computer system, which is suitable for implementing a controller used in embodiments of the present invention. -
FIGS. 5A-F are CD-SEMs of wafers processed by examples of embodiments of the invention. -
FIGS. 6A-C are graphs of results from the above examples of embodiments of the invention. -
FIG. 7 is a CD-SEM (top-down) of a wafer with a mask that illustrates LWR. -
FIG. 8 shows a typical sequence that is followed to obtain the LWR vs inspect length curve. - The present invention will now be described in detail with reference to a few preferred embodiments thereof as illustrated in the accompanying drawings. In the following description, numerous specific details are set forth in order to provide a thorough understanding of the present invention. It will be apparent, however, to one skilled in the art, that the present invention may be practiced without some or all of these specific details. In other instances, well known process steps and/or structures have not been described in detail in order to not unnecessarily obscure the present invention.
- To facilitate understanding,
FIG. 1 is a high level flow chart of a process that may be used in an embodiment of the invention, which reduces very low frequency line width roughness below a patterned photoresist mask. A wafer with a patterned photoresist mask is placed into an inductively coupled TCP chamber (step 102). The patterned photoresist mask is treated to reduce very low frequency line width roughness (LWR) (step 104). This step comprises flowing a H2 treatment gas into a process chamber (step 108), forming a plasma from the H2 treatment gas (step 112), which reduces the very low frequency line width roughness. Subsequent processing steps may be performed to complete the structure. The flow of the H2 treatment gas is stopped (step 116) to stop the treatment process. For example, in one embodiment an etch layer is etched (step 120) after the PR treatment. In this embodiment, the etch layer is an organic ARC layer, which is above a hard mask layer, which is above a conductive layer. The hard mask is then opened (step 124). The conductive layer is etched (step 128). The wafer is removed from the process chamber (step 132). - In an example of an implementation of the invention, a wafer is provided with an etch layer and a photoresist mask.
FIG. 2A is a cross-sectional view of an example of awafer 204 over which aconductive layer 208 is formed, over which ahard mask layer 212 is formed, over which an organic antireflective coating (ARC)layer 216 is formed, over which a patternedPR mask 220 is formed. In this example, the patternedPR mask 220 is of a 193 nm or higher generation photoresist material. Theorganic ARC layer 216 may be a BARC (bottom antireflective coating) material. Thehard mask layer 212 may be one or more layers of different materials, such as SiOx or SiNx. Theconductive layer 208 is of a conductive material such as polysilicon, amorphous silicon, or a metal such as TiN. In this example, thewafer 204 is a crystalline silicon wafer. - In this example, the patterned
photoresist mask 216 has a very low frequency line edge roughness. A very low frequency line width roughness repetition length of greater than 500 nm. More preferably, the very low line edge roughness repetition length is greater than 550 nm. Line width roughness is the 3σ value of line width in a given inspection area, which may be calculated according to: -
-
FIG. 7 is a CD-SEM (top-down) of a wafer with amask 704 that illustrates LWR. Aninspection length 708 is selected. Along the inspection length,line widths 712 are measured for a feature extending along the inspection length. The measuredline widths 712 are used inequation 1 to calculate LWR. -
FIG. 8 shows a typical sequence that is followed to obtain the LWR vs inspect length curve. Following image acquisition from the CD-SEM (top-down), at the optimal focus, beam alignment, and integration, an optimal LWR algorithm is applied to relevant features in the image. The variation of LWR is studied as a function of inspect length and the result is a curve that shows the high- and very low-frequency LWR components. The regions where the LWR curve flattens out (at two locations, inspect length ˜200 nm and ˜600 nm) correspond to the amplitudes of the high- and very low-frequency LWR, respectively. - The
wafer 204 is placed in an inductively coupled plasma processing chamber (step 102). -
FIG. 3 illustrates a processing tool that may be used in an implementation of the invention.FIG. 3 is a schematic view of aplasma processing system 300, including aplasma processing tool 301. Theplasma processing tool 301 is an inductively coupled plasma etching tool and includes aplasma reactor 302 having aplasma processing chamber 304 therein. A transformer coupled power (TCP)controller 350 and abias power controller 355, respectively, control aTCP power supply 351 and abias power supply 356 influencing theplasma 324 created withinplasma chamber 304. - The
TCP power controller 350 sets a set point forTCP power supply 351 configured to supply a radio frequency signal at 13.56 MHz, tuned by aTCP match network 352, to aTCP coil 353 located near theplasma chamber 304. An RFtransparent window 354 is provided toseparate TCP coil 353 fromplasma chamber 304 while allowing energy to pass fromTCP coil 353 toplasma chamber 304. - The
bias power controller 355 sets a set point forbias power supply 356 configured to supply an RF signal, tuned bybias match network 357, to achuck electrode 308 located within theplasma chamber 304 creating a direct current (DC) bias aboveelectrode 308 which is adapted to receive asubstrate 306, such as a semi-conductor wafer work piece, being processed. - A gas supply mechanism or
gas source 310 includes a source or sources of gas orgases 316 attached via agas manifold 317 to supply the proper chemistry required for the process to the interior of theplasma chamber 304. Agas exhaust mechanism 318 includes apressure control valve 319 andexhaust pump 320 and removes particles from within theplasma chamber 304 and maintains a particular pressure withinplasma chamber 304. - A
temperature controller 380 controls the temperature of a cooling recirculation system provided within thechuck electrode 308 by controlling acooling power supply 384. The plasma processing system also includeselectronic control circuitry 370. The plasma processing system may also have an end point detector. -
FIGS. 4A and 4B illustrate acomputer system 400, which is suitable for implementing a controller forcontrol circuitry 370 used in embodiments of the present invention.FIG. 4A shows one possible physical form of the computer system. Of course, the computer system may have many physical forms ranging from an integrated circuit, a printed circuit board, and a small handheld device up to a huge super computer.Computer system 400 includes amonitor 402, adisplay 404, ahousing 406, adisk drive 408, akeyboard 410, and amouse 412.Disk 414 is a computer-readable medium used to transfer data to and fromcomputer system 400. -
FIG. 4B is an example of a block diagram forcomputer system 400. Attached tosystem bus 420 is a wide variety of subsystems. Processor(s) 422 (also referred to as central processing units, or CPUs) are coupled to storage devices, includingmemory 424.Memory 424 includes random access memory (RAM) and read-only memory (ROM). As is well known in the art, ROM acts to transfer data and instructions uni-directionally to the CPU and RAM is used typically to transfer data and instructions in a bi-directional manner. Both of these types of memories may include any suitable of the computer-readable media described below. A fixeddisk 426 is also coupled bi-directionally toCPU 422; it provides additional data storage capacity and may also include any of the computer-readable media described below.Fixed disk 426 may be used to store programs, data, and the like and is typically a secondary storage medium (such as a hard disk) that is slower than primary storage. It will be appreciated that the information retained within fixeddisk 426 may, in appropriate cases, be incorporated in standard fashion as virtual memory inmemory 424.Removable disk 414 may take the form of any of the computer-readable media described below. -
CPU 422 is also coupled to a variety of input/output devices, such asdisplay 404,keyboard 410,mouse 412, andspeakers 430. In general, an input/output device may be any of: video displays, track balls, mice, keyboards, microphones, touch-sensitive displays, transducer card readers, magnetic or paper tape readers, tablets, styluses, voice or handwriting recognizers, biometrics readers, or other computers.CPU 422 optionally may be coupled to another computer or telecommunications network usingnetwork interface 440. With such a network interface, it is contemplated that the CPU might receive information from the network, or might output information to the network in the course of performing the above-described method steps. Furthermore, method embodiments of the present invention may execute solely uponCPU 422 or may execute over a network such as the Internet in conjunction with a remote CPU that shares a portion of the processing. - In addition, embodiments of the present invention further relate to computer storage products with a computer-readable medium that have computer code thereon for performing various computer-implemented operations. The media and computer code may be those specially designed and constructed for the purposes of the present invention, or they may be of the kind well known and available to those having skill in the computer software arts. Examples of tangible computer-readable media include, but are not limited to: magnetic media such as hard disks, floppy disks, and magnetic tape; optical media such as CD-ROMs and holographic devices; magneto-optical media such as floptical disks; and hardware devices that are specially configured to store and execute program code, such as application-specific integrated circuits (ASICs), programmable logic devices (PLDs) and ROM and RAM devices. Examples of computer code include machine code, such as produced by a compiler, and files containing higher level code that are executed by a computer using an interpreter. Computer readable media may also be computer code transmitted by a computer data signal embodied in a carrier wave and representing a sequence of instructions that are executable by a processor.
- The patterned
PR mask 220 is treated to reduce very low frequency line width roughness (step 104). This is accomplished by first flowing a treatment gas comprising H2 into the process chamber, where the treatment gas has a flow rate and the H2 has a flow rate that is at least 50% of the flow rate of the treatment gas. Preferably, the treatment gas consists essentially of H2 and Ar. More preferably, the treatment gas consists essentially of H2. The treatment is formed into a plasma using a low bias (step 112). Preferably, the bias voltage for the low bias is between 0 to 100 volts. More preferably, the bias voltage for the low bias is between 0 to 50 volts. Most preferably, the bias voltage for low bias is 0 volts. The flow of the treatment step is stopped (step 116), to end the PR mask treatment. - A specific example of a treatment recipe provides an H2 treatment gas of 100 sccm H2 and 100 sccm Ar at a pressure of 10 mT. Ranges of the treatment gas in this example recipe may provide 50-500 sccm H2 and 0-500 sccm Ar, at pressures between 2-40 mT. The power provided to form a plasma from the treatment gas is 200-1500 W at 13.56 MHz. More specifically, the power is 1000 W. The bias voltage is 0 volts. An electrostatic chuck temperature of 60° C. is provided. The treatment process is maintained for 5-60 seconds.
-
FIGS. 5A-F are CD-SEM (top-down) of wafers of various examples.FIG. 5A is a CD-SEM of a wafer before treatment. The CD of the wafer is 103.5 nm. The very low frequency LWR is 6.1 nm.FIG. 5B is the CD-SEM of the wafer ofFIG. 5A after the treatment process. The CD is 119.1 nm with a very low frequency LWR of 3.6 nm. Therefore, the very low LWR was reduced by the plasma treatment.FIG. 6A is a graph of the LWR reduction by the plasma treatment versus inspection length for the wafer ofFIG. 5B . The inspection length is related to the LWR frequency. -
FIG. 5C is a CD-SEM of another type of wafer before treatment. The CD of the wafer is 69.8 nm. The very low frequency LWR is 5.9 nm.FIG. 5D is the CD-SEM of the wafer ofFIG. 5C after the treatment process. The CD is 67.3 nm with a very low frequency LWR of 3.9 nm. Therefore, the very low LWR was reduced by the plasma treatment.FIG. 6B is a graph of the LWR reduction by the plasma treatment versus inspection length for the wafer ofFIG. 5D . -
FIG. 5E is a CD-SEM of another type of wafer before treatment. The CD of the wafer is 58.1 nm. The very low frequency LWR is 4.2 nm.FIG. 5F is the CD-SEM of the wafer ofFIG. 5E after the treatment process. The CD is 57.1 nm with a very low frequency LWR of 2.8 nm. Therefore, the very low LWR was reduced by the plasma treatment.FIG. 6C is a graph of the LWR reduction by the plasma treatment versus inspection length for the wafer ofFIG. 5F . - The
organic ARC layer 216 is then etched (step 120), using a conventional organic ARC open process based on the specific material of the etch layer.FIG. 2B is a schematic view of the stack after theorganic ARC layer 216 has been etched. Thehard mask layer 212 may be subsequently etched using the patternedPR mask 220 and/or theorganic ARC layer 216 as a patterned mask. Theconductive layer 208 may be etched using a conventional conductive layer etch, using thehard mask layer 212 as a patterned mask (step 128) During these process, the photoresist mask and organic ARC may be stripped away.FIG. 2C is a schematic view of the stack after theconductive layer 208 and thehard mask 212 have been etched, where the PR mask and organic ARC have been stripped away. Other processes may be used to further form semiconductor devices. The wafer is then removed from the inductively coupled TCP process chamber (step 132). Therefore, this example of the invention performs treatment to reduce very low frequency LWR, organic ARC open, hard mask open and conductive layer etch in situ in a single inductively coupled plasma process chamber. In this embodiment theorganic ARC layer 216 is the etch layer that is etched after the H2 treatment. - Without being bound by theory, it was thought that very low frequency line edge roughness with a repetition rate greater than 500 nm, preferably 550 nm, in a patterned photoresist mask could not be reduced. It was unexpectedly found that an H2 plasma treatment with low bias voltage would reduce very low frequency line width roughness.
- In other embodiments the H2 treatment to reduce very low frequency LWR may be performed on other patterned organic masks. For example, an organic ARC layer that has been opened using a conventional process may have very low frequency LWR. The H2 treatment may then be applied to the opened organic ARC layer to reduce the very low frequency LWR. In such an example, instead of the organic ARC layer being the etch layer, the hard mask layer is the etch layer that is etched subsequent to the H2 treatment.
- In other embodiment a high bias power may be used during the H2 treatment. In other embodiments the etch layer or other layers under the etch layer may be dielectric layers. Such embodiments may have an ARC layer or may not have an ARC layer or may have one or more additional layers. Such embodiments may or may not have a conductive layer and/or a hard mask layer. If the etch layer is a dielectric layer, an embodiment may use a capacitively coupled process chamber instead of an inductively coupled process chamber. In other embodiments, the treatment may be done in a different chamber than the etching.
- While this invention has been described in terms of several preferred embodiments, there are alterations, permutations, and various substitute equivalents, which fall within the scope of this invention. It should also be noted that there are many alternative ways of implementing the methods and apparatuses of the present invention. It is therefore intended that the following appended claims be interpreted as including all such alterations, permutations, and various substitute equivalents as fall within the true spirit and scope of the present invention.
Claims (18)
1. An apparatus for reducing very low frequency line width roughness (LWR) in forming etched features in an etch layer, disposed below a patterned organic mask with mask features, comprising:
a plasma processing chamber, comprising:
a chamber wall forming a plasma processing chamber enclosure;
a substrate support for supporting a wafer within the plasma processing chamber enclosure;
a pressure regulator for regulating the pressure in the plasma processing chamber enclosure;
at least one antenna for providing inductively coupled power to the plasma processing chamber enclosure for sustaining a plasma;
a gas inlet for providing gas into the plasma processing chamber enclosure; and
a gas outlet for exhausting gas from the plasma processing chamber enclosure;
a gas source in fluid connection with the gas inlet, comprising;
an etchant gas source; and
a H2 treatment gas source;
a controller controllably connected to the gas source and the at least one antenna, comprising:
at least one processor; and
computer readable media, comprising:
computer readable code for treating the patterned organic mask to reduce very low frequency line width roughness of the patterned organic mask, comprising:
computer readable code for flowing a treatment gas comprising H2, wherein the treatment gas has a flow rate and H2 has a flow rate that is at least 50% of the flow rate of the treatment gas;
computer readable code for forming a plasma from the treatment gas; and
computer readable code for stopping the flow of the treatment gas; and
computer readable code for etching the etch layer through the treated patterned organic mask with the reduced very low LWR.
2. The apparatus, as recited in claim 1 , wherein the computer readable code for forming a plasma comprises computer readable code for providing a low bias.
3. The apparatus, as recited in claim 2 , wherein the treatment gas is halogen free.
4. The apparatus, as recited in claim 2 , wherein the treatment gas consists essentially of Ar and H2.
5. The apparatus, as recited in claim 2 , wherein the treatment gas consists essentially of H2.
6. The apparatus, as recited in claim 5 , wherein the computer readable code for forming a plasma comprises computer readable code for using no more than 1500 watts of RF power.
7. The apparatus, as recited in claim 2 , wherein the low bias is between 0 to 100 volts.
8. The apparatus, as recited in claim 2 , wherein the low bias is between 0 to 50 volts.
9. The apparatus, as recited in claim 2 , wherein the low bias is 0 volts.
10. The apparatus, as recited in claim 1 , wherein the very low frequency LWR has a roughness repetition length of greater than 500 nm.
11. The apparatus, as recited in claim 10 , wherein the very low frequency LWR of the patterned organic mask after treatment is less than the very low frequency LWR before treatment.
12. The apparatus, as recited in claim 11 , further comprising:
computer readable code for placing a wafer with the etch layer and patterned organic mask in a process chamber before the treating the patterned organic mask; and
computer readable code for removing the wafer from the process chamber after etching the etch layer.
13. The apparatus, as recited in claim 12 , wherein the plasma processing chamber is an inductively coupled TCP process chamber.
14. The apparatus, as recited in claim 13 , wherein the organic mask is a photoresist mask.
15. The apparatus, as recited in claim 1 , wherein the treatment gas is halogen free.
16. The apparatus, as recited in claim 1 , wherein the treatment gas consists essentially of Ar and H2.
17. The apparatus for reducing very low frequency line width roughness (LWR) with a roughness repetition length of greater than 500 nm in forming etched features in an etch layer disposed below a patterned organic mask, wherein a hard mask layer is below the etch layer and a conductive layer is below the hard mask layer, comprising:
a plasma processing chamber, comprising:
a chamber wall forming a plasma processing chamber enclosure;
a substrate support for supporting a wafer within the plasma processing chamber enclosure;
a pressure regulator for regulating the pressure in the plasma processing chamber enclosure;
at least one antenna for providing inductively coupled power to the plasma processing chamber enclosure for sustaining a plasma;
a gas inlet for providing gas into the plasma processing chamber enclosure; and
a gas outlet for exhausting gas from the plasma processing chamber enclosure;
a gas source in fluid connection with the gas inlet, comprising;
an etchant gas source; and
a H2 treatment gas source;
a controller controllably connected to the gas source and the at least one antenna, comprising:
at least one processor; and
computer readable media, comprising:
computer readable code for treating the patterned organic mask to reduce very low frequency line width roughness with a roughness repetition length of greater than 500 nm of the patterned organic mask, comprising:
computer readable code for flowing a treatment gas comprising H2, wherein the treatment gas has a flow rate and H2 has a flow rate that is at least 50% of the flow rate of the treatment gas;
computer readable code for forming a plasma from the treatment gas;
computer readable code for stopping the flow of the treatment gas; and
computer readable code for etching the etch layer through the treated patterned organic mask with the reduced very low LWR;
computer readable code for etching the hard mask layer, and
computer readable code for etching the conductive layer, before removing the wafer from the process chamber, so that the treating the patterned organic mask, etching the etch layer, etching the hard mask layer, and etching the conductive layer are all done in situ in the same process chamber.
18. An apparatus for reducing very low frequency line width roughness (LWR) in forming etched features in a conductive layer disposed below a hard mask layer disposed below an ARC layer disposed below a patterned photoresist mask forming a stack on a wafer, comprising:
a plasma processing chamber, comprising:
a chamber wall forming a plasma processing chamber enclosure;
a substrate support for supporting a wafer within the plasma processing chamber enclosure;
a pressure regulator for regulating the pressure in the plasma processing chamber enclosure;
at least one antenna for providing inductively coupled power to the plasma processing chamber enclosure for sustaining a plasma;
a gas inlet for providing gas into the plasma processing chamber enclosure; and
a gas outlet for exhausting gas from the plasma processing chamber enclosure;
a gas source in fluid connection with the gas inlet, comprising;
an etchant gas source; and
a H2 treatment gas source;
a controller controllably connected to the gas source and the at least one antenna, comprising:
at least one processor; and
computer readable media, comprising:
computer readable code for placing the wafer in a process chamber;
computer readable code for treating the patterned photoresist mask to reduce very low frequency line width roughness of the patterned photoresist mask, comprising:
computer readable code for flowing a treatment gas comprising H2, wherein the treatment gas has a flow rate and H2 has a flow rate that is at least 50% of the flow rate of the treatment gas into the process chamber;
computer readable code for forming a plasma from the treatment gas; and
computer readable code for stopping the flow of the treatment gas;
computer readable code for etching the ARC layer through the treated patterned photoresist mask;
computer readable code for etching the hard mask layer through the ARC layer;
computer readable code for etching the conductive layer through the hard mask layer; and
computer readable code for removing the wafer from the process chamber, so that the treating the patterned organic mask, etching the ARC layer, etching the hard mask layer, and etching the conductive layer are all done in situ in the same process chamber.