US20130026507A1 - Multichip package structure and method of manufacturing the same - Google Patents
Multichip package structure and method of manufacturing the same Download PDFInfo
- Publication number
- US20130026507A1 US20130026507A1 US13/633,877 US201213633877A US2013026507A1 US 20130026507 A1 US20130026507 A1 US 20130026507A1 US 201213633877 A US201213633877 A US 201213633877A US 2013026507 A1 US2013026507 A1 US 2013026507A1
- Authority
- US
- United States
- Prior art keywords
- light
- surrounding
- semidrying
- reflecting frame
- substrate body
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Abstract
A method of manufacturing a multichip package structure includes: providing a substrate body; placing a plurality of light-emitting chips on the substrate body, where the light-emitting chips are electrically connected to the substrate body; surroundingly forming surrounding liquid colloid on the substrate body to surround the light-emitting chips; naturally drying an outer layer of the surrounding liquid colloid at a predetermined room temperature to form a semidrying surrounding light-reflecting frame, where the semidrying surrounding light-reflecting frame has a non-drying surrounding colloid body disposed on the substrate body and a dried surrounding colloid body totally covering the non-drying surrounding colloid body; and then forming a package colloid body on the substrate body to cover the light-emitting chips, where the semidrying surrounding light-reflecting frame contacts and surrounds the package colloid body.
Description
- This application is a Continuation-In-Part of pending U.S. patent application Ser. No. 12/557,462, filed on Sep. 10, 2009, and entitled “LED PACKAGE STRUCTURE FOR FORMING A STUFFED CONVEX LENS TO ADJUST LIGHT-PROJECTING ANGLE AND METHOD FOR MANUFACTURING THE SAME”, which claims priority of Taiwan Patent Application No. 098122751, filed on Jul. 6, 2009, the entirety of which is incorporated by reference herein.
- 1. Field of the Invention
- The instant disclosure relates to a multichip package structure and a method of manufacturing the same, in particular, to a multichip package structure for forming a stuffed convex lens to adjust the light-projecting angle thereof and a method for manufacturing the same.
- 2. Description of Related Art
- The invention of the lamp greatly changed the style of building construction and the living style of human beings, allowing people to work during the night. Without the invention of the lamp, we may stay in the living conditions of ancient civilizations.
- The LED lamp has a plurality of LED chips and a white frame surrounding the LED chips for increasing the light-emitting efficiency of the LED lamp. However, the white frame is manufactured by a prefabricated frame mold, thus the manufacturing cost is increased. In addition, when the shape of the white frame needs to be changed, the frame mold also needs to be changed according to the new shape of the white frame, thus the shape of the frame mold follows the shape of the white frame. Hence, when a new white frame is created for a new product, a new frame mold needs to be developed.
- One aspect of the instant disclosure relates to a multichip package structure and a method of manufacturing the same. The multichip package structure includes a semidrying surrounding light-reflecting frame formed without using any frame mold.
- One of the embodiments of the instant disclosure provides a multichip package structure, comprising: a substrate unit, a light-emitting unit, a frame unit and a package unit. The substrate unit includes a substrate body. The light-emitting unit includes a plurality of light-emitting chips disposed on the substrate body and electrically connected to the substrate body. The frame unit includes a semidrying surrounding light-reflecting frame surroundingly disposed on the substrate body, wherein the light-emitting chips are surrounded by the semidrying surrounding light-reflecting frame, and the semidrying surrounding light-reflecting frame has a non-drying surrounding colloid body disposed on the substrate body and a dried surrounding colloid body totally covering the non-drying surrounding colloid body. The package unit includes a package colloid body disposed on the substrate body to cover the light-emitting chips, wherein the semidrying surrounding light-reflecting frame contacts and surrounds the package colloid body.
- Another one of the embodiments of the instant disclosure provides a method of manufacturing a multichip package structure, comprising the steps of: providing a substrate body; placing a plurality of light-emitting chips on the substrate body, wherein the light-emitting chips are electrically connected to the substrate body; surroundingly forming surrounding liquid colloid on the substrate body to surround the light-emitting chips; naturally drying an outer layer of the surrounding liquid colloid at a predetermined room temperature to form a semidrying surrounding light-reflecting frame, wherein the semidrying surrounding light-reflecting frame has a non-drying surrounding colloid body disposed on the substrate body and a dried surrounding colloid body totally covering the non-drying surrounding colloid body; and then forming a package colloid body on the substrate body to cover the light-emitting chips, wherein the semidrying surrounding light-reflecting frame contacts and surrounds the package colloid body. Furthermore, after the step of forming the package colloid body, the method further comprises: solidifying the semidrying surrounding light-reflecting frame by natural drying at the predetermined room temperature or curing at a predetermined curing temperature to form a dried surrounding light-reflecting frame.
- Yet another one of the embodiments of the instant disclosure provides a method of manufacturing a multichip package structure, comprising the steps of: providing a substrate body; surroundingly forming surrounding liquid colloid on the substrate body; naturally drying an outer layer of the surrounding liquid colloid at a predetermined room temperature to form a semidrying surrounding light-reflecting frame, wherein the semidrying surrounding light-reflecting frame has a non-drying surrounding colloid body disposed on the substrate body and a dried surrounding colloid body totally covering the non-drying surrounding colloid body; placing a plurality of light-emitting chips on the substrate body, wherein the light-emitting chips are electrically connected to the substrate body and surrounded by the semidrying surrounding light-reflecting frame; and then forming a package colloid body on the substrate body to cover the light-emitting chips, wherein the semidrying surrounding light-reflecting frame contacts and surrounds the package colloid body. Furthermore, after the step of forming the package colloid body, the method further comprises: solidifying the semidrying surrounding light-reflecting frame by natural drying at the predetermined room temperature or curing at a predetermined curing temperature to form a dried surrounding light-reflecting frame.
- Moreover, the semidrying surrounding light-reflecting frame has a convex junction portion or a concave junction portion formed on the top surface thereof. The semidrying surrounding light-reflecting frame is extended from an initial point to a terminal point, and the position of the initial point and the position of the terminal point are substantially the same. The semidrying surrounding light-reflecting frame has an arc shape formed on the top surface thereof, the semidrying surrounding light-reflecting frame has a radius tangent and the angle of the radius tangent relative to the top surface of the substrate body is between 40° and 50°, the maximum height of the semidrying surrounding light-reflecting frame relative to the top surface of the substrate body is between 0.3 mm and 0.7 mm, the width of the bottom side of the semidrying surrounding light-reflecting frame is between 1.5 mm and 3 mm, the thixotropic index of the semidrying surrounding light-reflecting frame is between 4 and 6, and the semidrying surrounding light-reflecting frame is formed by mixing inorganic additive with white thermohardening colloid. The substrate unit includes a plurality of positive pads disposed on the top surface of the substrate body and a plurality of negative pads disposed on the top surface of the substrate body, wherein each light-emitting chip has a positive electrode and a negative electrode, the positive electrode of each light-emitting chip corresponds to at least two of the positive pads, and the negative electrode of each light-emitting chip corresponds to at least two of the negative pads. The positive electrode of each light-emitting chip is electrically connected to one of the two corresponding positive pads, and the negative electrode of each light-emitting chip is electrically connected to one of the two corresponding negative pads.
- Therefore, the semidrying surrounding light-reflecting frame can be formed on the substrate body without using any frame mold in the instant disclosure.
- To further understand the techniques, means and effects of the instant disclosure applied for achieving the prescribed objectives, the following detailed descriptions and appended drawings are hereby referred, such that, through which, the purposes, features and aspects of the instant disclosure can be thoroughly and concretely appreciated. However, the appended drawings are provided solely for reference and illustration, without any intention to limit the instant disclosure.
-
FIG. 1 shows a flowchart of the method of manufacturing a multichip package structure according to the first embodiment of the instant disclosure; -
FIG. 2A shows a perspective, schematic view of the step S100 according to the first embodiment of the instant disclosure; -
FIG. 2B shows a cross-sectional, schematic view of the step S100 according to the first embodiment of the instant disclosure; -
FIG. 3A shows a perspective, schematic view of the step S102 according to the first embodiment of the instant disclosure; -
FIG. 3B shows a cross-sectional, schematic view of the step S102 according to the first embodiment of the instant disclosure; -
FIG. 4A shows a perspective, schematic view of the step S104 according to the first embodiment of the instant disclosure; -
FIG. 4B shows a cross-sectional, schematic view of the step S104 according to the first embodiment of the instant disclosure; -
FIG. 5A shows a perspective, schematic view of the step S106 according to the first embodiment of the instant disclosure; -
FIG. 5B shows a cross-sectional, schematic view of the step S106 according to the first embodiment of the instant disclosure; -
FIG. 6A shows a perspective, schematic view of the step S108 according to the first embodiment of the instant disclosure; -
FIG. 6B shows a cross-sectional, schematic view of the step S108 according to the first embodiment of the instant disclosure; -
FIG. 7 shows a cross-sectional, schematic view of the step S110 according to the first embodiment of the instant disclosure; -
FIG. 8 shows a flowchart of the method of manufacturing a multichip package structure according to the second embodiment of the instant disclosure; -
FIG. 9A shows a cross-sectional, schematic view of the step S200 and S202 according to the second embodiment of the instant disclosure; -
FIG. 9B shows a cross-sectional, schematic view of the step S204 according to the second embodiment of the instant disclosure; -
FIG. 9C shows a cross-sectional, schematic view of the step S206 according to the second embodiment of the instant disclosure; -
FIG. 9D shows a cross-sectional, schematic view of the step S208 according to the second embodiment of the instant disclosure; -
FIG. 9E shows a cross-sectional, schematic view of the step S210 according to the second embodiment of the instant disclosure; -
FIG. 10 shows a partial, top, schematic view of using a plurality of standby pads according to the instant disclosure; -
FIG. 11 is a flowchart of the method of manufacturing a LED package structure according to the third embodiment of the instant disclosure; -
FIGS. 11A to 14B are schematic views of the LED package structure according to the third embodiment of the instant disclosure, at different stages of the packaging processes, respectively; -
FIG. 15 is a flowchart of the method of manufacturing a LED package structure according to the fourth embodiment of the instant disclosure; -
FIGS. 15A to 15C are schematic views of the LED package structure according to the fourth embodiment of the instant disclosure, at different stages of the packaging processes, respectively; -
FIG. 16A is a perspective, schematic view of the LED package structure according to the fifth embodiment of the instant disclosure; -
FIG. 16B is a cross-sectional, schematic view of the LED package structure according to the fifth embodiment of the instant disclosure; -
FIG. 17A is a perspective, schematic view of the LED package structure according to the sixth embodiment of the instant disclosure; and -
FIG. 17B is a cross-sectional, schematic view of the LED package structure according to the sixth embodiment of the instant disclosure. - Referring to
FIG. 1 toFIG. 7 , where the first embodiment of the instant disclosure provides a method of manufacturing a multichip package structure for increasing the light-emitting efficiency and the light-projecting angle. - Referring to
FIG. 1 , the method of manufacturing a multichip package structure of the first embodiment of the instant disclosure, comprising the steps of: providing a substrate body (S100); placing a plurality of light-emitting chips on the substrate body, wherein the light-emitting chips are electrically connected to the substrate body (S102); surroundingly forming surrounding liquid colloid on the substrate body to surround the light-emitting chips (S104); naturally drying an outer layer of the surrounding liquid colloid at a predetermined room temperature to form a semidrying surrounding light-reflecting frame, wherein the semidrying surrounding light-reflecting frame has a non-drying surrounding colloid body disposed on the substrate body and a dried surrounding colloid body totally covering the non-drying surrounding colloid body (S106); forming a package colloid body on the substrate body to cover the light-emitting chips, wherein the semidrying surrounding light-reflecting frame contacts and surrounds the package colloid body (S108); and then solidifying the semidrying surrounding light-reflecting frame by natural drying at the predetermined room temperature or curing at a predetermined curing temperature to form a dried surrounding light-reflecting frame (S110). - Referring to
FIGS. 1 , 2A and 2B, the method comprises: providing a substrate body 10 (step S100). For example, thesubstrate body 10 has a chip-mountingarea 11 disposed on the top surface thereof, and thesubstrate body 10 has acircuit substrate 100, a heat-dissipatinglayer 101 disposed on the bottom surface of thecircuit substrate 100, a plurality ofconductive pads 102 and a plurality of chip-mounting pads disposed on the top surface of thecircuit substrate 100, and an insulatinglayer 103 disposed on the top surface of thecircuit substrate 100 to expose theconductive pads 102. Hence, the heat-dissipating efficiency of thecircuit substrate 100 can be increased by using the heat-dissipatinglayer 101, and the insulatinglayer 103 may be a solder mask for only exposing theconductive pads 102. However, thesubstrate body 10 used in the first embodiment is merely an example and is not meant to limit the instant disclosure. - Referring to
FIGS. 1 , 3A and 3B, the method comprises: placing a plurality of light-emittingchips 20 on the substrate body 10 (step S102), where each light-emitting chip may be a LED chip, and the light-emittingchips 20 are disposed on the chip-mountingarea 11 and electrically connected to thesubstrate body 10. In other words, a predetermined chip-mountingarea 11 can be formed on thesubstrate body 10 in advance, thus the light-emittingchips 20 can be placed on the chip-mountingarea 11 of thesubstrate body 10 for electrically connecting to thesubstrate body 10. In the first embodiment, the light-emittingchips 20 can be electrically connected to thesubstrate body 10 by wire bonding. In addition, each chip-mounting pad is disposed between two correspondingconductive pads 102, and each light-emittingchip 20 is disposed each corresponding chip-mounting pad and electrically connected between two correspondingconductive pads 102. - Referring to
FIGS. 1 , 4A and 4B, the method comprises: surroundingly forming surrounding liquid colloid 30″ on thesubstrate body 10 to surround the light-emitting chips 20 (step S104), where the surrounding liquid colloid 30″ can be formed as a predetermined shape (such as a circular shape, a square or a rectangular shape etc.) on thesubstrate body 10 by coating according to different requirements. The thixotropic index of the surrounding liquid colloid 30″ may be between 4 and 6, the pressure of coating the surrounding liquid colloid 30″ on the top surface of thesubstrate body 10 may be between 350 kpa and 450 kpa, and the velocity of coating the surrounding liquid colloid 30″ on the top surface of thesubstrate body 10 may be between 5 mm/s and 15 mm/s. The surrounding liquid colloid 30″ can be surroundingly coated on the top surface of thesubstrate body 10 from an initial point to a terminal point, and the position of the initial point and the position of the terminal point are substantially the same. - Referring to
FIGS. 1 , 5A and 5B, the method comprises: naturally drying an outer layer of the surrounding liquid colloid 30″ at a predetermined room temperature (such as 25° or 20°˜30°) without any curing device to form a semidrying surrounding light-reflectingframe 30′, where the semidrying surrounding light-reflectingframe 30′ has a non-drying surroundingcolloid body 30A′ (such as surrounding liquid colloid that is not to be dried) disposed on thesubstrate body 10 and a dried surroundingcolloid body 30B′ (such as surrounding solidifying colloid that is dried) totally covering the non-drying surroundingcolloid body 30A′ (step S106). For example, the semidrying surrounding light-reflectingframe 30′ can be extended from an initial point to a terminal point, and the position of the initial point and the position of the terminal point are substantially the same, thus the semidrying surrounding light-reflectingframe 30′ has a convex orconcave junction portion 3000 formed on the top surface thereof. Moreover, the semidrying surrounding light-reflectingframe 30′ has an arc shape formed on the top surface thereof. The semidrying surrounding light-reflectingframe 30′ has a radius tangent T and the angle θ of the radius tangent T relative to the top surface of thesubstrate body 10 may be between 40° and 50°. The maximum height H of the semidrying surrounding light-reflectingframe 30′ relative to the top surface of thesubstrate body 10 may be between 0.3 mm and 0.7 mm, and the width D of the bottom side of the semidrying surrounding light-reflectingframe 30′ may be between 1.5 mm and 3 mm. The thixotropic index of the semidrying surrounding light-reflectingframe 30′ may be between 4 and 6, and the semidrying surrounding light-reflectingframe 30′ may be formed by mixing inorganic additive with white thermohardening colloid. In addition, the semidrying surrounding light-reflectingframe 30′ surrounds the light-emittingchips 20 to form a colloidposition limiting space 300 on the chip-mountingarea 11 of thesubstrate body 10. - Referring to
FIGS. 1 , 6A and 6B, the method comprises: forming apackage colloid body 40 on thesubstrate body 10 to cover the light-emittingchips 20, where the semidrying surrounding light-reflectingframe 30′ contacts and surrounds the package colloid body 40 (step S108). For example, thepackage colloid body 40 may be a light-transmitting resin body inside the colloidposition limiting space 300, and thepackage colloid body 40 has a convex top surface. - Hence, referring to
FIGS. 6A and 6B and the steps from S100 to S108, the first embodiment of the instant disclosure provides a multichip package structure for increasing the light-emitting efficiency and the light-projecting angle, comprising: asubstrate unit 1, a light-emittingunit 2, aframe unit 3 and a package unit 4. Thesubstrate unit 1 includes asubstrate body 10. The light-emittingunit 2 includes a plurality of light-emittingchips 20 disposed on thesubstrate body 10 and electrically connected to thesubstrate body 10. Theframe unit 3 includes a semidrying surrounding light-reflectingframe 30′ surroundingly disposed on thesubstrate body 10. The light-emittingchips 20 are surrounded by the semidrying surrounding light-reflectingframe 30′, and the semidrying surrounding light-reflectingframe 30′ has a non-drying surroundingcolloid body 30A′ disposed on thesubstrate body 10 and a dried surroundingcolloid body 30B′ totally covering the non-drying surroundingcolloid body 30A′. The package unit 4 includes apackage colloid body 40 disposed on thesubstrate body 10 to cover the light-emittingchips 20, and the semidrying surrounding light-reflectingframe 30′ contacts and surrounds thepackage colloid body 40. - Referring to
FIGS. 1 and 7 , after the step of forming the package colloid body 40 (the step S108), the method further comprises: solidifying the semidrying surrounding light-reflectingframe 30′ by natural drying at the predetermined room temperature or curing at a predetermined curing temperature to form a dried surrounding light-reflecting frame 30 (step S110). For example, in the first embodiment, each light-emittingchip 20 may be a blue LED chip, and thepackage colloid body 40 may be a phosphor resin body, thus blue light beams L1 generated by the light-emitting chips 20 (the blue LED chips) can pass through the package colloid body 40 (the phosphor resin body) to generate white light beams L2 that are similar to the light source generate by sun lamp. - In conclusion, when the position of the
package colloid body 40 can be limited in the colloidposition limiting space 300 by using the dried surrounding light-reflectingframe 30, the usage quantity of thepackage colloid body 40 can be controlled by the designer. In addition, the surface shape and the height of thepackage colloid body 40 can be adjusted by control the usage quantity of thepackage colloid body 40, thus light-projecting angle of the white light beams L2 can be adjusted by different surface shapes and heights of thepackage colloid body 40. Moreover, the blue light beams L1 generated by the light-emittingchips 20 can be reflected by an inner wall of the dried surrounding light-reflectingframe 30 in order to increase the light-emitting efficiency of the multichip package structure of the instant disclosure. In other words, the position of thepackage colloid body 40 such as the phosphor resin body can be limited inside the colloidposition limiting space 300 by using the dried surrounding light-reflectingframe 30, and the shape of thepackage colloid body 40 can be adjusted by using the dried surrounding light-reflectingframe 30, thus the light-emitting efficiency and the light-projecting angle of the multichip package structure of the instant disclosure can be increased. - Referring to
FIG. 8 andFIGS. 9A to 9E , where the second embodiment of the instant disclosure provides a method of manufacturing a multichip package structure for increasing the light-emitting efficiency and the light-projecting angle. - Referring to
FIG. 8 , the method of manufacturing a multichip package structure of the second embodiment of the instant disclosure, comprising the steps of: providing a substrate body (S200); surroundingly forming surrounding liquid colloid on the substrate body (S202); naturally drying an outer layer of the surrounding liquid colloid at a predetermined room temperature to form a semidrying surrounding light-reflecting frame, wherein the semidrying surrounding light-reflecting frame has a non-drying surrounding colloid body disposed on the substrate body and a dried surrounding colloid body totally covering the non-drying surrounding colloid body (S204); placing a plurality of light-emitting chips on the substrate body, wherein the light-emitting chips are electrically connected to the substrate body and surrounded by the semidrying surrounding light-reflecting frame (S206); forming a package colloid body on the substrate body to cover the light-emitting chips, wherein the semidrying surrounding light-reflecting frame contacts and surrounds the package colloid body (S208); and then solidifying the semidrying surrounding light-reflecting frame by natural drying at the predetermined room temperature or curing at a predetermined curing temperature to form a dried surrounding light-reflecting frame (S210). - Referring to
FIGS. 8 and 9A , the method comprises: providing a substrate body 10 (step S200). For example, thesubstrate body 10 has a chip-mounting area (not shown) disposed on the top surface thereof, and thesubstrate body 10 has acircuit substrate 100, a heat-dissipatinglayer 101 disposed on the bottom surface of thecircuit substrate 100, a plurality ofconductive pads 102 disposed on the top surface of thecircuit substrate 100, and an insulatinglayer 103 disposed on the top surface of thecircuit substrate 100 to expose theconductive pads 102. - Referring to
FIGS. 8 and 9B , the method comprises: surroundingly forming surrounding liquid colloid 30″ on the substrate body 10 (step S202), where the surrounding liquid colloid 30″ can be formed as a predetermined shape (such as a circular shape, a square or a rectangular shape etc.) on thesubstrate body 10 by coating according to different requirements. The surrounding liquid colloid 30″ can be surroundingly coated on the top surface of thesubstrate body 10 from an initial point to a terminal point, and the position of the initial point and the position of the terminal point are substantially the same. - Referring to
FIGS. 8 and 9B , the method comprises: naturally drying an outer layer of the surrounding liquid colloid 30″ at a predetermined room temperature (such as 25° or 20°˜30°) without any curing device to form a semidrying surrounding light-reflectingframe 30′, where the semidrying surrounding light-reflectingframe 30′ has a non-drying surroundingcolloid body 30A′ (such as surrounding liquid colloid that is not to be dried) disposed on thesubstrate body 10 and a dried surroundingcolloid body 30B′ (such as surrounding solidifying colloid that is dried) totally covering the non-drying surroundingcolloid body 30A′ (step S204). For example, the semidrying surrounding light-reflectingframe 30′ can be extended from an initial point to a terminal point, and the position of the initial point and the position of the terminal point are substantially the same, thus the semidrying surrounding light-reflectingframe 30′ has a convex or concave junction portion (not shown) formed on the top surface thereof. Moreover, the semidrying surrounding light-reflectingframe 30′ has an arc shape formed on the top surface thereof. The semidrying surrounding light-reflectingframe 30′ has a radius tangent T and the angle θ of the radius tangent T relative to the top surface of thesubstrate body 10 may be between 40° and 50°. The maximum height H of the semidrying surrounding light-reflectingframe 30′ relative to the top surface of thesubstrate body 10 may be between 0.3 mm and 0.7 mm, and the width D of the bottom side of the semidrying surrounding light-reflectingframe 30′ may be between 1.5 mm and 3 mm. The thixotropic index of the semidrying surrounding light-reflectingframe 30′ may be between 4 and 6, and the semidrying surrounding light-reflectingframe 30′ may be formed by mixing inorganic additive with white thermohardening colloid. In addition, the semidrying surrounding light-reflectingframe 30′ surrounds the light-emittingchips 20 to form a colloidposition limiting space 300 on the chip-mountingarea 11 of thesubstrate body 10. - Referring to
FIGS. 8 and 9C , the method comprises: placing a plurality of light-emittingchips 20 on thesubstrate body 10, where the light-emittingchips 20 are electrically connected to thesubstrate body 10 and surrounded by the semidrying surrounding light-reflectingframe 30′ (step S206). For example, each light-emitting chip may be a LED chip, and the light-emittingchips 20 can be electrically connected to thesubstrate body 10 by wire bonding. - Referring to
FIGS. 8 and 9D , the method comprises: forming apackage colloid body 40 on thesubstrate body 10 to cover the light-emittingchips 20, where the semidrying surrounding light-reflectingframe 30′ contacts and surrounds the package colloid body 40 (step S208). For example, thepackage colloid body 40 may be a light-transmitting resin body inside the colloidposition limiting space 300, and thepackage colloid body 40 has a convex top surface. - Hence, referring to
FIG. 9D and the steps from S200 to S208, the second embodiment of the instant disclosure provides a multichip package structure for increasing the light-emitting efficiency and the light-projecting angle, comprising: asubstrate unit 1, a light-emittingunit 2, aframe unit 3 and a package unit 4. Thesubstrate unit 1 includes asubstrate body 10. The light-emittingunit 2 includes a plurality of light-emittingchips 20 disposed on thesubstrate body 10 and electrically connected to thesubstrate body 10. Theframe unit 3 includes a semidrying surrounding light-reflectingframe 30′ surroundingly disposed on thesubstrate body 10. The light-emittingchips 20 are surrounded by the semidrying surrounding light-reflectingframe 30′, and the semidrying surrounding light-reflectingframe 30′ has a non-drying surroundingcolloid body 30A′ disposed on thesubstrate body 10 and a dried surroundingcolloid body 30B′ totally covering the non-drying surroundingcolloid body 30A′. The package unit 4 includes apackage colloid body 40 disposed on thesubstrate body 10 to cover the light-emittingchips 20, and the semidrying surrounding light-reflectingframe 30′ contacts and surrounds thepackage colloid body 40. - Referring to
FIGS. 8 and 9E , after the step of forming the package colloid body 40 (the step S208), the method further comprises: solidifying the semidrying surrounding light-reflectingframe 30′ by natural drying at the predetermined room temperature or curing at a predetermined curing temperature to form a dried surrounding light-reflecting frame 30 (step S210). For example, in the first embodiment, each light-emittingchip 20 may be a blue LED chip, and thepackage colloid body 40 may be a phosphor resin body, thus blue light beams L1 generated by the light-emitting chips 20 (the blue LED chips) can pass through the package colloid body 40 (the phosphor resin body) to generate white light beams L2 that are similar to the light source generate by sun lamp. - Referring to
FIG. 10 , thesubstrate unit 1 includes a plurality of positive pads P disposed on the top surface of thesubstrate body 10 and a plurality of negative pads N disposed on the top surface of thesubstrate body 10. For the scope defined by the imaginary line inFIG. 10 , each light-emittingchip 20 has a positive electrode 201 and a negative electrode 202, the positive electrode 201 of each light-emittingchip 20 corresponds to at least two of the positive pads P, and the negative electrode 202 of each light-emittingchip 20 corresponds to at least two of the negative pads N. In addition, the positive electrode 201 of each light-emittingchip 20 can be electrically connected to one of the two corresponding positive pads P by wire bonding, and the negative electrode 202 of each light-emittingchip 20 is electrically connected to one of the two corresponding negative pads N by wire bonding. - Referring to
FIG. 11 , the third embodiment of the instant disclosure provides a method of manufacturing a LED package structure for forming a stuffed convex lens to adjust light-projecting angle. The method includes: providing a substrate unit that has a substrate body and a chip-placing area disposed on a top surface of the substrate body; electrically arranging a plurality of LED chips on the chip-placing area of the substrate unit; surroundingly coating liquid resin on the top surface of the substrate body; hardening the liquid resin to form an annular reflecting resin body, and the annular reflecting resin body surrounding the LED chips that are disposed on the chip-placing area to form a resin position limiting space above the chip-placing area; cleaning an inner surface of the annular reflecting resin body to form a clean surface by plasma; and then forming a convex package resin body on the top surface of the substrate body in order to cover the LED chips (the convex package resin body is filled into the resin position limiting space, the convex package resin body has a peripheral surface tightly touched the clean surface of the annular reflecting resin body, the position and the volume of the convex package resin body is limited in the resin position limiting space, and the weight of the convex package resin body and the plane area of the resin position limiting space show a predetermined proportion). - Referring to FIGS. 11 and 11A-14B, the detail descriptions of the third embodiment of the instant disclosure are shown as follows:
- Referring to FIGS. 11 and 11A-11B (
FIG. 11B is a cross-section ofFIG. 11A ), the method includes providing a substrate unit 1 a that has asubstrate body 10 a and a chip-placingarea 11 a disposed on a top surface of thesubstrate body 10 a (step S300). In addition, thesubstrate body 10 a has acircuit substrate 100 a, a heat-dissipatinglayer 101 a disposed on a bottom surface of thecircuit substrate 100 a, a plurality ofconductive pads 102 a disposed on a top surface of thecircuit substrate 100 a, and aninsulative layer 103 a disposed on the top surface of thecircuit substrate 100 a in order to expose theconductive pads 102 a. Hence, the heat-dissipating efficiency of thecircuit substrate 100 a is increased by using the heat-dissipatinglayer 101 a, and theinsulative layer 103 a is a solder mask for exposing theconductive pads 102 a only in order to achieve local soldering. - However, the above-mentioned definition of the
substrate body 10 a does not limit the instant disclosure. Any types of substrate can be applied to the instant disclosure. For example, thesubstrate body 10 a can be a PCB (Printed Circuit Board), a flexible substrate, an aluminum substrate, a ceramic substrate, or a copper substrate. - Referring to FIGS. 11 and 12A-12B (
FIG. 12B is a cross-section ofFIG. 12A ), the method includes electrically arranging a plurality ofLED chips 20 a on the chip-placingarea 11 a of the substrate unit 1 a (step S302). In other words, designer can plan a predetermined chip-placingarea 11 a on the substrate unit 1 a in advance, so that the LED chips 20 a can be placed on the chip-placingarea 11 a of the substrate unit 1 a. In the third embodiment, the LED chips 20 a are electrically disposed on the chip-placingarea 11 a of the substrate unit 1 a by wire bonding. - Referring to FIGS. 11 and 13A-13B (
FIG. 13B is a cross-section ofFIG. 13A ), the method includes surroundingly coating liquid resin (not shown) on the top surface of thesubstrate body 10 a (step S304). In addition, the liquid resin can be coated on thesubstrate body 10 a by any shapes according to different requirements (such as a circular shape, a square or a rectangular shape etc.). The thixotropic index of the liquid resin is between 4 and 6, the pressure of coating the liquid resin on the top surface of thesubstrate body 10 a is between 350 kpa and 450 kpa, and the velocity of coating the liquid resin on the top surface of thesubstrate body 10 a is between 5 mm/s and 15 mm/s. The liquid resin is surroundingly coated on the top surface of thesubstrate body 10 a from a start point to a termination point, and the position of the start point and the position of the termination point are the same. Furthermore, after the step S304, the method includes hardening the liquid resin to form an annular reflectingresin body 30 a, and the annular reflectingresin body 30 a surrounding the LED chips 20 a that are disposed on the chip-placingarea 11 a to form a resinposition limiting space 300 a above the chip-placingarea 11 a (step S306). In addition, the liquid resin is hardened by baking (curing), the baking temperature is between 120° C. and 140° C., and the baking time is between 20 minute and 40 minute. - Moreover, the annular reflecting
resin body 30 a has an arc shape formed on a top surface thereof. The annular reflectingresin body 30 a has a radius tangent T, and the angle θ of the radius tangent T relative to the top surface of thesubstrate body 10 a is between 40° and 50°. The maximum height H of the annular reflectingresin body 30 a relative to the top surface of thesubstrate body 10 a is between 0.3 mm and 0.7 mm, and the width of a bottom side of the annular reflectingresin body 30 a is between 1.5 mm and 3 mm. The thixotropic index of the annular reflectingresin body 30 a is between 4 and 6. In addition, the resinposition limiting space 300 a has a cross section that can be a circular shape, an elliptical shape or a polygonal shape (such as a square or a rectangular shape etc). In the third embodiment, the cross section of the resinposition limiting space 300 a is a circular shape. - Referring to FIGS. 11 and 13A-13B (
FIG. 13B is a cross-section ofFIG. 13A ), the method includes cleaning an inner surface of the annular reflectingresin body 30 a to form a clean surface S by plasma (S308). - Referring to FIGS. 11 and 14A-14B (
FIG. 14B is a cross-section ofFIG. 14A ), the method includes forming a convexpackage resin body 40 a on the top surface of thesubstrate body 10 a in order to cover the LED chips 20 a; the convexpackage resin body 40 a is filled into the resinposition limiting space 300 a, the convexpackage resin body 40 a has a peripheral surface tightly touched the clean surface S of the annular reflectingresin body 30 a, the position and the volume of the convexpackage resin body 40 a is limited in the resinposition limiting space 300 a, and the weight of the convexpackage resin body 40 a and the plane area of the resinposition limiting space 300 a show a predetermined proportion (step S310). In addition, the annular reflectingresin body 30 a can be a white thermohardening reflecting body (opaque resin) mixed with inorganic additive, and the top surface of the convexpackage resin body 40 a is convex. The convexpackage resin body 40 a can be translucent or transparent. - Moreover, the viscosity of the convex
package resin body 40 a can be 900±200 cps (centipoises). The resinposition limiting space 300 a can be a circular form, a square or any shape. For example, when the resinposition limiting space 300 a is a circular form, the predetermined proportion of the weight of the convex package resin body and the plane area of the resin position limiting space is 0.5±0.05 g:572±0.5 mm2 or 1.5±0.05 g:1320±0.5 mm2. When the resinposition limiting space 300 a is a square, the predetermined proportion of the weight of the convex package resin body and the plane area of the resin position limiting space is 0.5±0.05 g:800±0.5 mm2. - In the third embodiment, each
LED chip 20 a can be a blue LED chip, and the convexpackage resin body 40 a can be a phosphor body. Hence, blue light beams L1 generated by the LED chips 20 a (the blue LED chips) can pass through the convexpackage resin body 40 a (the phosphor body) to generate white light beams L2 that are similar to the light source generate by sun lamp. - In other words, the convex
package resin body 40 a is limited in the resinposition limiting space 300 a by using the annular reflectingresin body 30 a in order to control the usage quantity of the convexpackage resin body 40 a. In addition, the surface shape and the height of the convexpackage resin body 40 a can be adjusted by control the usage quantity of the convexpackage resin body 40 a in order to light-projecting angles of the white light beams L2. Moreover, the blue light beams L1 generated by the LED chips 20 a can be reflected by an inner wall of the annular reflectingresin body 30 a in order to increase the light-emitting efficiency of the LED package structure of the instant disclosure. - Referring to
FIG. 15 , the fourth embodiment of the instant disclosure provides a method of manufacturing a LED package structure for forming a stuffed convex lens to adjust light-projecting angle. The method includes: providing a substrate unit that has a substrate body and a chip-placing area disposed on a top surface of the substrate body; surroundingly coating liquid resin on the top surface of the substrate body; hardening the liquid resin to form an annular reflecting resin body, and the annular reflecting resin body surrounding the LED chips that are disposed on the chip-placing area to form a resin position limiting space above the chip-placing area; cleaning an inner surface of the annular reflecting resin body to form a clean surface by plasma; electrically arranging a plurality of LED chips on the chip-placing area of the substrate unit; and then forming a convex package resin body on the top surface of the substrate body in order to cover the LED chips (the convex package resin body is filled into the resin position limiting space, the convex package resin body has a peripheral surface tightly touched the clean surface of the annular reflecting resin body, the position and the volume of the convex package resin body is limited in the resin position limiting space, and the weight of the convex package resin body and the plane area of the resin position limiting space show a predetermined proportion). - Referring to FIGS. 15 and 15A-15C, the detail descriptions of the fourth embodiment of the instant disclosure are shown as follows:
- Referring to
FIGS. 15 and 15A , the method includes providing asubstrate unit 1 b that has asubstrate body 10 b and a chip-placingarea 11 b disposed on a top surface of thesubstrate body 10 b (step S400). In addition, thesubstrate body 10 b has acircuit substrate 100 b, a heat-dissipatinglayer 101 b disposed on a bottom surface of thecircuit substrate 100 b, a plurality ofconductive pads 102 b disposed on a top surface of thecircuit substrate 100 b, and aninsulative layer 103 b disposed on the top surface of thecircuit substrate 100 b in order to expose theconductive pads 102 b. - Referring to
FIGS. 15 and 15A , the method includes surroundingly coating liquid resin (not shown) on the top surface of thesubstrate body 10 b (step S402). In addition, the liquid resin can be coated on thesubstrate body 10 b by any shapes according to different requirements (such as a circular shape, a square or a rectangular shape etc.). The thixotropic index of the liquid resin is between 4 and 6, the pressure of coating the liquid resin on the top surface of thesubstrate body 10 b is between 350 kpa and 450 kpa, and the velocity of coating the liquid resin on the top surface of thesubstrate body 10 b is between 5 mm/s and 15 mm/s. The liquid resin is surroundingly coated on the top surface of thesubstrate body 10 b from a start point to a termination point, and the position of the start point and the position of the termination point are the same. Furthermore, after the step S402, the method includes hardening the liquid resin to form an annular reflectingresin body 30 b, and the annular reflectingresin body 30 b surrounding the LED chips 20 b that are disposed on the chip-placingarea 11 b to form a resinposition limiting space 300 b above the chip-placingarea 11 b (step S404). In addition, the liquid resin is hardened by baking, the baking temperature is between 120° C. and 140° C., and the baking time is between 20 minute and 40 minute. - Moreover, the annular reflecting
resin body 30 b has an arc shape formed on a top surface thereof. The annular reflectingresin body 30 b has a radius tangent T, and the angle θ of the radius tangent T relative to the top surface of thesubstrate body 10 b is between 40° and 50°. The maximum height H of the annular reflectingresin body 30 b relative to the top surface of thesubstrate body 10 b is between 0.3 mm and 0.7 mm, and the width of a bottom side of the annular reflectingresin body 30 b is between 1.5 mm and 3 mm. The thixotropic index of the annular reflectingresin body 30 b is between 4 and 6. In addition, the resinposition limiting space 300 b has a cross section that can be a circular shape, an elliptical shape or a polygonal shape (such as a square or a rectangular shape etc). - Referring to
FIGS. 15 and 15A , the method includes cleaning an inner surface of the annular reflectingresin body 30 b to form a clean surface S by plasma (S406). - Referring to
FIGS. 15 and 15B , the method includes electrically arranging a plurality ofLED chips 20 b on the chip-placingarea 11 b of thesubstrate unit 1 b (step S408). In other words, designer can plan a predetermined chip-placingarea 11 b on thesubstrate unit 1 b in advance, so that the LED chips 20 b can be placed on the chip-placingarea 11 b of thesubstrate unit 1 b by wire bonding. - Of course, the steps of 5406 and 5408 can be reverse. In other words, firstly, the LED chips 20 b can be electrically disposed on the chip-placing
area 11 b of thesubstrate unit 1 b, and next the inner surface of the annular reflectingresin body 30 b is cleaned to form a clean surface S by plasma. - Referring to
FIGS. 15 and 15C , the method includes forming a convexpackage resin body 40 b on the top surface of thesubstrate body 10 b in order to cover the LED chips 20 b; the convexpackage resin body 40 b is filled into the resinposition limiting space 300 b, the convexpackage resin body 40 b has a peripheral surface tightly touched the clean surface S of the annular reflectingresin body 30 b, the position and the volume of the convexpackage resin body 40 b is limited in the resinposition limiting space 300 b, and the weight of the convexpackage resin body 40 b and the plane area of the resinposition limiting space 300 b show a predetermined proportion (step S410). In addition, the annular reflectingresin body 30 b can be a white thermohardening reflecting body (opaque resin) mixed with inorganic additive, and the top surface of the convexpackage resin body 40 b is convex. - Moreover, the viscosity of the convex
package resin body 40 a can be 900±200 cps (centipoises). The resinposition limiting space 300 a can be a circular form, a square or any shape. For example, when the resinposition limiting space 300 a is a circular form, the predetermined proportion of the weight of the convex package resin body and the plane area of the resin position limiting space is 0.5±0.05 g:572±0.5 mm2 or 1.5±0.05 g:1320±0.5 mm2. When the resinposition limiting space 300 a is a square, the predetermined proportion of the weight of the convex package resin body and the plane area of the resin position limiting space is 0.5±0.05 g:800±0.5 mm2. - In the fourth embodiment, each
LED chip 20 b can be a blue LED chip, and the convexpackage resin body 40 b can be a phosphor body. Hence, blue light beams L1 generated by the LED chips 20 b (the blue LED chips) can pass through the convexpackage resin body 40 b (the phosphor body) to generate white light beams L2 that are similar to the light source generate by sun lamp. - Hence, referring to
FIGS. 11 and 15 , the instant disclosure provides a method of manufacturing a LED package structure for forming a stuffed convex lens to adjust light-projecting angle, including: providing a substrate unit, and the substrate unit having a substrate body and a chip-placing area disposed on a top surface of the substrate body; and then selectively executing step (a) or (b). The step (a) is: electrically arranging a plurality of LED chips on the chip-placing area of the substrate unit, surroundingly coating liquid resin on the top surface of the substrate body, hardening the liquid resin to form an annular reflecting resin body, and then cleaning an inner surface of the annular reflecting resin body to form a clean surface by plasma. The step (b) is: surroundingly coating liquid resin on the top surface of the substrate body, hardening the liquid resin to form an annular reflecting resin body, cleaning an inner surface of the annular reflecting resin body to form a clean surface by plasma, and then electrically arranging a plurality of LED chips on the chip-placing area of the substrate unit. The annular reflecting resin body surrounds the LED chips that are disposed on the chip-placing area to form a resin position limiting space above the chip-placing area. Final, the method includes forming a convex package resin body on the top surface of the substrate body in order to cover the LED chips (the convex package resin body is filled into the resin position limiting space, the convex package resin body has a peripheral surface tightly touched the clean surface of the annular reflecting resin body, the position and the volume of the convex package resin body is limited in the resin position limiting space, and the weight of the convex package resin body and the plane area of the resin position limiting space show a predetermined proportion). - Furthermore, referring to
FIGS. 14A , 14B and 15C, the instant disclosure provides a LED package structure for forming a stuffed convex lens to adjust light-projecting angle by using the above-mentioned manufacturing method. The LED package structure includes a substrate unit (1 a, 1 b), a light-emitting unit (2 a, 2 b), a light-reflecting unit (3 a, 3 b) and a convex package unit (4 a, 4 b). - The substrate unit (1 a, 1 b) has a substrate body (10 a, 10 b) and a chip-placing area (11 a, 11 b) disposed on a top surface of the substrate body (10 a, 10 b). The light-emitting unit (2 a, 2 b) has a plurality of LED chips (20 a, 20 b) electrically disposed on the chip-placing area (11 a, 11 b).
- Moreover, the light-reflecting unit (3 a, 3 b) has an annular reflecting resin body (30 a, 30 b) surroundingly formed on the top surface of the substrate body (10 a, 10 b) by coating. The annular reflecting resin body (30 a, 30 b) surrounds the LED chips (20 a, 20 b) that are disposed on the chip-placing area (11 a, 11 b) to form a resin position limiting space (300 a, 300 b) above the chip-placing area (11 a, 11 b), and the annular reflecting resin body (3 a, 3 b) has an inner surface that has been cleaned by plasma to form a clean surface S.
- In addition, the convex package unit (4 a, 4 b) has a convex package resin body (40 a, 40 b) disposed on the top surface of the substrate body (10 a, 10 b) in order to cover the LED chips (20 a, 20 b). In addition, the convex package resin body (40 a, 40 b) is filled into the resin position limiting space (300 a, 300 b), the convex package resin body (40 a, 40 b) has a peripheral surface tightly touched the clean surface S of the annular reflecting resin body (30 a, 30 b), the position and the volume of the convex package resin body (40 a, 40 b) is limited in the resin position limiting space (300 a, 300 b), and the weight of the convex package resin body (40 a, 40 b) and the plane area of the resin position limiting space (300 a, 300 b) show a predetermined proportion.
- Furthermore, the substrate unit (1 a, 1 b) and the light-reflecting unit (3 a, 3 b) can be combined to form a LED package structure for forming a stuffed convex lens to adjust light-projecting angle. In other words, any types of light-emitting elements can be applied to the LED package structure.
- Referring to
FIGS. 16A and 16B , the difference between the fifth embodiment and the third and the fourth embodiments is that: in the fifth embodiment, the resinposition limiting space 300 d has a cross section as a square. Hence, the LED package structure of the fifth embodiment can generate a light-emitting area similar to a square. In other words, the cross-sectional area of the substrate unit 1 d is increased (the heat-dissipating area of the substrate unit 1 d is increased) in order to increase the heat-dissipating efficiency of the light-emittingunit 2 d. - Referring to
FIGS. 17A and 17B , the difference between the sixth embodiment and the third and the fourth embodiments is that: in the sixth embodiment, the resinposition limiting space 300 e has a cross section as a rectangular form. Hence, the LED package structure of the sixth embodiment can generate a light-emitting area similar to a long strip shape. In other words, the cross-sectional area of the substrate unit 1 e is increased (the heat-dissipating area of the substrate unit 1 e is increased) in order to increase the heat-dissipating efficiency of the light-emittingunit 2 e. - In conclusion, the semidrying surrounding light-reflecting
frame 30′ can be formed on thesubstrate body 10 without using any frame mold in the instant disclosure. Moreover, the instant disclosure can form an annular reflecting resin body (an annular white resin body) with any shapes by coating method. In addition, the position of a convex package resin body such as phosphor resin can be limited in the resin position limiting space by using the annular reflecting resin body, and the shape of the convex package resin body can be adjusted by using the annular reflecting resin body. Therefore, the instant disclosure can apply to increase light-emitting efficiency of LED chips and control light-projecting angle of LED chips. - In other words, the convex package resin body is limited in the resin position limiting space by using the annular reflecting resin body in order to control the usage quantity of the convex package resin body. In addition, the surface shape and the height of the convex package resin body can be adjusted by control the usage quantity of the convex package resin body in order to light-projecting angles of the white light beams. Moreover, the blue light beams generated by the LED chips can be reflected by an inner wall of the annular reflecting resin body in order to increase the light-emitting efficiency of the LED package structure of the instant disclosure.
- Moreover, the inner surface of the annular reflecting resin body is cleaned by plasma to form a clean surface, so that the peripheral surface can be tightly touched the clean surface of the annular reflecting resin body. In addition, the weight of the convex package resin body (40 a, 40 b) and the plane area of the resin position limiting space (300 a, 300 b) show a predetermined proportion.
- The above-mentioned descriptions merely represent the preferred embodiments of the instant disclosure, without any intention or ability to limit the scope of the instant disclosure which is fully described only within the following claims. Various equivalent changes, alterations or modifications based on the claims of instant disclosure are all, consequently, viewed as being embraced by the scope of the instant disclosure.
Claims (20)
1. A multichip package structure, comprising:
a substrate unit including a substrate body;
a light-emitting unit including a plurality of light-emitting chips disposed on the substrate body and electrically connected to the substrate body;
a frame unit including a semidrying surrounding light-reflecting frame surroundingly disposed on the substrate body, wherein the light-emitting chips are surrounded by the semidrying surrounding light-reflecting frame, and the semidrying surrounding light-reflecting frame has a non-drying surrounding colloid body disposed on the substrate body and a dried surrounding colloid body totally covering the non-drying surrounding colloid body; and
a package unit including a package colloid body disposed on the substrate body to cover the light-emitting chips, wherein the semidrying surrounding light-reflecting frame contacts and surrounds the package colloid body.
2. The multichip package structure of claim 1 , wherein the semidrying surrounding light-reflecting frame has a convex junction portion or a concave junction portion formed on the top surface thereof.
3. The multichip package structure of claim 1 , wherein the semidrying surrounding light-reflecting frame is extended from an initial point to a terminal point, and the position of the initial point and the position of the terminal point are substantially the same.
4. The multichip package structure of claim 1 , wherein the semidrying surrounding light-reflecting frame has an arc shape formed on the top surface thereof, the semidrying surrounding light-reflecting frame has a radius tangent and the angle of the radius tangent relative to the top surface of the substrate body is between 40° and 50°, the maximum height of the semidrying surrounding light-reflecting frame relative to the top surface of the substrate body is between 0.3 mm and 0.7 mm, the width of the bottom side of the semidrying surrounding light-reflecting frame is between 1.5 mm and 3 mm, the thixotropic index of the semidrying surrounding light-reflecting frame is between 4 and 6, and the semidrying surrounding light-reflecting frame is formed by mixing inorganic additive with white thermohardening colloid.
5. The multichip package structure of claim 1 , wherein the substrate unit includes a plurality of positive pads disposed on the top surface of the substrate body and a plurality of negative pads disposed on the top surface of the substrate body, wherein each light-emitting chip has a positive electrode and a negative electrode, the positive electrode of each light-emitting chip corresponds to at least two of the positive pads, and the negative electrode of each light-emitting chip corresponds to at least two of the negative pads.
6. The multichip package structure of claim 5 , wherein the positive electrode of each light-emitting chip is electrically connected to one of the two corresponding positive pads, and the negative electrode of each light-emitting chip is electrically connected to one of the two corresponding negative pads.
7. A method of manufacturing a multichip package structure, comprising the steps of:
providing a substrate body;
placing a plurality of light-emitting chips on the substrate body, wherein the light-emitting chips are electrically connected to the substrate body;
surroundingly forming surrounding liquid colloid on the substrate body to surround the light-emitting chips;
naturally drying an outer layer of the surrounding liquid colloid at a predetermined room temperature to form a semidrying surrounding light-reflecting frame, wherein the semidrying surrounding light-reflecting frame has a non-drying surrounding colloid body disposed on the substrate body and a dried surrounding colloid body totally covering the non-drying surrounding colloid body; and
forming a package colloid body on the substrate body to cover the light-emitting chips, wherein the semidrying surrounding light-reflecting frame contacts and surrounds the package colloid body.
8. The method of claim 7 , wherein after the step of forming the package colloid body, the method further comprises: solidifying the semidrying surrounding light-reflecting frame by natural drying at the predetermined room temperature or curing at a predetermined curing temperature to form a dried surrounding light-reflecting frame.
9. The method of claim 7 , wherein the semidrying surrounding light-reflecting frame has a convex junction portion or a concave junction portion formed on the top surface thereof.
10. The method of claim 7 , wherein the semidrying surrounding light-reflecting frame is extended from an initial point to a terminal point, and the position of the initial point and the position of the terminal point are substantially the same.
11. The method of claim 7 , wherein the semidrying surrounding light-reflecting frame has an arc shape formed on the top surface thereof, the semidrying surrounding light-reflecting frame has a radius tangent and the angle of the radius tangent relative to the top surface of the substrate body is between 40° and 50°, the maximum height of the semidrying surrounding light-reflecting frame relative to the top surface of the substrate body is between 0.3 mm and 0.7 mm, the width of the bottom side of the semidrying surrounding light-reflecting frame is between 1.5 mm and 3 mm, the thixotropic index of the semidrying surrounding light-reflecting frame is between 4 and 6, and the semidrying surrounding light-reflecting frame is formed by mixing inorganic additive with white thermohardening colloid.
12. The method of claim 7 , wherein the substrate unit includes a plurality of positive pads disposed on the top surface of the substrate body and a plurality of negative pads disposed on the top surface of the substrate body, wherein each light-emitting chip has a positive electrode and a negative electrode, the positive electrode of each light-emitting chip corresponds to at least two of the positive pads, and the negative electrode of each light-emitting chip corresponds to at least two of the negative pads.
13. The method of claim 12 , wherein the positive electrode of each light-emitting chip is electrically connected to one of the two corresponding positive pads, and the negative electrode of each light-emitting chip is electrically connected to one of the two corresponding negative pads.
14. A method of manufacturing a multichip package structure, comprising the steps of:
providing a substrate body;
surroundingly forming surrounding liquid colloid on the substrate body;
naturally drying an outer layer of the surrounding liquid colloid at a predetermined room temperature to form a semidrying surrounding light-reflecting frame, wherein the semidrying surrounding light-reflecting frame has a non-drying surrounding colloid body disposed on the substrate body and a dried surrounding colloid body totally covering the non-drying surrounding colloid body;
placing a plurality of light-emitting chips on the substrate body, wherein the light-emitting chips are electrically connected to the substrate body and surrounded by the semidrying surrounding light-reflecting frame; and
forming a package colloid body on the substrate body to cover the light-emitting chips, wherein the semidrying surrounding light-reflecting frame contacts and surrounds the package colloid body.
15. The method of claim 14 , wherein after the step of forming the package colloid body, the method further comprises: solidifying the semidrying surrounding light-reflecting frame by natural drying at the predetermined room temperature or curing at a predetermined curing temperature to form a dried surrounding light-reflecting frame.
16. The method of claim 14 , wherein the semidrying surrounding light-reflecting frame has a convex junction portion or a concave junction portion formed on the top surface thereof.
17. The method of claim 14 , wherein the semidrying surrounding light-reflecting frame is extended from an initial point to a terminal point, and the position of the initial point and the position of the terminal point are substantially the same.
18. The method of claim 14 , wherein the semidrying surrounding light-reflecting frame has an arc shape formed on the top surface thereof, the semidrying surrounding light-reflecting frame has a radius tangent and the angle of the radius tangent relative to the top surface of the substrate body is between 40° and 50°, the maximum height of the semidrying surrounding light-reflecting frame relative to the top surface of the substrate body is between 0.3 mm and 0.7 mm, the width of the bottom side of the semidrying surrounding light-reflecting frame is between 1.5 mm and 3 mm, the thixotropic index of the semidrying surrounding light-reflecting frame is between 4 and 6, and the semidrying surrounding light-reflecting frame is formed by mixing inorganic additive with white thermohardening colloid.
19. The method of claim 14 , wherein the substrate unit includes a plurality of positive pads disposed on the top surface of the substrate body and a plurality of negative pads disposed on the top surface of the substrate body, wherein each light-emitting chip has a positive electrode and a negative electrode, the positive electrode of each light-emitting chip corresponds to at least two of the positive pads, and the negative electrode of each light-emitting chip corresponds to at least two of the negative pads.
20. The method of claim 19 , wherein the positive electrode of each light-emitting chip is electrically connected to one of the two corresponding positive pads, and the negative electrode of each light-emitting chip is electrically connected to one of the two corresponding negative pads.