UA88527C2 - method of production of rolled wire on continuous wire mill - Google Patents
method of production of rolled wire on continuous wire millInfo
- Publication number
- UA88527C2 UA88527C2 UAA200713449A UAA200713449A UA88527C2 UA 88527 C2 UA88527 C2 UA 88527C2 UA A200713449 A UAA200713449 A UA A200713449A UA A200713449 A UAA200713449 A UA A200713449A UA 88527 C2 UA88527 C2 UA 88527C2
- Authority
- UA
- Ukraine
- Prior art keywords
- breakdown
- rolling
- mill
- water cooling
- temperature
- Prior art date
Abstract
The invention relates to rolling engineering, namely to the methods of production of the rolled wire on the high-speed continuous wire mills. A method includes heating billets in a continuous heating furnace to the temperature of 1050… 1150 °C, subsequent rolling with alternation of the direction of reduction for 90° in roughing, run-down and finishing groups of block type stands, water cooling of the surface of breakdown before and behind of the finishing group of stands of block type with obtaining before subsequent air cooling on the roller conveyor of a rolled wire with surface temperature, which makes 750… 1050 °C. In the finishing group of block type stands additional stepped water cooling of the surface of breakdown is carried out in the lines of water cooling, which length is proportional to the maximum speed of rolling on the mill and makes at the first and second stage 0.08·Vmax and 0.07· Vmax respectively, under the pressure of cooling water 10… 12 bars. The temperature of the surface of breakdown after additional stepped water cooling at the first stage is maintained at the level of 670… 680 °C, and at the second stage - 520… 530 °C. The invention provides possibility of organizing thermomechanical treatment of the rolled wire in the production line of mill due to rolling in the range of temperatures of 750… 1050 °C with a gradient of temperature over the section of breakdown at the outlet from the mill of 50… 70 °C, which ensures increase of consumer properties of the finished products.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| UAA200713449A UA88527C2 (en) | 2007-12-03 | 2007-12-03 | method of production of rolled wire on continuous wire mill |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| UAA200713449A UA88527C2 (en) | 2007-12-03 | 2007-12-03 | method of production of rolled wire on continuous wire mill |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| UA88527C2 true UA88527C2 (en) | 2009-10-26 |
Family
ID=50637043
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| UAA200713449A UA88527C2 (en) | 2007-12-03 | 2007-12-03 | method of production of rolled wire on continuous wire mill |
Country Status (1)
| Country | Link |
|---|---|
| UA (1) | UA88527C2 (en) |
-
2007
- 2007-12-03 UA UAA200713449A patent/UA88527C2/en unknown
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN102387874B (en) | Method and device for preparing hot-rolling stock | |
| KR102018370B1 (en) | Process and apparatus for preparing steel stock before hot rolling | |
| CN109890524B (en) | Method for producing a metal strip in a casting and rolling plant | |
| RU2008122938A (en) | METHOD FOR PRODUCING HOT-STEEL STEEL STRIP AND COMBINED PLANT FOR IMPLEMENTING THIS METHOD | |
| CN108994078A (en) | A kind of middle bar controlled rolling and controlled cooling method | |
| RU2537629C2 (en) | Method and machine for metal strip ingot-less rolling | |
| CN111036693B (en) | Rolling force energy checking and calculating method for hot-rolled high-speed wire rod | |
| CN104259199A (en) | Rolling technology for stainless steel wire rod | |
| RU2526644C2 (en) | Steel strip hot rolling and rolling mill to this end | |
| WO2011018217A3 (en) | Device and method for producing a thin hot-rolled strip | |
| UA107981C2 (en) | Method for producing a metal strip by continuous rolling or semi-rolling | |
| UA109012C2 (en) | Apparatus and method for production of metal elongated products | |
| RU2381847C1 (en) | Method and relates to it installation for manufacturing of steel strips with discontinuity | |
| CN101618406A (en) | A method for controlling surface color difference of hot-rolled pickled sheet | |
| ES2176042T3 (en) | METHOD AND APPLIANCE TO PRODUCE ROUND BARS. | |
| CA2611396A1 (en) | Process and related plant for manufacturing steel long products without interruption | |
| RU2344889C1 (en) | Method of casting with further rolling, when high speeds of casting are provided, and further hot rolling of relatively thin metal stocks, in particular, steel ones, and suitable device | |
| CN101748256A (en) | Rolling and solution treatment method for 304 stainless strip steel | |
| UA88527C2 (en) | method of production of rolled wire on continuous wire mill | |
| CN110883107B (en) | Rolling force energy checking and calculating method for common hot-rolled bar | |
| CN105473247A (en) | Casting and rolling plant and method for producing slabs | |
| CN101862750B (en) | A kind of production method of titanium or titanium alloy T profile | |
| CN103042055B (en) | Hot-rolled billet steel rough-rolling descaling method | |
| CN102145349A (en) | Method for stably controlling finish rolling temperature of oriented silicon steel | |
| CN204503752U (en) | Torrid zone continuous casting and rolling Heat treating machine set |