UA84102C2 - Способ наращивания гарнисажа в руднотермической печи - Google Patents
Способ наращивания гарнисажа в руднотермической печиInfo
- Publication number
- UA84102C2 UA84102C2 UAA200710013A UAA200710013A UA84102C2 UA 84102 C2 UA84102 C2 UA 84102C2 UA A200710013 A UAA200710013 A UA A200710013A UA A200710013 A UAA200710013 A UA A200710013A UA 84102 C2 UA84102 C2 UA 84102C2
- Authority
- UA
- Ukraine
- Prior art keywords
- skull
- furnace
- ore
- growing
- thermal furnace
- Prior art date
Abstract
Изобретение относится к цветной металлургии, а именно к способу наращивания гарнисажа в руднотермической печи. Способ наращивания гарнисажа в руднотермической печи включает загрузку на голый под на каждый метр диаметра печи титанового шлака в количестве 10-12 т и мелкого железного лома в количестве 9-10 т, потом загрузку железотитанового концентрата и восстановителя, содержание которого 7-12 % от общей массы шихты, до уровня летки руднотермической печи порциями от 0,4-0,5 т до 1,0-1,5 т на каждый метр диaметра печи, интервал между загрузками определяется затратой электроэнергии 1,2-1,5 тыс. кВт/т шихты, расплавление и доводка ее присадкой восстановителя до со�
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| UAA200710013A UA84102C2 (ru) | 2007-09-07 | 2007-09-07 | Способ наращивания гарнисажа в руднотермической печи |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| UAA200710013A UA84102C2 (ru) | 2007-09-07 | 2007-09-07 | Способ наращивания гарнисажа в руднотермической печи |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| UA84102C2 true UA84102C2 (ru) | 2008-09-10 |
Family
ID=50724266
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| UAA200710013A UA84102C2 (ru) | 2007-09-07 | 2007-09-07 | Способ наращивания гарнисажа в руднотермической печи |
Country Status (1)
| Country | Link |
|---|---|
| UA (1) | UA84102C2 (ru) |
-
2007
- 2007-09-07 UA UAA200710013A patent/UA84102C2/ru unknown
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Emi | Steelmaking technology for the last 100 years: toward highly efficient mass production systems for high quality steels | |
| CN104611502B (zh) | 一种含铝含硫系列齿轮钢冶炼工艺 | |
| MX2012013486A (es) | Metodo para controlar ti extremadamente bajo en acero con alsi reposado extra bajo en carbono. | |
| CN103627853A (zh) | 一种低碳低硅钢制造方法 | |
| CN102828098A (zh) | 一种炉外加锰矿提高钢水终点锰含量的方法 | |
| CN105018855B (zh) | 一种油气集输用抗硫管线钢圆坯的生产方法 | |
| CN101962700A (zh) | 使用半钢冶炼低磷钢水的方法 | |
| Conejo et al. | Recycling MgO-C refractory in electric arc furnaces | |
| CN102994871A (zh) | 一种使用含钒钛铁水冶炼中高碳硬线用钢的方法 | |
| CN103014241A (zh) | 一种lf炉sphd钢冶炼渣的控制方法 | |
| CN103643056B (zh) | 低碳锰铁的冶炼方法 | |
| CN105331776B (zh) | 一种超低碳高铝钢的钙处理方法 | |
| MXPA01011628A (es) | Metodo para la reduccion de contenido de metal no ferroso en la escoria en la produccion de metales no ferrosos que se presentan en un horno de fusion en suspension. | |
| CN101476019A (zh) | 微铝的硅钡钙镁复合合金 | |
| UA84102C2 (ru) | Способ наращивания гарнисажа в руднотермической печи | |
| CN104263875A (zh) | 一种顶吹转炉采用高磷铁水生产合金焊线钢的脱磷方法 | |
| CN104651704A (zh) | 低硅孕育剂 | |
| CN102212650A (zh) | 一种低碳低硅铝镇静钢中氧的控制方法 | |
| CN101962704B (zh) | 一种采用特定芯粉配方喂线生产低磷低硫微碳及低碳锰硅合金的方法 | |
| RU2145356C1 (ru) | Способ конвертерной плавки с использованием металлизованных материалов | |
| CN102758058B (zh) | 一种炼钢用硅锰粉煤灰脱氧剂及其制备方法 | |
| CN101597668A (zh) | 一种利用顶底复吹转炉的铁水脱磷处理方法 | |
| CN202885551U (zh) | 冶金炉虹吸放渣装置 | |
| CN101603105A (zh) | 一种高炉炼铁虹吸出铁装置 | |
| CN102816887A (zh) | 一种转炉直接冶炼高钛铁水的方法 |