[go: up one dir, main page]

TWI314899B - Protective film - Google Patents

Protective film Download PDF

Info

Publication number
TWI314899B
TWI314899B TW94145175A TW94145175A TWI314899B TW I314899 B TWI314899 B TW I314899B TW 94145175 A TW94145175 A TW 94145175A TW 94145175 A TW94145175 A TW 94145175A TW I314899 B TWI314899 B TW I314899B
Authority
TW
Taiwan
Prior art keywords
layer
scratch
protective film
group
glare
Prior art date
Application number
TW94145175A
Other languages
Chinese (zh)
Other versions
TW200724381A (en
Inventor
Yu Sheng Teng
Original Assignee
Univacco Technology Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Univacco Technology Inc filed Critical Univacco Technology Inc
Priority to TW94145175A priority Critical patent/TWI314899B/en
Publication of TW200724381A publication Critical patent/TW200724381A/en
Application granted granted Critical
Publication of TWI314899B publication Critical patent/TWI314899B/en

Description

1314899 九、發明說明: 【發明所屬之技術領域】 本發明係關於一種保護膜,尤指一種防刮、防眩及防 止油污污染之保護膜’該基材向上逐層設有防刮抗眩層及 抗污層’膝黏層設於基材下方以供黏貼吸附,防刮與眩屬 添加金屬乳化物尽高分子粒子以提高與抗污層之連結,且 控制霧度(Haze)於0. 2%~309ί間。 【先前技術】 按,隨著科技技術日新月異,傳統電子產品逐漸被重 量輕、體積小之新式電子產品所取代,特別是螢幕形態逐 漸以液晶勞幕或電漿螢幕為主’具有重量輕、體積縮小、 無輻射及亮度高之優點。 由於許多隨身型電子產品使用液晶螢幕,例如手機、 PDA、MP3隨身聽…等等,在走動或置放時,難免會有碰撞 或接觸’使得螢幕表面受傷之機率大增,為了防止螢幕表 面被刮傷,一般會於表面貼附保護膜結構,不僅出廠前保 持原狀與美觀,使用時,保護膜可防止濺濕、防眩光或刮 傷。 請參閱第三圖所示,現有結構之保護膜(9)包含基材 (91)、防刮層(92)及膠黏層(93),防到層(92)設於基材(91) 上,其具有一定厚度及硬度,可抵抗撞擊及刮傷,膠黏層 (93) 設於基材(91)下方以供黏貼吸附用,例如吸附於液晶 螢幕、玻璃表面。 然而,防刮層(92)僅能提供部分防撞、防刮之功能, 且所使用之材質具有親水性,故對水接觸角心較小,當水 (94) 或液體、油污潑濺到保護膜(9)上,或者是汗水、指紋 1314899 之附著,即使甩動或擦拭,也不易將完全弄乾,長期下來, 將造成保護膜(9)貼附之電子產品受潮而損壞,或是保護骐 (9)被弄污後,不易擦拭乾淨,使得產品外觀骯髒、影響 覺效果。 緣此,本案之發明人累積多年設計製造之經驗,經不 斷w考、製造及修正,遂有本發明之誕生以解決上述問 【發明内容】1314899 IX. Description of the Invention: [Technical Field] The present invention relates to a protective film, in particular to a protective film which is scratch-resistant, anti-glare and oil-stain-resistant. The substrate is provided with a scratch-resistant anti-glare layer layer by layer. And the anti-fouling layer 'knee adhesive layer is set under the substrate for adhesive adsorption, anti-scratch and sorrow are added metal emulsion to make polymer particles to improve the connection with the anti-fouling layer, and control the haze (Haze) at 0. 2%~309ί. [Prior Art] According to the rapid development of technology, traditional electronic products have gradually been replaced by newer electronic products that are lighter in weight and smaller in size. In particular, the screen form is gradually dominated by LCD screens or plasma screens. Reduced, no radiation and high brightness. Since many portable electronic products use LCD screens, such as mobile phones, PDAs, MP3 players, etc., when moving or placing, it is inevitable that there will be collision or contact, which will increase the chance of screen surface damage, in order to prevent the screen surface from being damaged. Scratch, generally attached to the surface of the protective film structure, not only maintain the original shape and aesthetics before leaving the factory, when used, the protective film can prevent splashing, anti-glare or scratch. Referring to the third figure, the protective film (9) of the prior structure comprises a substrate (91), a scratch-resistant layer (92) and an adhesive layer (93), and the anti-layer (92) is provided on the substrate (91). The upper layer has a certain thickness and hardness and is resistant to impact and scratches. The adhesive layer (93) is disposed under the substrate (91) for adhesion and adsorption, for example, to the liquid crystal screen or the glass surface. However, the scratch-resistant layer (92) can only provide partial anti-collision and anti-scratch functions, and the material used is hydrophilic, so the contact angle to the water is small, when water (94) or liquid or oil splashes. On the protective film (9), or the adhesion of sweat and fingerprint 1314899, even if it is shaken or wiped, it is not easy to dry completely. In the long run, the electronic product attached to the protective film (9) will be damaged by moisture, or After the protective 骐 (9) is stained, it is not easy to wipe clean, which makes the appearance of the product dirty and affects the effect. Therefore, the inventor of the present case has accumulated many years of experience in designing and manufacturing, and has been diagnosed and manufactured by the inventor, and has been born to solve the above problems.

一本發明之主要目的係提供一種保護膜,其具有更佳之 /由污保護效果,不僅不易沾污,且更容易擦拭清潔。 本發明之另-目的係提供—種保㈣,其提供防刮抗 眩功能,使保護臈之反射率降低,並提高透光率。 為了達到上述目的,本發明之保護膜包含基材、防刮 j層、抗污層及膠黏層’防刮抗眩層設於基材上且具有 疋程度之硬度及可降低光線反射,抗污層設於防刮抗眩 ^思抗污層内含氟化物且對水接觸角大,防刮抗眩層内 :金屬氧化物及高分子粒子,以增加與抗污層之連結程 度,膠黏層設於基材下方以供黏貼。 【實施方式】 本發明所運用之技術内容、發明目的及其達成之 有更完整且清楚的揭露’兹於下詳細制之,並請一 併參閱所揭之圖式及圖號: 及—圖所示,其為本發明保護膜⑴,其包含 到抗眩層〇2)、抗污層03)及勝黏層(⑷, 齡护rpr)取之材料係為聚對笨二甲酸乙二醇酯(PET)、聚碳 win..n"甲基丙稀酸甲醋(PMMA)或聚乙稀環烧酸鹽 或其他適當之材料,防刮抗眩層(12)設於 1314899 【圖式簡單說明】 第一圖:本發明之刮視圖 第二圖:本發明之應用示意圖 第三圖:現有結構之剖視圖 【主要元件符號說明】 <本發明> (1) 保護膜 (11) 基材 (12) 防刮抗眩層 (13) 抗污層 (14) 膠黏層 (15) 離形層 (2) 液晶螢幕 Θ 2 對水接觸角 <現有技術> (9) 保護膜 (91) 基材 (92) 防刮層 (93) 膠黏層 (94) 水 Θ 1 對水接觸角 10A primary object of the present invention is to provide a protective film which has a better/staining protection effect, is not only less susceptible to staining, and is easier to wipe clean. Another object of the present invention is to provide a type of protection (4) which provides a scratch and anti-glare function, which reduces the reflectance of the protective enamel and increases the light transmittance. In order to achieve the above object, the protective film of the present invention comprises a substrate, a scratch-resistant layer, an anti-staining layer and an adhesive layer. The scratch-resistant anti-glare layer is provided on the substrate and has a hardness of a certain degree and can reduce light reflection and resistance. The stain layer is provided in the anti-scratch and anti-glare anti-fouling layer containing fluoride and has a large contact angle with water, and the anti-scratch and anti-glare layer: metal oxide and polymer particles to increase the degree of connection with the anti-fouling layer, the glue The adhesive layer is placed under the substrate for adhesion. DETAILED DESCRIPTION OF THE INVENTION The technical content, the object of the invention and the accomplishment of the present invention are more fully and clearly disclosed. Please refer to the drawings and drawings. As shown, it is the protective film (1) of the present invention, which comprises the anti-glare layer 〇 2), the anti-staining layer 03) and the smear layer ((4), the age guard rpr). The material is polyethylene terephthalate. Ester (PET), polycarbon win..n" methyl methacrylate methyl vinegar (PMMA) or polyethylene ring oxylate or other suitable material, scratch-resistant anti-glare layer (12) is set at 1314899 BRIEF DESCRIPTION OF THE DRAWINGS First: Scratch view of the present invention Second view: Schematic diagram of application of the present invention Third drawing: Cross-sectional view of the prior art [Description of main components] <The present invention> (1) Protective film (11) base Material (12) Scratch and anti-glare layer (13) Anti-fouling layer (14) Adhesive layer (15) Release layer (2) Liquid crystal screen Θ 2 Water contact angle <Priority> (9) Protective film ( 91) Substrate (92) Scratch resistant layer (93) Adhesive layer (94) Water raft 1 Pair of water contact angle 10

Claims (1)

13148991314899 申請專利範圍:Patent application scope: 1· 一種保護膜,其包含基材、防刮抗眩層、抗污層及膠黏 層,防刮抗眩層設於基材上,抗污層設於防刮抗眩層 上,膠黏層設於基材下方以供黏貼吸附;其中,該基材 係選自聚對苯二曱酸乙二醇酯(PET)、聚碳酸酯(pc)、 聚甲基丙烯酸甲酯(PMMA)或聚乙烯環烷酸鹽(pen)所組 成之群組之至少一聚合物;防刮抗眩層之成份包括UV 硬化型樹脂及混合其中之高分子粒子;該抗污層内含氟 化物;該膠黏層之材質係選自壓克力、矽利康(silicon) 或橡膠所組成之群組之至少一種材質。 2.如申請專利範圍第1項所述之保護膜,其中膠黏層下貼 附有離形層,以供撕離後膠黏層貼附於物體上,該離形 層之材質係選自聚酉旨、聚丙稀、聚乙浠或紙中之其中一 種材質。 3.如申請專利範圍第1項所述之保護膜,其中抗污層對水 接觸角介於90至120度。1 . A protective film comprising a substrate, a scratch-resistant anti-glare layer, an anti-fouling layer and an adhesive layer, the anti-scratch and anti-glare layer is disposed on the substrate, and the anti-fouling layer is disposed on the anti-scratch and anti-glare layer, and is adhesive The layer is disposed under the substrate for adhesive adsorption; wherein the substrate is selected from the group consisting of polyethylene terephthalate (PET), polycarbonate (pc), polymethyl methacrylate (PMMA) or At least one polymer of the group consisting of polyethylene naphthenates; the component of the scratch-resistant anti-glare layer comprises a UV-curable resin and a polymer particle mixed therein; the fluoride in the anti-fouling layer; The material of the adhesive layer is at least one selected from the group consisting of acrylic, silicone or rubber. 2. The protective film according to claim 1, wherein a release layer is attached under the adhesive layer for attaching the adhesive layer to the object after peeling, and the material of the release layer is selected from the group consisting of One of the materials of Polyethylene, Polypropylene, Polyethylene or Paper. 3. The protective film of claim 1, wherein the anti-fouling layer has a water contact angle of from 90 to 120 degrees. 4‘如申請專利範圍第1項所述之保護膜’其中防刮抗眩層 内含金屬氧化物以增加與抗污層之連結程度,其中金屬 氧化物係選自二氧化鈦、二氧化矽、三氧化二鋁、氧化 銦錫或氧化錫銻所組成之群組之至少一種化合物。 5. 如申請專利範圍第4項所述之保護膜,其中金屬氧化物 佔防刮抗眩層之重量百分比為0.01%〜20%。 6. 如申請專利範圍第4項所述之保護膜,其中金屬氧化物 之粒徑介於3nm〜3G//m。 7 ’如申δ青專利範圍第1項所述之保護膜’其中面分子粒子 之粒徑介於1/im〜30/zm。 11 J314899 8如申咬皇 申μ專利範圍第1項戶d 之霧度介於〇.找〜30%。 、/、中防刮抗眩層 其中防刮抗眩層 •如申請專利範圍第1項所述之保護膜 之硬度大於1H。 、 124' The protective film of claim 1, wherein the anti-scratch anti-glare layer contains a metal oxide to increase the degree of bonding with the anti-fouling layer, wherein the metal oxide is selected from the group consisting of titanium dioxide, cerium oxide, and the like. At least one compound of the group consisting of alumina, indium tin oxide or tin oxide. 5. The protective film of claim 4, wherein the metal oxide comprises from 0.01% to 20% by weight of the anti-scratch anti-glare layer. 6. The protective film of claim 4, wherein the metal oxide has a particle size of from 3 nm to 3 G//m. 7' The protective film of the first aspect of the patent application scope of the invention, wherein the particle size of the surface molecular particles is between 1/im and 30/zm. 11 J314899 8 If Shen Zhihuang Shen μ patent range, the haze of the first item d is between 〇. Find ~30%. / /, medium anti-scratch anti-glare layer, which is anti-scratch and anti-glare layer. The hardness of the protective film as described in claim 1 is greater than 1H. , 12
TW94145175A 2005-12-20 2005-12-20 Protective film TWI314899B (en)