[go: up one dir, main page]

TW200836983A - Stainless steel container and method for making the same - Google Patents

Stainless steel container and method for making the same Download PDF

Info

Publication number
TW200836983A
TW200836983A TW96107021A TW96107021A TW200836983A TW 200836983 A TW200836983 A TW 200836983A TW 96107021 A TW96107021 A TW 96107021A TW 96107021 A TW96107021 A TW 96107021A TW 200836983 A TW200836983 A TW 200836983A
Authority
TW
Taiwan
Prior art keywords
stainless steel
container
plate
steel container
welding
Prior art date
Application number
TW96107021A
Other languages
Chinese (zh)
Other versions
TWI314122B (en
Inventor
Li-Yu Yang
Original Assignee
Golden Sunlight Ind Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Golden Sunlight Ind Co Ltd filed Critical Golden Sunlight Ind Co Ltd
Priority to TW96107021A priority Critical patent/TW200836983A/en
Publication of TW200836983A publication Critical patent/TW200836983A/en
Application granted granted Critical
Publication of TWI314122B publication Critical patent/TWI314122B/zh

Abstract

Disclosed is a stainless steel container and method for making the same, including; a tubular body made by wrapping a stainless steel plate, which defines a receiving space, a first open end and a second open end. A first stainless steel plate is laser welded to the first open end of the tubular body to seal it and a second stainless steel plate is laser welded to the second open end of the tubular body to seal it. The stainless steel materials are joined by laser welding without using solder during the manufacturing so as to form an integrated unit in a seamless manner, thus ensuring precise, quick and sanitary effects. Not only can this invention ensure high safety and durability for the stainless steel container, but also ensure that no residuals are left in the container due to the seamless welding design. Embosses provided to the container top also allow the mouth to be connected to the cap and affixed to the surface of the first stainless steel plate. Furthermore, thermal sublimation pattern transfer-printing process is applied to the outer edges of the stainless steel container to add beauty, prevent flaking off of the patterns, enhance the appearance and economic values, and resolve many problems encountered in the prior art.

Description

200836983 I i 九、發$說明: 【發明所屬之技術領域】 本發明係有關於-種容器 / 關於-種不銹鋼容器及其製法。w 。平吕之’係有 【先前技術】 習知的不銹鋼容哭兔 、交低之鋼材製作,因;該_;力:=’大J使用純度 '銲料填料之包覆方i脾尤綠 易於穹折、延展,且可以 -容器,但以往採㈣件間的縫隙填補並接合形成 接點薄弱、容器内部抗二:接:法具有易产'生氧化、焊 以氬弧焊之方气則右:±#作繁瑣等諸多缺點,若 接的影塑了 熱變形大之問題,都直 以習知技術所制m 加工成本與製造良率,而 以辅助桿接,而鲜 j於而要杯科以及助銲劑 ,接合處=Γ=銲編,以將銲料吻^ 補並非嫁接,所以易產生焊縫,也因為填 裝盛有液體會因為使;純度不=:,且經久置或 钱,通常鑛㈣Ή八门士 秀鋼材而產生氧化鏽 職的1兄#因為容置物之不同而有 鏽蝕產生,除此之外, f度的 表面毛細孔也是食用安強的助銲劑殘留在金屬 ^ ^ 王之大問題,以不銹鋼絮之士 為例’請參閱第1A、1B m ^ 方辦衣之酒亞 體,常常使得不錄4 回’由衣瓜的是含有酒精之液 使得裝盛的美酒變質,且央雜著氧 ^鱗’如此反而 人濰耆虱化後的鋼綠,若經飲用 U0180 5 200836983 ‘對Λ體的健康是一大傷害匕 V冰—士 酉3^内面氧化鏽兹的問題。 此外’在酒壺外側還會因為習 接方式需要#而口所& 、秀鋼容器的填料焊 ^ m ^ ^ 研心扎先而造成了填料焊接 厚度過厚又易產生銲縫’而經研磨處理後又 一:ί溥而致破裂之問題,也因為上述之問題而需要 土修補導致焊接點相、操作繁料缺點。 罢另外,習知不銹鋼容器例如為不 谷置飲品時都雲单矣蓄裳人 亞I衣作在 才都而要亞盍盍合避免濺灑,而為免壺# ϊ5 &、虫 失多將壺蓋15以連接之巧兇亞座15的适 苔15的、… 於酒壺1之表面,而習知壺 ^ 9連接係於酒壺i上穿孔再 垃 17穿入該穿孔並銲接於酒壺1Jl,正因妾;^之連接件 ... 兑上止因為又以穿孔及捏i主 式’而使得鏽蝕的可能性增加。 上下ΓΓ的不鱗鋼酒壺為了掩飾其填料得接之處,會於 摺邊;二之:衝墨再响^ 1,此J法係為了焊接接合後在士 皮並防止貼皮移動脫h日Μ,接°後在心1外緣貼 衝壓AM 也為了掩飾摺邊⑴、131 延展之製法所造成摺邊111、131大小不一之門 =外」傳統的不鱗鋼酒壺在上下蓋摺邊iu、心 2以接合上非^不易填料焊接,而為了美化焊二 所知以的研磨也不易實 i相對的就形成貼皮無法平貼於 酒…成凹凸不平,此時 得貼由夕士所w 2才1U ’則會使 人皮貝受化損壞;若改以彩料塗佈於壺身之方式, 又f因為酒類的溢 '六 i 工 、、^卜沾、广+ ¥致亞身10的彩料受侵蝕而產生 /x 、H,非常的不美觀也使得整體實用度降低。 110180 6 200836983 ,19】地’壺口19為焊接於上蓋11上,必須加長壺口 =長度並穿出該上蓋n,再以填人銲料之方式焊接於上 因鱗接處常受到液體與空氣的接觸,所以非常 : ⑸匕生鏽的問題,此時’裝盛於壺内的就不再是 =田而是帶有產生氧化的銅綠液體,不僅不安全,更不 場使用。 目此’為有效解決前揭技術所存在之 可於不銹鋼容器焊接加工時,免 ]毛出 ^ 光除填補鋅料所造成的食用 成鐘=及避免加使用純度較低之鋼材所造 成鏽飿之問題,並能避免研声 生,且提古㈣6入^先焊接點造成鮮縫之產 目么制h、增加錢度、提升耐用度,正是 目則製作不銹鋼容器所亟待解決之課題。 疋 【發明内容】 、 鑒於以上所述先前技術之缺點, 於提供-種不錄鋼容器及其製法‘:::在 鋒料填補焊接處並達製造精確、快速、、ς^Γ 法,目的在讀供—種不錄鋼容器及其製 卑使谷置物不易殘留於容器内。 本發明之另一目的在於提供— 法,俾可以圖案美化不不t鋼μ及其製 剝落。 抑之外緣亚能防止圖案退化 為達上揭目的以及其他目的 容器,係包括管狀本體,# 種不銹鋼 定出一交署不銹鋼板環接而成者,並界 工間、第一開放側與第二開放側;第—不錄2 Π0180 7 200836983 合板,’係j^f射焊接焊合封烟管狀本體之第一開放 :卜並具有-開口及鄰近該第一開放側之第一倒角;以及 ::::鋼結合板,係平行相對於該第一開放側並以雷射 該管狀本體之第二開放側,並具有鄰近該第 * Η之,倒角,以於結合至管狀本體後形成該容置 和俾使第一不錄鋼結合板與管狀本體及第二不 =二板相結合’並將相互接合處以雷射焊接熔融接缝 處之=銹鋼材使成為-體,再辅以接縫處之研磨拋光。 :遠裝置中,管狀本體之第一開放側及第二開放側之 邊、·象係相互平行’以供雷射焊接為筒狀容置空間時盘第一 =鋼結合板及第二不銹鋼結合板所需之接合處精密度, 其中,該管狀本體彎折成筒狀容置空間時, ㈣鋼、為唬303系列、不銹鋼編號3〇4系列、及 ^虎316糸列之其中一者’於_較佳實施例中,該不錄鋼 板係❹純不銹鋼編號316系列所製成,以提供較佳之耐 女全性’更佳地’該管狀本體係採用食品級之不銹 鋼材料,俾供裝盛食品之食用安全功效。 之不銹 而上述本發明之不銹鋼 選自不銹鋼編號 303系列、 鋼編號316系列之其中一者 不銹鋼結合板係使用純不錄 供較佳之耐用度及安全性, 係採用食品級之不銹鋼材料 各器’該第一不銹鋼結合板係 不銹鋼編號304系列、及不銹 於一較佳實施例中,該第一 鋼編號316系列所製成,以提 更佳地,該第一不銹鋼結合板 ,俾供裝盛食品之食用安全功 110180 8 200836983 ,效,’而該第一不銹鋼結合 狀本體之第-開放側,並中^朴接线地焊接於管 本體之當一 ,、 5亥罘一不銹鋼結合板與管狀 鋼銲件之接i =接縫錢μ射焊接直接熔融兩不銹 ==第一不錢鋼結合板與該第-開放側之焊 .細度。此外,兮第n/ 面具有高品質之表面精 ^ 不銹鋼結合板復包括一嘴頭,而該嘴 =雷射焊接焊合於第一不錄鋼結合板口:: 頭與開口無縫結合,以避.羽4押杜* 以使為 習知嘴頭與酒壺接人日士,峻白口干丄料生鏽的問題以及 Hg /M _ 13 ^,鳴頭需製作較長以供焊接之問 而可避免因嘴頭於㈣長度之剩餘 將 置物完全倒出之困難。 Τ木月b肘今 d述本發明之不錄鋼容器,該第二不錢鋼結合板俜 砥自不銹鋼編號303系列、$咏 卞 锢编,# J不錄鋼編號304系列、及不銹 鋼、、扁號3!6糸列之其中一者,於一較佳實施例中, ,::秀鋼結合板係使用純不銹鋼編號31 用度及安全性更佳地,該第二不銹』合S ,畏口口級之不銹鋼材料’俾供裝盛食品之食 八 效,而该第二不銹鋼結合板係雷接 ^ 狀本體之第二開放側,其中,“射Off地焊接於管 ,^ 鑌弟一不銹鋼結合板盥瞢壯 第二開放側之接縫處係以雷射焊接直接熔融衫 編牛之接缝’以形成精確且高品質之焊接面,益須埴補 :二:較佳地,該第二不銹鋼結合板與該第二開放侧: 接處係研磨有第二倒角,以使焊接面具有高品質之表面精 110180 9 200836983 -細度。 1 ^ * 刖违本發明之不銹鋼容器,復包括—瓶蓋及瓶頂, 乂第不銹鋼結合板復包括一嘴頭,其中,該嘴頭係選 自,銹鋼編號303系列、不銹鋼編號3〇4系列、及不銹鋼 編说316系列之其中一者,於一較佳實施例中,該嘴頭係 •,用不㈣編號3G4系列所製成,以提供較佳之财用度及 •,王n ’ ^避m純度較低之不銹鋼壺口易生鐵之問 = 為了衣以純度較兩之不錄鋼材,該嘴頭係經衝壓後 製成,以避免習知壺口鱼 又 號31系列之鋼材車銷刀 1 = ’車銷〜鋼編 部係供套設該瓶蓋,以供該瓶 於亥瓶頂之一端 、瓶1鎖固於该嘴頭,另一端部 供谭接時聚熱於該凸點並炫融該凸點, 争:”技::於弟一不銹鋼結合板之表面,據此,得以解 補白=術需於壺身穿孔並將連接件穿入焊接造成銲料填 補易‘致鏽敍之問題。 /、 狀本lb=前述本發明之不銹鋼容器,復包括形成於該管 圏安心•.圖案’較佳地,該熱昇華轉印 先在表面塗饰有-層轉印漆之管狀本體, =熱:爭之方式將熱昇華轉印圖案轉印於表面一 运中,再將载有熱昇華轉印圖宰 — 鋼製之管狀太雕參;r4 木之貼紙去除,即可於不銹 γ之g狀本肢表面形成變化之. 為達前揭目的以及其他 : 鋼容器之製法,其步驟包含#明復提供—種不錄 知(、一管狀本體,俾由該管 Π0180 10 200836983 .狀·本體界定出一容置空間、第一開放 雷射焊接方式將第一不綠力^ Α· 〃昂一開放侧;以 第-開放侧;…二封閉該管狀本體之 合封閉該管狀本體之第二式將#二不鱗鋼結合板焊 上述本發明之不銹鋼容器之製法中 :係,鋼板環繞出管形狀,並以治具定疒 =朴接方式將不㈣板接合 缝 地形成該管狀本體。 彳早使無縫坏接 傷上述本發明之不錢鋼容器之譽法中,上女笛 合板復包括-開口,⑽ 中该弟一不録鋼結 壓後製成再以M、/ 係供增設嘴頭’該嘴頭係經衝 % ".田、焊接方式將嘴頭之一端無縫地焊接於該 弟—不銹鋼板之開口卜 作 圩如万、及 該瓶頂之一端部 %卜,仅匕括一瓶蓋及瓶頂之設置, 頭m ^、以瓶蓋,以供該瓶蓋鎖固於該嘴 俾使易於:接:第凸設―凸點,以— 知谷於罘一不銹鋼結合板之表面。 管狀=外鋼容器之製法’復包括形成於該 案製法户裎彳 I 二汁華轉印圖案製法,該熱昇華轉印圖 表面^二’、—载有熱昇華轉印圖案之貼紙包覆於預先在 即可= 表面塗佈之漆層中,再將該貼紙去除, 即可於該管狀本體表面形成圖案式樣。 以兀:於本兔明所提出之不銹鋼容器及其製法,主要係由 出環接!成者一管狀本體,俾由該管狀本體界定 谷置二間、第一開放側與第二開放側,以雷射焊接方 11 110180 200836983 ,式‘將第-不錢鋼結合板谭合封閉 側、及以雷射焊接方式將第二不 j本肢之弟一開放 管狀本體之第二開放側,又以:二反二合封閉至該 不錄鋼材使相接成為一體 =式义谷融接縫處之 芒日车处、辟洛杜m ▲ 早使各#件間無缝接合且於势 避免使料料補烊接處 方、衣 生之效,且配合無縫谭接嘴頭之^衣1確、快速、衛 物不易殘留於容哭内、,# 又,以確保使用時容置 勿坎Μ万、谷态内,亚藉瓶頂之凸 供瓶蓋結合,並固定於第一 ’又σ ,使嗔碩得以 配人嘥曰芏Μ 、 、秀鋼結合板之表面,此外再 配口熱计爭轉印圖案之製程再 外緣並能防止圖案退化剝落,二 值,一併解決先前技術所存在之問度及經濟價 【實施方式】 請參閱第2 Α圖,係Α太八RR 本發明之不錢鋼容器,=1 不錄鋼容器之爆炸圖。 體η,俾由該管狀本 放側2U盘第-門^ 置空間22、第一開 銹鋼結合板23焊合封閉至兮戽肚士 接方式將弟一不 其中,令第二 本體之第-開放側叫, 二開放=結合板23係具有-開 焊接方式將第不^相對於該第—開放側211,且以雷射 之第二開二板25辉合封閉至該管狀本體 ^ ",,俾使該第二不銹鋼結合板25社人至兮 官狀本體21後形成該容置空間 板、、。:= 焊接係將第一不銹鋼社人 -和”射 不錄鋼結合板25與第? Ί 一開放侧213相互接合處以精確、快 110180 12 200836983 ,速丨、1¾焊接品質之方式您融接縫_ ^ i鮭 L处之不銹鋼材使兩銲件相 接成為一體,再辅以接縫處之研磨拋光。 冑搭配第2B圖參閱,上述本發明之不錄鋼容哭,該 以板片幫折而成之管狀本體21,其不錄鋼板環接處:以雷 射焊接熔融亚加以表㈣光處理,俾使該板片益縫接人, • 成形具有極高之表面品質,較佳地,該管:本 •胆21係廷自不鐵鋼編號3〇3系列、不鱗鋼編號綱系列、 及不鎊鋼編號則系列之其中一者,於本實施例令,該其 狀本體21係使用純不銹鋼編號316系列製造,以供較佳: 耐用度及安全性,但於其他實施例中,該管狀本體Μ ^使 用例如食品級之不錄鋼材製作,符合所需之耐用度及安全 性即可,故非以不銹鋼編號316系列為限。 王 此外,上述本發明之不銹鋼容器,該第一不鱗鋼結合 板23與第-開放側211、及第二不銹鋼結合板25與第二 開放側213得、以無銲料之雷射珲接方式無缝地焊接兩焊 件’俾使焊接完成後施以表面處理時,.不會因為需研磨抛 光而使得焊接處過薄而有破裂之虞的問題產生。而為於銲 件相接處研磨拋光’該第一不銹鋼結合板23與第一開放側 211、及第二不銹鋼結合板25舆第二開放側213係任一選 較尽之板材,並於相接處形咸倒角,俾得更佳之矣而口、 質,/其中,該第一不銹鋼結合板23及第二不銹鋼結合板 5係%自不銹,編號3〇3系列、不銹鋼編號3〇4系列、及 不銹鋼編號316系列之其中一者,於本實施例中,該第— 不銹鋼結合板23及第二不銹鋼結合板25係使用純^銹鋼 110180 13 200836983 .編號3心列製造1供較佳之耐用度及安全性 他實施例中,該第-不銹鋼結合板23 仁於/、 25係使用例如食D绍 不鱗鋼結合板 文㈣如f…級不銹鋼材製作.,符合所 安全性即可,且亦非以z綠 ί用度及 且丌非以不銹鋼編號316系列為限。 本發明之不銹鋼容器之第一不鱗鋼結合板 一嘴頭加,該嘴頭232係經衝壓後再以雷接 合於第-不銹鋼結合板23之開口加,頭2== 231之焊接方式及材質選用同於前述第-不錄紗γΓ23 與管狀本體21之焊接方式及材質制,故在此不;;贅板十 因而,由上述可知,本發明之X#細Α在此不予負述。 明之不銹鋼容器的特點乃在於雷 射焊接無填銲料及無缝的加工俾使習知技術於壺口㈣時 容=銲料與空氣及水分接觸而產生生鑛之問 相以避免,1因热須填銲料之故,該嘴頭232深入管狀 本體21之長度得以縮減為與開口 23丨相接齊即可。. 此外,請參閱第2C圖,本發明之不鱗鋼容器為 裝盛#於缝之液體復包括一瓶蓋234及瓶頂235,其中 該瓶頂235之-端部係供套設該瓶蓋234,以供該瓶蓋咖 鎖固於該嘴頭232,另-端部係凸設—凸點2351,以供焊 接時聚熱於該凸點2351,而易於悍接至第—不錄鋼块 23之表面。 、口 口攸 請參閱第2D圖,上述本發明之不錄鋼容器復包括教 昇華轉印圖案27,該熱昇華轉印圖# 27係包覆於預μ 表面塗佈有一層轉印漆之管狀本體21,,再以埶昇華之方 式將熱昇華轉印圖案27轉印於表面之塗饰漆層中,再將载 110180 14 200836983 .有‘熱昇哿轉印圖案π之貼紙Μ去陝, 管狀本體21,表面形成變化之式俨*,即可於不銹鋼製之 皮不平整與液體溢流損壞表面美供避免習知技術貼 ,第3圖,係為本發明之;鱗= 之示意圖,本發明之不錄鋼 盖益弟五貫施例 相等,故不在此為言贅述,而該不述結構大致上 處係為該管狀本體21係以泸勃/ ’谷态之結構不同之 施-,該管狀二 成,但於其他較佳之實施例中片==相接: 接成二角柱體之構造,或以五-、秀鋼板% 之構造,符合該構造之靜即H’板%接成五角柱體 之形式,可供任選裝盛香水、胡 -糖、牙鐵之其中-者,於其他較佳實施例中,亦 可砥擇性製作較大之開口 231,以 灰缸之其中一者。 /、作為化瓶、燭台、煙 她於習知技術,本發明所提出之不銹鋼容器,主要 =由以=銹鋼板環接而成—管狀本體,俾由該管狀本體界 疋出一容置空間、第-開放側與第二開放側,再配合第一 =銹鋼結合板、及第二不銹鋼結合板與管狀本體焊接結 t ’又以雷射;接方絲融接縫處之不義材使相接成為 -體’俾使各_件間無縫接合且於製造時能避免使用鲜料 填補知接處並達製造精確、快速、衛生之效,且配合無縫 焊接嘴頭之設置,以確保使用時容置物不易殘留於容器 内,亚藉瓶頂之凸點設計,使嘴頭得以供瓶蓋結合,並固 15 110180 200836983 ,疋,於第二不銹鋼結合板之表面, 宰之f裎,以徂同奋、, 此外再配合熱昇華轉印圖 Γ化不1 秀鋼容蕃之外緣並能防正二 退化剝洛,俾增加其美觀度及經萍 α " 術所存在之問題。 Η只,一併解決先前技 上述實施例僅例示性說明本 非用於限制本發明。任何熟f X ^原理及其功效,而 背本發明之精神及範轉下 、技之人士均可在不違 變。因此,本發明之權利保边實施例進行修•與改 範圍所列。 圍’應如後述之申請專利 【圖式簡單說明】 第1A圖係為習知不鑄士 第1B圖係為習知不銹鋼洒組合示意圖; 第2A圖係為本發明不録鋼“圖, 第2B圖係為本發明鋼二,實^例爆炸圖; 組合示意圖;鋼合為之一貫施例雷射焊接 第2C圖係為本發明 合示意圖; 、秀鋼容器第二實施例之焊接組 第2D圖係為本發明 昇華轉印示意圖;以及 '鋼容器第三實施例之表面熱 第3圖係為本發明不 【主要元件符號說明】”鋼容器第四實施例之示意圖。 I 酒壺 10 壺身 II 上蓋 110180 16 200836983 111 t 摺邊 ► 13 下蓋 131 摺邊 15 壺蓋 17 連接件 19 壺口 21、2r 管狀本體 211 第一開放侧 213 第二開放側 22 容置空間 23 第一不銹鋼結合板 231 開口 232 嘴頭 234 瓶蓋 235 瓶頂 2351 凸點 25 第二不銹鋼結合板 27 熱昇華轉印圖案 28 貼紙 17 110180200836983 I i IX. STATEMENT: TECHNICAL FIELD OF THE INVENTION The present invention relates to a container/about-type stainless steel container and a method of manufacturing the same. w. Ping Luzhi's [previous technology] The well-known stainless steel Rongshe rabbit, the low-cut steel is made, because; the force: = 'big J uses the purity' of the solder filler coating i spleen green is easy to lick Folded, extended, and can be - container, but in the past, the gap between the pieces (four) was filled and joined to form a weak joint, the internal resistance of the container is two: the method is easy to produce 'oxidation, the right side of the welding with argon arc welding is right :±# is a cumbersome and many other shortcomings. If the film is shaped by the problem of large thermal deformation, the processing cost and manufacturing yield of the m technology are directly obtained by the conventional technology, and the auxiliary rod is connected, and the fresh cup is required. Branch and flux, joint = Γ = weld, to make the solder kiss ^ is not grafted, so it is easy to produce welds, but also because the filling contains liquid will be; purity is not =:, and long-term or money, Usually the mine (four) Ή eight men's shoes show the steel oxidized rust 1 brother # because of the different contents of the rust caused by the rust, in addition, the surface of the f fine pores is also edible A strong flux residue in the metal ^ ^ Wang Zhida’s problem, taking the stainless steel floc as an example. Please refer to section 1A, 1B m ^ The sub-body of the clothing wine often makes it impossible to record 4 times. 'The melon is made of alcohol-containing liquid, so that the wine that is contained in the wine is degraded, and the center is mixed with oxygen and scales. Drinking U0180 5 200836983 'The health of the carcass is a major injury 匕 V ice - gentry 3 ^ inside the surface of the problem of oxidation. In addition, 'the outside of the jug will also need to be used because of the way of picking up the mouth and the mouth, and the filler welding of the steel container ^ m ^ ^ to the heart of the first to cause the filler weld thickness is too thick and easy to produce welds' After the grinding process, another problem: the problem of cracking, and the above-mentioned problems require the repair of the soil to cause the welding point phase and the operation of the material. In addition, the conventional stainless steel container, for example, does not have a drink when the grain is stored in the cloud, and the singularity of the person is in the genius. The lid 15 is connected to the surface of the hip flask 1 of the moss 15 of the skillful seat 15, and the conventional pot is connected to the jug i and pierced into the perforation and welded to the perforation. The jug 1Jl, just because of the 妾; ^ the connection of the ... ... with the last because of the perforation and pinch i main type 'to increase the possibility of rust. In order to disguise the filler, the non-scale steel jug will fold over the edge; the second: the ink will re-sound ^ 1, this J method is used to weld the joint in the skin and prevent the skin from moving off. In the future, after the °, the outer edge of the heart 1 is stamped with AM. In order to cover the folds (1), 131, the method of extension is caused by the folding of 111, 131. The size of the door is different. The traditional non-scale steel jug is folded up and down. The side iu, the heart 2 is not easy to be welded by the joint, and the polishing is not easy to be used for the purpose of beautifying the welding. The skin is not formed in the skin. Shishi w 2 only 1U 'will make people Pibe suffer damage; if it is changed to the way the color material is applied to the body, f because of the overflow of the wine 'six i workers, ^ 卜 di, wide + ¥ The color of the body 10 is eroded to produce /x, H, and the great beauty is also reduced. 110180 6 200836983, 19] The ground's spout 19 is welded to the upper cover 11, and the length of the spout must be lengthened and the upper cover n must be worn out, and then welded to the upper part by the solder to the liquid and air. The contact, so very: (5) the problem of rusting, at this time 'installed in the pot is no longer = field but with a oxidized patina liquid, not only unsafe, but also not used. In order to effectively solve the problems of the pre-existing technology, it can be used in the welding process of stainless steel containers, and the rust caused by the use of steel with low purity is avoided. The problem, and can avoid research and sound, and mention the ancient (four) 6 into the first welding point to create the production of fresh seams, increase the amount of money, improve durability, it is the subject of the need to solve the problem of stainless steel containers.疋[Summary of the Invention] In view of the above-mentioned shortcomings of the prior art, the invention provides a non-recording steel container and a method for manufacturing the same: ':: In the front material filling the welding place and achieving the precision, rapid, and 制造^ method, the purpose The reading and supply of the non-recorded steel container and its preparation are not easy to remain in the container. Another object of the present invention is to provide a method in which the pattern can be beautified and not peeled off. The outer edge can prevent the pattern from degrading into a container for other purposes, including a tubular body, and the stainless steel is made up of a stainless steel plate, and the first open side is The second open side; the first - not recorded 2 Π 0180 7 200836983 ply, 'the first opening of the tubular body of the welding and sealing of the j^f welding: the opening and the first chamfer adjacent to the first open side And a :::: steel bonded plate parallel to the first open side and to the second open side of the tubular body, and having a chamfer adjacent to the first Η, to be bonded to the tubular body After the formation and the arranging, the first non-recording steel bonding plate is combined with the tubular body and the second non-second plate, and the joints are joined by laser welding to weld the rust steel at the joint to become a body. It is supplemented by grinding and polishing at the seam. : In the far device, the first open side and the second open side of the tubular body are parallel to each other's for the laser welding to be the cylindrical accommodating space, the first plate = the steel bonded plate and the second stainless steel combined The joint precision required for the board, wherein the tubular body is bent into a cylindrical accommodating space, (4) steel, one of the 唬303 series, the stainless steel number 3〇4 series, and the ^虎316 ' In the preferred embodiment, the non-recorded steel plate is made of pure stainless steel No. 316 series to provide better resistance to women's 'better'. The tubular system is made of food grade stainless steel material. The food safety effect of Sheng food. The stainless steel of the present invention is selected from the stainless steel No. 303 series and the steel No. 316 series. The stainless steel bonding board is purely non-recorded for better durability and safety, and is made of food grade stainless steel material. 'The first stainless steel bonded plate series stainless steel No. 304 series, and the stainless steel in a preferred embodiment, the first steel number 316 series is made, in order to better, the first stainless steel bonded plate, for the first The food safety function of the food is 110180 8 200836983, and the first stainless steel is combined with the first open side of the body, and the middle is welded to the tube body, and the 5th stainless steel joint plate Connected with the tubular steel weldment i = seam money micro-shot welding direct melting two stainless == the first non-coin steel bond plate with the first-open side of the weld. Fineness. In addition, the n/face has a high-quality surface finish. The stainless steel bonded plate includes a mouth, and the mouth = laser welded to the first unrecorded steel plate:: the head and the opening are seamlessly combined, In order to avoid the problem of rusting and Hg /M _ 13 ^ for the mouth and the hip flask, and the Hg /M _ 13 ^, the head needs to be made longer for welding. It is difficult to avoid the difficulty of completely pouring out the contents due to the remaining length of the mouth. Τ木月b elbow today describes the non-recorded steel container of the present invention, the second non-coin steel combined plate from stainless steel number 303 series, $咏卞锢编, #J不录钢号304 series, and stainless steel, One of the squaring numbers 3!6, in a preferred embodiment, ::: Siu steel combined plate system uses pure stainless steel number 31. The degree of use and safety is better, the second stainless steel S, the stainless steel material of the mouth-mouth level is provided with eight foods for feeding food, and the second stainless steel bonding plate is connected to the second open side of the body, wherein "the ground is welded to the tube, ^ The younger brother of a stainless steel joint plate is strong and the joint of the second open side is laser welded directly to melt the seam of the cow's seam to form a precise and high-quality welding surface, which is beneficial: 2: better The second stainless steel bonding plate and the second open side: the joint is ground with a second chamfer so that the welding surface has a high quality surface finish 110180 9 200836983 - fineness. 1 ^ * 刖 according to the invention The stainless steel container includes a cap and a bottle top, and the stainless steel joint plate includes a mouth, wherein The mouth is selected from one of the stainless steel No. 303 series, the stainless steel number 3〇4 series, and the stainless steel 316 series. In a preferred embodiment, the mouthpiece is used, and the (4) number is 3G4. Made of series to provide better financial efficiency and •, Wang n ' ^ avoids the purity of the stainless steel, the purity of the stainless steel, the mouth of the iron is easy to ask = for the purity of the clothes compared to the two, the mouth is stamped After the production, in order to avoid the knowledge of the Hukou fish No. 31 series of steel pin knife 1 = 'car pin ~ steel braided department for the cap, for the bottle at the top of the bottle top, bottle 1 Locked on the mouth, the other end is used to gather the heat on the bump and smash the bump, and strives for: "Technology:: The surface of the stainless steel joint plate of Yudi, according to which, the white is replaced. It is necessary to perforate the body of the kettle and put the connecting member into the welding to cause the solder to fill the problem of rusting. /, lb = the above-mentioned stainless steel container of the present invention, including the formation of the tube 圏 peace of mind.. Pattern 'better, the sublimation transfer is first coated on the surface with a layer of transfer paint tubular body, = Heat: the way of arbitrating the transfer of the sublimation transfer pattern onto the surface, and then carrying the sublimation transfer diagram - steel tubular tortoise; r4 wood sticker removed, can be in stainless γ The shape of the g-shaped limb is changed. For the purpose of the pre-existing and other: The method of manufacturing the steel container, the steps of which include #明复供--not recorded (, a tubular body, 俾 from the tube Π 0180 10 200836983. · The body defines an accommodating space, the first open laser welding method is to open the first non-green force ^ Α 〃 ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; The second type combines #二不鳞钢 in combination with the above-mentioned stainless steel container of the present invention: the steel plate is wrapped around the shape of the tube, and the tubular shape is formed by the joint of the fixture. The main body. 彳 Early to make seamless damage to the above-mentioned invention In the reputation method, the upper female flute plate includes - opening, (10) the younger one does not record the steel after the pressure is made and then M, / for the addition of the mouth 'the mouth is rushed by the % " The welding method seamlessly welds one end of the mouth to the opening of the younger-stainless steel plate, such as the opening of one of the tops of the top of the bottle, and only includes a cap and a top of the bottle, the head m ^ The bottle cap is used to lock the cap to the mouth to make it easy: connect: the convex-bump, to - the surface of the stainless steel joint plate of the Zhigu. The tubular method = the method of making the outer steel container The method comprises the following steps: forming a method for preparing a transfer pattern of the bismuth I, and transferring the surface of the transfer pattern to the surface of the film, the sticker carrying the sublimation transfer pattern is coated on the surface in advance; In the lacquer layer, the sticker is removed, and a pattern can be formed on the surface of the tubular body. 兀: The stainless steel container and the method for preparing the same according to the present invention are mainly made up of a ring-shaped body;俾The second body, the first open side and the second open side are defined by the tubular body, and the laser welding side 11 1 10180 200836983, the type 'the first-side of the open-tubular body of the second-side side of the open-tubular body, the second open side of the open-tubular body Closed to the non-recorded steel to make the joints become one-in- right side of the valley joints of the Mangri, the loduo m ▲ early to make the # seamless joints and the potential to avoid the material to make up the prescription The effect of clothing and clothing, and with the seamless tanned mouth of the ^ clothing 1 indeed, fast, and the refuge is not easy to remain in Rong Chuang, #, to ensure that the use of the time is not tough, the valley, The crown of the bottle is combined with the bottle cap and fixed to the first 'also σ, so that the 嗔 得以 can be matched with the surface of the plate, and the hot plate is used to transfer the pattern. The outer edge of the process can prevent the pattern from degrading and peeling off. The binary value solves the problem and economic price of the prior art together. [Embodiment] Please refer to the second figure, the system is not a steel container of the invention. ,=1 The explosion map of the steel container is not recorded. The body η, 俾 is welded and closed by the tubular front-side 2U disk first-door space 22, the first open-rust steel bonding plate 23 to the 兮戽 士 接 接 将 将 将 将 将 将 将 , , - open side, two open = combined plate 23 has an open-welding method that will not be opposite to the first open side 211, and the second open second plate 25 of the laser is closed to the tubular body ^ &quot The second stainless steel bonding plate 25 is formed by the second stainless steel bonding plate 25 to form the accommodating space plate. := The welding system will be the first stainless steel body - and the "unrecorded steel binding plate 25 and the first 侧 an open side 213 joint with each other in a precise, fast 110180 12 200836983, fast 丨, 13⁄4 welding quality way you melt the seam _ ^ i鲑L at the stainless steel material so that the two weldments are joined together, and then supplemented by the grinding and polishing of the joint. 胄 With reference to Figure 2B, the above-mentioned invention does not record steel to cry, the plate The tubular body 21 is folded and folded, and the steel plate is not connected: the laser welding is performed by melting the sub-surface (4) light treatment, so that the plate is sewed, and the forming has a very high surface quality, preferably Ground, the tube: one of the series of the series of the 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd, 3rd The 21 series is manufactured using a pure stainless steel No. 316 series for better: durability and safety, but in other embodiments, the tubular body is manufactured using, for example, food grade non-recorded steel to meet the required durability and Safety is fine, so it is not limited to stainless steel No. 316 series. In addition, in the above-mentioned stainless steel container of the present invention, the first non-scale steel bonding plate 23 and the first-open side 211, and the second stainless steel bonding plate 25 and the second open side 213 are obtained in a solderless laser-free manner. Sew-welding two weldments '俾When the surface finish is applied after the welding is completed, there is no problem that the weld is too thin and cracked due to the need for grinding and polishing. However, the weld is welded at the joint of the weldment. 'The first stainless steel bonding plate 23 and the first open side 211, and the second stainless steel bonding plate 25 and the second open side 213 are any selected plates, and are chamfered at the joints. Preferably, the first stainless steel bonding plate 23 and the second stainless steel bonding plate 5 are free from stainless steel, number 3〇3 series, stainless steel number 3〇4 series, and stainless steel number 316 series. In this embodiment, the first stainless steel bonding plate 23 and the second stainless steel bonding plate 25 are made of pure steel 110180 13 200836983. No. 3 is manufactured in a row for better durability and safety. Medium, the first-stainless steel bonding plate 23 is in /, 25 It is made of, for example, food D Shaoshao steel combined with plate (4) such as f... grade stainless steel. It can be safe, and it is not limited to z green and is not limited to stainless steel No. 316 series. The first non-square steel binding plate of the stainless steel container of the present invention is added to the mouth, and the nozzle 232 is stamped and then joined to the opening of the first-stainless steel bonding plate 23 by lightning, and the welding method of the head 2==231 And the material is selected to be the same as the welding method and the material of the first-non-recording yarn γΓ23 and the tubular body 21, so it is not here; the 赘板十, thus, it can be seen from the above that the X# Α of the present invention is not described herein. The stainless steel container of Mingshi is characterized by laser soldering without soldering and seamless processing, so that the conventional technology can avoid the contact between the solder and the air and moisture, and the heat is generated. To fill the solder, the length of the mouth 232 deep into the tubular body 21 can be reduced to be aligned with the opening 23丨. In addition, referring to FIG. 2C, the non-scale steel container of the present invention comprises a bottle cap 234 and a bottle top 235, wherein the end of the bottle top 235 is provided with the bottle. a cover 234 for the cap coffee to be locked to the mouth 232, and the other end portion is convexly provided with a bump 2351 for gathering heat on the bump 2351 during welding, and is easy to be connected to the first The surface of the steel block 23. Referring to FIG. 2D, the above-mentioned non-recording steel container of the present invention includes a teaching sublimation transfer pattern 27, and the thermal sublimation transfer pattern #27 is coated on the pre-μ surface and coated with a layer of transfer paint. The tubular body 21, and then the sublimation transfer pattern 27 is transferred to the surface of the finishing lacquer layer by means of sublimation, and then the 110180 14 200836983 is loaded with a sticker of the hot-lifting transfer pattern π. , the tubular body 21, the surface of the surface of the change of the formula , *, can be stainless steel skin unevenness and liquid overflow damage surface to avoid the conventional technology stickers, Figure 3 is the invention; scale = schematic The five-part embodiment of the non-recorded steel cover of the present invention is equal, so it is not described here, and the structure is not generally described as the structure of the tubular body 21 which is different in the structure of the 泸博/'谷 state. - the tubular 20%, but in other preferred embodiments, the sheet == meet: the structure of the two-corner cylinder, or the structure of the five- and the fine steel plate, which conforms to the static of the structure, ie the H' plate% In the form of a pentagonal cylinder, it can be optionally filled with perfume, Hu-sugar, and dental iron. In other preferred embodiments, the abrasive also can be made larger Optional of openings 231, to which one of the ashtray. /, as a chemistry bottle, candlestick, smoke, she knows the technology, the stainless steel container proposed by the present invention is mainly composed of a rust steel plate and a tubular body, and a space is formed by the tubular body. , the first open side and the second open side, together with the first = rust steel binding plate, and the second stainless steel bonding plate and the tubular body welded knot t 'and the laser; the joint of the square wire melt joints of the unreliable material The joints become the body-body, so that the joints can be seamlessly joined and can avoid the use of fresh materials to fill the joints and achieve precise, fast and hygienic effect, and with the seamless welding head setting, Make sure that the contents are not easy to remain in the container during use, and the bumps on the top of the bottle are designed so that the mouth can be combined for the cap and solidified. 15 110180 200836983, 疋, on the surface of the second stainless steel bonded plate, slaughter With the same enthusiasm, and in addition to the sublimation transfer map Γ化不1 秀钢容蕃外缘 and can prevent the degeneration of the second degeneration, 俾 increase its aesthetics and the problems of Jingping α " . The prior art is only used to limit the present invention. Any familiarity and efficacy, and the spirit of the invention and the skills of the technology can not be violated. Accordingly, the claims of the present invention are set forth in the scope of the modifications and modifications. The enclosing 'should be patented as described later. [Simple description of the drawing] The first drawing is a schematic diagram of the conventional stainless steel sprinkling assembly. The second drawing is a schematic diagram of the conventional stainless steel sprinkler. 2B is the explosion diagram of the steel of the invention, the actual example; the schematic diagram of the combination; the second embodiment of the laser welding is the schematic diagram of the invention; the welding group of the second embodiment of the steel container The 2D drawing is a schematic diagram of the sublimation transfer of the present invention; and the surface heat of the third embodiment of the steel container is a schematic view of the fourth embodiment of the steel container of the present invention. I hip flask 10 body II upper cover 110180 16 200836983 111 t hem ► 13 lower cover 131 hem 15 lid 17 connecting piece 19 spout 21, 2r tubular body 211 first open side 213 second open side 22 accommodating space 23 First stainless steel bond plate 231 Opening 232 Mouth 234 Cap 235 Bottle top 2351 Bump 25 Second stainless steel bond plate 27 Sublimation transfer pattern 28 Sticker 17 110180

Claims (1)

200836983 十.、申諱專利範圍·· ^ 一種:鎊:f器之製法,其步驟包含: ^η 32 g狀本體,俾由該管狀本體界定出一容置 開放侧與第二開放側; 管狀本2焊接方式將第—不銹鋼結合板焊合封閉該 ^狀本體之第—開放侧;以及 管二不錢鋼結合板焊合封閉該 2 第1項之不錄鋼容器之製法’該管狀 也2⑼以不錄鋼板環繞出管形狀,並以治具定 融^化狀’再以雷射焊接方式將不銹鋼板接合處熔 以無縫焊接之方式形成該管狀本體。 c範圍第i項之不録鋼容器之製法,其中, 不銹鋼結合板復包括_開口,該開口係供增設 4· 2請專利範圍第3項之不銹鋼容器之製法,其中, ^碩係_壓成形,俾以雷射焊射式將該嘴頭之 螭热縫地焊接至該第一不銹鋼板之開口。 开如I請專·圍第3項之不銹鋼容器之製法,復包括 2成—瓶蓋及_’使該瓶蓋套設於該瓶頂之一端 ς ’ μ供該瓶蓋鎖固於該嘴頭,另_端㈣凸設—凸 :綠μ在焊接時聚熱㈣凸點,俾使w焊接於第一 6· 不銹鋼結合板之表面。 如申請專利範圍第1項之不銹辦容器之製法,復包括 110180 18 200836983 •.尹織管狀本體外表面形成熱昇華轉印圖案。 7.如申請專利範圍第6項之不銹鋼容器之製法,其令 :-载有熱昇華轉印圖案之貼紙包覆於預先在: 轉印漆之管狀本體,以熱昇華方式將熱昇華轉印 H印於表面塗佈之漆層中,再將該貼紙去除,即可 於该官狀本體表面形成圖案式樣。 8.如申請專利範圍第i項之不録鋼容器之製法,該 體係以複數不銹鋼板環接而成。 9· 一種不銹鋼容器,係包括: —管狀本體,係以不錄鋼板環接而成者,並界定出 一容f空間、第-開放側與第二開放側; 狀太:一^錄鋼結合板,係以雷射焊接焊合封閉該管 門:Γ開放侧,並形成有-開口及鄰近該第-开1放側之弟一倒角;以及 狀太二一,鋼結合板’係以雷射焊接焊合封閉該管 t本體:弟二開放侧’並形成有鄰近該第二開放側之 弟二倒角。 本利軌圍第9項之不銹鋼容器,其中,該管狀 邊緣。開放側之邊緣係平行於第二開放側之 1如申睛專利範圍第9 員之不銹鋼容器,該管狀本體係 奴數不銹鋼板環接而成。 圍第1〇項之不銹鋼容器,其中,該管狀 錄鋼板環繞相接係以雷射焊接祕融結合。 110180 19 200836983 • 13,·如申*請專利範圍第9項之不銹鋼容器,其中,該管狀 本體係選自不銹鋼編號303系列、不绣鋼編號3〇4系 列、及不銹鋼編號316系列之其中一者。 14·如申請專利範圍第9項之不銹鋼容器,其中,該管狀 本體係食品級不銹鋼材。 .15·如申請專利範圍第9項之不銹鋼容器,其中,該第一 ^銹鋼結合板係選自不銹鋼編號3〇3系列、不銹鋼編 號304系列、及不銹鋼編號316系列之其中一者。 如申凊專利範圍第9項之不銹鋼容器,其中,該第一 不銹鋼結合板係食品級不銹鋼材。 7·如申請專利範圍第9項之不銹鋼容器,1中,該第— ,鋼結合板仙雷射焊接無縫地焊接衫料體之 弗一開放側。 18.如申請專利範圍第17項之不銹鋼容器,其中,該第— 不銹鋼結合板與管狀本體之第—開放側之接:、 雷射谭接熔融兩不銹鋼銲件之接缝,以形夢: 品質之焊接面。 7精確且高 Ή請專利範圍第9項之不軸容器,其中 倒角係位於第一不銹鋼结合_ u亥弟一 處,《使焊接面具二之焊接 2〇 a 、〈表面精細度。 .如申請專利範圍第19項之 甸角係選自圓弧面、斜面之其中一者。,、中,該第- 21.如申請專利範圍第9項之不銹鋼容器 不銹鋼結合板復包括一嘴頭。 /、.,該第一 Π0180 20 200836983 ,22:如申請專利範圍第21項之不錢鋼容器,其中,該嘴頭 係以雷射焊接於第一不銹鋼結合板之開口。 23. 如申請專利範圍帛22項之不録鋼容器幵,其。中,該嘴頭 係選自不銹鋼編號303系列、不録鋼編號綱系列、 及不銹鋼編號316系列之其中一者。 24. 如申明專利範圍第22項之不銹鋼容器,其中,該嘴頭 係食品級不錄鋼材。 25. 士申„月專利範圍第9項之不銹鋼容器,其中,該第二 春不錢鋼結合板係選自不錄鋼編號3〇3系列、不錄鋼編 號304系列、及不銹鋼編號316系列之其中一者。 26. 如申明專利粑圍第9項之不銹麵容器,其中,該第二 不銹鋼結合板係食品級不銹鋼材。 27. 如申請專利範圍第9項之不銹鋼容器,直中,該第二 I銹鋼結合板係以雷射焊接無縫地焊接於管狀本體之 弟一開放側。 • 士申明專利範圍第27項之不銹鋼容器,JL中,該第二 ‘=錄鋼結合板與管狀本體H放侧之接縫處係以一 ••射焊祕融料義銲件之接缝,㈣成精確且高 品質之焊接面。 . Μ.如申請專利範圍帛9項之不錄鋼容器,其中,該第二 2角係位於第二不銹鋼結合板與該第二開放側之焊接 處’以使焊接面具有高品質之表面精細度。 申明專利fe圍第9項之不_鋼容器,其中,復包括 一瓶蓋及瓶頂’該第-不銹鋼結合板復包括—嘴頭。 110180 21 200836983 ‘ 31:如申請專利範圍第30項之不銹鋼容器,其中,該瓶頂 之一鈿。卩係供套設該瓶盍,以供該瓶蓋鎖固於該嘴 頭、,另-端部係凸設-凸點,以供焊接時聚熱於該凸 點並易於焊接於第一不銹鋼結合板之表面。 32.如申請專利範圍第9項之不錄鋼容器,其中,復包括 • &amp;成於狀本體外表面之熱昇華轉印®案。 青專利範圍第”項之不銹鋼容器’、 管狀本體==先在表面塗佈有-層轉印漆之 於表面之塗佈漆層= ^華轉印圖案轉印 紙去除,即可於又力再舲载有熱汁華轉印圖案之貼 式樣。 ;秀鋼製之官狀本體表面形成變化之 110180 22200836983 X., 申讳专利范围·· ^ A: Pound: f-fabrication method, the steps of which include: ^η 32 g-shaped body, 俾 defined by the tubular body with an open side and a second open side; The welding method of the second welding method closes the first-open side of the first-shaped body; and the welding method of the non-recorded steel container of the second item is closed; 2(9) The tubular body is formed by seamlessly welding the stainless steel plate joint by laser welding by wrapping the steel tube around the shape of the tube and fixing it with a fixture. The method for manufacturing the non-recorded steel container of the i-th item, wherein the stainless steel bonding plate comprises an opening, and the opening is for the addition of the stainless steel container of the third item of the patent scope, wherein the system is _ pressure After forming, the nozzle is welded to the opening of the first stainless steel plate by laser welding. Open the method of making a stainless steel container of the third item, including the 20% bottle cap and _' so that the bottle cap is placed on one end of the bottle top μ 'μ for the bottle cap to be locked in the mouth Head, another _ end (four) convex - convex: green μ gathers heat (four) bumps during welding, so that w is welded to the surface of the first 6· stainless steel bonded plate. For example, the method for preparing a stainless steel container according to item 1 of the patent application includes 110180 18 200836983. • The outer surface of the woven tubular body forms a sublimation transfer pattern. 7. The method for manufacturing a stainless steel container according to claim 6 of the patent scope, which comprises: - a sticker carrying a sublimation transfer pattern is coated on a tubular body previously in the transfer paint, and the sublimation transfer is carried out by sublimation H is printed on the surface-coated lacquer layer, and the sticker is removed to form a pattern on the surface of the official body. 8. If the method for manufacturing a non-recorded steel container in the scope of patent application is i, the system is formed by looping a plurality of stainless steel plates. 9· A stainless steel container, comprising: a tubular body, which is formed by not recording a steel plate, and defines a space f, a first open side and a second open side; The plate is closed by laser welding: the open side of the crucible is formed with an opening and a chamfer adjacent to the first open side; and the shape is too much, the steel joint plate is The laser welding weld closes the body of the tube t: the second open side of the second side and is formed with a second chamfer adjacent to the second open side. The stainless steel container of the ninth section of the Benley rail, wherein the tubular edge. The edge of the open side is parallel to the second open side, such as the stainless steel container of the ninth member of the patent application scope, and the tubular system is made up of a number of stainless steel plates. A stainless steel container according to the first aspect, wherein the tubular recording steel plate is joined to the joining system by laser welding. 110180 19 200836983 • 13,·Please apply for the stainless steel container of the ninth patent range, wherein the tubular system is selected from one of the stainless steel number 303 series, the stainless steel number 3〇4 series, and the stainless steel number 316 series. By. 14. A stainless steel container according to item 9 of the patent application, wherein the tubular food grade stainless steel material. .15. The stainless steel container of claim 9, wherein the first steel bonded plate is selected from the group consisting of a stainless steel number 3〇3 series, a stainless steel number 304 series, and a stainless steel number 316 series. A stainless steel container according to claim 9, wherein the first stainless steel bonded plate is a food grade stainless steel. 7. If the stainless steel container of claim 9 is applied, in the first, the steel-bonded plate is welded to the open side of the woven body. 18. The stainless steel container of claim 17, wherein the first-stainless steel bonding plate is connected to the first open side of the tubular body: the laser is joined to the joint of the two stainless steel weldments to form a dream: Quality welding surface. 7 Accurate and high Please refer to the non-axis container of the ninth patent range, in which the chamfering is located in the first stainless steel joint _ u haidi, "the welding mask 2 welding 2 〇 a, < surface fineness. For example, the horn of the 19th item of the patent application is selected from one of a circular surface and a slope. ,, and, the first - 21. The stainless steel container of the ninth application patent scope includes a mouthpiece. /,., the first Π 0180 20 200836983, 22: The steel container of claim 21, wherein the nozzle is laser welded to the opening of the first stainless steel bonded plate. 23. If the scope of the patent application is 22, the steel container is not recorded. The mouth is selected from one of a stainless steel number 303 series, a non-recorded steel series series, and a stainless steel number 316 series. 24. The stainless steel container of claim 22, wherein the mouth is of a food grade and no steel is recorded. 25. Shishen „month patent scope ninth stainless steel container, wherein the second spring non-coin steel combination board is selected from the non-recorded steel number 3〇3 series, the unrecorded steel number 304 series, and the stainless steel number 316 series 26. A non-rust noodle container according to claim 9 of the patent, wherein the second stainless steel bonded plate is a food grade stainless steel. 27. The stainless steel container of claim 9 is straight. The second I-rust steel bonding plate is seamlessly welded to the open side of the tubular body by laser welding. • The stainless steel container of the 27th patent scope of the patent, JL, the second '= record steel The seam between the joint plate and the side of the tubular body H is a joint of the welder of the weldment, and (4) a precise and high-quality weld surface. 如. If the patent application scope is 9 The steel container is not recorded, wherein the second 2 angle is located at the welding joint of the second stainless steel bonding plate and the second open side to make the welding surface have high quality surface fineness. _ steel container, wherein the complex includes a cap and bottle top 'this - Stainless steel bonded plate includes - mouth. 110180 21 200836983 ' 31: A stainless steel container according to claim 30, wherein one of the tops of the bottle is provided for the bottle cap. Locked to the mouth, the other end is convex-bump for heat gathering on the bump during welding and is easy to be welded to the surface of the first stainless steel bonding plate. 32. The non-recorded steel container, in which the complex includes &amp; is formed on the outer surface of the thermal sublimation transfer ® case. The patent scope of the "stainless steel container", the tubular body == first coated on the surface - layer The coating layer of the transfer paint on the surface = ^ Hua transfer pattern transfer paper is removed, and then it can be loaded with the hot juice transfer pattern. The surface of the official body of Xiugang is changed 110110 22
TW96107021A 2007-03-01 2007-03-01 Stainless steel container and method for making the same TW200836983A (en)