TW200501258A - Method of polishing semiconductor copper interconnect integrated with extremely low dielectric constant material - Google Patents
Method of polishing semiconductor copper interconnect integrated with extremely low dielectric constant materialInfo
- Publication number
- TW200501258A TW200501258A TW092116479A TW92116479A TW200501258A TW 200501258 A TW200501258 A TW 200501258A TW 092116479 A TW092116479 A TW 092116479A TW 92116479 A TW92116479 A TW 92116479A TW 200501258 A TW200501258 A TW 200501258A
- Authority
- TW
- Taiwan
- Prior art keywords
- dielectric constant
- extremely low
- low dielectric
- constant material
- polishing
- Prior art date
Abstract
A method of polishing metal and barrier layer interconnect integrated with an extremely low dielectric constant material in a semiconductor process includes steps of (A) preparing a to-be-polished wafer covered with a copper layer integrated with an extremely low dielectric constant material, (B) treating the copper layer chemically to produce a hard and brittle very near surface layer product formed on the surface of the copper layer, (C) keeping polishing the very near surface layer product by ultrasonic waves, and (D) polishing a barrier layer of the wafer by the ultrasonic waves, thereby achieving polishing effectiveness.
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| TW092116479A TW200501258A (en) | 2003-06-17 | 2003-06-17 | Method of polishing semiconductor copper interconnect integrated with extremely low dielectric constant material |
| US10/617,679 US20040259481A1 (en) | 2003-06-17 | 2003-07-14 | Method of polishing semiconductor copper interconnect integrated with extremely low dielectric constant material |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| TW092116479A TW200501258A (en) | 2003-06-17 | 2003-06-17 | Method of polishing semiconductor copper interconnect integrated with extremely low dielectric constant material |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| TW200501258A true TW200501258A (en) | 2005-01-01 |
| TWI302350B TWI302350B (en) | 2008-10-21 |
Family
ID=33516546
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| TW092116479A TW200501258A (en) | 2003-06-17 | 2003-06-17 | Method of polishing semiconductor copper interconnect integrated with extremely low dielectric constant material |
Country Status (2)
| Country | Link |
|---|---|
| US (1) | US20040259481A1 (en) |
| TW (1) | TW200501258A (en) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN112809456A (en) * | 2021-01-13 | 2021-05-18 | 南京尚吉增材制造研究院有限公司 | Micro-nano bubble enhanced plasma polishing method |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| TW200846137A (en) * | 2007-05-17 | 2008-12-01 | Nat Univ Chung Cheng | Low-stress polishing apparatus |
Family Cites Families (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| NL163370C (en) * | 1972-04-28 | 1980-08-15 | Philips Nv | METHOD FOR MANUFACTURING A SEMI-CONDUCTOR DEVICE WITH A CONDUCTOR PATTERN |
| US5399234A (en) * | 1993-09-29 | 1995-03-21 | Motorola Inc. | Acoustically regulated polishing process |
| US5688364A (en) * | 1994-12-22 | 1997-11-18 | Sony Corporation | Chemical-mechanical polishing method and apparatus using ultrasound applied to the carrier and platen |
| US6051500A (en) * | 1998-05-19 | 2000-04-18 | Lucent Technologies Inc. | Device and method for polishing a semiconductor substrate |
| US6656842B2 (en) * | 1999-09-22 | 2003-12-02 | Applied Materials, Inc. | Barrier layer buffing after Cu CMP |
| US6682396B1 (en) * | 2000-04-11 | 2004-01-27 | Taiwan Semiconductor Manufacturing Co., Ltd | Apparatus and method for linear polishing |
-
2003
- 2003-06-17 TW TW092116479A patent/TW200501258A/en not_active IP Right Cessation
- 2003-07-14 US US10/617,679 patent/US20040259481A1/en not_active Abandoned
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN112809456A (en) * | 2021-01-13 | 2021-05-18 | 南京尚吉增材制造研究院有限公司 | Micro-nano bubble enhanced plasma polishing method |
| CN112809456B (en) * | 2021-01-13 | 2023-02-24 | 南京尚吉增材制造研究院有限公司 | Micro-nano bubble enhanced plasma polishing method |
Also Published As
| Publication number | Publication date |
|---|---|
| TWI302350B (en) | 2008-10-21 |
| US20040259481A1 (en) | 2004-12-23 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| TW200501270A (en) | Apparatus and method for depositing and planarizing thin films of semiconductor wafers | |
| WO2009019837A1 (en) | Silicon carbide semiconductor device and method for producing the same | |
| WO2003092041A3 (en) | Method for fabricating a soi substrate a high resistivity support substrate | |
| TW200515534A (en) | Improved chemical planarization performance for copper/low-k interconnect structures | |
| EP1386949A3 (en) | Aqueous dispersion for chemical mechanical polishing and its use for semiconductor device processing | |
| ATE445034T1 (en) | INTEGRATED METAL DEPOSITION AND PLANARIZATION METHOD AND APPARATUS THEREOF | |
| WO2003023848A3 (en) | Apparatus and method of surface treatment for electrolytic and electroless plating of metals in integrated circuit manufacturing | |
| TW200503054A (en) | Substrate processing method and substrate processing apparatus | |
| TW200520150A (en) | A method for forming dummy structures for improved CMP and reduced capacitance | |
| TW200710980A (en) | Method for manufacturing semiconductor device | |
| WO2003088318A3 (en) | Method of fabricating vertical structure leds | |
| TW200640612A (en) | Polishing pad, method of producing the same and method of producing semiconductor device by using the same | |
| TW200733218A (en) | Manufacturing method of semiconductor device | |
| EP1261021A3 (en) | Method of production of circuit board, semiconductor device, and plating system | |
| MY124499A (en) | Method for manufacturing semiconductor chips | |
| TW200501199A (en) | Methods of forming semiconductor mesa structures including self-aligned contact layers and related devices | |
| TW200707632A (en) | Semiconductor device and forming method thereof | |
| TW200605227A (en) | Semiconductor device and manufacturing method thereof | |
| TW200511422A (en) | Treatment or processing of substrate surfaces | |
| WO2003022523A1 (en) | Dressing tool, dressing device, dressing method, processing device, and semiconductor device producing method | |
| EP1039530A3 (en) | Method for manufacturing semiconductor device capable of avoiding flaws and erosion caused by metal chemical-mechanical polishing process | |
| EP1191128A3 (en) | Plating method and plating apparatus | |
| SG132691A1 (en) | Wafer processing method and wafer processing apparatus | |
| TW200420380A (en) | Polishing method | |
| TW200501258A (en) | Method of polishing semiconductor copper interconnect integrated with extremely low dielectric constant material |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| MK4A | Expiration of patent term of an invention patent |