SU92065A1 - Способ изготовлени пробужденного бетона из доменных шлаков - Google Patents
Способ изготовлени пробужденного бетона из доменных шлаковInfo
- Publication number
- SU92065A1 SU92065A1 SU419609A SU419609A SU92065A1 SU 92065 A1 SU92065 A1 SU 92065A1 SU 419609 A SU419609 A SU 419609A SU 419609 A SU419609 A SU 419609A SU 92065 A1 SU92065 A1 SU 92065A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- concrete
- awakened
- blast furnace
- making
- furnace slag
- Prior art date
Description
В насто щее врем при изготовлении пробужденного бетона дл производства шлаковых изделий из доменных шлаков (гранулированных и отвальных) в качестве активной добавки примен етс преимущественно цемент и реже известь, причем на 1 м пробужденного бетона расходуетс в среднем 100 кг цемента или 150 кг извести.
Предлагаетс заменить цемент и известь необожженной глиной и хлористым кальцием.
Приче1м глину вводить в шлак в виде порошка до его помола на бегунах, а хлористый кальций-в процессе помола в виде 10%-ного водного раствораБетон , изготовленный по предлагаемому способу, имеет прочность не ниже пробужденного бетона, изготовленного на основе обычных активизаторов.
Предмет изобретени
Способ изготовлени пробужденного бетона из доменных шлаков путем помола их с активизируюшими добавками, отличающийс тем, что в качестве активизаторов примен ют глину и хлористый кальций.