[go: up one dir, main page]

SU51595A1 - Method for making black oil lacquers - Google Patents

Method for making black oil lacquers

Info

Publication number
SU51595A1
SU51595A1 SU??-6032A SU6032A SU51595A1 SU 51595 A1 SU51595 A1 SU 51595A1 SU 6032 A SU6032 A SU 6032A SU 51595 A1 SU51595 A1 SU 51595A1
Authority
SU
USSR - Soviet Union
Prior art keywords
black oil
asphaltite
making black
sadkinsky
oil lacquers
Prior art date
Application number
SU??-6032A
Other languages
Russian (ru)
Other versions
SU4639A1 (en
Inventor
В.В. Жебровский
Б.С. Юдин
Original Assignee
В.В. Жебровский
Б.С. Юдин
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Publication of SU4639A1 publication Critical patent/SU4639A1/en
Application filed by В.В. Жебровский, Б.С. Юдин filed Critical В.В. Жебровский
Priority to SU??-6032A priority Critical patent/SU51595A1/en
Application granted granted Critical
Publication of SU51595A1 publication Critical patent/SU51595A1/en

Description

Насто щее изобретение касаетс  способа изготовлени  черного масл ного лака с применением садкинского асфальтита. Садкинский асфальтит по своим свойствам резко отличаетс  от других известных битумов. В то врем , как последние плав тс , соедин ютс  с льн ным маслом при 250° в отношении 1:1 и 1 :2 и раствор ютс  в обычных растворител х, Садкинский асфальтит не обладает всеми перечисленными свойствами.The present invention relates to a method for producing a black lacquer using Sadkinsky asphaltite. Sadkinsky asphaltite is very different in properties from other known bitumen. While the latter are melted, combined with linseed oil at 250 ° in the ratio of 1: 1 and 1: 2 and dissolved in conventional solvents, Sadkinsky asphaltite does not possess all of these properties.

Дл  плавлени  садкинского асфальтита требуетс  прибавление к нему до 50% канифоли, причем даже и этот плав соедин етс  с маслом лишь в отношении 3:1. Прибавление 50% канифоли в лак  вл етс  нежелательным , так как это ухудшает качество пленки.To melt Sadkinsky asphaltite, it is necessary to add to it up to 50% rosin, and even this melt is combined with oil only in the ratio of 3: 1. The addition of 50% rosin to the lacquer is undesirable because it impairs the quality of the film.

Эти особенности садкинского асфальтита не позвол ют примен ть его дл  изготовлени  лака обычным способом .These features of Sadkin asphaltite do not allow its use for the manufacture of varnish in the usual way.

Предлагаемый, согласно насто щему изобретению, способ заключаетс  в следующем. Садкинский асфальтит в смеси с канифолью и свинцовомарганцевым линолеатом нагреваетс  с сырым льн ным маслом до 250- 350°. В отличие от обычного процессаThe method according to the present invention is as follows. Sadkinsky asphaltite mixed with rosin and lead-manganese linoleate is heated with raw flax oil to 250-350 °. Unlike the normal process

приготовлени  битуминозных лаков смол на  часть нагреваетс  не со всем потребным количеством льн ного масла , а лишь с частью его, не превышающей 25% от всего сплава асфальтита с канифолью, и нагревание производитс  без уваривани .preparing tar tar paints for a part is not heated with all the required amount of linseed oil, but only with a part of it not exceeding 25% of the whole asphaltite alloy with rosin, and heating is performed without boiling down.

Льн ное масло примен етс  в сыром виде в отличие от обычных способов, когда примен ютс  главным образом полимеризованные или оксидированные масла.Flaxseed oil is used raw, unlike conventional methods, when mainly polymerized or oxidized oils are used.

Нагретому до указанной температуры плаву дают охладитьс  до 180- 200°, после чего заливают растворитель-скипидар , уайт-спирт и по охлаждении всей массы добавл ют остальное потребное количество сырого льн ного масла.The melt heated to the specified temperature is allowed to cool to 180-200 °, then the turpentine solvent and white alcohol are poured, and after cooling the whole mass, the remaining required amount of raw linseed oil is added.

Полученный описанным способом лак по своим качествам не уступает другим, изготовленным на более дорогом сырье.The varnish obtained by the described method is not inferior in its qualities to others produced on more expensive raw materials.

Предмет изобретени .The subject matter of the invention.

Способ изготовлени  черных масл ных лаков, отличающийс  тем, что Садкинский асфальтит с добавлением свинцово-марганцевого линолеата и канифоли нагревают вместе с частьюA method of manufacturing black oil varnishes, characterized in that the Sadkinsky asphaltite with the addition of lead-manganese linoleate and rosin is heated together with a part of

{до 25% от веса смеси) сырого льн ного масла, до 250-350° без уваривани , заливают растворителем, после{up to 25% by weight of the mixture) crude linseed oil, up to 250-350 ° without boiling down, is poured with solvent, after

чего массу охлаждают и на холоду добавл ют остальное количество сырого льн ного масла.then the mass is cooled and the rest of the crude linseed oil is added in cold.

SU??-6032A 1937-03-26 1937-03-26 Method for making black oil lacquers SU51595A1 (en)