[go: up one dir, main page]

SU1365537A1 - Soldering paste for low-temperature soldering - Google Patents

Soldering paste for low-temperature soldering

Info

Publication number
SU1365537A1
SU1365537A1 SU3994110/27A SU3994110A SU1365537A1 SU 1365537 A1 SU1365537 A1 SU 1365537A1 SU 3994110/27 A SU3994110/27 A SU 3994110/27A SU 3994110 A SU3994110 A SU 3994110A SU 1365537 A1 SU1365537 A1 SU 1365537A1
Authority
SU
USSR - Soviet Union
Prior art keywords
soldering
paste
low
temperature
hydroxypolyoxyethylene
Prior art date
Application number
SU3994110/27A
Other languages
Russian (ru)
Inventor
Е.М. Григорьева
Т.В. Архипова
Original Assignee
Е.М. Григорьева
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Е.М. Григорьева filed Critical Е.М. Григорьева
Priority to SU3994110/27A priority Critical patent/SU1365537A1/en
Application granted granted Critical
Publication of SU1365537A1 publication Critical patent/SU1365537A1/en

Abstract

FIELD: tinning and soldering. SUBSTANCE: paste has components at the following ratio, wt. -%: colophony 7.0-9.5; hydroxy-derivative compound of alkylamine order (dibutanolamine, triethanolamine, butylethanolamine) 7.0-9.5; hydroxypolyoxyethylene of molecular mass 1500-20000 0.75-1.5, and solder powder - the rest. Storage time of soldering paste without stratification is 3 months, retentivity coefficient is 95%. EFFECT: enhanced quality of paste and soldered welds. 2 tbl
SU3994110/27A 1985-10-21 1985-10-21 Soldering paste for low-temperature soldering SU1365537A1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
SU3994110/27A SU1365537A1 (en) 1985-10-21 1985-10-21 Soldering paste for low-temperature soldering

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
SU3994110/27A SU1365537A1 (en) 1985-10-21 1985-10-21 Soldering paste for low-temperature soldering

Publications (1)

Publication Number Publication Date
SU1365537A1 true SU1365537A1 (en) 1996-06-10

Family

ID=60533827

Family Applications (1)

Application Number Title Priority Date Filing Date
SU3994110/27A SU1365537A1 (en) 1985-10-21 1985-10-21 Soldering paste for low-temperature soldering

Country Status (1)

Country Link
SU (1) SU1365537A1 (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
RU2591920C1 (en) * 2015-04-13 2016-07-20 Акционерное общество "Научно-производственный центр "Алмаз-Фазотрон" Solder paste
RU2767945C1 (en) * 2020-09-25 2022-03-22 Олег Арсентьевич Шапошников Solder paste preparation method

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
RU2591920C1 (en) * 2015-04-13 2016-07-20 Акционерное общество "Научно-производственный центр "Алмаз-Фазотрон" Solder paste
RU2767945C1 (en) * 2020-09-25 2022-03-22 Олег Арсентьевич Шапошников Solder paste preparation method

Similar Documents

Publication Publication Date Title
JPS5439341A (en) Diffusion welding of copper and stainless steel
MX167124B (en) FUEL COMPOSITION CONTAINING A METAL COMPOUND AND AN OXIME
DE2960939D1 (en) Novel n,n'-bis(trifluoromethylsulfonyl)oxamides, chemiluminescent compositions containing them and processes for generating chemiluminescence employing said compositions
SU1365537A1 (en) Soldering paste for low-temperature soldering
JPS5486635A (en) First liquid of cold-wave lotion
GB1436496A (en) Aluminothermic reaction mixture based on copper oxide
EP0291064A3 (en) Conductive paste composition
JPS51132108A (en) Alloy for hydrogen storage
EP0628370A4 (en) Soldering method and apparatus.
JPS57116003A (en) Novel herbicide
JPS5357425A (en) Transformer with sealed insulation medium
AU554432B2 (en) High concentration amine oxide formulations
JPS51144984A (en) Connecting method of terminal
SU1340197A1 (en) ALLOY BASED ON ALUMINUM
JPS51117574A (en) Semiconductor equipment
EP0063328A3 (en) Compositions containing secretin and method for preventing the adsorption of secretin
JPS5379782A (en) Protein adsorbing substance
Storchai et al. The Effect of Gap Size and Composition of the Flux Bath on Capillary Flow of Solder in the Joining of Aluminum
JPS5212621A (en) High strength copper-base alloy for electroconductor
Kehrer et al. WEICHLOETEN VON GOLDOBERGLAECHEN...(SOFT SOLDERING OF GOLD SURFACES IN ELECTRICAL ENGINEERING)
SU1339983A1 (en) FLUX FOR HIGH-TEMPERATURE SOLDERING
GB917173A (en) Improvements in or relating to soldering bits
Muller et al. Solderability of Gold-Flashed Nickel Plate
Sarma et al. Soldering--Equally Contributes to the Reliability of a System
JPS53122611A (en) Desulfurizing agent for molten metal