RU176135U1 - STAMP FOR CUTTING A STEEL FASTENING ELEMENT FROM A SOCKET OF A FASTENING SCREW OF ELECTROMAGNETIC RELAY - Google Patents
STAMP FOR CUTTING A STEEL FASTENING ELEMENT FROM A SOCKET OF A FASTENING SCREW OF ELECTROMAGNETIC RELAY Download PDFInfo
- Publication number
- RU176135U1 RU176135U1 RU2017114590U RU2017114590U RU176135U1 RU 176135 U1 RU176135 U1 RU 176135U1 RU 2017114590 U RU2017114590 U RU 2017114590U RU 2017114590 U RU2017114590 U RU 2017114590U RU 176135 U1 RU176135 U1 RU 176135U1
- Authority
- RU
- Russia
- Prior art keywords
- matrix
- plate
- punch holder
- punch
- sleeve
- Prior art date
Abstract
Предлагаемое техническое решение относится к области разборки электромагнитных реле с целью их утилизации с использованием штампов и может быть использовано для вырубки стального крепежного элемента из барашка крепежного винта электромагнитного реле 3-го поколения железнодорожной автоматики и телемеханики. Задача заявляемого технического решения - утилизация элементов автоматики и телемеханики железнодорожного транспорта. При решении поставленной задачи достигается технический результат, заключающийся в повышении производительности разборки электромагнитных реле, исключении ручного труда. Указанный технический результат достигается штампом для вырубки стального крепежного элемента из барашка крепежного винта электромагнитного реле, имеющего симметричное диагональное расположение направляющих колонок и втулок, содержащий верхнюю подвижную плиту с закрепленными на ней пуансонодержателем, прокладкой, расположенной между верхней плитой и пуансонодержателем, пуансон, закрепленный в пуансонодержателе, выполненный в виде двух соосных цилиндров, вырубающего и крепежного, соединенных цилиндрическим буртиком, кожух верхний, закрепленный на пуансонедержателе, кожух верхний выполнен в виде втулки, имеет цилиндрическую часть и торец, которой прижат к пуансону держателю, неподвижную, нижнюю плиту, установленную на опорной плите, матрицу, и кожух нижний, установленные на нижней плите, матрицу, выполненную в виде втулки, имеющей цилиндр и буртик, цилиндр входит в отверстие основания кожуха нижнего и в отверстие плиты нижней, а буртик входит в проточку, выполненную в основании кожуха, кожух нижний выполнен в виде втулки, имеющей цилиндрическую часть и торец, которой прижат к плите нижней, на внутренней стороне торца втулки выполнены две проточки, большего диаметра, для установки барашка крепежного элемента, меньшего диаметра, для установки матрицы.The proposed technical solution relates to the field of disassembling electromagnetic relays for the purpose of their disposal using dies and can be used to cut down a steel fastener from a wing of a fastening screw of an electromagnetic relay of the 3rd generation of railway automation and telemechanics. The objective of the proposed technical solution is the disposal of elements of automation and telemechanics of railway transport. When solving this problem, a technical result is achieved, consisting in increasing the performance of disassembling electromagnetic relays, eliminating manual labor. The specified technical result is achieved by a stamp for cutting a steel fastener from a wing of a fastening screw of an electromagnetic relay having a symmetrical diagonal arrangement of guide columns and bushings, containing an upper movable plate with a punch holder fixed thereon, a gasket located between the upper plate and the punch holder, a punch fixed in the punch holder made in the form of two coaxial cylinders, cutting and fixing, connected by a cylindrical collar, the upper casing mounted on the punch holder, the upper casing is made in the form of a sleeve, has a cylindrical part and an end to which the holder is pressed against the punch, a fixed, lower plate mounted on a base plate, a matrix, and a lower casing mounted on a lower plate, a matrix made in the form a sleeve having a cylinder and a flange, the cylinder enters the hole in the base of the lower casing and in the hole of the bottom plate, and the collar enters the groove made in the base of the casing, the lower casing is made in the form of a sleeve having a cylindrical part and an end face, which pressed to the bottom plate, on the inner side of the end face of the sleeve two grooves are made, of a larger diameter, for installing a lamb of a fastener, of a smaller diameter, for installing the matrix.
Description
Предлагаемое техническое решение относится к области разборки электромагнитных реле с целью их утилизации с использованием штампов и может быть использовано для вырубки стального крепежного элемента из барашка крепежного винта электромагнитного реле 3-го поколения железнодорожной автоматики и телемеханики.The proposed technical solution relates to the field of disassembling electromagnetic relays for the purpose of their disposal using dies and can be used to cut down a steel fastener from a wing of a fixing screw of an electromagnetic relay of the 3rd generation of railway automation and telemechanics.
Широко известно применение штампов различных конструкций, в том числе и для разделительных операций (Справочник конструктора штампов: Листовая штамповка / Под общей редакцией Л.И. Рудмана - М.: Машиностроение, 1988 г. - 496 с. стр. 48-168). В качестве недостатка представленных конструкций штампов следует отметить их невозможность применения при разборке электромагнитных реле, когда требуется выполнять операции отрезки на готовом изделии в целом иди на отдельных его узлах. Для каждой разделительной операции, при разборке электромагнитных реле с целью их утилизации, конструктивно необходимо разрабатывать отдельный штамп, с учетом особенностей выполняемой операции, конструкции детали, узла и устройства реле в целом.It is widely known the use of stamps of various designs, including for separating operations (Handbook of the stamp designer: Sheet stamping / Under the general editorship of LI Rudman - M .: Mechanical Engineering, 1988 - 496 p. 48-168). As a drawback of the stamp designs presented, it should be noted that they cannot be used when disassembling electromagnetic relays, when it is necessary to carry out segment operations on the finished product as a whole, go to its individual nodes. For each separation operation, when disassembling electromagnetic relays for the purpose of their disposal, it is structurally necessary to develop a separate stamp, taking into account the features of the operation performed, the design of the part, assembly and relay device as a whole.
Задача заявляемого технического решения является утилизация элементов автоматики и телемеханики железнодорожного транспорта.The objective of the proposed technical solution is the disposal of elements of automation and telemechanics of railway transport.
При решении поставленной задачи достигается технический результат, заключающийся в повышении производительности разборки электромагнитных реле, исключении ручного труда.When solving this problem, a technical result is achieved, consisting in increasing the performance of disassembling electromagnetic relays, eliminating manual labor.
Указанный технический результат достигается штампом для вырубки стального крепежного элемента из барашка крепежного винта электромагнитного реле, имеющего симметричное диагональное расположение направляющих колонок и втулок, содержащий верхнюю подвижную плиту с закрепленными на ней пуансонодержателем, прокладкой, расположенной между верхней плитой и пуансонодержателем, пуансон, закрепленный в пуансонодержателе, выполненный в виде двух соосных цилиндров, вырубающего и крепежного, соединенных цилиндрическим буртиком, кожух верхний, закрепленный на пуансонедержателе, кожух верхний выполнен в виде втулки, имеет цилиндрическую часть и торец, которой прижат к пуансону держателю, неподвижную, нижнюю плиту, установленную на опорной плите, матрицу, и кожух нижний, установленные на нижней плите, матрицу, выполненную в виде втулки, имеющей цилиндр и буртик, цилиндр входит в отверстие основания кожуха нижнего и в отверстие плиты нижней, а буртик входит в проточку, выполненную в основании кожуха, кожух нижний выполнен в виде втулки, имеющей цилиндрическую часть и торец, которой прижат к плите нижней, на внутренней стороне торца втулки выполнены две проточки, большего диаметра, для установки барашка крепежного элемента, меньшего диаметра, для установки матрицы. Кроме этого, пуансонодержатель и плита верхняя соединены с помощь винтов, матрица выполнены из углеродистой инструментальной стали и имеют твердость (59-62) HRC, цилиндрическая часть кожуха нижнего в цилиндрическая часть кожуха верхнего, образуя замкнутую камеру, на кожухе нижнем неподвижно закреплена ручка, матрица запрессована в основание кожух нижнего, а пуансон в запрессован в пуансонодержатель, на плите верхней закреплен хвостовик, для соединения с приводом.The specified technical result is achieved by a stamp for cutting a steel fastener from a wing of a fixing screw of an electromagnetic relay having a symmetrical diagonal arrangement of guide columns and bushings, containing an upper movable plate with a punch holder fixed thereon, a gasket located between the upper plate and the punch holder, a punch fixed in the punch holder made in the form of two coaxial cylinders, cutting and fixing, connected by a cylindrical collar, the upper casing mounted on the punch holder, the upper casing is made in the form of a sleeve, has a cylindrical part and an end to which the holder is pressed against the punch, a fixed, lower plate mounted on a base plate, a matrix, and a lower casing mounted on a lower plate, a matrix made in the form a sleeve having a cylinder and a flange, the cylinder enters the hole in the base of the lower casing and in the hole of the bottom plate, and the collar enters the groove made in the base of the casing, the lower casing is made in the form of a sleeve having a cylindrical part and an end face, which pressed to the bottom plate, on the inner side of the end face of the sleeve two grooves are made, of a larger diameter, for installing a lamb of a fastener, of a smaller diameter, for installing the matrix. In addition, the punch holder and the upper plate are connected by screws, the matrix is made of carbon tool steel and have a hardness of (59-62) HRC, the cylindrical part of the lower casing into the cylindrical part of the upper casing, forming a closed chamber, the handle is fixedly fixed on the lower casing, the matrix the lower casing is pressed into the base, and the punch is pressed into the punch holder; the shank is fixed to the upper plate to connect to the drive.
Заявляемое техническое решение поясняется чертежами, на которых показаны: на фиг. 1 - вид штампа в плане, по сечению А-А фиг. 3, на фиг. 2 - вид штампа в плане, по сечению Б-Б фиг. 4, на фиг. 3 - нижняя часть штампа, вид сверху, на фиг. 4 - верхняя плита, вид сверху, на фиг. 5 - пуансон, на фиг. 6 - матрица втулка, на фиг. 7 - верхний кожух, на фиг. 8 - нижний кожух в сборе с матрицей и ручкой.The claimed technical solution is illustrated by drawings, which show: in FIG. 1 is a plan view of a stamp along section AA of FIG. 3, in FIG. 2 is a plan view of a stamp along section BB of FIG. 4, in FIG. 3 - lower part of the stamp, top view, in FIG. 4 - top plate, top view, in FIG. 5 is a punch, in FIG. 6 - matrix sleeve, in FIG. 7 - the upper casing, in FIG. 8 - lower casing complete with a matrix and a handle.
Штамп для вырубки стального крепежного элемента из барашка крепежного винта электромагнитного реле, состоит из диагонально расположенных направляющих колонок 1 и втулок 2, содержит верхнюю подвижную плиту 3 с закрепленными на ней пуансонодержателем 5, прокладкой 4, расположенной между верхней плитой 3 и пуансонодержателем 5. Пуансон 6 закреплен в пуансонодержателе 5, выполнен в виде двух соосных цилиндров, вырубающего 6.1 и крепежного 6.2, соединенных цилиндрическим буртиком 6.3. Кожух 7 верхний, закреплен на пуансонодержателе 5, кожух 7 верхний выполнен в виде втулки, имеет цилиндрическую часть 7.1 и торец 7.2, которой прижат к пуансонодержателю 5. Неподвижная, нижняя плита 8, установлена на опорной плите 9. Матрица 10 и кожух 11 нижний установлены на нижней плите 8. Матрица 10 выполнена в виде втулки, имеющей цилиндр 10.1 и буртик 10.2, цилиндр 10.1 входит в отверстие основания 11.1 кожуха 11 нижнего и в отверстие 8.1 плиты 8 нижней, а буртик 10.2 входит в проточку, выполненную в основании 11.1 кожуха 11. Кожух 11 нижний выполнен в виде втулки, имеющей цилиндрическую часть 11.2 и основание (торец) 11.1, которой прижат к плите 8 нижней. На внутренней стороне торца 11.1 втулки выполнены две проточки, большего диаметра, для установки барашка крепежного элемента (на фиг. 3 показан контур барашка), меньшего диаметра, для установки матрицы 8. Пуансонодержатель 5 и плита 4 верхняя соединены с помощь винтов 12. Матрица выполнены из углеродистой инструментальной стали и имеют твердость (59-62) HRC. Цилиндрическая часть 11.2 кожуха 11 нижнего входит в цилиндрическую часть 7.1 кожуха 7 верхнего, образуя замкнутую камеру 13. На кожухе 11 нижнем неподвижно закреплена ручка 14. Матрица 10 запрессована в основание 11.1 кожух 11 нижнего, а крепежная часть 6.2 пуансон 6 в запрессован в пуансонодержатель 5, на плите 3 верхней закреплен хвостовик 15, для соединения с приводом.The stamp for cutting the steel fastener from the lamb of the fixing screw of the electromagnetic relay, consists of diagonally arranged
Штамп работает следующим образом. Для вырубки стального крепежного элемента из барашка крепежного винта электромагнитного реле, пуансон 6 с верхней плитой 5 отводится вверх относительно матрицы 10. Барашек устанавливается в проточку на нижнем кожухе 11. Во время рабочего хода пуансона 6 с плитой 5 происходит вырубание стольного крепежного элемента. Предлагаемое техническое решение позволяет быстро, с минимальными затратами ручного труда отделить крепежный элемент из барашка крепежного винта электромагнитного реле. Штамп для вырубки стального крепежного элемента из барашка крепежного винта электромагнитного реле, проходит производственные испытания на Камышловском электротехническом заводе.The stamp works as follows. For cutting the steel fastener from the wing of the fastening screw of the electromagnetic relay, the
Claims (7)