JP2013067868A - 金属連続体の溶融浸漬被覆装置 - Google Patents
金属連続体の溶融浸漬被覆装置 Download PDFInfo
- Publication number
- JP2013067868A JP2013067868A JP2013008305A JP2013008305A JP2013067868A JP 2013067868 A JP2013067868 A JP 2013067868A JP 2013008305 A JP2013008305 A JP 2013008305A JP 2013008305 A JP2013008305 A JP 2013008305A JP 2013067868 A JP2013067868 A JP 2013067868A
- Authority
- JP
- Japan
- Prior art keywords
- container
- metal
- guide passage
- height
- continuous body
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
【解決手段】 金属連続体1″′を溶融浸漬被覆するための装置であって、この装置が、 −溶融した被覆金属2″′を収容する容器3″′を備え、この容器を通って前記金属連続体1″′が垂直に案内され、 −金属連続体の搬送方向Rでこの容器の手前に接続配置された案内通路4″′を備え、この案内通路の領域内において、少なくとも2個のインダクタ5が、被覆金属2″′を容器3″′内に保持するために、金属連続体1″′の両側において配置され且つこの容器から間隔をあけられており、
その際、少なくとも2つの管11が、被覆金属2″′の側方からの供給のために備えられており、これら管が、インダクタ5の垂直方向の高さHの半分の高さH/2において、水平方向に前記案内通路4″′内へと開口している。
【選択図】 図9
Description
金属連続体を溶融浸漬被覆するための装置であって、この装置が、
−溶融した被覆金属を収容する容器を備え、この容器を通って前記金属連続体が垂直に案内され、
−金属連続体の搬送方向でこの容器の手前に接続配置された案内通路を備え、この案内通路の領域内において、少なくとも2個のインダクタが、被覆金属を容器内に保持するために、金属連続体の両側において配置され且つこの容器から間隔をあけられており、
その際、少なくとも2つの管が、被覆金属の側方からの供給のために備えられており、これら管が、インダクタの垂直方向の高さHの半分の高さH/2において、水平方向に前記案内通路内へと開口していることによって解決される。
1′ 金属連続体
1″ 金属連続体
1″′ 金属連続体
2 被覆金属
2′ 被覆金属
2″ 被覆金属
2″′ 被覆金属
3 容器
3′ 容器
3″ 容器
3″′ 容器
3a 底
3a′ 底
3a″ 底
3a″′ 底
3b 通過穴
3b′ 通過穴
3b″ 通過穴
3b″′ 通過穴
4 案内通路
4′ 案内通路
4″ 案内通路
4″′ 案内通路
4a 範囲
4a′ 範囲
4a″ 範囲
4a″′ 範囲
5 インダクタ
6 縦壁
6′ 縦壁
6″ 縦壁
6″′ 縦壁
7 横壁
8 上側のインダクタエッジ
9 壁中断部
10 膨らみ部
11 管
B1 下側の幅
B1′ 下側の幅
B2 上側の幅
B2′ 上側の幅
H 高さ
H/2 半分の高さ
H/3 3分の1の高さ
R 搬送方向
RS 環状隙間
U 下端
V 容積
X 間隔
Claims (2)
- 金属連続体(1″′)を溶融浸漬被覆するための装置であって、この装置が、
−溶融した被覆金属(2″′)を収容する容器(3″′)を備え、この容器を通って前記金属連続体(1″′)が垂直に案内され、
−金属連続体の搬送方向(R)でこの容器の手前に接続配置された案内通路(4″′)を備え、この案内通路の領域内において、少なくとも2個のインダクタ(5)が、被覆金属(2″′)を容器(3″′)内に保持するために、金属連続体(1″′)の両側において配置され且つこの容器から間隔をあけられており、
その際、少なくとも2つの管(11)が、被覆金属(2″′)の側方からの供給のために備えられており、これら管が、インダクタ(5)の垂直方向の高さ(H)の半分の高さ(H/2)において、水平方向に前記案内通路(4″′)内へと開口していることを特徴とする装置。 - 案内通路(4″′)が長方形の横断面を有していることと、前記長方形の横断面の各々の短辺に少なくとも1本の管(11)が開口していることを特徴とする請求項1に記載の装置。