[go: up one dir, main page]

JP2008281968A - How to decorate resin frames - Google Patents

How to decorate resin frames Download PDF

Info

Publication number
JP2008281968A
JP2008281968A JP2007150954A JP2007150954A JP2008281968A JP 2008281968 A JP2008281968 A JP 2008281968A JP 2007150954 A JP2007150954 A JP 2007150954A JP 2007150954 A JP2007150954 A JP 2007150954A JP 2008281968 A JP2008281968 A JP 2008281968A
Authority
JP
Japan
Prior art keywords
resin
decorative plate
temple
plate
frame
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2007150954A
Other languages
Japanese (ja)
Inventor
Masatomo Kuroda
正知 黒田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
PLUS JACK KK
Original Assignee
PLUS JACK KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by PLUS JACK KK filed Critical PLUS JACK KK
Priority to JP2007150954A priority Critical patent/JP2008281968A/en
Publication of JP2008281968A publication Critical patent/JP2008281968A/en
Pending legal-status Critical Current

Abstract

【課題】樹脂製テンプル表面の装飾片の剥がれ等をなくす事。
【解決手段】樹脂製フレーム(10)の表面にポリウレタン樹脂系のプライマー(11)を塗布し、乾燥後、その上に金属製の長尺プレート、又は印刷を施された長尺の樹脂プレート(20)を置き、更にその上からクリアーな二液性のエポキシ樹脂接着剤(15)を被覆、又は前記装飾プレートを埋設させるように塗布した事を特徴とする樹脂製フレームの加飾方法を採用した
【選択図】図2
[PROBLEMS] To eliminate peeling of decorative pieces on the surface of a resin temple.
A polyurethane resin-based primer (11) is applied to the surface of a resin frame (10), dried, and then a metal long plate or a long resin plate printed thereon ( 20) and then a resinous frame decorating method characterized in that it is coated with a clear two-component epoxy resin adhesive (15) or coated so that the decorative plate is embedded. [Selection figure] Figure 2

Description

本発明は可撓性を有する樹脂製フレーム、特にテンプルに対する加飾方法に関する。  The present invention relates to a flexible resin frame, and more particularly to a method for decorating a temple.

従来、眼鏡の場合、可撓性を有する樹脂製フレーム、特にテンプルに装飾片を形成する装飾方法としては、所謂有機七宝と言われる熱硬化性のエポキシ樹脂を使用した装飾が昔から行われて来た。例えば、実開昭61−29313号の様に、図8の様に眼鏡枠体の一部に凹部を設け、樹脂層を形成し装飾板を載せ、更にその上部に透明エポキシ樹脂を流し込み七宝装飾30を形成させた眼鏡枠が提案されて来ている。  Conventionally, in the case of eyeglasses, as a decoration method for forming a decorative piece on a flexible resin frame, particularly a temple, decoration using a thermosetting epoxy resin called so-called organic cloisonne has been performed for a long time. I came. For example, as shown in Japanese Utility Model Publication No. 61-29313, as shown in FIG. 8, a concave portion is provided on a part of the spectacle frame, a resin layer is formed and a decorative plate is placed thereon, and a transparent epoxy resin is poured on the upper part to make a cloisonne decoration A spectacle frame in which 30 is formed has been proposed.

実開昭61−29313Shokai 61-29313

しかしながら上記手段に於いては、眼鏡枠、テンプルの一部分、スポット的にしか装飾を設ける事は出来なかった。それは、テンプルの長さ方向にある程度延長された装飾板を、ある程度可撓性を有するテンプルを眼鏡を掛ける際に、曲げる事を繰り返す事により接着面又は、装飾板と接着剤の境界面から剥がれて来るという問題が生じていた為にテンプルの一部分にしか装飾板を取り付ける事が出来なかったのである。  However, in the above-mentioned means, the decoration can be provided only in the spectacle frame, a part of the temple, or as a spot. It is peeled off from the bonding surface or the boundary surface between the decorative plate and the adhesive by repeatedly bending the decorative plate extended to some extent in the length direction of the temple when wearing the temple with some flexibility. Because of the problem of coming, it was possible to attach a decorative plate to only a part of the temple.

そこで上記課題を解決する為に、樹脂製フレームの表面にポリウレタン樹脂系のプライマーを塗布し、乾燥後、その上に装飾プレートを置き、更にその上からクリアーな二液性のエポキシ樹脂接着剤を被覆、又は前記装飾プレートを埋設させるように塗布した事を特徴とする樹脂製フレームの加飾方法を採用した。そして、前記装飾プレートが金属製の長尺プレート、又は印刷を施された長尺の樹脂プレートにした。  Therefore, in order to solve the above problems, a polyurethane resin primer is applied to the surface of the resin frame, and after drying, a decorative plate is placed on the primer, and a clear two-component epoxy resin adhesive is further applied thereon. A method of decorating a resin frame, which is characterized by being coated or coated so as to embed the decorative plate, was adopted. The decorative plate is a metal long plate or a printed long resin plate.

上記方法を採る事により、テンプルを開閉の際、或いは、外側に曲げても、ある程度長い装飾板(プレート)が剥がれる事も無く、接着剤の部分も皺や白濁を起す事無く装飾がはっきり視認出来た。繰り返しの実験では、樹脂製のテンプル本体の樹脂であるアセテートや、セルロース等に皺や白濁が起こるほどであった。  By adopting the above method, even if the temple is opened and closed or bent outward, the decorative plate (plate) that is long to some extent will not peel off, and the decoration will be clearly visible without causing wrinkles or cloudiness in the adhesive part. done. In repeated experiments, wrinkles and white turbidity occurred in acetate, cellulose, etc., which is a resin of the resin temple body.

樹脂製フレームの表面にポリウレタン樹脂系のプライマーを塗布し、乾燥後、その上に長尺の金属製又は樹脂製の装飾プレートを置き、更にその上からクリアーな二液性のエポキシ樹脂接着剤を被覆、又は前記装飾プレートを埋設させるように塗布した事を特徴とする樹脂製フレームの加飾方法。  Apply a polyurethane resin primer on the surface of the resin frame, and after drying, place a long metal or resin decorative plate on it, and then apply a clear two-part epoxy resin adhesive on it. A method of decorating a resin frame, characterized in that the coating is applied so as to embed the decoration plate.

図1は本発明の実施例の装飾が施された樹脂テンプル10の正面図であり、図2はそのA−A断面図である。この場合は芯穴12が加工されたか又は芯金13が挿入された後のテンプルの表面の所定の場所に、プライマーとしてポリウレタン系接着剤11を塗布し、その上に長尺の装飾プレート20を設置する。ここで長尺とは約2〜10cmである。更にその上に、常温の二液性のエポキシ系接着剤15を前記装飾プレート20を被覆又は埋設する様に厚く塗布し、乾燥させる。  FIG. 1 is a front view of a resin temple 10 with a decoration according to an embodiment of the present invention, and FIG. In this case, the polyurethane adhesive 11 is applied as a primer to a predetermined place on the surface of the temple after the core hole 12 is processed or the core bar 13 is inserted, and the long decorative plate 20 is applied thereon. Install. Here, the long length is about 2 to 10 cm. Further, a two-component epoxy adhesive 15 at room temperature is applied thickly so as to cover or embed the decorative plate 20 and dried.

又、図3、図4の様に、樹脂テンプル10aに凹部16を設けて、その中にポリウレタン系のプライマーを塗布し、そこに装飾プレート20aを設置し、更にその上から前記装飾プレート20aを被覆又は埋設するように厚く塗布し乾燥させる。  Also, as shown in FIGS. 3 and 4, a recess 16 is provided in the resin temple 10a, a polyurethane primer is applied therein, a decorative plate 20a is installed therein, and the decorative plate 20a is further mounted thereon. Apply thick to cover or embed and dry.

図5の場合は、図1,2の場合の要部拡大断面図であり、更に詳しく説明すると、樹脂テンプル10の表面にポリウレタン系プライマー11を塗布し、自然乾燥で約24時間又は、機械乾燥で50〜90℃で約20分〜60分掛けて乾燥させ、その上に装飾プレート20を設置する。この装飾プレート20は、表面に装飾を施してあるか又は装飾を施して無い金属製の材料、例えば、アルミ、金銀白金等の貴金属類、樹脂製の装飾プレート等が可能である。そして、その装飾プレートの上から常温の二液性のエポキシ系接着剤15を、前記装飾プレートを被覆又は埋設する様に厚く塗布する。ここでこのエポキシ系接着剤は透明又は半透明であることが好ましい。そして、上記二液性のエポキシ系接着剤として、例えば、接着剤としては低粘度グレードの可撓性タイプのエポキシ樹脂(粘度4〜9P/25℃、エポキシ当量390〜470、常温液状)、そして、硬化剤としては低粘度グレードの変性脂肪族ポリアミン、又は脂肪族アミン、及びそれらの混合が好ましい。そしてその後約50〜80℃で3〜6時間乾燥させると出来上がる。  5 is an enlarged cross-sectional view of the main part in the case of FIGS. 1 and 2. More specifically, the polyurethane primer 11 is applied to the surface of the resin temple 10 and is naturally dried for about 24 hours or mechanically dried. And drying at 50 to 90 ° C. for about 20 to 60 minutes, and the decorative plate 20 is placed thereon. The decorative plate 20 can be a metal material with or without decoration on its surface, for example, a noble metal such as aluminum, gold, silver, or platinum, or a resin decorative plate. Then, a two-component epoxy adhesive 15 at room temperature is applied thickly on the decorative plate so as to cover or embed the decorative plate. Here, the epoxy adhesive is preferably transparent or translucent. And as said two-component epoxy adhesive, for example, as an adhesive, a low viscosity grade flexible type epoxy resin (viscosity 4-9P / 25 ° C., epoxy equivalent 390-470, liquid at normal temperature), and The curing agent is preferably a low-viscosity grade modified aliphatic polyamine or aliphatic amine, and a mixture thereof. And it will be completed if it is made to dry for 3 to 6 hours at about 50-80 degreeC after that.

そして、図6は図3,4の場合の要部拡大断面図であり、樹脂テンプル10a凹部16を設けて、その中にポリウレタン系プライマー11aを塗布し、自然乾燥で約24時間、機械乾燥で約50〜90℃で20〜60分掛けて乾燥させ、その上に装飾プレート20aを載せる。そして前記凹部16と装飾プレート20aを埋め尽くすように常温の二液性エポキシ樹脂系接着剤15aを塗布又は注ぐ。そして約50〜80℃で約3〜6時間乾燥させ本装飾を得た。  FIG. 6 is an enlarged cross-sectional view of a main part in the case of FIGS. 3 and 4, a resin temple 10 a recess 16 is provided, and a polyurethane primer 11 a is applied therein, followed by natural drying for about 24 hours and mechanical drying. It is dried at about 50 to 90 ° C. for 20 to 60 minutes, and the decorative plate 20a is placed thereon. Then, an ordinary temperature two-component epoxy resin adhesive 15a is applied or poured so as to fill the recess 16 and the decorative plate 20a. And it dried at about 50-80 degreeC for about 3 to 6 hours, and obtained this decoration.

そして、図7の如く、外への曲げ試験を目視で行ったが装飾板20と接着部15、樹脂テンプル10と接着部15の間の境界面に異常は認められなかった。  Then, as shown in FIG. 7, the outward bending test was visually performed, but no abnormality was found on the boundary surface between the decorative plate 20 and the bonding portion 15 and between the resin temple 10 and the bonding portion 15.

図8は実開昭61−29313の従来図である。眼鏡枠体40の一部に凹部を設け、樹脂層を形成し装飾板を載せ、更にその上部に透明エポキシ樹脂を流し込み七宝装飾30を形成させた眼鏡枠を表している。  FIG. 8 is a conventional diagram of Japanese Utility Model Laid-Open No. 61-29313. A spectacle frame is shown in which a concave portion is formed in a part of the spectacle frame body 40, a resin layer is formed and a decorative plate is placed thereon, and a transparent epoxy resin is poured into the upper portion to form a cloisonne decoration 30.

本発明の実施例による樹脂テンプルの正面図The front view of the resin temple by the Example of this invention 図1のA−A断面図AA sectional view of FIG. 本発明の実施例による樹脂テンプルの正面図The front view of the resin temple by the Example of this invention 図3のB−B断面図BB sectional view of FIG. 図1,2の要部拡大断面図1 and 2 are enlarged cross-sectional views of essential parts. 図3,4の要部拡大断面図3 and 4 main part enlarged sectional view 本発明の樹脂テンプルの平面図Plan view of the resin temple of the present invention 従来図Conventional diagram

符号の説明Explanation of symbols

10 樹脂テンプル
11 プライマー層
12 芯穴
13 芯金
15 接着剤層
16 凹部
20 装飾プレート
30 七宝装飾部
40 眼鏡枠体
DESCRIPTION OF SYMBOLS 10 Resin temple 11 Primer layer 12 Core hole 13 Core metal 15 Adhesive layer 16 Recess 20 Decoration plate 30 Cloisonne decoration part 40 Eyeglass frame

Claims (2)

樹脂製眼鏡フレームの加飾方法であって、樹脂製フレームの表面にポリウレタン樹脂系のプライマーを塗布し、乾燥後、その上に装飾プレートを置き、更にその上からクリアーな二液性のエポキシ樹脂接着剤を被覆、又は前記装飾プレートを埋設させるように塗布した事を特徴とする樹脂製フレームの加飾方法。A method for decorating a plastic spectacle frame, which is a two-part epoxy resin that is coated with a polyurethane resin primer on the surface of the resin frame, dried, and then placed on a decorative plate. A method for decorating a resin frame, characterized in that an adhesive is coated or applied so as to embed the decorative plate. 前記装飾プレートが金属製の長尺プレート、又は印刷、装飾を施された長尺の樹脂プレートである事を特徴とする請求項1に記載の樹脂製フレームの加飾方法。The method for decorating a resin frame according to claim 1, wherein the decorative plate is a long metal plate or a long resin plate that is printed and decorated.
JP2007150954A 2007-05-10 2007-05-10 How to decorate resin frames Pending JP2008281968A (en)