FI872003A7 - Menetelmä korroosionestoaineiden vaikutuksen parantamiseksi vesisysteemeissä - Google Patents
Menetelmä korroosionestoaineiden vaikutuksen parantamiseksi vesisysteemeissäInfo
- Publication number
- FI872003A7 FI872003A7 FI872003A FI872003A FI872003A7 FI 872003 A7 FI872003 A7 FI 872003A7 FI 872003 A FI872003 A FI 872003A FI 872003 A FI872003 A FI 872003A FI 872003 A7 FI872003 A7 FI 872003A7
- Authority
- FI
- Finland
- Prior art keywords
- improving
- effect
- corrosion inhibitors
- water systems
- systems
- Prior art date
Links
- 238000005260 corrosion Methods 0.000 title 1
- 230000007797 corrosion Effects 0.000 title 1
- 239000003112 inhibitor Substances 0.000 title 1
- 238000000034 method Methods 0.000 title 1
- XLYOFNOQVPJJNP-UHFFFAOYSA-N water Substances O XLYOFNOQVPJJNP-UHFFFAOYSA-N 0.000 title 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C09—DYES; PAINTS; POLISHES; NATURAL RESINS; ADHESIVES; COMPOSITIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
- C09D—COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR
- C09D133/00—Coating compositions based on homopolymers or copolymers of compounds having one or more unsaturated aliphatic radicals, each having only one carbon-to-carbon double bond, and at least one being terminated by only one carboxyl radical, or of salts, anhydrides, esters, amides, imides, or nitriles thereof; Coating compositions based on derivatives of such polymers
- C09D133/24—Homopolymers or copolymers of amides or imides
-
- C—CHEMISTRY; METALLURGY
- C09—DYES; PAINTS; POLISHES; NATURAL RESINS; ADHESIVES; COMPOSITIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
- C09D—COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR
- C09D135/00—Coating compositions based on homopolymers or copolymers of compounds having one or more unsaturated aliphatic radicals, each having only one carbon-to-carbon double bond, and at least one being terminated by a carboxyl radical, and containing at least another carboxyl radical in the molecule, or of salts, anhydrides, esters, amides, imides or nitriles thereof; Coating compositions based on derivatives of such polymers
-
- C—CHEMISTRY; METALLURGY
- C09—DYES; PAINTS; POLISHES; NATURAL RESINS; ADHESIVES; COMPOSITIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
- C09D—COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR
- C09D5/00—Coating compositions, e.g. paints, varnishes or lacquers, characterised by their physical nature or the effects produced; Filling pastes
- C09D5/08—Anti-corrosive paints
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23F—NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23F11/00—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
- C23F11/08—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23F—NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23F11/00—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
- C23F11/08—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids
- C23F11/10—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids using organic inhibitors
- C23F11/173—Macromolecular compounds
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Life Sciences & Earth Sciences (AREA)
- Wood Science & Technology (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US86176386 | 1986-05-09 | ||
| US06/861,763 US4752443A (en) | 1986-05-09 | 1986-05-09 | Cooling water corrosion inhibition method |
Publications (4)
| Publication Number | Publication Date |
|---|---|
| FI872003A0 FI872003A0 (fi) | 1987-05-06 |
| FI872003A7 true FI872003A7 (fi) | 1987-11-10 |
| FI93738B FI93738B (fi) | 1995-02-15 |
| FI93738C FI93738C (fi) | 1995-05-26 |
Family
ID=25336694
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| FI872003A FI93738C (fi) | 1986-05-09 | 1987-05-06 | Menetelmä korroosionestoaineiden vaikutuksen parantamiseksi vesisysteemeissä |
Country Status (17)
| Country | Link |
|---|---|
| US (1) | US4752443A (fi) |
| EP (1) | EP0244584B1 (fi) |
| JP (1) | JPS63121682A (fi) |
| CN (1) | CN1034684C (fi) |
| AT (1) | ATE78882T1 (fi) |
| AU (1) | AU597972B2 (fi) |
| BR (1) | BR8702350A (fi) |
| CA (1) | CA1330390C (fi) |
| DE (1) | DE3780692T2 (fi) |
| DK (1) | DK171302B1 (fi) |
| ES (1) | ES2042509T3 (fi) |
| FI (1) | FI93738C (fi) |
| GR (1) | GR3005830T3 (fi) |
| MX (1) | MX170512B (fi) |
| PT (1) | PT84847B (fi) |
| TR (1) | TR25006A (fi) |
| ZA (1) | ZA873304B (fi) |
Families Citing this family (49)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4919821A (en) * | 1986-03-21 | 1990-04-24 | Nalco Chemical Company | Modified maleic anhydride polymers and the like for use as scale inhibitors |
| US4904413A (en) * | 1986-03-26 | 1990-02-27 | Nalco Chemical Company | Cooling water corrosion control method and composition |
| ATE56051T1 (de) * | 1986-03-26 | 1990-09-15 | Nalco Chemical Co | Korrosionsinhibition zusammensetzungen. |
| US4923634A (en) * | 1986-05-09 | 1990-05-08 | Nalco Chemical Company | Cooling water corrosion inhibition method |
| US4952642A (en) * | 1987-10-26 | 1990-08-28 | Nalco Chemical Company | Process for making acrylamido methane sulfonic acid polymers |
| US4869828A (en) * | 1988-02-26 | 1989-09-26 | Nalco Chemical Company | Stabilization of iron in aqueous systems |
| US5441713A (en) * | 1988-04-29 | 1995-08-15 | Nalco Fuel Tech | Hardness suppression in urea solutions |
| US5616307A (en) * | 1988-04-29 | 1997-04-01 | Nalco Fuel Tech | Boiler operation with decreased NOx and waste water discharge |
| US5061373A (en) * | 1988-07-29 | 1991-10-29 | Union Oil Company Of California | Process for treating condensate of steam derived from geothermal brine |
| US4963267A (en) * | 1988-10-12 | 1990-10-16 | Nalco Chemical Company | Stabilization of manganese in aqueous systems |
| US5035806A (en) * | 1989-05-15 | 1991-07-30 | Nalco Chemical Company | Scaling salt threshold inhibition and dispersion with hydrophilic/hydrophobic polymers |
| GB2236314A (en) * | 1989-09-06 | 1991-04-03 | Grace W R & Co | Inhibition of deposition in aqueous systems. |
| AU643899B2 (en) * | 1991-07-24 | 1993-11-25 | Nalco Chemical Company | Hydroxamic acid containing polymers used as corrosion inhibitors |
| US5593850A (en) | 1991-08-30 | 1997-01-14 | Nalco Chemical Company | Monitoring of industrial water quality using monoclonal antibodies to polymers |
| CA2075695C (en) * | 1991-08-30 | 2003-05-20 | Robert L. Wetegrove | Monoclonal antibodies to sulfonated polymers |
| GB9204409D0 (en) | 1992-02-29 | 1992-04-15 | Ciba Geigy Ag | Determination method |
| US5302293A (en) * | 1992-07-13 | 1994-04-12 | Nalco Chemical Company | Method of controlling iron in produced oilfield waters |
| US5358640A (en) * | 1992-07-20 | 1994-10-25 | Nalco Chemical Company | Method for inhibiting scale formation and/or dispersing iron in reverse osmosis systems |
| US5256303A (en) * | 1992-07-20 | 1993-10-26 | Nalco Chemical Company | Method for inhibiting scale formation and/or dispersing iron in reverse osmosis systems |
| TW238257B (fi) * | 1992-07-24 | 1995-01-11 | Malco Puel Tech | |
| US5589106A (en) * | 1995-02-14 | 1996-12-31 | Nalco Chemical Company | Carbon steel corrosion inhibitors |
| EP0807695A1 (en) * | 1996-05-15 | 1997-11-19 | Nalco Chemical Company | A non-phosphorus corrosion inhibitor for industrial cooling water systems and airwasher systems |
| US6348219B1 (en) | 1998-06-01 | 2002-02-19 | Albemarle Corporation | Processes for preparing concentrated aqueous liquid biocidal compositions |
| US8293795B1 (en) | 1998-06-01 | 2012-10-23 | Albemarle Corporation | Preparation of concentrated aqueous bromine solutions and biocidal applications thereof |
| US6068861A (en) | 1998-06-01 | 2000-05-30 | Albemarle Corporation | Concentrated aqueous bromine solutions and their preparation |
| US8414932B2 (en) | 1998-06-01 | 2013-04-09 | Albemarie Corporation | Active bromine containing biocidal compositions and their preparation |
| US7087251B2 (en) | 1998-06-01 | 2006-08-08 | Albemarle Corporation | Control of biofilm |
| US6652889B2 (en) * | 1998-06-01 | 2003-11-25 | Albemarle Corporation | Concentrated aqueous bromine solutions and their preparation and use |
| US6511682B1 (en) | 1998-06-01 | 2003-01-28 | Albemarle Corporation | Concentrated aqueous bromine solutions and their preparation |
| US6352725B1 (en) | 1998-06-01 | 2002-03-05 | Albemarle Corporation | Continuous processes for preparing concentrated aqueous liquid biocidal composition |
| US6299909B1 (en) | 1998-06-01 | 2001-10-09 | Albemarle Corporation | Concentrated aqueous bromine solutions and their preparation |
| US6506418B1 (en) | 1999-09-24 | 2003-01-14 | Albemarle Corporation | Concentrated aqueous bromine solutions and their preparation |
| GB9924358D0 (en) * | 1999-10-14 | 1999-12-15 | Brad Chem Technology Ltd | Corrosion inhibiting compositions |
| US6375991B1 (en) | 2000-09-08 | 2002-04-23 | Albemarle Corporation | Production of concentrated biocidal solutions |
| US6986910B2 (en) * | 2001-06-28 | 2006-01-17 | Albemarle Corporation | Microbiological control in poultry processing |
| WO2003011033A1 (en) * | 2001-06-28 | 2003-02-13 | Solution Biosciences, Inc. | Microbiological control in animal processing |
| US6908636B2 (en) | 2001-06-28 | 2005-06-21 | Albermarle Corporation | Microbiological control in poultry processing |
| DE10320388A1 (de) | 2003-05-06 | 2004-11-25 | Basf Ag | Polymere für die Wasserbehandlung |
| US7901276B2 (en) * | 2003-06-24 | 2011-03-08 | Albemarle Corporation | Microbiocidal control in the processing of meat-producing four-legged animals |
| WO2006029354A1 (en) * | 2004-09-07 | 2006-03-16 | Albemarle Corporation | Concentrated aqueous bromine solutions and their preparation |
| US7459513B2 (en) | 2004-11-05 | 2008-12-02 | Basf Aktiengesellschaft | Acrylic-acid-based homopolymers comprising taurine modified for the treatment of water |
| EP2314165B1 (en) * | 2004-12-23 | 2014-10-01 | Albemarle Corporation | Microbiocidal control in the processing of meat-producing four-legged animals |
| JP2008528746A (ja) | 2005-01-28 | 2008-07-31 | ビーエーエスエフ ソシエタス・ヨーロピア | 腐食防止被膜を施すための調合剤及び腐食防止被膜を施す方法 |
| CN100419124C (zh) * | 2005-02-07 | 2008-09-17 | 长江大学 | 一种控制电偶腐蚀的缓蚀剂 |
| US9452229B2 (en) * | 2005-06-10 | 2016-09-27 | Albemarle Corporation | Highly concentrated, biocidally active compositions and aqueous mixtures and methods of making the same |
| GB2432154B (en) * | 2005-11-10 | 2010-12-29 | Rhodia Uk Ltd | Corrosion inhibition |
| BRPI0620851B1 (pt) | 2005-12-01 | 2016-08-23 | Albemarle Corp | método para controle microbiano no processo de produção de carne de animais quadrúpedes |
| WO2017063188A1 (en) | 2015-10-16 | 2017-04-20 | Ecolab Usa Inc. | Maleic anhydride homopolymer and maleic acid homopolymer and the method for preparing the same, and non-phosphorus corrosion inhibitor and the use thereof |
| US11421326B2 (en) | 2020-06-22 | 2022-08-23 | Saudi Arabian Oil Company | Hyperbranched polymers with active groups as efficient corrosion inhibitors |
Family Cites Families (27)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3332904A (en) * | 1963-10-02 | 1967-07-25 | Union Carbide Corp | Water-soluble interpolymers of acrylamido-alkylsulfonates |
| FR1544503A (fr) * | 1966-11-16 | 1968-10-31 | Benckiser Gmbh Joh A | Produits détartrants |
| US3692673A (en) * | 1971-02-12 | 1972-09-19 | Lubrizol Corp | Water-soluble sulfonate polymers as flocculants |
| US3898037A (en) * | 1972-06-01 | 1975-08-05 | Betz Laboratories | Acrylamido-sulfonic acid polymers and their use |
| US3992318A (en) * | 1973-10-09 | 1976-11-16 | Drew Chemical Corporation | Corrosion inhibitor |
| FR2288113A1 (fr) * | 1974-10-18 | 1976-05-14 | Anvar | Polymeres hydrosolubles portant des fonctions iminodiacetiques |
| US4288327A (en) * | 1975-09-08 | 1981-09-08 | Betz Laboratories, Inc. | Copolymers for the control of the formation and deposition of materials in aqueous mediums |
| US4159922A (en) * | 1978-10-12 | 1979-07-03 | Nalco Chemical Company | Accelerated process for causticization of Kraft green liquor |
| US4277359A (en) * | 1979-04-04 | 1981-07-07 | Mogul Corporation | Water treatment to inhibit corrosion and scale and process |
| US4324684A (en) * | 1979-10-29 | 1982-04-13 | Betz Laboratories, Inc. | Stable compositions for use as corrosion inhibitors |
| US4317744A (en) * | 1979-04-25 | 1982-03-02 | Drew Chemical Corporation | Corrosion inhibitor |
| US4303568A (en) * | 1979-12-10 | 1981-12-01 | Betz Laboratories, Inc. | Corrosion inhibition treatments and method |
| US4297237A (en) * | 1980-03-06 | 1981-10-27 | Calgon Corporation | Polyphosphate and polymaleic anhydride combination for treating corrosion |
| US4384979A (en) * | 1980-10-31 | 1983-05-24 | Atlantic Richfield Company | Corrosion inhibitor |
| US4328180A (en) * | 1981-11-04 | 1982-05-04 | Atlantic Richfield Company | Cooling water corrosion inhibitor |
| US4443340A (en) * | 1981-10-09 | 1984-04-17 | Betz Laboratories, Inc. | Control of iron induced fouling in water systems |
| US4588519A (en) * | 1982-01-29 | 1986-05-13 | Dearborn Chemical Company | Method of inhibiting corrosion of iron base metals |
| US4547540A (en) * | 1982-05-03 | 1985-10-15 | Nalco Chemical Company | Corrosion protection in cooling water systems |
| GB2124607B (en) * | 1982-07-16 | 1986-02-05 | Katayama Chemical Works Co | Scale-inhibiting agent |
| EP0122013B1 (en) * | 1983-03-07 | 1988-12-21 | Calgon Corporation | Polymeric additives for water |
| JPS60118295A (ja) * | 1983-10-26 | 1985-06-25 | ベッツ・インターナショナル・インコーポレイテッド | 用水処理用ポリマーとその使用方法 |
| US4640793A (en) * | 1984-02-14 | 1987-02-03 | Calgon Corporation | Synergistic scale and corrosion inhibiting admixtures containing carboxylic acid/sulfonic acid polymers |
| GB2155919B (en) * | 1984-03-20 | 1987-12-02 | Dearborn Chemicals Ltd | A method of inhibiting corrosion in aqueous systems |
| US4536292A (en) * | 1984-03-26 | 1985-08-20 | Calgon Corporation | Carboxylic/sulfonic/quaternary ammonium polymers for use as scale and corrosion inhibitors |
| US4566973A (en) * | 1984-08-06 | 1986-01-28 | The B. F. Goodrich Company | Scale inhibition in water systems |
| US4575425A (en) * | 1984-12-24 | 1986-03-11 | Calgon Corporation | Process for controlling calcium oxalate scale over a wide pH range |
| US4650591A (en) * | 1985-08-29 | 1987-03-17 | Calgon Corporation | Acrylic acid/2-acrylamido-2-methylpropylsulfonic acid/2-acrylamido-2-methylpropyl phosphonic acid polymers as scale and corrosion inhibitors |
-
1986
- 1986-05-09 US US06/861,763 patent/US4752443A/en not_active Expired - Lifetime
-
1987
- 1987-03-04 DE DE8787103070T patent/DE3780692T2/de not_active Expired - Lifetime
- 1987-03-04 AT AT87103070T patent/ATE78882T1/de not_active IP Right Cessation
- 1987-03-04 EP EP87103070A patent/EP0244584B1/en not_active Expired - Lifetime
- 1987-03-04 ES ES87103070T patent/ES2042509T3/es not_active Expired - Lifetime
- 1987-05-04 AU AU72478/87A patent/AU597972B2/en not_active Ceased
- 1987-05-06 FI FI872003A patent/FI93738C/fi not_active IP Right Cessation
- 1987-05-07 MX MX006386A patent/MX170512B/es unknown
- 1987-05-08 PT PT84847A patent/PT84847B/pt unknown
- 1987-05-08 CA CA000536674A patent/CA1330390C/en not_active Expired - Fee Related
- 1987-05-08 TR TR87/0376A patent/TR25006A/xx unknown
- 1987-05-08 ZA ZA873304A patent/ZA873304B/xx unknown
- 1987-05-08 CN CN87103379A patent/CN1034684C/zh not_active Expired - Fee Related
- 1987-05-08 DK DK234887A patent/DK171302B1/da not_active IP Right Cessation
- 1987-05-08 BR BR8702350A patent/BR8702350A/pt not_active IP Right Cessation
- 1987-05-09 JP JP62113407A patent/JPS63121682A/ja active Granted
-
1992
- 1992-09-30 GR GR920402161T patent/GR3005830T3/el unknown
Also Published As
| Publication number | Publication date |
|---|---|
| ATE78882T1 (de) | 1992-08-15 |
| DK234887A (da) | 1987-11-10 |
| CN87103379A (zh) | 1987-12-16 |
| JPH0143838B2 (fi) | 1989-09-22 |
| FI93738B (fi) | 1995-02-15 |
| CA1330390C (en) | 1994-06-28 |
| JPS63121682A (ja) | 1988-05-25 |
| FI872003A0 (fi) | 1987-05-06 |
| DK171302B1 (da) | 1996-08-26 |
| GR3005830T3 (fi) | 1993-06-07 |
| EP0244584B1 (en) | 1992-07-29 |
| FI93738C (fi) | 1995-05-26 |
| AU7247887A (en) | 1987-11-12 |
| AU597972B2 (en) | 1990-06-14 |
| MX170512B (es) | 1993-08-27 |
| PT84847A (en) | 1987-06-01 |
| TR25006A (tr) | 1992-08-26 |
| ZA873304B (en) | 1987-11-02 |
| BR8702350A (pt) | 1988-02-17 |
| DE3780692D1 (de) | 1992-09-03 |
| DK234887D0 (da) | 1987-05-08 |
| DE3780692T2 (de) | 1992-12-10 |
| CN1034684C (zh) | 1997-04-23 |
| US4752443A (en) | 1988-06-21 |
| PT84847B (pt) | 1990-02-08 |
| ES2042509T3 (es) | 1993-12-16 |
| EP0244584A3 (en) | 1988-07-20 |
| EP0244584A2 (en) | 1987-11-11 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| FI872003A7 (fi) | Menetelmä korroosionestoaineiden vaikutuksen parantamiseksi vesisysteemeissä | |
| NO163536C (no) | Korrosjonsinhibitor til bruk i syrer og anvendelse derav. | |
| ES542332A0 (es) | "un metodo para inhibir la corrosion de superficies metali- cas en agua en un sistema acuoso" | |
| PT80917A (en) | Method for scale inhibition in water systems | |
| DE3672865D1 (de) | Verfahren zur teilzaehlung der energieverbrauchskosten. | |
| BR8406851A (pt) | Inibidor de corrosao metalica,sistema aquoso com inibidor de corrosao e metodo para inibir corrosao metalica | |
| NO175001C (no) | Fremgangsmåte for å hindre manganavsetning i vannledningssystemer | |
| ZA847192B (en) | Method of inhibiting corrosion in aqueous systems | |
| IT1211113B (it) | Metodo e composizione per inibire la corrosione in un sistema acquoso | |
| NO834835L (no) | Fremgangsmaate for inhibering av avsetning av leire i vann | |
| IT8222867A0 (it) | Metodo per il trattamento disistemi acquosi. | |
| GB8327911D0 (en) | Salts as corrosion inhibitors | |
| DE3586086D1 (de) | Verfahren zur korrosionshemmung in waessrigen systemen. | |
| DE3586325D1 (de) | Verfahren zur korrosionsinhibierung in waessrigen systemen. | |
| IT1155064B (it) | Composizione acquosa inibitrice di corrosione e procedimento per la sua preparazione | |
| DE3668190D1 (de) | Verfahren zur korrosionsinhibierung in dampfkesseln und zusammensetzungen hierfuer. | |
| DK463084D0 (da) | Korrosionsinhibitorer til saltoploesninger med hoej vaegtfylde | |
| IT8548114A0 (it) | Impiantistica perfezionamento nelle tubazioni per | |
| DE3671003D1 (de) | Verfahren zur wasserbehandlung. | |
| GB8310366D0 (en) | Corrosion inhibitors | |
| FI894855A7 (fi) | Vesisysteemin käsitteleminen korroosion ja kattilakiven muodostumisen estämiseksi | |
| DE3677786D1 (de) | Korrosionsinhibitoren. | |
| RO93906A (ro) | ADITIV INHIBITOR DE COROZIUNE PENTRU APA SI PROCEDEU PENTRU PREPARљREA ACESTUIA | |
| GB8712215D0 (en) | Inhibitors against corrosion | |
| PT77688B (de) | Verfahren zur meerwasseraufbereitung |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| BB | Publication of examined application | ||
| FG | Patent granted |
Owner name: NALCO CHEMICAL COMPANY |
|
| MA | Patent expired |