DE974207C - Verfahren zur Wanderbad-Formierung von vorzugsweise aus Aluminium bestehenden Elektrodenfolien fuer elektrolytische Kondensatoren - Google Patents
Verfahren zur Wanderbad-Formierung von vorzugsweise aus Aluminium bestehenden Elektrodenfolien fuer elektrolytische KondensatorenInfo
- Publication number
- DE974207C DE974207C DES16094D DES0016094D DE974207C DE 974207 C DE974207 C DE 974207C DE S16094 D DES16094 D DE S16094D DE S0016094 D DES0016094 D DE S0016094D DE 974207 C DE974207 C DE 974207C
- Authority
- DE
- Germany
- Prior art keywords
- formation
- aluminum
- electrolytic capacitors
- preferably made
- traveling
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zur Wanderbad-Formierung von vorzugsweise aus Aluminium bestehenden Elektrodenfolien für elektrolytische Kondensatoren Aluminiumfolien für elektrolytische Kondensatoren werden bekanntlich in verschiedenen Bädern im sogenannten Wanderbadverfahren vorformiert, wobei das Bad, in welchem hauptsächlich die Bildung der dielektrischen Schicht erfolgt, aus einer Lösung von Borsäure und Borax in destilliertem Wasser besteht. Während es bekannt ist, als Betriebselektrolyt auch gesättigte oder sogar übersättigte Borsäurelösung zu verwenden, werden für die Vorformierung im Wanderbadverfahren im allgemeinen Lösungen von etwa 18 bis 2o °/o Borsäure und o, i °/o Borax verwendet. Das Bad arbeitet bei Siedetemperatur, so daß, abgesehen von den Borsäureverlusten durch den eigentlichen Formiervorgang, ein großer Verbrauch an destilliertem Wasser sowie auch ein Verlust an den gelösten Substanzen durch mitgerissene und herausgespritzte Anteile entsteht. Um die Formierungsbedingungen stets konstant zu halten, ist es notwendig, das Bad durch Analysen genau zu überwachen. Es stellte sich heraus, daß eine Überwachung des Bades mit direkt anzeigenden Instrumenten etwa auf der Basis von Leitfähigkeits- und pH-Messungen technisch nicht ohne weiteres durchführbar ist. Daher mußten stets zeitraubende und teure chemische Analysen durchgeführt werden.
- Es wird daher ein Verfahren zur Wanderbadformierung von vorzugsweise aus Aluminium bestehenden Elektrodenfolien für elektrolytische Kondensatoren, bei dem die Formierungsbedingungen während des Betriebes möglichst konstant gehalten werden, vorgeschlagen, bei dem das Formierungsbad bei Siedetemperatur betrieben wird und bei dieser Temperatur als eine gesättigte Lösung von Borsäure mit Bodenkörper aus Borsäure, gegebenenfalls mit geringem Zusatz von Borax, etwa o,1 °/o, benutzt wird. Es ist dann nur noch notwendig, durch Analysen lediglich den Boraxgehalt zu kontrollieren. Da der Boraxgehalt sich relativ wenig ändert, auch nicht von weittragendem Einfluß ist, wird die analytische Arbeit durch die vorgeschlagene Erfindung bedeutend herabgesetzt.
Claims (1)
- PATENTANSPRUCH: Verfahren zur Wanderbadformierung von vorzugsweise aus Aluminium bestehenden Elektrodenfolien für elektrolytische Kondensatoren, bei dem die Formierungsbedingungen während des Betriebes möglichst konstant gehalten werden, dadurch gekennzeichnet, daß das Formierungsbad bei Siedetemperatur betrieben und daß es bei dieser Temperatur als eine gesättigte Lösung von Borsäure mit Bodenkörper aus Borsäure, gegebenenfalls mit geringem Zusatz von Borax, etwa o,1 °/a, benutzt wird. In Betracht gezogene Druckschriften USA.-Patentschriften Nr. 1 270 78q., 1 710 073, 1976 7oo, z 174 844 2193 711; Buch von Günther Schulze und Betz, Elektrolyth-Kondensatoren, 1937, S. 1o6/=07.