DE1865573U - SINGLE-SIDED CLAMPED BIMETAL STRIP WITH SNAP ATTACHMENT AT THE FREE END. - Google Patents
SINGLE-SIDED CLAMPED BIMETAL STRIP WITH SNAP ATTACHMENT AT THE FREE END.Info
- Publication number
- DE1865573U DE1865573U DE1960M0034423 DEM0034423U DE1865573U DE 1865573 U DE1865573 U DE 1865573U DE 1960M0034423 DE1960M0034423 DE 1960M0034423 DE M0034423 U DEM0034423 U DE M0034423U DE 1865573 U DE1865573 U DE 1865573U
- Authority
- DE
- Germany
- Prior art keywords
- dome
- strip
- free end
- bimetal
- bimetal strip
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
MüllerMüller
. ','".,""" Erauenalt) über Karlsruhe \. ',' ".," "" Erauenalt) via Karlsruhe \
[us] Heiaeioerg Wiesenweg 2o / [us] Heiaeioerg Wiesenweg 2o /
■ " ι 54 - TeSsSm 255»■ "ι 54 - TeSsSm 255»
Einseitig eingespannter, am freien Ende Kontakte tragender umschnapp"barer BimetallstreifenSnap-on bimetallic strip clamped on one side and carrying contacts at the free end
Die Feuerung bezieht sich auf einen einseitig eingespannten, am freien lüde Kontakte tragenden umscbnappoaren Bimetallstreifen für direkte oder indirekte Beheizung, der mit einer flach gehaltenen kalottenartigen Vertiefung von der Breite des Streifens und mit mindestens einer von der Kalotte ausgehenden sich nach dem freien Ende zu erstreckenden Einprägung versehen ist. Zweck der Neuerung ist es, den Anwendungsbereich solcher Bimetallstreifen mit einfachen Mitteln erhe"blich zu erweitern.The furnace refers to a one-sided clamped, bimetallic strips with bimetallic strips on the free lude contacts for direct or indirect heating, the one with a flat dome-like depression the width of the strip and is provided with at least one indentation starting from the dome and extending to the free end. purpose the innovation is to extend the scope of such bimetallic strips can be expanded considerably with simple means.
Es ist "bekannt, den Bimetallstreifen nach Art einer dreiseitigen Pyramide zu formen, wotei sich von der kalottenartigen Vertiefung nach dem freien Ende des Streifens eine Einprägung erstreckt, und die 3?orm der kalottenartigen Vertiefung verschiedenartig gestaltet sein kann. Es hat sich nun gezeigt, daß die Ausbildung des Bimetallstreifens nach Art einer dreiseitigen Pyramide für viele Anwendungsfälle A"bkühlzeiten von. zu langer Dauer zur !Folge hat. Außerdem sind durch das Anbringen der Kontaktnieten Deformierungen des Bimetallstreifens kaum zu vermeiden.It is "known, the bimetal strip in the manner of a three-sided To form a pyramid, an impression is made from the dome-like depression to the free end of the strip extends, and the 3? form of the dome-like depression differently can be designed. It has now been shown that the formation of the bimetal strip in the manner of a three-sided pyramid for many applications it results in cooling times of too long duration. In addition, the attachment of the contact rivets Deformation of the bimetal strip can hardly be avoided.
Der Neuerung liegt nun die Aufgabe zugrunde, den Bimetallstreifen fertigungsmäßig in einfacher Weise so zu variieren, daß die Ein- und Ausschaltzeiten über einen größeren Bereich hin entsprechend den jeweils gewünschten Betriebsbedingungen vorherbestimmbar sind, ohne daß die dem Bimetallstreifen direkt oder indirekt zugeführte Beheizungs-Energie oder die Abmessungen des Bimetallstreifens verändert werden müssen. Diese Aufgabe wird nach der vorliegenden Neuerung dadurch gelöst, daß wahlweise mehrere Einprägungen, vorzugsweise strahlenförmig, von der kalottenartigen Vertiefung je nach "beiden Enden des Streifens hin verlaufend angebracht sind. Da"bei können die Einprägungen auch "bis in die kalottenartige Vertiefung reichen, wo"bei einzelne oder mehrere Einprägungen sich "bis in den Mittelloch-Bereich erstrecken.The innovation is now based on the task of the bimetallic strip to vary in terms of production in a simple manner, that the switch-on and switch-off times over a larger range depending on the desired operating conditions can be determined in advance without the heating energy supplied directly or indirectly to the bimetallic strip or the dimensions of the bimetal strip must be changed. This task is achieved according to the present innovation in that optionally several impressions, preferably radially, of the dome-like depression depending on "both ends of the strip are attached to run. The imprints can do that also "extend into the dome-like depression where" at single or multiple impressions "up to the center hole area extend.
Es sind gewölkte "biinetallische Platten unter der Bezeichnung "SpencerscheiToen" bekannt, die eine zweite zentrale kalottenförmige Wölhung hahen. Letztere kann wohl mit der zentralen Ealotte "beim Bimetallstreifen nach der Feuerung, nicht aher mit den außerhalb dieser Kalotte liegenden Einprägungen verglichen werden. Eine solche zweite ICaIotte könnte "bei Bimetallstreifen nach der feuerung von geringen Stärken von 0,06 his 0,08 ram, höchstens Ms o,15 mm, gar nicht genügend variiert werden, um wesentlich andere Ahkühlzeiten "bis zum Zurückschnappen des Streifens zu erreichen. Bei derart dünnen Folien, wie es die Bimetallstreifen nach der !feuerung sind, können überhaupt nicht zwei Kalotten wie "bei den "bekannten "Spencerscheiben" vorgesehen werden, wohei die Scheihe seihst schon nach einer Kalotte gewölht ist. Das ist erst hei größeren Materialstärken möglich, wie sie die "birnetallische Platte "Spencerscheihe11 hat. Mit diesen Platten wiederum lassen sich aher keine Ausschalttemperaturen von loo G und weniger erreichen. Dies ist a"ber gerade die Aufgahe der "bekannten Bimetallstreifen mit Einprägungen na Gh Art einer dreiseitigen Pyramide sowie der vorliegenden Feuerung. lach letzterer soll ehen hei den Bimetallstreifen mit Sinprä,-gungen nach Art einer dreiseitigen Pyramide für Ausschalttemperaturen von möglichst unter loo C zusätzlich auch ein Variieren der Ahkühlzeit his zum Zurückschnappen ermöglicht werden. Diese Aufgahe könnte mit einem Yariieren der zweiten kalottenförmigen Einprägung "bei der "bekannten himetallischen Platte "Spencerscheihe" nicht gelöst werden. Sie wird neuerungsgemäß gelöst durch das Variieren der Einprägungen, "bei den "bekannten Bimetallstreifen. Während mit diesen "bekannten Bimetallstreifen mit Einprägungen ein TJmschnappen zum Ausschalten des Streifens hei höchstens 80 G möglich ist, kann dies mit nach der Feuerung variierten Einprägungen "beispielsweise schon "bei 5ο C erreicht werden. Diese niedrigere 'Temperaturhöhe "bringt außerdem einen geringeren Energieverbrauch mit sich.Curved "biinetallic plates" are known under the designation "SpencerscheiToen", which have a second central dome-shaped vault. The latter can probably be compared with the central Ealotte "in the bimetallic strip after firing, not with the impressions lying outside this dome. Such a second ICaIotte could "in bimetal strips after firing of small thicknesses of 0.06 to 0.08 ram, at most Ms 0.15 mm, not be varied enough to achieve significantly different cooling times" until the strip snaps back. With foils as thin as the bimetallic strips after firing, two domes like "the" known "Spencer disks" cannot be provided at all, whereby the row is already curved after a domed. This is only possible with larger material thicknesses, such as the "pear-shaped plate" Spencerscheihe 11 has. With these plates, on the other hand, no switch-off temperatures of 100 G or less can be achieved. This is just the job of the well-known bimetallic strips with imprints like a three-sided pyramid as well as the present furnace. In the latter case, the bimetallic strip with embossing in the manner of a three-sided pyramid for switch-off temperatures of as low as possible below 100 C should also allow the cooling time to be varied until it snaps back. This task could not be solved by jarring the second dome-shaped embossing "in the" known himetallic plate "Spencerscheihe". According to the innovation, it is solved by varying the embossing, "with the" known bimetallic strips. While with these "known bimetallic strips with embossings a TJmschnappen to turn off the strip at a maximum of 80 G is possible, this can be achieved with embossings varied according to the firing" for example "already" at 5o C. This lower 'temperature level "also brings with it a lower energy consumption themselves.
Ss ist ferner ein Bimetall-Element "bekannt, hei dem das Element direkt im Stromkreis liegt und durch den Eigenwiderstand erwärmt wird. Letzterer wird gebildet durch das zwischen zwei Schlitzen "befindliche Material, das wiederum durch Yariieren des Ahständes der Schlitze in seinem Querschnitt geändert wird.Ss is also a bimetallic element "known, that is to say Element lies directly in the circuit and is heated by the inherent resistance. The latter is formed by that between two Slitting "located material, which in turn is made by yaring of the Ahstehes of the slots is changed in its cross section.
Hierdurch soll dieses Element verschiedenen. Stromstärken a«gepaßt werden können. Es wird da"bei nur die Lage der Schlitze zueinander, aber nicht deren Anzahl und deren Länge geändert. Abgesehen davon ist "bei diesem Bimetall-Element eine kalottenförmige Einprägung überhaupt nicht vorhanden. HaGh der feuerung dagegen werden wahlweise die Anzahl, die Länge und die Richtung der Einprägungen geändert. Auch hei direkter Beheizung des Bimetall streif ens nach der Heuerung spielt das Material zwischen den Einprägungen keine ausschlaggebende Holle, da ja keine Materialunterbrechung vorliegt wie "bei den Schlitzen des "bekannten Bimetall-Elementes, lach der Heuerung werden also wesentlich andere Mittel angewendet. Mit Schlitzen wie hei dem "bekannten Bimetall-Element könnte zudem "bei der geringen Materialstärke der Bimetallstreifen nach der Heuerung auch gar nicht gearbeitet werden.This is intended to make this element different. Current strengths a «matched can be. Only the position of the slots in relation to one another is changed, but not their number and length. Apart from that, "is a dome-shaped element in this bimetal element Imprint not present at all. HaGh of Fire on the other hand, the number, the length and the direction of the impressions can be changed. Also with direct heating of the bimetal Just after the hiring, the material between the impressions does not play a decisive role, because none Material interruption is present as is known "in the case of the slots of the" Bimetal element, laughing at the hiring, so significantly different means are used. With slots like hot one "Well-known bimetal element could also" given the low material thickness the bimetallic strip also not worked at all after the hiring will.
Bei einer noch weiter "bekannten Schnappvorrichtung ist weder ein Bimetall-Slement noch eine zentrale Kalotte vorhanden. Diese Schnappvorrichtung ist so ausgebildet, daß die Tiefe der Ausprägungen und das Yerdünnen des Materials an diesen Stellen in Abhängigkeit steht zum gewünschten Wirkungsparameter der Scheibe. Die Aufgabe und Lösung bei dem Bimetallstreifen nach der Heuerung haben hiermit gar keinen Zusammenhang.In a still further "known snap device is neither a bimetallic slement still has a central dome. This snap device is designed so that the depth of the stampings and thinning the material at these points in Dependency is related to the desired effect parameter of the disc. The task and solution with the bimetal strip after hiring have no connection with this.
Durch die neuartige Ausbildung des Bimetallstreifens nach der Heuerung, vor allem für Bimetall—Verzögerungsschalter, wird erreicht, daß die gewünschten Schaltzeiten a) Aufheizzeit und b) Abkühlzeit (das ist die Zeit bis zum Zurückschnappen) für die jeweils vorliegenden Anwendungsfälle genau vorausbestimmt werden können. Wenn ein Schalter mit einem solchen Bimetallstreifen nach der Heuerung als Thermostat verwendet wird, können, bei vorheriger Auswahl der passenden Einprä-gungen Temperaturen von 2 C Differenz erreicht werden, wie Versuche mit Anwendungsfällen bewiesen. Die Streifen können bei wesentlich niedrigeren Temperaturen, und zwar etwa von 5o C, schon zum Umschnappen gebracht werden, während bei den bekannten Bimetallstreifen mit Einprägungen nach Art einer dreiseitigen Pyramide die untere G-renze etwa bei 80 ö liegt.Due to the new design of the bimetal strip after hiring, especially for bimetal delay switches achieved that the desired switching times a) heating time and b) cooling time (that is the time until it snaps back) for precisely predetermines the respective application cases can be. If a switch with such a bimetal strip is used as a thermostat after hiring, temperatures can be set, provided the appropriate memorizations have been selected beforehand of 2 C difference can be achieved, as tests with application cases have proven. The streaks can be at much lower Temperatures, about 5o C, can already be brought to snap, while with the known bimetal strips Embossed like a three-sided pyramid the lower border is about 80 ö.
Anhand von Versuchsergebnissen kann nachgewiesen werden, daß die Ausschaltzeiten, d.h. die Abkühlzeiten bis zum Zurück-On the basis of test results it can be demonstrated that the switch-off times, i.e. the cooling times until the
- 4 - f- 4 - f
schnappen des Birne tall streif ens, "bei einer Aufheizzeit von. β sec. zwischen 2,2 und 8 see. vorherbestimiribar sind, wenn strahlenförmige oder parallele Einprägungen verschiedener Länge vorgesehen werden. Dahei wurden diese Versuche mit Bimetallstreifen von 22 mm Länge, 8 mm Breite und 0,08 mm Stärke, ferner "bei 12 Volt und o,2 Amp. einheitlich durchgeführt.snap of the pear-tall stripe, "with a heating-up time of. β sec. between 2.2 and 8 see. are vorbestimiribar if radial-shaped or parallel impressions of different lengths are provided. These attempts were made with bimetal strips 22 mm long, 8 mm wide and 0.08 mm thick, furthermore "carried out uniformly at 12 volts and 0.2 amps.
In der Zeichnung wird die !feuerung anhand zweier Ausführungs-"beispiele näher erläutert.In the drawing, the fire is illustrated using two exemplary embodiments explained in more detail.
Pig. 1 zeigt in Draufsicht einen Bimetallstreifen mit drei strahlenförmigen Sinprägungen auf "beiden Seiten der kalottenartigen Vertiefung.Pig. 1 shows a plan view of a bimetal strip with three Radial embossing on both sides of the dome-like Deepening.
Pig. 2 zeigt ebenfalls in Draufsicht einen Bimetallstreifen, "bei dem von der kalottenförmigen Vertiefung ausgehend je nach, "beiden Seiten des Streifens zviei strahlenförmige Einprägungen verlaufen.Pig. 2 also shows a bimetallic strip in plan view, "in the case of the dome-shaped depression depending on "There are two radial embossings on both sides of the strip get lost.
Der Bimetallstreifen 19 nach Pig. 1 hat in seiner Mitte die kaum wahrnehmbare kalottenartige Vertiefung 3 mit der zentralen Öffnung 2. Der mit der Befestigungsöffnung 1 versehene Teil des Bimetallstreifens 19 hat die Einprägungen 5, 6 und 7j während der den Kontakt 4 tragende Teil des Bimetallstreifens 19 mit den Sinprägungen 8, 9 und Io versehen ist. Die vier Sinprägungen 5 und 7 sowie 8 und Io verlaufen strahlenförmig, während die Einprägungen 6 und 9 zwischen diesen strahlenförmigen Einprägungen parallel zu den Längskanten des Bimetallstreifens 19 verlaufen.The bimetallic strip 19 according to Pig. 1 has the barely perceptible dome-like depression 3 with the central one in its center Opening 2. The part of the bimetallic strip 19 provided with the fastening opening 1 has the impressions 5, 6 and 7j during the part of the bimetallic strip 19 carrying the contact 4 is provided with the embossings 8, 9 and Io. The four imprints 5 and 7 as well as 8 and Io run radially, while the embossments 6 and 9 run parallel to the longitudinal edges of the bimetallic strip 19 between these radial impressions.
Bei dem Ausführungsheispiel nach Pig. 2 hat der Bimetallstreifen 2o mit der kalottenartigen Vertiefung 13, der zentralen Öffnung 12, der Befestigungsöffnung 11 und dem Kontakt 14 vier strahlenförmig verlaufende Einprägungen 15, 16, 17 und 18. Diese vier Einprägungen verlaufen nach den vier Ecken des Bimetallstreifens 2o. Auf diese Weise gehen die vier Einprägungen dem Bimetallstreifen 2o eine Porm ähnlich einer vierseitigen Pyramide.In the embodiment according to Pig. 2 has the bimetal strip 2o with the dome-like recess 13, the central opening 12, the fastening opening 11 and the contact 14 four Radial embossings 15, 16, 17 and 18. These four embossments run to the four corners of the bimetal strip 2o. In this way, the four impressions make the bimetal strip 2o a shape similar to a four-sided pyramid.
Bei den Bimetallstreifen nach den "beiden Ausführungsheispielen verlaufen die strahlenförmigen Einprägungen von der kalottenförmigen Vertiefung oder etwa von dieser nach den "beiden Enden der Streifen. Da"bei hat sich, tiberraschenderweise heraus-With the bimetallic strips according to the "two exemplary embodiments run the radial impressions from the dome-shaped depression or approximately from this to the "two" Ends of the strips. Surprisingly, it turned out
gestellt, daß der Anwendungsbereich des BimetallStreifens nicht nur durch die Anzahl und Anordnung der Einprägungen., sondern auch noch durch deren Länge variiert werden kann, wenn sich nämlich die Sinprägungen in die kalottenförmige Vertiefung hinein und sogar "bis in den Mittelloch-Bereich erstrecken.put that the scope of the bimetal strip is not only by the number and arrangement of the impressions., but can also be varied by their length, namely when the Sinprägungen in the dome-shaped recess into and even "extend into the center hole area.
2 Schutzansprüche2 claims for protection
Claims (2)