CN201979082U - 薄板坯连铸用的浸入式水口 - Google Patents
薄板坯连铸用的浸入式水口 Download PDFInfo
- Publication number
- CN201979082U CN201979082U CN2010206733268U CN201020673326U CN201979082U CN 201979082 U CN201979082 U CN 201979082U CN 2010206733268 U CN2010206733268 U CN 2010206733268U CN 201020673326 U CN201020673326 U CN 201020673326U CN 201979082 U CN201979082 U CN 201979082U
- Authority
- CN
- China
- Prior art keywords
- molten steel
- section
- flow
- expansion section
- submerged nozzle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种薄板坯连铸用的浸入式水口。该浸入式水口的一端设置有用于钢液流入直管状碗口和与该直管状碗口的下部相连通的两侧径向向外扩展的扁平形状的第一扩展段和第二扩展段,所述第二扩展段的下部对称地设置有两个由内到外截面相同的圆形水平流出口,第二扩展段的底部中心有一个缓解钢液流速的分流体。由于本实用新型采用坡度较缓的分流体和斜流出口,以及由内到外截面不变的水平流出口,使降低钢液流速的钢液平稳地入进了金属结晶器,既避免了紊流又挡住了保护渣的流入,提高了薄板坯质量,且该水口的结构简单,制作方便。
Description
技术领域
本实用新型涉及一种将中间包的钢液引入结晶器内的水口,特别是一种薄板坯连铸用的浸入式水口。
背景技术
在连续铸钢过程,浸入式水口将钢液由中间包导入内有水冷壁的金属结晶器中,浸入水口除了具有防止钢水氧化的作用外,更主要的是控制和改善钢水在结晶器内的流动状态,降低钢水对已凝固坯壳的冲击,分散主流带入的热量,促使在结晶器内形成的坯壳稳定,并促进杂物在结晶器内上浮,有效防止卷渣,抑制铸坯裂纹产生。薄板坯连铸与普通连铸相比,其特点是结晶器空间小,拉速快,容易发生钢液表面波动大而引起卷渣,流场分布不合理产生拉漏等事故。
现有薄板坯浸入式水口的基本结构是水口一对前壁形状的收敛和另一对前壁形状扩张的形状,使水口内腔形状从水口碗部的圆形以某种方式逐渐变成长轴和短轴不断变化的一个矩形或一个近似于矩形内切椭圆形状,该结构的水口虽基本合理,但仍不能完全满足生产要求。中国专利2007200118526公开的名称为“薄板坯连铸用高钢水量浸入式水口,它的结构式由钢液流入端和左右对称的四开孔结构钢液流出端以及连接钢液流入端与流出端的细长截面筒状体构成,钢液流出端底部设置有一个水平导流角β为75-80度的中心导流体,该四开孔结构的两个吐出孔外小内大,该浸入水口由于中心导流体的水平导流角β太大及吐出孔外小内大,对降低钢液流速不利,又不能较理想稳定钢液,使钢水进入结晶器的瞬间流速加快,易使保护渣卷入钢水中,极易造成钢坯表面和内部缺陷,该水口易致使结晶液面波动,保护渣覆盖均匀,结晶器内流场不均匀等弊病。
发明内容
本实用新型的目的是通过自身结构的改变达到降低钢液流速及避免产生紊流的解决保护渣覆盖均匀性,内流场均匀性等问题的薄板坯连铸用的浸入式水口。
本实用新型所提出的薄板坯连铸用的浸入式水口的一端设置有用于钢液流入直管状碗口和与该直管状碗口的下部相连通的两侧径向向外扩展的扁平形状的第一扩展段和第二扩展段,所述第二扩展段的下部对称地设置有两个由内到外截面相同的圆形水平流出口,第二扩展段的底部中心有一个缓解钢液流速的分流体。
所述第一扩展段的侧壁与中线夹角β1为8-12度。所述第二扩展段的侧壁与中线夹角β2为12-18度。所述的第二扩展段的底部为伞形;所述分流体的上部为光滑的圆弧形。
所述的分流体侧壁与水平线的夹角α为30-60度。
由于本实用新型采用坡度较缓的分流体和斜流出口,以及由内到外截面不变的水平流出口,将经过第一扩展段和第二扩展段降低流速的钢液平稳地引进了金属结晶器,既避免了紊流又挡住了保护渣的流入,从而使结晶液面平稳,保护渣覆盖均匀,结晶器内流场均匀,提高了薄板坯质量,且该水口的结构简单,制作方便。
附图说明
附图1是本实用新型所提出的薄板坯连铸用的浸入式水口剖面结构示意图;
附图2是图1的侧视剖面结构示意图。
具体实施方式
参见图1和图2,这两幅图给出本实用新型所提出的薄板坯连铸用的浸入式水口一个实施例整体结构,该浸入式水口的一端设置有用于钢液流入直管1状碗口2,以及与直管1的下部相接通的第一扩展段3和第二扩展段4,第一扩展段3与第二扩展段4呈两侧径向向外扩展的扁平形状,第一扩展段3的侧壁与水口中线的夹角β1为8-12度,第二扩展段4的侧壁与水口中线的夹角β2为12-18度,第二扩展段4的下部对称地设置有两个圆形水平流出口41,圆形水平流出口41由内到外截面相同,第二扩展段4的下部中心有一个分流体42,分流体42侧壁与水平线夹角α为30-60度,分流体42上部为光滑的圆弧形,该分流体42将第二扩展段4底部分成了两个斜流出口43,第二扩展段4的底部为伞形。
Claims (5)
1.薄板坯连铸用的浸入式水口,该浸入式水口的一端设置有用于钢液流入直管状碗口和与该直管状碗口的下部相连通的两侧径向向外扩展的扁平形状的第一扩展段和第二扩展段,其特征在于:所述第二扩展段的下部对称地设置有两个由内到外截面相同的圆形水平流出口,第二扩展段的底部中心有一个缓解钢液流速的分流体。
2.根据权利要求1所述的浸入式水口,其特征在于:所述第一扩展段的侧壁与中线夹角β1为8-12度。
3.根据权利要求1所述的浸入式水口,其特征在于:所述第二扩展段的侧壁与中线夹角β2为12-18度。
4.根据权利要求1所述的浸入式水口,其特征在于:所述的分流体侧壁与水平线的夹角α为30-60度。
5.根据权利要求1所述的浸入式水口,其特征在于:所述的第二扩展段的底部为伞形;所述分流体的上部为光滑的圆弧形。