CN201346796Y - Fireproof plate with solid wood veneer - Google Patents
Fireproof plate with solid wood veneer Download PDFInfo
- Publication number
- CN201346796Y CN201346796Y CNU2009201291600U CN200920129160U CN201346796Y CN 201346796 Y CN201346796 Y CN 201346796Y CN U2009201291600 U CNU2009201291600 U CN U2009201291600U CN 200920129160 U CN200920129160 U CN 200920129160U CN 201346796 Y CN201346796 Y CN 201346796Y
- Authority
- CN
- China
- Prior art keywords
- solid wood
- surface layer
- wood surface
- fire
- wood veneer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses a fireproof plate with a solid wood veneer, which comprises a fireproof basal layer (1) and a solid wood veneer (2) bonded on the front surface of the fireproof basal layer (1). An integral middle layer interlining paper (3) is bonded between the fireproof basal layer (1) and the solid wood veneer (2) for preventing the splice of the solid wood veneer (2) from being easily fractured, and the middle layer interlining paper (3) and the solid wood veneer (2) have the same or substantially same degree of thermal expansion and cold shrinkage. During the usage process of the fireproof plate, the solid wood veneer has low liability of fracture and flexural deformation. The fireproof plate with the solid wood veneer can be widely used in architectural decoration materials such as wall surfaces, ceiling boards and fireproof doors.
Description
Technical field
The utility model relates to a kind of ornament materials, relates in particular to a kind of fire-proof board that has solid wood surface layer.
Background technology
In the prior art, fire-proof board is a kind of building and ornament materials commonly used, be widely used on smallpox, partition wall liner plate, the fireproof door, but because the material of fire-proof board is more coarse, for attractive in appearance, usually directly paste one deck architectural surface on the surface of fire-proof board, and wherein solid wood surface layer is subjected to people's welcome most.As a rule, in order to obtain the wood grain pattern unanimity, attractive in appearance, the solid wood skin that is used for surface layer all is the wooden skin that adopts truncation, such sheet material is spliced by the wooden skin of polylith truncation possibly, yet because the degree of expanding with heat and contract with cold of fire-proof board and solid wood surface layer is inconsistent, solid wood surface layer is easy to split, come off in the weakest splicing place, can't satisfy requirement of client thus.
The utility model content
The technical problems to be solved in the utility model is to provide a kind of fire-proof board of solid wood surface layer difficult drop-off.
The technical scheme in the invention for solving the above technical problem is, manufactures and designs a kind of fire-proof board with solid wood surface layer, comprising: PLASTIC LAMINATED basic unit and be attached to the solid wood surface layer in this PLASTIC LAMINATED basic unit front, and its special feature is:
The middle level holding paper of the globality that also is used to prevent that splicing place of solid wood surface layer from ftractureing easily with one deck between described PLASTIC LAMINATED basic unit and solid wood surface layer, described middle level holding paper has identical or essentially identical degree of expanding with heat and contract with cold with described solid wood surface layer.
Described middle level holding paper can adopt the monoblock solid wood skin of brown paper or rotary-cutting type.
The thickness of described middle level holding paper is 0.2 millimeter to 0.4 millimeter.
The thickness of described solid wood surface layer is 0.3 millimeter to 0.6 millimeter.
The back side of described PLASTIC LAMINATED basic unit also with the brown paper or the solid wood skin bottom of the bonding pulling force on this PLASTIC LAMINATED basic unit two sides of a layer equilibration, can prevent fire-proof board flexural deformation in use, can prevent indirectly that also positive solid wood surface layer from ftractureing because of crooked.
Compare with prior art, fire-proof board with solid wood surface layer of the present utility model is owing to increased the middle level holding paper that one deck and solid wood surface layer have identical or basic identical degree of expanding with heat and contract with cold, the phenomenon of effectively having avoided solid wood surface layer in use to ftracture, come off in the splicing place generation of weakness easily between PLASTIC LAMINATED basic unit and solid wood surface layer; But increase the bonding pulling force on one deck brown paper or its two sides of solid wood skin bottom balance at the PLASTIC LAMINATED basic unit back side, prevent PLASTIC LAMINATED flexural deformation.PLASTIC LAMINATED of the present utility model is attractive and durable, the needs on the fine satisfied decoration of energy.
Description of drawings
Fig. 1 is the cross-sectional view that the utlity model has the fire-proof board of solid wood surface layer.
The specific embodiment
Be described in further detail below in conjunction with the most preferred embodiment shown in the accompanying drawing.
As shown in Figure 1, the fire-proof board with solid wood surface layer of the present utility model comprises from the bottom to top successively: PLASTIC LAMINATED basic unit 1, middle level holding paper 3 and solid wood surface layer 2.Wherein:
Described PLASTIC LAMINATED basic unit 1 is the PLASTIC LAMINATED of national A level fire prevention authentication, the composite plate of being made up of materials such as magnesia, perlite, wood chip, glass cloth.
Described solid wood surface layer 2 adopts general flat cut type solid wood skin, and its thickness is 0.3 millimeter to 0.6 millimeter, adopts 0.6 millimeter thickness in the utility model.
Described middle level holding paper 3 is the lining paper of a monoblock, and has identical or essentially identical degree of expanding with heat and contract with cold with described solid wood surface layer 2, its thickness is 0.2 millimeter to 0.4 millimeter, adopts the brown paper of 0.3 millimeters thick or the monoblock solid wood skin of rotary-cutting type in the utility model.Like this, in use, degree of the collapsing basically identical of outermost solid wood surface layer 2 and middle level holding paper 3, therefore, solid wood surface layer 2 is not easy cracking and comes off.In addition,, also be not easy cracking even have than big-difference with the degree of expanding with heat and contract with cold of PLASTIC LAMINATED basic unit 1 because middle level holding paper 3 is a globality lining paper, though cracking owing to be positioned at interlayer, outwardly less than, can not influence the outward appearance of fire-proof board.
In addition, for the double-edged bonding pulling force of balance fire-proof board, as shown in Figure 1, can also can prevent to produce when fire-proof board from using flexural deformation at the back side applying one deck brown paper or the solid wood skin bottom 5 of described PLASTIC LAMINATED basic unit 1.This solid wood skin bottom 5 can adopt the wooden skin of truncation or rotary-cut.
The processing step that its solid wood skin of fire-proof board of the present utility model is fitted is as follows:
1) with the high-speed wideband sander PLASTIC LAMINATED basic unit 1 is carried out sanding and handle, make its surfacing smooth;
2) glue 6 that modulates evenly is applied in PLASTIC LAMINATED basic unit 1 surface by gluing machine, entirely be placed on above the PLASTIC LAMINATED basic unit 1 cutting out good middle level holding paper 3, and sheet material is placed on the pressing plate of hot press and carry out hot-pressing processing, the temperature of hot press transfers to 80 ℃ to 100 ℃, adopts 95 ℃ hot pressing temperature in the utility model;
3) same, the glue 6 that modulates evenly is applied in middle level holding paper 3 surfaces by gluing machine, entirely be placed on above the middle level holding paper 3 cutting out good solid wood surface layer 2, and sheet material is placed on the pressing plate of hot press and carry out hot-pressing processing, the temperature of hot press transfers to 80 ℃ to 100 ℃, adopts 95 ℃ hot pressing temperature in the utility model;
4) wait to do and cooling after, the fire-proof board with hot pressing after fixing is placed on and on the fine sand ray machine described solid wood surface layer 2 is carried out sanding and handle, and makes its surfacing smooth, can obtain fire-proof board finished product of the present utility model.
In order to prevent to produce flexural deformation after fire-proof board from having grown service time, also can adopt and step 2) or 3) identical method is with brown paper or solid wood skin bottom 5 is pasted and hot pressing is fixed on the back side of described PLASTIC LAMINATED basic unit 1, with the bonding pulling force on balance PLASTIC LAMINATED basic unit 1 two sides.
Described glue can be selected vacuum plastic-absorption for use, is a kind of albescent water based emulsion, and the about 300CPS of its viscosity (3#/30rpm/27 ℃) has heatproof, good springiness, adhesive strength height, the good characteristic of pulverability.Between described middle level holding paper 3 or bottom 5 and the PLASTIC LAMINATED basic unit 1 and the gluing thickness between middle level holding paper 3 and the solid wood surface layer 2 can be 0.4 millimeter to 0.6 millimeter, gluing thickness adopts 0.5 millimeter in the present embodiment.
Fire-proof board with solid wood surface layer of the present utility model has fire-proof function, can reach the standard of national regulation one class building A level incombustible material, have simultaneously the characteristic of decorative panel again concurrently, have fire prevention, waterproof, mothproof, corrosion-resistant characteristics, its light weight, attractive and durable, flexible one-tenth cambered surface, available cutter cuts; In addition, fire-proof board of the present utility model is all adopted inorganic asepsis environment-protecting material, even can place fish jar interior as the plaque use, is suitable as very much the class building and ornament materials with fire protection requirement, and meets national construction standards fully.
Claims (5)
1, a kind of fire-proof board with solid wood surface layer comprises: PLASTIC LAMINATED basic unit (1) and be attached to the positive solid wood surface layer (2) of this PLASTIC LAMINATED basic unit (1) is characterized in that:
The middle level holding paper (3) of the globality that also is used to prevent that solid wood surface layer (2) splicing place from ftractureing easily with one deck between described PLASTIC LAMINATED basic unit (1) and solid wood surface layer (2), described middle level holding paper (3) has identical or essentially identical degree of expanding with heat and contract with cold with described solid wood surface layer (2).
2, the fire-proof board with solid wood surface layer according to claim 1 is characterized in that: described middle level holding paper (3) adopts the monoblock solid wood skin of brown paper or rotary-cutting type.
3, the fire-proof board with solid wood surface layer according to claim 1 and 2 is characterized in that: the thickness of described middle level holding paper (3) is 0.2 millimeter to 0.4 millimeter.
4, the fire-proof board with solid wood surface layer according to claim 1 and 2 is characterized in that: the thickness of described solid wood surface layer (2) is 0.3 millimeter to 0.6 millimeter.
5, the fire-proof board with solid wood surface layer according to claim 1 and 2 is characterized in that: the back side of described PLASTIC LAMINATED basic unit (1) also has the brown paper or the solid wood skin bottom (5) of the bonding pulling force on this PLASTIC LAMINATED basic unit (1) two sides of a layer equilibration.