[go: up one dir, main page]

CN204867311U - 铸造用大气压力冒口 - Google Patents

铸造用大气压力冒口 Download PDF

Info

Publication number
CN204867311U
CN204867311U CN201520600079.1U CN201520600079U CN204867311U CN 204867311 U CN204867311 U CN 204867311U CN 201520600079 U CN201520600079 U CN 201520600079U CN 204867311 U CN204867311 U CN 204867311U
Authority
CN
China
Prior art keywords
riser
diameter
casting
rising head
atmospheric pressure
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN201520600079.1U
Other languages
English (en)
Inventor
李可丹
王瑞金
刘松奇
彭德楼
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
XISHAN XIBENG SPECIAL FOUNDING CO Ltd
Original Assignee
XISHAN XIBENG SPECIAL FOUNDING CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by XISHAN XIBENG SPECIAL FOUNDING CO Ltd filed Critical XISHAN XIBENG SPECIAL FOUNDING CO Ltd
Priority to CN201520600079.1U priority Critical patent/CN204867311U/zh
Application granted granted Critical
Publication of CN204867311U publication Critical patent/CN204867311U/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本实用新型提出了一种铸造用大气压力冒口,其特点是包括冒口的锥形压力窝、冒口底窝、冒口颈,冒口高度为冒口直径的一点五倍,冒口锥底直径是冒口直径的一半,冒口锥角深度是冒口直径的一半,冒口底窝高度是冒口直径的五分之一。本实用新型通过对冒口结构尺寸的改进,冒口结构简单,模具制造方便,铸造成型后轮廓清晰,冒口补缩效率高。

Description

铸造用大气压力冒口
技术领域
本实用新型属于铸造技术领域,涉及铸造用大气压力冒口,是汽车排气管铸造时防止铸件内部出现缩孔、缩松缺陷而使用的一种冒口。
背景技术
在铸型中,冒口的型腔是存贮液态金属的空腔,在铸件形成时补给金属,有防止缩孔、缩松、排气和集渣的作用,而冒口的主要作用是补缩。
汽车排气管是根据发动机布局设计而来,其结构奇形怪状,从铸造角度来说,加工工艺难度大。在铸件凝固成型的过程中,由于铁液自身凝固收缩,需要冒口对热节部位进行补缩,防止铸件内部出现缩孔、缩松缺陷。
目前,常用的大气压力冒口,在冒口顶部插放一个细砂芯,或将冒口顶部做成锥形。对于前者,一个冒口额外增加一个细砂芯,假如一支4缸排气管需要放置4个冒口,那么就需要额外增加4个细砂芯。一个细砂芯原材料、电费、人工成本需要1元,那么4个细砂芯就额外增加成本4元,并且增加细砂芯大大降低了造型下芯效率。对于后者,冒口顶部锥形角一般设计成40°-45°,由于冒口直径的限制,锥角深度一般只有10-15mm,砂型铸出后,深度更小,这样的大气压力冒口补缩效率低。
发明内容
本实用新型所要解决的技术问题是设计一种铸造用大气压力冒口,该冒口结构简单,便于加工制造,其生产成本低,补缩效率高。
为解决上述技术问题,本实用新型所采取的技术方案是:一种铸造用大气压力冒口,包括冒口的锥形压力窝、冒口底窝、冒口颈,所述冒口高度为冒口直径的一点五倍,冒口锥底直径是冒口直径的一半,冒口锥角深度是冒口直径的一半,冒口底窝高度是冒口直径的五分之一。
本实用新型采用上述技术方案所设计的铸造用大气压力冒口,通过对冒口结构尺寸的改进,冒口结构简单,模具制造方便,铸造成型后轮廓清晰,冒口补缩效率高。本实用新型适合排气管法兰、涡轮增压器壳体等铸件。
附图说明
图1表示本实用新型铸造用大气压力冒口的主视结构示意图;
图2表示图1中A-A向的结构示意图;
图3表示本实用新型的右视结构示意图;
图4表示本实用新型的立体结构示意图。
具体实施方式
下面结合附图对本实用新型铸造用大气压力冒口的结构作具体说明。
参见图1至图4,本实用新型铸造用大气压力冒口,包括冒口4的锥形压力窝1、冒口底窝2、冒口颈3,其中,冒口4的冒口高h1为冒口直径D的一点五倍,即h1=1.5D。冒口4的锥底直径d是冒口直径D的一半,即d=D/2。冒口4的锥角深度h2是冒口直径D的一半,即h2=D/2。冒口4的底窝高度h3是冒口直径D的五分之一,即h3=D/5。
本实用新型经试制试用,目前已成功应用于康明斯3104237排气管中。通过解剖观察,新型大气压力冒口补缩效率高,铸件没有出现缩孔、缩松缺陷。

Claims (1)

1.一种铸造用大气压力冒口,包括冒口的锥形压力窝、冒口底窝、冒口颈,其特征是所述冒口高度为冒口直径的一点五倍,冒口锥底直径是冒口直径的一半,冒口锥角深度是冒口直径的一半,冒口底窝高度是冒口直径的五分之一。
CN201520600079.1U 2015-08-11 2015-08-11 铸造用大气压力冒口 Expired - Lifetime CN204867311U (zh)