CN1172620A - Method for making 100% cotton anti-wrinkle shirt - Google Patents
Method for making 100% cotton anti-wrinkle shirt Download PDFInfo
- Publication number
- CN1172620A CN1172620A CN 96120300 CN96120300A CN1172620A CN 1172620 A CN1172620 A CN 1172620A CN 96120300 CN96120300 CN 96120300 CN 96120300 A CN96120300 A CN 96120300A CN 1172620 A CN1172620 A CN 1172620A
- Authority
- CN
- China
- Prior art keywords
- shirt
- temperature
- cotton
- carried out
- wrinkle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
| Physical index | The cotton shirt standard that Japan orders | The cotton shirt parameter that the present invention produces |
| Wash and wear (W δ W) level | 〉=3.3 grades | 〉=3.8 grades |
| Do recovery angle (T+W, slow) | 〉=280 degree | 〉=320 degree |
| Removing residue formaldehyde amount on the cloth | ????≤75PPM | ????≤38PPM |
| Washing shrinkage (warp/latitude) | ≤ ± 1 centimetre | ≤ ± 0.5 centimetre |
| The broadwise brute force | Do not examine | 〉=20 kilograms |
| Broadwise is torn | 〉=600 grams | 〉=750 grams |
Claims (3)