CN103803863A - Building mixed brick - Google Patents
Building mixed brick Download PDFInfo
- Publication number
- CN103803863A CN103803863A CN201210456080.2A CN201210456080A CN103803863A CN 103803863 A CN103803863 A CN 103803863A CN 201210456080 A CN201210456080 A CN 201210456080A CN 103803863 A CN103803863 A CN 103803863A
- Authority
- CN
- China
- Prior art keywords
- building
- brick
- cement
- coal gangue
- building waste
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a building mixed brick which is prepared from 60% of building waste, 10% of coal gangue, 20% of cement and 10% of ceramsite. A production method of the building mixed brick comprises the following steps: proportionally grinding the building waste and coal gangue with a grinder; adding the ceramsite and cement, adding a proper amount of water and stirring and mixing with a stirrer; and putting the mixture into a mould; and performing vibration moulding, demoulding and natural airing to obtain the finished product. Compared with the prior art, the building mixed brick has the advantages that the state requirements for environmental protection are met, the brick is light, the labor intensity of workers can be reduced, the usable area of the house can be increased, the price is low, the building waste can be treated and the like, and is particularly suitable for the building industry.
Description
Technical field
The present invention relates to material of construction, especially relate to a kind of building mixed brick.
Background technology
At present, the production of the loess brick using in traditional architecture construction, because construction market has been exited in the restriction in soil exploitation.Its surrogate great majority are Industry Waste slag brick, and with clinker brick consumption maximum.And in cinder, contain sulfide, and content of radioactive substance is high, is unfavorable for that room for building uses.
Summary of the invention
The object of the invention is the drawback of the existence in producing or using for loess brick or clinker brick, and a kind of brick that utilizes construction waste to produce is provided, its feature of environmental protection is good, and cost is low, to replace currently available products.
For realizing above-mentioned technical purpose, the technical solution used in the present invention is: a kind of building mixed brick, it is to use the synthetic method of conventional pulverizing to make with building waste, coal gangue, haydite, cement, and each component proportion is: building waste 60%, coal gangue 10 %, cement 20%, haydite 10%; Its production method is: proportionally first building waste, coal gangue are pulverized with pulverizer, then haydite, cement are added, add appropriate water stirrer and be uniformly mixed, pack mould into, after vibratory compaction, the demoulding, natural airing, get product.
The present invention compared with prior art, has the national requirements for environmental protection of meeting, lightweight, can reduce labor strength, can increase house usable floor area, low price, and can solve the advantages such as building waste, be particularly suitable for building trade and use.
Embodiment:
Below in conjunction with embodiment, the present invention will be further described:
A kind of building mixed brick, first the coal gangue of 60% building waste, 10 % is pulverized and mixed with pulverizer according to proportioning, then the haydite of 10 %, 20% cement are added, add appropriate water stirrer and be uniformly mixed, pack mould into, through vibratory compaction, the demoulding, natural airing, get product.
Claims (1)
1. a building mixed brick, it is to use the synthetic method of conventional pulverizing to make with building waste, coal gangue, haydite, cement, each component proportion is: building waste 60%, coal gangue 10 %, cement 20%, haydite 10%; Its production method is: proportionally first building waste, coal gangue are pulverized with pulverizer, then haydite, cement are added, add appropriate water stirrer and be uniformly mixed, pack mould into, get product through vibratory compaction, the demoulding, natural airing.