[go: up one dir, main page]

CN1030739A - The resin-emery abrasive wheel of glass-cutting - Google Patents

The resin-emery abrasive wheel of glass-cutting Download PDF

Info

Publication number
CN1030739A
CN1030739A CN 87105037 CN87105037A CN1030739A CN 1030739 A CN1030739 A CN 1030739A CN 87105037 CN87105037 CN 87105037 CN 87105037 A CN87105037 A CN 87105037A CN 1030739 A CN1030739 A CN 1030739A
Authority
CN
China
Prior art keywords
resin
glass
phenol
cutting
emery
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 87105037
Other languages
Chinese (zh)
Inventor
谷文学
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 87105037 priority Critical patent/CN1030739A/en
Publication of CN1030739A publication Critical patent/CN1030739A/en
Pending legal-status Critical Current

Abstract

A kind of resin-emery abrasive wheel of glass-cutting and manufacturing process thereof.The emery wheel major ingredient is phenol, formaldehyde, silicon carbide etc.The present invention can cut and grinding glass and marble, especially for glass-cutting, can electronic or manually cut the glass of various areas and all thickness.

Description

The resin-emery abrasive wheel of glass-cutting
The present invention relates to a kind of glass-cutting or marmorean resin-emery grinding wheel, be specially adapted to cut glass with the grinding all size.
Existing glass cutting cutter all is that main raw material is made with the diamond.Its shortcoming is, expensive raw material price, and when cutting heavy sheet glass and small area glass, frangible, yield rate is low, and can only cut, and can not carry out ground finish.
Task of the present invention is to overcome the above-mentioned shortcoming in the prior art, produces a kind of can the cutting and grinding marble and glass, particularly resin-the emery grinding wheel of cutting and various areas of grinding and all thickness glass.
Resin-emery grinding wheel of the present invention, its main raw material is:
Silicon carbide (green silicon carbide): content is more than 99%;
Phenol (CHOH): content is 97~99%;
Formaldehyde (CHO): content is 37~40%
Gypsum.
The proportioning of various compositions is:
In the resin:
Phenol: formaldehyde is 1: (1.1~1.2) (ratio of gram branch)
Ammoniacal liquor: phenol is 100: (5.5~6.0) (weight ratio)
In the emery wheel:
Silicon carbide: resin is 100: (10~13) (weight ratio)
The portions of resin gypsum is 32: (6~9) (weight ratio)
Manufacturing process of the present invention is:
Make resin:
By proportioning phenol and formaldehyde are prepared in the container of packing into, container is immersed in the water to 2/3rds places of container, feedwater is heated, and makes phenol and formaldehyde solvate temperature in the container rise to 72~80 ℃.Afterwards, add ammoniacal liquor in proportion and stirred 4~5 minutes, container is built, continue feedwater and heat, make that temperature rises to 95~100 ℃ in the container, and keep water temperature to be about 90 ℃, ammoniacal liquor boiling and constantly boiling are 40~50 minutes in container, make resin.Resin with the cooling of 2 times cold water, after 24 hours is removed water, treat 3 days again after, resin can use.
Make emery wheel:
With silicon carbide, resin and gypsum prepare in proportion, stir, and treat 6~10 minutes, make its moulding.
The shape base is put into stoving oven, make furnace temperature rise to 180 ℃, continue oven dry 5.5~6.5 hours, underhardening oven dry, its drying time is assigned as:
1~65 ℃ 0.5 hour
65~90 ℃ 1.5 hours
90~115 ℃ 2 hours
115~140 ℃ 1.5 hours
140~180 ℃ 1 hour
Stop after the heating, temperature keeping 4 hours, the blow-on temperature of loosing is taken out product.
Compare with prior art, the invention has the advantages that:
Can cut, also can grinding glass and marble, cutting yield rate height can be contained on the electrically powered machine, also can manually use, and can cut the glass of various areas and thickness.
Embodiment one:
The resin proportioning:
Phenol: the ratio of formaldehyde 1: 1.15(gram branch)
Ammoniacal liquor: phenol 100: the 5.8(weight ratio)
The emery wheel proportioning:
Silicon carbide: resin 100: 13
Portions of resin gypsum 32: 6
Embodiment two (most preferred embodiment):
The resin proportioning:
Phenol: the ratio of formaldehyde 1: 1.1(gram branch)
Ammoniacal liquor: phenol 100: the 5.5(weight ratio)
The emery wheel proportioning:
Silicon carbide: resin 100: the 12(weight ratio)
Portions of resin gypsum 32: the 7(weight ratio)

Claims (3)

1, a kind of resin-emery grinding wheel of glass-cutting is made up of phenol, formaldehyde, silicon carbide, ammoniacal liquor, gypsum, it is characterized in that:
The various proportioning components of resin are:
Phenol: formaldehyde 1: (1.1~1.2) (ratio of gram branch)
Ammoniacal liquor: phenol 100: (5.5~6.0) (weight ratio)
The various proportioning components of emery wheel are:
Silicon carbide: resin 100: (10~13) (weight ratio)
Portions of resin gypsum 32: (6~9) (weight ratio)
2, according to the resin-emery grinding wheel of claim 1, it is characterized in that:
The best proportioning of resin is:
Phenol: the ratio of formaldehyde 1: 1.1(gram branch)
Ammoniacal liquor: phenol 100: the 5.5(weight ratio)
The best proportioning of emery wheel is:
Silicon carbide: resin 100: the 12(weight ratio)
Portions of resin gypsum 32: the 7(weight ratio)
3, a kind of manufacturing process of resin-emery grinding wheel of glass-cutting, the fused back of phenol and formaldehyde is warming up to 72~80 ℃ indirectly with water when it is characterized in that resin manufacture, after adding ammoniacal liquor, keep about 90 ℃ of water temperature after temperature rises to 95~100 ℃ in the container, when making emery wheel, the sclerosis of employing first drying, the time is 5.5~6.5 hours.
CN 87105037 1987-07-20 1987-07-20 The resin-emery abrasive wheel of glass-cutting Pending CN1030739A (en)