CN103044819A - Rigid plastic keel and manufacturing method thereof - Google Patents
Rigid plastic keel and manufacturing method thereof Download PDFInfo
- Publication number
- CN103044819A CN103044819A CN201210582977XA CN201210582977A CN103044819A CN 103044819 A CN103044819 A CN 103044819A CN 201210582977X A CN201210582977X A CN 201210582977XA CN 201210582977 A CN201210582977 A CN 201210582977A CN 103044819 A CN103044819 A CN 103044819A
- Authority
- CN
- China
- Prior art keywords
- keel
- soft plastic
- mixture
- manufacturing
- rigid plastic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a rigid plastic keel and a manufacturing method thereof. The rigid plastic keel is prepared from 85 to 90 percent of polyvinyl chloride and 10 to 15 percent of soft plastic, wherein the common soft plastic is one type or a mixture of polypropylene (PP), low-density polyethylene (LDPE), polyethylene terephthalate (PET) and polystyrene (PS). The manufacturing method comprises the following steps: mixing the PVC material and the common soft plastic according to the formula; melting at the temperature of between 240 and 260 DEG C; stirring uniformly; pouring into a die; drilling a hole on the mixture after the temperature of the mixture is reduced to be 60 to 80 DEG C; and after the mixture is completely cooled, mounting a bolt in the hole. The rigid plastic keel and the manufacturing method thereof have the advantages that the hardness reaches the appointed requirement; decay is avoided; the cost is saved; the waste plastic is recycled; and the price is low.
Description
Technical field
The invention belongs to a kind of prescription and preparation method thereof technical field of rigidity plastics keel.
Background technology
Keel are framework materials the most commonly used in the house decoration, and being widely used in furred ceiling, partition wall, the solid wooden floor board carcasing now, the house building keel are to use wooden keel basically entirely.And that wooden keel exist is perishable, go mouldy, easy naked light, and simultaneously a large amount of timber use the forest that needs felling a large amount of, and this is very serious to environmental hazard.General wooden keel simultaneously, length will have during less than 3 centimeters 50% material to waste because of cracking in the process of construction punching.
Summary of the invention
The present invention in order to overcome the problems referred to above defective, provides a kind of rigidity plastics just, fact proved that this rigidity plastics can substitute traditional wooden keel fully, and does not damage rigidity plastics itself when this rigidity plastics boring.
The present invention adopts following technical scheme to realize.
A kind of rigidity plastics keel, raw material of the present invention are PVC material and common soft plastic, fill a prescription as the PVC material accounts for 85% ~ 90%, and soft plastic accounts for 10% ~ 15%; Wherein common soft plastic is: the mixture of one or more of PP, LDPE, PET, PS.
The step of making method of the present invention is, after PVC material and common soft plastic mixed according to prescription, under 240 ℃ ~ 260 ℃ temperature, melt, after stirring, to mould, during thing drop in temperature to 60 to be mixed ℃ ~ 80 ℃, boring is thereon installed bolt additional and is finished in punching after cooling off fully.
Beneficial effect of the present invention is 1) hardness reaches the appointment requirement; 2) be difficult for occuring to rot; 3) raw material can adopt waste and old PVC material, such as pvc pipe, sole, toy, door and window, wire outer skin, stationery; Common soft plastic goods such as mineral water bottle, carbonated drink bottle, preservative film, bowl dress bubble face box; When adopting waste and old raw material, namely can save cost, again can the recycle waste plastic.4) adopt to make boring when processing midway, material can the cracking phenomenon; 5) cheap: the common anticorrosion timber keel price in market is 6000 yuan/cubic metre, and common timber keel price is 2000 yuan/cubic metre; And the extraordinary rigidity plastics keel of quality price only is 1200 yuan/cubic metre, and comparatively speaking the rigidity plastics keel are very economical and practical.
Below in conjunction with specific embodiment the present invention is done further explanation.
Embodiment
A kind of rigidity plastics keel, raw material of the present invention are PVC material and common soft plastic, fill a prescription as the PVC material accounts for 85% ~ 90%, and soft plastic accounts for 10% ~ 15%; Wherein common soft plastic is: the mixture of one or more of PP, LDPE, PET, PS.
The step of making method of the present invention is, after PVC material and common soft plastic mixed according to prescription, under 240 ℃ ~ 260 ℃ temperature (preferred 250 ℃), melt, after stirring, to mould, during thing drop in temperature to 60 to be mixed ℃ ~ 80 ℃ (preferred 70 ℃), boring is thereon installed bolt additional and is finished in punching after cooling off fully.
The rigidity plastics raw material comes from the Industry Waste plastics of collection, and building waste or used plastics pipeline, with after the waste or used plastics high temperature melting again casting mold be that the common building keel shapes such as square, I shape, C font get final product.Rigidity plastics keel hardness of the present invention reaches country and specifies requirement, can save cost, again can the recycle waste plastic.Rigidity plastics keel shell by test is widely used in the building inside and outside wall end face, and ground can be used for cladding system simultaneously.
Claims (2)
1. rigidity plastics keel is characterized in that, raw material is PVC material and common soft plastic, fill a prescription as the PVC material accounts for 85% ~ 90%, and soft plastic accounts for 10% ~ 15%; Wherein common soft plastic is: the mixture of one or more of PP, LDPE, PET, PS.
2. the making method of a kind of rigidity plastics keel as claimed in claim 1, it is characterized in that, step is, after PVC material and common soft plastic mixed according to prescription, under 240 ℃ ~ 260 ℃ temperature, melt, after stirring, to mould, during thing drop in temperature to 60 to be mixed ℃ ~ 80 ℃, boring is thereon installed bolt additional and is finished in punching after cooling off fully.