CN102251432A - 提高装饰原纸综合性能的方法 - Google Patents
提高装饰原纸综合性能的方法 Download PDFInfo
- Publication number
- CN102251432A CN102251432A CN 201110181377 CN201110181377A CN102251432A CN 102251432 A CN102251432 A CN 102251432A CN 201110181377 CN201110181377 CN 201110181377 CN 201110181377 A CN201110181377 A CN 201110181377A CN 102251432 A CN102251432 A CN 102251432A
- Authority
- CN
- China
- Prior art keywords
- titanium dioxide
- calcined kaolin
- base paper
- paper
- iron oxide
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种提高装饰原纸综合性能的方法,属于造纸技术领域。该方法增加煅烧高岭土,降低二氧化钛的比例,白色装饰原纸原料配方为:煅烧高岭土、二氧化钛、纸浆;浅色装饰原纸原料配方为:煅烧高岭土、二氧化钛、氧化铁黄、氧化铁红、纸浆;深色装饰原纸原料配方为:煅烧高岭土、二氧化钛、氧化铁黄、氧化铁红、纸浆。本发明采用的煅烧高岭土是一种多孔无定型的微粒结构,容重较二氧化钛小,因此配用煅烧高岭土的装饰原纸,松厚度、透气度得到明显改善;纸张渗透性,浸胶性能明显改善,提高了印刷适应性;减少了二氧化钛的用量,降低了生产成本。
Description
技术领域
本发明属于造纸技术领域。
背景技术
装饰原纸是造纸业的特种产品之一,主要用于加工制造各种家俱板材、强化木地板、防火板材等装饰材料,优良的装饰原纸,应该具有良好的遮盖性能、吸收性能,对于印刷类装饰原纸还应具备良好的印刷适应性能。
装饰原纸(又称钛白纸)大量使用贵重化工原料二氧化钛(俗称钛白粉),用量约占装饰原纸重量的30-40%,因此其制造成本相对较高。并且二氧化钛容重较大,制约了纸张松厚性能和吸收性能的提高。
发明内容
本发明的目的是提供一种提高装饰原纸综合性能的方法,解决现有技术成本高、纸张松厚度差及吸收性差等问题。
本发明解决其技术问题所采用的技术方案是增加煅烧高岭土,降低二氧化钛的比例,具体配方配比为:
1、白色装饰原纸原料配方及重量百分比:煅烧高岭土10-20%、二氧化钛20-25%、纸浆60-70%。
2、浅色装饰原纸原料配方及重量百分比:煅烧高岭土8-17%、二氧化钛17-22%、氧化铁黄8-12%、氧化铁红1.2-1.5%、纸浆55-65%。
3、深色装饰原纸原料配方及重量百分比:煅烧高岭土10-15%、二氧化钛4-6%、氧化铁黄10-15%、氧化铁红10-15%、纸浆55-65%。
采用本发明的积极效果是:
1、由于煅烧高岭土是一种多孔无定型的微粒结构,容重较二氧化钛小,因此配用煅烧高岭土的装饰原纸,松厚度、透气度得到明显改善;
2、纸张渗透性能好,浸胶性能明显改善,提高了印刷适应性;
3、减少了二氧化钛的用量,降低了生产成本。
具体实施方式
实施例1
以制造白色装饰原纸为例,增加煅烧高岭土,降低二氧化钛的比例,原料具体重量百分比为:煅烧高岭土比例:12%;二氧化钛比例:23%;纸浆比例:65%。
实施例2
以制造浅色(浅黄色、浅棕色)装饰原纸为例,增加煅烧高岭土,降低二氧化钛的比例,原料具体重量百分比为:煅烧高岭土比例:12%;二氧化钛比例:18%;氧化铁黄比例:10%;氧化铁红比例:1.3%。纸浆比例:58.7%。
实施例3
以制造深色(棕红色、深棕色)装饰原纸为例,增加煅烧高岭土,降低二氧化钛的比例,原料具体重量百分比为:
煅烧高岭土比例:14%;二氧化钛比例:5.5%;氧化铁黄比例:10%;氧化铁红比例:14%;纸浆比例:56.5%。
本发明生产工艺与现有技术相同,通过调整原料比例,可制造出若干颜色的系列产品。
Claims (1)
1.一种提高装饰原纸综合性能的方法,其特征是增加煅烧高岭土,降低二氧化钛的比例,白色装饰原纸原料配方及重量百分比为:煅烧高岭土10-20%、二氧化钛20-25%纸浆60-70%;浅色装饰原纸原料配方及重量百分比为:煅烧高岭土8-17%、二氧化钛17-22%氧化铁黄8-12%、氧化铁红1.2-1.5%、纸浆55-65%;深色装饰原纸原料配方及重量百分比为:煅烧高岭土10-15%、二氧化钛4-6%、氧化铁黄10-15%、氧化铁红10-15%、纸浆55-65%。