CN102211411A - Method for repairing broken belt with large inclination angle - Google Patents
Method for repairing broken belt with large inclination angle Download PDFInfo
- Publication number
- CN102211411A CN102211411A CN2011100513653A CN201110051365A CN102211411A CN 102211411 A CN102211411 A CN 102211411A CN 2011100513653 A CN2011100513653 A CN 2011100513653A CN 201110051365 A CN201110051365 A CN 201110051365A CN 102211411 A CN102211411 A CN 102211411A
- Authority
- CN
- China
- Prior art keywords
- belt
- sides
- fracture
- high angle
- adhesion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a method for repairing a broken belt, which is in particular fit for repairing the broken belt with a large inclination angle. The method comprises the following steps: 1) cleaning: using a cleaning agent to clean a reverse side of a broken part of the belt, positive and negative sides of an adhesion ribbon and one sides of front and back edge-pressing ribbons; 2) coating an adhesion agent on the reverse side of the broken part of the belt, covering the adhesion ribbon on the reverse side of the broken part, tamping the belt by using a mallet, evicting air therebetween, thereby thoroughly adhering the belt; 3) respectively coating the adhesion agent on the cleaned sides of the front and back edge-pressing ribbons, respectively adhering the front and back edge-pressing ribbons to the front and back sides of the adhesion ribbon, tamping the belt by using the mallet, and evicting air therebetween, thereby thoroughly adhering; respectively fastening 2-5 rows of hobnails at left and right ends of the adhesion ribbon and firmly binding the belt with the adhesion ribbon; and 5) stapling buckles on front and back sides of the belt.
Description
Technical field
The present invention relates to a kind of belt fracture restorative procedure, be particularly suitable for the reparation of high angle belt conveyer fracture.
Background technology
The various auxiliary materials of steel-making all are the feed bins of transporting to the converter top by high angle belt conveyer.High angle belt conveyer can continuously provide the auxiliary material of various needs for converter, and is difficult for that there was a mechanical failure.Shortcoming is that the interface of belt ftractures easily.In order to overcome this defective, attempted a lot of methods, such as, at the additional again one deck offset plate of interface, sulfuration at high temperature was through 8 hours curing.After installing and using, because belt is stressed bigger, just fracture then and there always.
Summary of the invention
In order to overcome the shortcoming of prior art, the invention provides a kind of high angle belt conveyer fracture restorative procedure, its method is simple, long service life.
The present invention includes following steps: (1), cleaning: reverse side, adherent zone positive and negative and the forward and backward flanging band one side at belt cracking place are cleaned up with cleaning agent; (2), on the reverse side at belt cracking place applying adhesive, adherent zone is covered up, pound belt with mallet, the air in the middle of driving out of, make belt bonding thoroughly; (3), on the face that forward and backward flanging band cleans up applying adhesive respectively, forward and backward flanging band is sticked to the both sides, front and back of former belt respectively, pound belt with mallet, the air in the middle of driving out of makes it bonding thoroughly; (4), pound 2-5 row tack respectively at the two ends, the left and right sides of adherent zone, belt is ordered firmly with adherent zone is in the same place; (5), both sides nail on belt fastener before and after belt.
Described adherent zone is the offset plate of inner band steel wire.
The cleaning agent of described step (1) is a 120# gasoline.
The adhesive of described step (2) is belt BD958.
The spacing of described step (5) belt fastener is 300mm.
The inventive method is simple, long service life.
Description of drawings
The present invention is further described below in conjunction with drawings and Examples.
Accompanying drawing is a schematic diagram of the present invention.
The specific embodiment
1., clean the present invention includes following steps:: reverse side, adherent zone 6 one sides and forward and backward flanging band 4,5 one sides at belt 1 cracking place are cleaned up with 120# gasoline; 2., on the reverse side at belt 1 cracking place the coating belt use the BD958 adhesive, adherent zone is covered up, pound belt with mallet, the air in the middle of driving out of, make belt bonding thoroughly; 3., on the face that forward and backward flanging band 4,5 cleans up, apply belt BD958 adhesive respectively, forward and backward flanging band 4,5 is sticked to the both sides, front and back of belt 1 respectively, pound belt with mallet, the air in the middle of driving out of makes it bonding thoroughly; 4., pound 3 row's tacks 2 respectively at the two ends, the left and right sides of adherent zone 6, belt 1 is ordered firmly with adherent zone 6 is in the same place; 5., misplacing respectively in both sides, belt 1 front and back nails on belt fastener 3, the spacing of belt fastener 3 is 300mm.
The width dimensions of described belt 1 is 1000mm.Described adherent zone 6 is of a size of 1000 * 3000mm.Described forward and backward flanging band 4,5 is of a size of 150 * 3000mm.
Claims (5)
1. a high angle belt conveyer fracture restorative procedure is characterized in that: comprise the steps: 1., clean: reverse side, adherent zone (6) one side and forward and backward flanging band (4, the 5) one side at belt (1) cracking place are cleaned up with cleaning agent; 2., on the reverse side at belt (1) cracking place applying adhesive, adherent zone (6) is covered, pound belt with mallet, the air in the middle of driving out of, make belt bonding thoroughly; 3., on the face that forward and backward flanging band (4,5) cleans up applying adhesive respectively, forward and backward flanging band (4,5) is sticked to the both sides, front and back of belt (1) respectively, pound belt with mallet, the air in the middle of driving out of makes it bonding thoroughly; 4., pound 2-5 row tack (2) respectively at the two ends, the left and right sides of adherent zone (6), belt (1) and adherent zone (6) are ordered together firmly; 5., both sides nail on belt fastener (3) before and after belt (1).
2. high angle belt conveyer fracture restorative procedure according to claim 1 is characterized in that: described adherent zone (6) is the offset plate of inner band steel wire.
3. high angle belt conveyer fracture restorative procedure according to claim 1, it is characterized in that: the cleaning agent of described step (1) is a 120# gasoline.
4. high angle belt conveyer fracture restorative procedure according to claim 1, it is characterized in that: the adhesive of described step (2) is belt BD958.
5. high angle belt conveyer fracture restorative procedure according to claim 1, it is characterized in that: the spacing of described step (5) belt fastener (3) is 300mm.