CN102154819A - Curly hair moisturizing finishing agent for wig and preparation method thereof - Google Patents
Curly hair moisturizing finishing agent for wig and preparation method thereof Download PDFInfo
- Publication number
- CN102154819A CN102154819A CN 201010541091 CN201010541091A CN102154819A CN 102154819 A CN102154819 A CN 102154819A CN 201010541091 CN201010541091 CN 201010541091 CN 201010541091 A CN201010541091 A CN 201010541091A CN 102154819 A CN102154819 A CN 102154819A
- Authority
- CN
- China
- Prior art keywords
- minutes
- gram
- add
- stirred
- parts
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention relates to a curly hair moisturizing finishing agent for wig and a preparation method thereof. The finishing agent is prepared from the following raw materials in part by weight by compatible synthesis: 10 to 18 parts of glycerin, 1 to 4 parts of sorbitol, 5 to 8 parts of peregal O-15, 15 to 20 parts of efficient penetrating agent, 3 to 10 parts of octadecane trimethyl ammonia chloride, and 40 to 66 parts of deionized water. By using thermostatic stirring, the raw material components are completely reacted more easily, and the generated product is more stable; and the particle diameter of emulsion is smaller by homogenizing and emulsifying, the whole emulsion is uniform and is not demixed, and the whole synthesis process is simpler.
Description
Technical field
The invention belongs to chemical technology, the mutual interleaving techniques of biotechnology field, be specifically related to a kind of wig curly hair wet keeping finishing agent and preparation method thereof.
Background technology
The finishing auxiliaries that present hair products are used is based on the amido silicon oil finishing agent, and there is following defective in it: (1), typing curvature duration are short, and elasticity is relatively poor, and (2), feel are bad, and be relatively drier, greasy sometimes, (3), large usage quantity, cost height.
Summary of the invention
The objective of the invention is to overcome above-mentioned the deficiencies in the prior art and provide that a kind of good hand touch, typing curvature effect are lasting, good springiness and nontoxic, non-stimulated, the simple wig of manufacture craft be with curly hair wet keeping finishing agent and preparation method thereof.
The object of the present invention is achieved like this:
A kind of wig curly hair wet keeping finishing agent is characterized in that: be fused into through compatibility according to parts by weight by following raw materials and make: 10~18 parts of glycerol, 1~4 part of sorbierite, paregal O-15 5~8 part, 15~20 parts of high-efficient penetrants, 3~10 parts of octadecane agent trimethyl sal-ammoniacs, 40~66 parts of deionized waters.
Described deionization hardness of water≤0.03 milli rubs/liter.
A kind of above-mentioned wig preparation method of curly hair wet keeping finishing agent, it is characterized in that: carry out: in deionized water, slowly add glycerol according to following steps, stirred 15 minutes, after leaving standstill 20 minutes, add octadecane agent trimethyl sal-ammoniac, stirred 30 minutes, after 20 minutes, add paregal O-15 and sorbierite, stirred 30 minutes, add high-efficient penetrant then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, cool to room temperature, after leaving standstill 20 minutes, carried out emulsifying 45 minutes, leave standstill and got final product in 30 minutes.
The curly hair wet keeping finishing agent is adorned with blue thick PVC Plastic Drum sealing, and shady and cool place preserves.
The present invention has following advantage: utilize constant temperature to stir, raw material components is easier to react completely, and product is more stable, emulsifying makes particle size of emulsion littler, whole emulsion is evenly not stratified, whole synthesis technique is fairly simple, can reach that good hand touch, typing curvature effect are lasting, good springiness and nontoxic, non-stimulated advantage, and its technical indicator and data are: good hand touch is meant that the MIU value is 0.256; The typing curvature is meant that lastingly G/ (mN.m) value is 0.0063; Good springiness is meant that the L/m value is 0.0350.
The specific embodiment
A kind of wig curly hair wet keeping finishing agent is characterized in that: be fused into through compatibility according to parts by weight by following raw materials and make: 10~18 parts of glycerol, 1~4 part of sorbierite, paregal O-15 5~8 part, 15~20 parts of high-efficient penetrants, 3~10 parts of octadecane agent trimethyl sal-ammoniacs, 40~66 parts of deionized waters.Described deionization hardness of water≤0.03 milli rubs/liter.
A kind of above-mentioned wig preparation method of curly hair wet keeping finishing agent, it is characterized in that: carry out: in deionized water, slowly add glycerol according to following steps, stirred 15 minutes, after leaving standstill 20 minutes, add octadecane agent trimethyl sal-ammoniac, stirred 30 minutes, after 20 minutes, add paregal O-15 and sorbierite, stirred 30 minutes, add high-efficient penetrant then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, cool to room temperature, after leaving standstill 20 minutes, carried out emulsifying 45 minutes, leave standstill and got final product in 30 minutes.
Embodiment 1: a kind of wig curly hair wet keeping finishing agent is fused into through compatibility according to the weight in grams number by following raw materials and makes: glycerol 10 grams, sorbierite 1 gram, paregal O-15 5 gram, high-efficient penetrant 15 grams, octadecane agent trimethyl sal-ammoniac 3 grams, deionized water 66 grams.
Slowly add 10 gram glycerol in the deionized waters at 66 grams, stirred 15 minutes, leave standstill 20 minutes after, add 3 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, wait 20 minutes afterwards after, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, add 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, and cooled to room temperature, leave standstill 20 minutes after, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes.The curly hair wet keeping finishing agent is adorned with blue thick PVC Plastic Drum sealing, and shady and cool place preserves.
Embodiment 2: a kind of wig curly hair wet keeping finishing agent is fused into through compatibility according to the weight in grams number by following raw materials and makes: glycerol 18 grams, sorbierite 1 gram, paregal O-15 5 gram, high-efficient penetrant 15 grams, octadecane agent trimethyl sal-ammoniac 3 grams, deionized water 40 grams.
Slowly add 18 gram glycerol in the deionized waters at 40 grams, stirred 15 minutes, leave standstill 20 minutes after, add 3 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, wait 20 minutes afterwards after, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, add 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, and cooled to room temperature, leave standstill 20 minutes after, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes.The curly hair wet keeping finishing agent is adorned with blue thick PVC Plastic Drum sealing, and shady and cool place preserves.
Embodiment 3: a kind of wig curly hair wet keeping finishing agent is fused into through compatibility according to the weight in grams number by following raw materials and makes: glycerol 10 grams, sorbierite 4 grams, paregal O-15 5 gram, high-efficient penetrant 15 grams, octadecane agent trimethyl sal-ammoniac 3 grams, deionized water 40 grams.
Slowly add 10 gram glycerol in the deionized waters at 40 grams, stirred 15 minutes, leave standstill 20 minutes after, add 3 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, wait 20 minutes afterwards after, add 5 gram paregal Os-15 and 4 gram sorbierites, stirred 30 minutes, add 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, and cooled to room temperature, leave standstill 20 minutes after, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes.The curly hair wet keeping finishing agent is adorned with blue thick PVC Plastic Drum sealing, and shady and cool place preserves.
Embodiment 4: a kind of wig curly hair wet keeping finishing agent is fused into through compatibility according to the weight in grams number by following raw materials and makes: glycerol 10 grams, sorbierite 1 gram, paregal O-15 8 gram, high-efficient penetrant 15 grams, octadecane agent trimethyl sal-ammoniac 3 grams, deionized water 40 grams.
Slowly add 10 gram glycerol in the deionized waters at 40 grams, stirred 15 minutes, leave standstill 20 minutes after, add 3 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, wait 20 minutes afterwards after, add 8 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, add 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, and cooled to room temperature, leave standstill 20 minutes after, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes.The curly hair wet keeping finishing agent is adorned with blue thick PVC Plastic Drum sealing, and shady and cool place preserves.
Embodiment 5: a kind of wig curly hair wet keeping finishing agent is fused into through compatibility according to the weight in grams number by following raw materials and makes: glycerol 10 grams, sorbierite 1 gram, paregal O-15 5 gram, high-efficient penetrant 20 grams, octadecane agent trimethyl sal-ammoniac 3 grams, deionized water 40 grams.
Slowly add 10 gram glycerol in the deionized waters at 40 grams, stirred 15 minutes, leave standstill 20 minutes after, add 3 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, wait 20 minutes afterwards after, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, add 20 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, and cooled to room temperature, leave standstill 20 minutes after, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes.The curly hair wet keeping finishing agent is adorned with blue thick PVC Plastic Drum sealing, and shady and cool place preserves.
Embodiment 6: a kind of wig curly hair wet keeping finishing agent is fused into through compatibility according to the weight in grams number by following raw materials and makes: glycerol 10 grams, sorbierite 1 gram, paregal O-15 5 gram, high-efficient penetrant 15 grams, octadecane agent trimethyl sal-ammoniac 10 grams, deionized water 40 grams.
Slowly add 10 gram glycerol in the deionized waters at 40 grams, stirred 15 minutes, leave standstill 20 minutes after, add 10 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, wait 20 minutes afterwards after, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, add 20 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, and cooled to room temperature, leave standstill 20 minutes after, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes.The curly hair wet keeping finishing agent is adorned with blue thick PVC Plastic Drum sealing, and shady and cool place preserves.
Embodiment 7: a kind of wig curly hair wet keeping finishing agent is fused into through compatibility according to the weight in grams number by following raw materials and makes: glycerol 10 grams, sorbierite 1 gram, paregal O-15 5 gram, high-efficient penetrant 15 grams, octadecane agent trimethyl sal-ammoniac 3 grams, deionized water 40 grams.
Slowly add 10 gram glycerol in the deionized waters at 40 grams, stirred 15 minutes, leave standstill 20 minutes after, add 3 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, wait 20 minutes afterwards after, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, add 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, and cooled to room temperature, leave standstill 20 minutes after, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes.The curly hair wet keeping finishing agent is adorned with blue thick PVC Plastic Drum sealing, and shady and cool place preserves.
Embodiment 8: a kind of wig curly hair wet keeping finishing agent is fused into through compatibility according to the weight in grams number by following raw materials and makes: glycerol 18 grams, sorbierite 4 grams, paregal O-15 8 gram, high-efficient penetrant 20 grams, octadecane agent trimethyl sal-ammoniac 10 grams, deionized water 66 grams.
Slowly add 18 gram glycerol in the deionized waters at 66 grams, stirred 15 minutes, leave standstill 20 minutes after, add 10 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, wait 20 minutes afterwards after, add 8 gram paregal Os-15 and 4 gram sorbierites, stirred 30 minutes, add 20 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, and cooled to room temperature, leave standstill 20 minutes after, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes.The curly hair wet keeping finishing agent is adorned with blue thick PVC Plastic Drum sealing, and shady and cool place preserves.
Embodiment 9: a kind of wig curly hair wet keeping finishing agent is fused into through compatibility according to the weight in grams number by following raw materials and makes: glycerol 15 grams, sorbierite 2 grams, paregal O-15 7 gram, high-efficient penetrant 18 grams, octadecane agent trimethyl sal-ammoniac 8 grams, deionized water 50 grams.
Slowly add 15 gram glycerol in the deionized waters at 50 grams, stirred 15 minutes, leave standstill 20 minutes after, add 8 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, wait 20 minutes afterwards after, add 7 gram paregal Os-15 and 4 gram sorbierites, stirred 30 minutes, add 18 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, and cooled to room temperature, leave standstill 20 minutes after, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes.The curly hair wet keeping finishing agent is adorned with blue thick PVC Plastic Drum sealing, and shady and cool place preserves.
Embodiment 10: slowly add 10 gram glycerol in 65 gram deionized waters, stirred 15 minutes, after leaving standstill 20 minutes, add 4 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, after 20 minutes, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, and added 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, cool to room temperature, after leaving standstill 20 minutes, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes. with blue thick PVC Plastic Drum sealing dress, shady and cool place preserves with the curly hair wet keeping finishing agent.
Embodiment 11: slowly add 10 gram glycerol in 66 gram deionized waters, stirred 15 minutes, after leaving standstill 20 minutes, add 3 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, after 20 minutes, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, and added 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, cool to room temperature, after leaving standstill 20 minutes, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes. with blue thick PVC Plastic Drum sealing dress, shady and cool place preserves with the curly hair wet keeping finishing agent.
Embodiment 12: slowly add 10 gram glycerol in 64 gram deionized waters, stirred 15 minutes, after leaving standstill 20 minutes, add 5 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, after 20 minutes, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, and added 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, cool to room temperature, after leaving standstill 20 minutes, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes. with blue thick PVC Plastic Drum sealing dress, shady and cool place preserves with the curly hair wet keeping finishing agent.
Embodiment 13: slowly add 10 gram glycerol in 63 gram deionized waters, stirred 15 minutes, after leaving standstill 20 minutes, add 6 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, after 20 minutes, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, and added 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, cool to room temperature, after leaving standstill 20 minutes, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes. with blue thick PVC Plastic Drum sealing dress, shady and cool place preserves with the curly hair wet keeping finishing agent.
Embodiment 14: slowly add 10 gram glycerol in 62 gram deionized waters, stirred 15 minutes, after leaving standstill 20 minutes, add 7 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, after 20 minutes, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, and added 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, cool to room temperature, after leaving standstill 20 minutes, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes. with blue thick PVC Plastic Drum sealing dress, shady and cool place preserves with the curly hair wet keeping finishing agent.
Embodiment 15: slowly add 10 gram glycerol in 61 gram deionized waters, stirred 15 minutes, after leaving standstill 20 minutes, add 8 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, after 20 minutes, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, and added 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, cool to room temperature, after leaving standstill 20 minutes, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes. with blue thick PVC Plastic Drum sealing dress, shady and cool place preserves with the curly hair wet keeping finishing agent.
Embodiment 16: slowly add 10 gram glycerol in 60 gram deionized waters, stirred 15 minutes, after leaving standstill 20 minutes, add 9 gram octadecane agent trimethyl sal-ammoniacs, stirred 30 minutes, after 20 minutes, add 5 gram paregal Os-15 and 1 gram sorbierite, stirred 30 minutes, and added 15 gram high-efficient penetrants then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, cool to room temperature, after leaving standstill 20 minutes, carried out emulsifying 45 minutes, and left standstill and got final product in 30 minutes. with blue thick PVC Plastic Drum sealing dress, shady and cool place preserves with the curly hair wet keeping finishing agent.
Claims (3)
1. wig curly hair wet keeping finishing agent is characterized in that: be fused into through compatibility according to parts by weight by following raw materials and make: 10~18 parts of glycerol, 1~4 part of sorbierite, paregal O-15 5~8 part, 15~20 parts of high-efficient penetrants, 3~10 parts of octadecane agent trimethyl sal-ammoniacs, 40~66 parts of deionized waters.
2. wig curly hair wet keeping finishing agent according to claim 1 is characterized in that: described deionization hardness of water≤0.03 milli rubs/liter.
3. a wig as claimed in claim 1 is with the preparation method of curly hair wet keeping finishing agent, it is characterized in that: carry out: in deionized water, slowly add glycerol according to following steps, stirred 15 minutes, after leaving standstill 20 minutes, add octadecane agent trimethyl sal-ammoniac, stirred 30 minutes, after 20 minutes, add paregal O-15 and sorbierite, stirred 30 minutes, add high-efficient penetrant then, heat up and stir, when temperature reaches 50 ℃, keep constant temperature, continue to stir 30 minutes, cool to room temperature, after leaving standstill 20 minutes, carried out emulsifying 45 minutes, leave standstill and got final product in 30 minutes.