[go: up one dir, main page]

CN104826385A - 一种新型环保改性活性炭过滤材料及其制备方法 - Google Patents

一种新型环保改性活性炭过滤材料及其制备方法 Download PDF

Info

Publication number
CN104826385A
CN104826385A CN201510212479.XA CN201510212479A CN104826385A CN 104826385 A CN104826385 A CN 104826385A CN 201510212479 A CN201510212479 A CN 201510212479A CN 104826385 A CN104826385 A CN 104826385A
Authority
CN
China
Prior art keywords
parts
powder
active carbon
novel environment
hour
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510212479.XA
Other languages
English (en)
Inventor
成正平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Tian Cheng Environmental Protection Machinery Co Ltd
Original Assignee
Anhui Tian Cheng Environmental Protection Machinery Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Tian Cheng Environmental Protection Machinery Co Ltd filed Critical Anhui Tian Cheng Environmental Protection Machinery Co Ltd
Priority to CN201510212479.XA priority Critical patent/CN104826385A/zh
Publication of CN104826385A publication Critical patent/CN104826385A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种新型环保改性活性炭过滤材料,其特征在于,由下列重量份的原料制备制成:木质活性炭134-150、蓖麻酸1.5-2.5、松叶油2-3、氯化铜5-7、亚硒酸钠0.4-0.7、正癸酸3-5、甘氨酸1-2、山梨酸钠0.5-1、乳酸3-4、沸石分子筛8-11、铝粉7-9、吸附助剂4-6、水适量;本发明通过添加铝粉、沸石分子筛等与活性炭一同经过处理,可以有效去除多种挥发性有害气体;添加吸附助剂,具有多种孔道结构和大的比表面积,能够提高吸附效率;本发明配方科学合理,生产过程无有毒有害物质生成,制成的过滤材料工艺简单,成本低,吸附过滤效果,用于制作空调过滤网等。

Description

一种新型环保改性活性炭过滤材料及其制备方法
技术领域
本发明涉及一种过滤材料及其制备方法,特别是一种新型环保改性活性炭过滤材料及其制备方法。
背景技术
过滤材料用途极为广泛,主要应用于涂料、油墨、染料、塑料、制药、电镀、饮料、化妆品、橡胶、印刷、电子管生产、线路板生产、垃圾焚烧、化工生产等各领域内。最常见的有过滤材料用于空气调节系统,现在环境大气污染十分严重,雾霾天气给人们带来了极大的危害,空气吸附过滤材料能将空气的各种有害颗粒物,如PM2.5吸附,防止进入人们的生活或工作环境,减少人体肺部对颗粒物等有害物质的吸入,提高人们的生活质量,减少疾病的发生。现有过滤材料主要有蜂窝陶瓷、滤纸、活性炭、钢丝网等。活性炭又称活性炭黑具有矿晶分子结构的颗粒,其孔多,孔隙大,呈晶体排列,针对车内甲醛、苯系、氨、TVOC、异味、细菌螨虫等有害物质的消毒净化功能尤为显著,同时释放氧离子,可循环使用,无二次污染。
发明内容
本发明的目的是提供一种新型环保改性活性炭过滤材料及其制备方法。
为了实现本发明的目的,本发明通过以下方案实施:
一种新型环保改性活性炭过滤材料,由下列重量份的原料制备制成:木质活性炭134-150、蓖麻酸1.5-2.5、松叶油2-3、氯化铜5-7、亚硒酸钠0.4-0.7、正癸酸3-5、甘氨酸1-2、山梨酸钠0.5-1、乳酸3-4、沸石分子筛8-11、铝粉7-9、吸附助剂4-6、水适量;
所述吸附助剂由以下重量份的原料制成:微粉硅胶2-4、碎木屑10-13、纳米硅藻土13-16、氧化镁2-3、铁矿尾渣1-2、生石膏1.5-2.5、竹纤维 0.5-0.8;制备方法是将碎木屑在100℃-120℃条件下干燥1-1.5小时,粉碎成40-60目粉末,然后加入适量水与除竹纤维之外的其余剩余成分搅拌均匀,形成泥状物,然后放入400℃-500℃的炭化炉中炭化2-3小时,取出冷却后粉碎成80-100目粉末,加入竹纤维以及纯水研磨1-2小时,最后喷雾干燥即得。
本发明所述一种新型环保改性活性炭过滤材料,由以下具体步骤制成:
(1)将氯化铜、亚硒酸钠、沸石分子筛、铝粉中加入适量的水,不断搅拌制成浆料,然后加入蓖麻酸、松叶油、乳酸,加热至45℃-60℃,保温并不断搅拌1.5-2小时,得到混合浆料待用;
(2)将木质活性炭粉碎与混合浆料混合均匀,置于马弗炉中在350℃~450℃下,活化60~90分钟,冷却后粉碎成100-120目粉末;
(3)将粉末中加入其余剩余成分,混合搅拌均匀即得过滤材料。
本发明的有益效果是:本发明通过添加铝粉、沸石分子筛等与活性炭一同经过处理,可以有效去除多种挥发性有害气体;添加吸附助剂,具有多种孔道结构和大的比表面积,能够提高吸附效率;本发明配方科学合理,生产过程无有毒有害物质生成,制成的过滤材料工艺简单,成本低,吸附过滤效果,用于制作空调过滤网等。
具体实施方案
下面通过具体实例对本发明进行详细说明。
一种新型环保改性活性炭过滤材料,由下列重量份(公斤)的原料制备制成:木质活性炭134、蓖麻酸1.5、松叶油2、氯化铜5、亚硒酸钠0.4、正癸酸3、甘氨酸1、山梨酸钠0.5、乳酸3、沸石分子筛8、铝粉7、吸附助剂4、水适量;
所述吸附助剂由以下重量份(公斤)的原料制成:微粉硅胶2、碎木屑10、纳米硅藻土13、氧化镁2、铁矿尾渣1、生石膏1.5、竹纤维 0.5;制备方法是将碎木屑在100℃-120℃条件下干燥1-1.5小时,粉碎成40-60目粉末,然后加入适量水与除竹纤维之外的其余剩余成分搅拌均匀,形成泥状物,然后放入400℃-500℃的炭化炉中炭化2-3小时,取出冷却后粉碎成80-100目粉末,加入竹纤维以及纯水研磨1-2小时,最后喷雾干燥即得。
本发明所述一种新型环保改性活性炭过滤材料,由以下具体步骤制成:
(1)将氯化铜、亚硒酸钠、沸石分子筛、铝粉中加入适量的水,不断搅拌制成浆料,然后加入蓖麻酸、松叶油、乳酸,加热至45℃-60℃,保温并不断搅拌1.5-2小时,得到混合浆料待用;
(2)将木质活性炭粉碎与混合浆料混合均匀,置于马弗炉中在350℃~450℃下,活化60~90分钟,冷却后粉碎成100-120目粉末;
(3)将粉末中加入其余剩余成分,混合搅拌均匀即得过滤材料。
利用本发明过滤材料制得的滤网进行性能测试,主要技术参数为:废气净化处理装置的技术指标为:捕获的粉尘颗粒最小粒径范围0.5-10μm;捕集微尘效率≥99%;经过4小时的作用,甲醛浓度下降84.9%。

Claims (2)

1.一种新型环保改性活性炭过滤材料,其特征在于,由下列重量份的原料制备制成:木质活性炭134-150、蓖麻酸1.5-2.5、松叶油2-3、氯化铜5-7、亚硒酸钠0.4-0.7、正癸酸3-5、甘氨酸1-2、山梨酸钠0.5-1、乳酸3-4、沸石分子筛8-11、铝粉7-9、吸附助剂4-6、水适量;
所述吸附助剂由以下重量份的原料制成:微粉硅胶2-4、碎木屑10-13、纳米硅藻土13-16、氧化镁2-3、铁矿尾渣1-2、生石膏1.5-2.5、竹纤维 0.5-0.8;制备方法是将碎木屑在100℃-120℃条件下干燥1-1.5小时,粉碎成40-60目粉末,然后加入适量水与除竹纤维之外的其余剩余成分搅拌均匀,形成泥状物,然后放入400℃-500℃的炭化炉中炭化2-3小时,取出冷却后粉碎成80-100目粉末,加入竹纤维以及纯水研磨1-2小时,最后喷雾干燥即得。
2.根据权利要求1所述一种新型环保改性活性炭过滤材料,其特征在于,由以下具体步骤制成:
(1)将氯化铜、亚硒酸钠、沸石分子筛、铝粉中加入适量的水,不断搅拌制成浆料,然后加入蓖麻酸、松叶油、乳酸,加热至45℃-60℃,保温并不断搅拌1.5-2小时,得到混合浆料待用;
(2)将木质活性炭粉碎与混合浆料混合均匀,置于马弗炉中在350℃~450℃下,活化60~90分钟,冷却后粉碎成100-120目粉末;
(3)将粉末中加入其余剩余成分,混合搅拌均匀即得过滤材料。
CN201510212479.XA 2015-04-29 2015-04-29 一种新型环保改性活性炭过滤材料及其制备方法 Pending CN104826385A (zh)