[go: up one dir, main page]

CN104397909B - 多组分易护理面料的生产工艺 - Google Patents

多组分易护理面料的生产工艺 Download PDF

Info

Publication number
CN104397909B
CN104397909B CN201410808319.7A CN201410808319A CN104397909B CN 104397909 B CN104397909 B CN 104397909B CN 201410808319 A CN201410808319 A CN 201410808319A CN 104397909 B CN104397909 B CN 104397909B
Authority
CN
China
Prior art keywords
polyester fiber
speed
yarn
australia
silkworm silk
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201410808319.7A
Other languages
English (en)
Other versions
CN104397909A (zh
Inventor
杨毅方
顾士清
杨丽萍
朱庆燕
薛勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangyin Huanju Textile Co ltd
Original Assignee
Jiangsu Nijiaxiang Group Worsted Textile Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Nijiaxiang Group Worsted Textile Co Ltd filed Critical Jiangsu Nijiaxiang Group Worsted Textile Co Ltd
Priority to CN201410808319.7A priority Critical patent/CN104397909B/zh
Publication of CN104397909A publication Critical patent/CN104397909A/zh
Application granted granted Critical
Publication of CN104397909B publication Critical patent/CN104397909B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种多组分易护理面料的生产工艺,包括:(1)将80支澳毛、1.5D聚酯纤维和蚕丝条染复精梳的步骤;(2)将80支澳毛条、1.5D聚酯纤维条和蚕丝条纺纱的步骤;(3)织造的步骤;(4)后处理的步骤。本发明生产的布料色彩鲜艳、手感爽、弹性足、立体感强、透气性好,同时具有时尚和实用的特点,具有优越的性能,既舒适又富有美感,适于制作男士休闲服饰。

Description

多组分易护理面料的生产工艺
技术领域
本发明涉及一种面料的生产工艺,尤其是涉及一种多组分易护理面料的生产工艺。
背景技术
随着社会经济水平的提高,人们不再一味奔波于忙碌的生活,而开始注意生活质量、享受生活。尤其男士对于休闲服饰的要求也越来越高,现有的用于生产男士休闲服饰的面料均过于干爽,且颜色多呈单一的黑、灰、蓝等深色,商务性较强,既不美观,穿着之后又不够舒适。而且由于过于干爽,用这样的面料做成的服饰还不易护理。
发明内容
本发明为了解决目前男士休闲服饰的面料不够美观,且不易护理的问题,为此提供了一种多组分易护理面料的生产工艺,包括:
(1)将80支澳毛、1.5D聚酯纤维和蚕丝条染复精梳的步骤;
(2)将80支澳毛条、1.5D聚酯纤维条和蚕丝条纺纱的步骤;
(3)织造的步骤;
(4)后处理的步骤;
步骤(1)包括将80支澳毛、1.5D聚酯纤维和蚕丝依次分别松球→染色→复洗→混条→针梳→精梳→针梳→精梳→针梳→制成80支澳毛条、1.5D聚酯纤维条和蚕丝条;
步骤(2)包括将80支澳毛条、1.5D聚酯纤维条和蚕丝条进行混条→头针→二针→三针→四针→粗纱→细纱→自络筒→并线→倍捻→蒸纱→制成规格为92支/2,Z捻捻度为900捻/米的经纱和48支/1,Z捻捻度为1050捻/米的莱卡包芯纱为纬纱;
步骤(3)包括整经→穿综、穿筘→织造→坯检;
步骤(4)包括平煮→烘呢→刷毛→烧毛→平煮→烘呢→定型→中检→熟修→刷毛→剪毛→给湿→高压蒸→罐蒸→烘呢软→中检→罐蒸→成检。
本发明多组分易护理面料的生产工艺,步骤(1)中采用散纤维染色,将80支澳毛、1.5D聚酯纤维和蚕丝分别染色、冲洗,烘干后再和毛。为保证和毛均匀,染色后的处理过程十分重要。车间在染色后尽量洗尽纤维表面浮色和染色的助剂,并通过烘干工序使纤维保持蓬松不粘并,和毛时加入油水和抗静电剂,使纤维表面平滑减少梳理时的摩擦损伤,和毛为至少两次,和好的原料在毛仓内储存24小时来让和毛油水和抗静电剂充分渗透吸收,达到均衡的所需回潮率,为下道梳理成条创造条件。
本发明多组分易护理面料的生产工艺,步骤(2)中头针次数为至少两次,加油水后间隔时间至少为12小时,细纱机上纺制48支/1莱卡包芯纱时控制莱卡的牵伸倍数为2.5倍;
经纱强捻纱,为防止毛纱因捻度过高在倍捻机上生产时产生脆断,倍捻机车速初始时为8000转/分,并逐渐降低至6000转/分;
蒸纱时为防止强捻纱产生小辫子纱,为两次蒸纱,温度90℃,时间1.5小时。
本发明多组分易护理面料的生产工艺,步骤(3)中织造时的线速度为320米/分,倒轴速度为50米/分,纱线张力为3.5公斤,倒轴张力为1公斤;
后梁前后位置105cm,高度-1cm,停经高度-2cm,前后位置56cm,张力200kg,开口时间315度。以确保开口清晰,解决纬弓纱、跳花等疵点;
织机车速初始时为360转/分,并逐渐降低至300转/分。
本发明多组分易护理面料的生产工艺,步骤(4)中烘呢温度为130℃,门幅开158CM,上超喂6%下超喂4%,呢速30米/分;
烧毛呢速90米/分,压力13mbar,一正一反,前后进行两次烧毛,保证成品呢面的光洁度,使产品的特征更能凸显;
定型温度为188℃,门幅开158CM,下机159-160CM,呢速16.5米/分
剪毛时呢速15米/分,4正2反;
烘呢软:温度130℃,门幅开154CM,下机152-153CM,呢速28米/分,3#柔软剂,0.3kg/槽,室温,1浸1轧。
本发明的有益效果是:
本发明将80支澳毛、1.5D聚酯纤维和蚕丝等多组成份混纺,经纱采用强捻纱,纬纱采用加莱卡的弹力纱织造而成,把经纱的干爽与纬纱的弹力特性有效的结合,制成了一种风格独特色彩艳丽的时尚易护理面料。面料色彩鲜艳、手感爽、弹性足、立体感强、透气性好,同时具有时尚和实用的特点,具有优越的性能,既舒适又富有美感,适于制作男士休闲服饰。
具体实施方式
本说明书中公开的所有特征,或公开的所有方法或过程中的步骤,除了互相排斥的特征和/或步骤以外,均可以以任何方式组合。
本说明书中公开的任一特征,除非特别叙述,均可被其他等效或具有类似目的的替代特征加以替换。即,除非特别叙述,每个特征只是一系列等效或类似特征中的一个例子而已。
一种多组分易护理面料的生产工艺,包括:
(1)将80支澳毛、1.5D聚酯纤维和蚕丝条染复精梳的步骤;
(2)将80支澳毛条、1.5D聚酯纤维条和蚕丝条纺纱的步骤;
(3)织造的步骤;
(4)后处理的步骤;
步骤(1)包括将80支澳毛、1.5D聚酯纤维和蚕丝依次分别松球→染色→复洗→混条→针梳→精梳→针梳→精梳→针梳→制成80支澳毛条、1.5D聚酯纤维条和蚕丝条;
步骤(2)包括将80支澳毛条、1.5D聚酯纤维条和蚕丝条进行混条→头针→二针→三针→四针→粗纱→细纱→自络筒→并线→倍捻→蒸纱→制成规格为92支/2,Z捻捻度为900捻/米的经纱和48支/1,Z捻捻度为1050捻/米的莱卡包芯纱为纬纱;
步骤(3)包括整经→穿综、穿筘→织造→坯检;
步骤(4)包括平煮→烘呢→刷毛→烧毛→平煮→烘呢→定型→中检→熟修→刷毛→剪毛→给湿→高压蒸→罐蒸→烘呢软→中检→罐蒸→成检。
其中,步骤(1)中采用散纤维染色,将80支澳毛、1.5D聚酯纤维和蚕丝分别染色、冲洗,烘干后再和毛。为保证和毛均匀,染色后的处理过程十分重要。车间在染色后尽量洗尽纤维表面浮色和染色的助剂,并通过烘干工序使纤维保持蓬松不粘并,和毛时加入油水和抗静电剂,使纤维表面平滑减少梳理时的摩擦损伤,和毛为至少两次,和好的原料在毛仓内储存24小时来让和毛油水和抗静电剂充分渗透吸收,达到均衡的所需回潮率,为下道梳理成条创造条件。
步骤(2)中头针次数为至少两次,加油水后间隔时间至少为12小时,细纱机上纺制48支/1莱卡包芯纱时控制莱卡的牵伸倍数为2.5倍;经纱强捻纱,为防止毛纱因捻度过高在倍捻机上生产时产生脆断,倍捻机车速初始时为8000转/分,并逐渐降低至6000转/分;蒸纱时为防止强捻纱产生小辫子纱,为两次蒸纱,温度90℃,时间1.5小时。
步骤(3)中织造时的线速度为320米/分,倒轴速度为50米/分,纱线张力为3.5公斤,倒轴张力为1公斤;后梁前后位置105cm,高度-1cm,停经高度-2cm,前后位置56cm,张力200kg,开口时间315度。以确保开口清晰,解决纬弓纱、跳花等疵点;织机车速初始时为360转/分,并逐渐降低至300转/分。
步骤(4)中烘呢温度为130℃,门幅开158CM,上超喂6%下超喂4%,呢速30米/分;
烧毛呢速90米/分,压力13mbar,一正一反,前后进行两次烧毛,保证成品呢面的光洁度,使产品的特征更能凸显;
定型温度为188℃,门幅开158CM,下机159-160CM,呢速16.5米/分;
剪毛时呢速15米/分,4正2反;
烘呢软:温度130℃,门幅开154CM,下机152-153CM,呢速28米/分,3#柔软剂,0.3kg/槽,室温,1浸1轧。
本发明并不局限于前述的具体实施方式。本发明扩展到任何在本说明书中披露的新特征或任何新的组合,以及披露的任一新的方法或过程的步骤或任何新的组合。

Claims (3)

1.一种多组分易护理面料的生产工艺,其特征在于,包括:
(1)将80支澳毛、1.5D聚酯纤维和蚕丝条染复精梳的步骤;
(2)将80支澳毛条、1.5D聚酯纤维条和蚕丝条纺纱的步骤;
(3)织造的步骤;
(4)后处理的步骤;
步骤(1)包括将80支澳毛、1.5D聚酯纤维和蚕丝依次分别松球→染色→复洗→混条→针梳→精梳→针梳→精梳→针梳→制成80支澳毛条、1.5D聚酯纤维条和蚕丝条;
步骤(2)包括将80支澳毛条、1.5D聚酯纤维条和蚕丝条进行混条→头针→二针→三针→四针→粗纱→细纱→自络筒→并线→倍捻→蒸纱→制成规格为92支/2,Z捻捻度为900捻/米的经纱和48支/1,Z捻捻度为1050捻/米的莱卡包芯纱为纬纱,该步骤(2)的过程中,头针次数为至少两次,加油水后间隔时间至少为12小时,细纱机上纺制48支/1莱卡包芯纱时控制莱卡的牵伸倍数为2.5倍;倍捻机车速初始时为8000转/分,并逐渐降低至6000转/分,蒸纱为两次蒸纱,温度90℃,时间1.5小时;
步骤(3)包括整经→穿综、穿筘→织造→坯检,该步骤(3)的过程中,织造时的线速度为320米/分,倒轴速度为50米/分,纱线张力为3.5公斤,倒轴张力为1公斤;后梁前后位置105cm,高度-1cm,停经高度-2cm,前后位置56cm,张力200kg,开口时间315度;织机车速初始时为360转/分,并逐渐降低至300转/分;
步骤(4)包括平煮→烘呢→刷毛→烧毛→平煮→烘呢→定型→中检→熟修→刷毛→剪毛→给湿→高压蒸→罐蒸→烘呢软→中检→罐蒸→成检。
2.根据权利要求1所述的多组分易护理面料的生产工艺,其特征在于,步骤(1)中采用散纤维染色,将80支澳毛、1.5D聚酯纤维和蚕丝分别染色、冲洗,烘干后再和毛,和毛时加入油水和抗静电剂,和毛为至少两次,和好的原料在毛仓内储存24小时。
3.根据权利要求1所述的多组分易护理面料的生产工艺,其特征在于,步骤(4)中烘呢温度为130℃,门幅开158CM,上超喂6%下超喂4%,呢速30米/分;
烧毛呢速90米/分,压力13mbar,一正一反,前后进行两次烧毛;
定型温度为188℃,门幅开158CM,下机159-160CM,呢速16.5米/分;
剪毛时呢速15米/分,4正2反;
烘呢软:温度130℃,门幅开154CM,下机152-153CM,呢速28米/分,3#柔软剂,0.3kg/槽,室温下,1浸1轧。
CN201410808319.7A 2014-12-22 2014-12-22 多组分易护理面料的生产工艺 Expired - Fee Related CN104397909B (zh)