MXPA02010119A - Process that improves recovery, degree and kinetic of copper, reducing the consumption of metallic milling means and of the ph modifier reactive during copper concentration by floatation. - Google Patents
Process that improves recovery, degree and kinetic of copper, reducing the consumption of metallic milling means and of the ph modifier reactive during copper concentration by floatation.Info
- Publication number
- MXPA02010119A MXPA02010119A MXPA02010119A MXPA02010119A MX PA02010119 A MXPA02010119 A MX PA02010119A MX PA02010119 A MXPA02010119 A MX PA02010119A MX PA02010119 A MXPA02010119 A MX PA02010119A
- Authority
- MX
- Mexico
- Prior art keywords
- copper
- milling
- kinetic
- reducing
- abs
- Prior art date
Abstract
Herein is provided a process to improve recovery, degree, kinetic and at the same time the consumption reduction of milling metallic means in copper floatation using ammonium bisulphite (ABS). The process comprises the addition of (ABS) to the primary milling feeding water giving enough conditioning time (achievable in a cycle of 6 to 8 minutes in a standard milling circuit, with no conditioning tanks or other additional equipment) for reducing or eliminating the oxygen dissolved in the pulp. Another addition points include the pulp of the cyclones discharge of the milling mill and the cleansing flotation section. The quantity of added (ABS) should be enough to control (reduce) the pyrite floatability as well as for minimizing the oxygen dissolved in the pulp in all the circuit. The process is applicable to a large range of copper sulphurous minerals and also to mixtures of sulphurous and non-sulphurous minerals.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| MXPA02010119 MXPA02010119A (en) | 2002-10-14 | 2002-10-14 | Process that improves recovery, degree and kinetic of copper, reducing the consumption of metallic milling means and of the ph modifier reactive during copper concentration by floatation. |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| MXPA02010119 MXPA02010119A (en) | 2002-10-14 | 2002-10-14 | Process that improves recovery, degree and kinetic of copper, reducing the consumption of metallic milling means and of the ph modifier reactive during copper concentration by floatation. |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| MXPA02010119A true MXPA02010119A (en) | 2004-04-28 |
Family
ID=34075059
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| MXPA02010119 MXPA02010119A (en) | 2002-10-14 | 2002-10-14 | Process that improves recovery, degree and kinetic of copper, reducing the consumption of metallic milling means and of the ph modifier reactive during copper concentration by floatation. |
Country Status (1)
| Country | Link |
|---|---|
| MX (1) | MXPA02010119A (en) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US9885095B2 (en) | 2014-01-31 | 2018-02-06 | Goldcorp Inc. | Process for separation of at least one metal sulfide from a mixed sulfide ore or concentrate |
-
2002
- 2002-10-14 MX MXPA02010119 patent/MXPA02010119A/en active IP Right Grant
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US9885095B2 (en) | 2014-01-31 | 2018-02-06 | Goldcorp Inc. | Process for separation of at least one metal sulfide from a mixed sulfide ore or concentrate |
| US10370739B2 (en) | 2014-01-31 | 2019-08-06 | Goldcorp, Inc. | Stabilization process for an arsenic solution |
| US11124857B2 (en) | 2014-01-31 | 2021-09-21 | Goldcorp Inc. | Process for separation of antimony and arsenic from a leach solution |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN113976307B (en) | Flotation separation method of lead zinc sulfide ore difficult to separate and zinc blende inhibitor thereof | |
| US5110455A (en) | Method for achieving enhanced copper flotation concentrate grade by oxidation and flotation | |
| CN112264197A (en) | Combined inhibitor for high-magnetic pyrite type copper-sulfur ore and beneficiation method thereof | |
| CN111468304A (en) | Composite inhibitor for pyrite and pumice in copper-sulfur ores and flotation separation method thereof | |
| CN111804440A (en) | A method for regulating sulfide ore flotation by dissolved oxygen content in pulp | |
| CN110369122A (en) | A kind of beneficiation method of the high sulfur type gold-copper ore of high efficiente callback | |
| CN117696260A (en) | Combined collector for chalcopyrite in low-copper high-sulfur copper-sulfur ore and application thereof | |
| CN109482352B (en) | A kind of beneficiation method of ferric zinc oxide ore preactivated by sulfuric acid | |
| CN116273485B (en) | Pyrite flotation separation combined inhibitor and application thereof | |
| CN118385028A (en) | Low-alkali asynchronous separation method for copper sulfide ore containing arsenic | |
| CN104941789A (en) | Beneficiation method for molybdenum-sulfur bulk concentrate | |
| CN109550597A (en) | A kind of adjustable copper-cobalt ore method for floating for the treatment of capacity | |
| CN113233426A (en) | Method for recovering sulfur from zinc oxygen pressure leaching high-sulfur slag | |
| CN113856911B (en) | Beneficiation method for high-sulfur copper gold and silver ore | |
| MXPA02010119A (en) | Process that improves recovery, degree and kinetic of copper, reducing the consumption of metallic milling means and of the ph modifier reactive during copper concentration by floatation. | |
| CN107899756B (en) | A method of it being enriched with lead and zinc bulk concentrate from refined gold ore cyaniding tailings and separates | |
| CN112264195B (en) | Cassiterite mineral flotation inhibitor and application thereof | |
| CN108704767B (en) | Combined inhibitor and application thereof in separation of molybdenum-containing and other metal sulfide ores | |
| CN118751411A (en) | Method for recovering lead-zinc mixed concentrate from sulfur concentrate by flotation | |
| RU2134616C1 (en) | Method of flotation of copper-nickel sulfide cuprous ores | |
| CN114950740B (en) | Chalcocite and blue chalcocite combined inhibitor and application thereof | |
| CN115090421A (en) | A method for eliminating copper ions to activate sphalerite and sphalerite flotation | |
| CN104624386B (en) | Copper-lead bulk concentrate flotation separation inhibitor and preparation method and beneficiation method thereof | |
| CN119897222B (en) | Suppressed sphalerite activator and application thereof | |
| CN119565767B (en) | Ion regulating inhibitor for preventing ore mud covering, application thereof and lepidolite ore beneficiation method |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FG | Grant or registration |