Li et al., 2005 - Google Patents
Interfacial reactions between Pb-free solders and metallized substrate surfacesLi et al., 2005
View PDF- Document ID
- 1843876006773816164
- Author
- Li D
- Liu C
- Conway P
- Publication year
- Publication venue
- 2005 6th International Conference on Electronic Packaging Technology
External Links
Snippet
The interfacial reactions and the resultant intermetallics between lead free solders, ie, Sn- 3.8 Ag-0.7 Cu, Sn-3.5 Ag and Sn-0.7 Cu, and substrates with different metallisation, namely, Cu, electroless Ni (EN), immersion Ag on Cu (CuImAg) and electroless Ni immersion gold …
- 229910000679 solder 0 title abstract description 74
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K35/00—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
- B23K35/22—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
- B23K35/24—Selection of soldering or welding materials proper
- B23K35/26—Selection of soldering or welding materials proper with the principal constituent melting at less than 400 degrees C
- B23K35/262—Sn as the principal constituent
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L2924/00—Indexing scheme for arrangements or methods for connecting or disconnecting semiconductor or solid-state bodies as covered by H01L24/00
- H01L2924/01—Chemical elements
- H01L2924/01029—Copper [Cu]
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L2924/00—Indexing scheme for arrangements or methods for connecting or disconnecting semiconductor or solid-state bodies as covered by H01L24/00
- H01L2924/013—Alloys
- H01L2924/0132—Binary Alloys
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L2924/00—Indexing scheme for arrangements or methods for connecting or disconnecting semiconductor or solid-state bodies as covered by H01L24/00
- H01L2924/01—Chemical elements
- H01L2924/01006—Carbon [C]
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L2924/00—Indexing scheme for arrangements or methods for connecting or disconnecting semiconductor or solid-state bodies as covered by H01L24/00
- H01L2924/01—Chemical elements
- H01L2924/0103—Zinc [Zn]
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L24/00—Arrangements for connecting or disconnecting semiconductor or solid-state bodies; Methods or apparatus related thereto
- H01L24/01—Means for bonding being attached to, or being formed on, the surface to be connected, e.g. chip-to-package, die-attach, "first-level" interconnects; Manufacturing methods related thereto
- H01L24/10—Bump connectors ; Manufacturing methods related thereto
- H01L24/11—Manufacturing methods
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Korhonen et al. | Reactions of lead-free solders with CuNi metallizations | |
| KR100902163B1 (en) | Lead-free solder and alloy element joining method to prevent brittle fracture | |
| Kotadia et al. | Reactions of Sn-3.5 Ag-based solders containing Zn and Al additions on Cu and Ni (P) substrates | |
| US8679964B2 (en) | Prevention and control of intermetallic alloy inclusions | |
| KR100718169B1 (en) | Joining method of nickel surface-treated electronic parts and electroless nickel surface-treated electronic parts | |
| Jee et al. | Effects of Zn addition on the drop reliability of Sn–3.5 Ag–xZn/Ni (P) solder joints | |
| Sun et al. | Intermetallic compound formation in Sn-Co-Cu, Sn-Ag-Cu and eutectic Sn-Cu solder joints on electroless Ni (P) immersion Au surface finish after reflow soldering | |
| Sharif et al. | Interfacial reactions on electrolytic Ni and electroless Ni (P) metallization with Sn–In–Ag–Cu solder | |
| Li et al. | Interfacial reactions between Pb-free solders and metallized substrate surfaces | |
| Liu et al. | Effects of Sn-Ag-x leveling layers on the microstructure and mechanical properties of SnBi low-temperature solder joints | |
| Lin et al. | Solid-state interfacial reactions at the solder joints employing Au/Pd/Ni and Au/Ni as the surface finish metallizations | |
| Yoon et al. | Comparison of Interfacial Stability of Pb-Free Solders (Sn—3.5 Ag, Sn—3.5 Ag—0.7 Cu, and Sn—0.7 Cu) on ENIG-Plated Cu During Aging | |
| Zolhafizi et al. | The effect of Bismuth on intermetallics growth between lead-free solders and electroless nickel immersion silver (ENIMAG) surface Finish | |
| Li et al. | The formation and evolution of IMC and its effect on the solder joint properties | |
| Sohn et al. | Effect of intermetallics spalling on the mechanical behavior of electroless Ni (P)/Pb-free solder interconnection | |
| Wang et al. | Effect of Ni (P) thickness of ultrathin ENEPIG on the interfacial reaction and board level reliability of solder joints | |
| Sohn et al. | Study of spalling behavior of intermetallic compounds during the reaction between electroless Ni-P metallization and lead-free solders | |
| Li et al. | Influence of interfacial reaction between molten SnAgCu solder droplet and Au/Ni/Cu pad on IMC evolution | |
| Xia et al. | Effect of Aluminum Concentration on the Interfacial Reactions of Sn-3.0 Ag-x Al Solders with Copper and ENIG Metallizations | |
| Gim et al. | A Study on Combination of ENEPIG Surface Finish and Solder Ball for Solder Joint Reliability | |
| Islam et al. | Interfacial reactions of Cu-containing lead-free solders with Au/NiP metallization | |
| Alam et al. | Reaction kinetics of Pb-Sn and Sn-Ag solder balls with electroless Ni-P/Cu pad during reflow soldering in microelectronic packaging | |
| Yang et al. | Reflow study of Pb-free Sn-3.5 Ag solder with Ni-Sn-P metallization | |
| Li et al. | Interactions between liquid Sn-Bi based solders and contact metals for high temperature applications | |
| Yang et al. | Kinetics of interfacial reaction between Sn-3.0 Ag-0.5 Cu solder and Co-4.0 P or Co-8.0 P metallization |